Construction site test block standard curing chamber
By designing a combination of spray water pipes and heating partitions in the test block standard curing room, and using atomizing nozzles to provide moist heat, the problem of insufficient temperature and humidity in the test block curing environment is solved, electrical short circuits are avoided, and the test block is able to withstand pressure. Strength accuracy and safety.
Patent Information
- Application Number
- CN202420288549.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-07
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2034-02-07
AI Technical Summary
The standard indoor temperature and humidity of the test blocks at the construction site did not meet the requirements, resulting in inaccurate compressive strength of the test blocks, and the heating appliances were prone to short-circuit in humid environments, posing safety risks.
A standard curing room for test blocks is designed that includes an operation room and a maintenance room. The curing room is equipped with a test block placement rack, a water supply pool, a spray water pipe and a heating device. The spray water pipe is equipped with multiple atomizing nozzles to provide There is a heating compartment at the bottom of the pool, and the heating device is installed separately in the compartment. Water pumps and spray pipes are used to provide moist heat through atomizing nozzles. Moisture and heat sensors monitor environmental conditions, and drainage ditches and sedimentation pools are recycled.
It is possible to meet the temperature and humidity conditions for test block maintenance at the construction site, avoid electrical short circuits, save water, and reduce project costs.
Smart Images

Figure CN221793202U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of curing of concrete test blocks and mortar test blocks, and particularly relates to a test block standard curing room at a construction site. Background Art
[0002] As long as there is a construction project, it will involve the concrete pouring construction process and the masonry construction process. Whether it is a public building or a civil building, it will involve the curing of concrete compressive test blocks and masonry mortar compressive test blocks. In the past construction process, there often occurred situations where the storage space for test blocks was small, and when multiple buildings were under construction simultaneously, the storage conditions for a large number of test blocks did not meet the requirements; in addition, in spring or winter, the temperature was relatively low, and the temperature in the standard curing room did not meet the requirements. If electric heaters or air conditioners were used for heating, the electrical appliances were prone to short - circuit in a humid environment, posing a safety hazard.
[0003] Through observation and research, it is found that the standard value of the compressive strength of test blocks cannot truly reflect the strength of the concrete mix. Since the curing environment of the compressive test blocks does not meet the specification requirements, there may even occur situations where the compressive strength does not meet the design requirements of the components, causing a lot of troubles and problems to the project department. Content of the Utility Model
[0004] The purpose of the utility model is to provide a test block standard curing room at a construction site to solve the problems that the temperature and humidity in the standard curing room do not meet the requirements and the heating electrical appliances are prone to short - circuit in a humid environment.
[0005] The technical solution of the utility model is: a test block standard curing room at a construction site, which includes an operation room and a curing room. In the curing room, there are test block placement racks, a water supply pool, a spray water pipe, and a heating device. A water pump is arranged in the water supply pool, the water outlet end of the water pump is connected to the spray water pipe, the spray water pipe is arranged in the top space of the curing room, and a plurality of atomizing nozzles are arranged on the spray water pipe. A heating partition layer is arranged at the bottom of the water supply pool, and the heating device is arranged in the heating partition layer.
[0006] As a further improvement of the utility model, the spray water pipe is arranged in a '丰' - shaped configuration.
[0007] As a further improvement of the utility model, a humidity - heat sensor is arranged in the curing room.
[0008] As a further improvement of the utility model, a sedimentation pool and a drainage ditch are arranged in the curing room. The drainage ditch is arranged around the periphery of the ground of the curing room, one end of the drainage ditch is connected to the sedimentation pool, and the sedimentation pool and the water supply pool are connected through a connecting pipe, and the connecting pipe is located above the sedimentation pool.
[0009] As a further improvement of the utility model, the drainage ditch has a slope, and the sedimentation pool is connected to the low - level end of the drainage ditch.
[0010] As a further improvement of the utility model, the top of the drainage ditch is flush with the ground of the maintenance room, and a drainage ditch grate is provided on the top of the drainage ditch.
[0011] As a further improvement of the utility model, the top of the water supply tank and the top of the sedimentation tank are flush with the ground of the curing room, and the first grate and the second grate are respectively provided on the top of the water supply tank and the top of the sedimentation tank.
[0012] As a further improvement of the utility model, a sleeve is provided outside the connecting pipe, a fixed wing ring is provided outside the sleeve, asbestos cement is filled between the sleeve and the connecting pipe, and both ends of the asbestos cement are sealed by waterproof sealing paste.
[0013] As a further improvement of the utility model, a standard maintenance box and a test tool cabinet are provided in the operating room.
[0014] As a further improvement of the present invention, the operation room and the maintenance room are assembled structures, and the wall panels of the operation room and the maintenance room are composed of double-layer color steel plates, light steel keels and rock wool, and the light steel keels and rock wool are located between the double-layer color steel plates.
[0015] The beneficial effects of the utility model are:
[0016] 1. The standard curing room of the utility model is provided with an operation room and a curing room, which is convenient for the curing of test blocks and meets the storage and curing of test blocks on the construction site. The utility model is provided with a plurality of atomizing nozzles in the curing room, and water is taken through the water pump in the water supply tank for spray humidification. When the temperature in the curing room is low, the water in the water supply tank can be heated by the heating device, so that the curing room is heated by spraying, and the water vapor is used to make the temperature in the curing room meet the standard curing conditions, with good uniformity, which is conducive to the curing of test blocks; the heating device is separately arranged in the heating compartment, separated from the moisture in the curing room, to avoid electrical short circuits and eliminate safety hazards.
[0017] 2. After condensation, the water mist flows into the drainage ditch and then into the sedimentation tank. After sedimentation, it flows back to the water supply tank, which can be recycled and save water.
[0018] 3. The utility model has a simple structure, and the assembled structure can be used repeatedly, thereby reducing the project construction cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the plane structure of the utility model;
[0020] Figure 2 It is a plan layout diagram of the spray water pipe in the utility model;
[0021] Figure 3 yes Figure 1 AA view in;
[0022] Figure 4 yes Figure 1 View B-B therein;
[0023] Figure 5 It is a schematic structural view of the reinforcing angle steel in the present utility model;
[0024] Figure 6 It is a schematic structural view of the casing in the present utility model;
[0025] Figure 7 It is a schematic structural view of the wall panel in the present utility model.
[0026] In the figure: 1 - operation room; 2 - curing room; 3 - test block placement rack; 4 - water supply tank; 5 - sedimentation tank; 6 - spray water pipe; 7 - heating device; 8 - water pump; 9 - drainage ditch; 10 - heating partition; 11 - connecting pipe; 12 - first grid; 13 - second grid; 14 - drainage ditch grid; 15 - reinforcing angle steel; 16 - anchor reinforcement; 17 - standard curing box; 18 - test tool cabinet; 19 - color steel plate; 20 - light steel keel; 21 - rock wool; 22 - first door; 23 - second door; 24 - casing; 25 - fixed wing ring; 26 - asbestos cement; 27 - waterproof sealant; 28 - atomizing nozzle; 29 - wall panel; 30 - concrete pier; 31 - humidity and heat sensor; 32 - anti-fog lamp. Specific embodiments
[0027] The present utility model will be further described in detail below in conjunction with the accompanying drawings and specific embodiments.
[0028] As Figure 1-7 shown, a test block standard curing room at the construction site includes an operation room 1 and a curing room 2. Inside the curing room 2, there are a test block placement rack 3, a water supply tank 4, a spray water pipe 6, and a heating device 7. Inside the water supply tank 4, there is a water pump 8. The water outlet end of the water pump 8 is connected to the spray water pipe 6. The spray water pipe 6 is arranged in the top space of the curing room 2. There are multiple atomizing nozzles 28 on the spray water pipe 6. At the bottom of the water supply tank 4, there is a heating partition 10, and the heating device 7 is arranged inside the heating partition 10.
[0029] The water supply tank 4 is made of steel. Concrete piers 30 are arranged around the inside of the heating partition 10 to support the water supply tank 4.
[0030] The spray water pipe 6 is arranged in a cross shape.
[0031] Inside the curing room 2, there is a humidity and heat sensor 31.
[0032] Inside the curing room 2, there is a sedimentation tank 5 and a drainage ditch 9. The drainage ditch 9 is arranged around the perimeter of the ground of the curing room 2. One end of the drainage ditch 9 is connected to the sedimentation tank 5. The sedimentation tank 5 and the water supply tank 4 are connected through a connecting pipe 11, and the connecting pipe 11 is located above the sedimentation tank 5.
[0033] The drainage ditch 9 has a slope, and the sedimentation tank 5 is connected to the lower end of the drainage ditch 9 .
[0034] The top of the drainage ditch 9 is flush with the ground of the curing room 2, and a drainage ditch grate 14 is provided on the top of the drainage ditch 9. Reinforcement angle steels 15 are provided on both sides of the top of the drainage ditch 9, and anchor steel bars 16 are provided on the reinforcement angle steels 15. The anchor steel bars 16 are buried in the concrete structure, and the drainage ditch grate 14 is placed on the reinforcement angle steels 15.
[0035] The top of the water supply tank 4 and the top of the sedimentation tank 5 are flush with the ground of the curing room 2. The tops of the water supply tank 4 and the sedimentation tank 5 are respectively provided with a first grate 12 and a second grate 13. Similarly, reinforcement angle steels 15 are also provided around the tops of the water supply tank 4 and the sedimentation tank 5, and the reinforcement angle steels 15 are anchored in the concrete structure by anchor steel bars 16.
[0036] A sleeve 24 is provided outside the connecting pipe 11 , and a fixed wing ring 25 is provided outside the sleeve 24 . The fixed wing ring 25 is buried in the surrounding wall. Asbestos cement 26 is filled between the sleeve 24 and the connecting pipe 11 , and both ends of the asbestos cement 26 are sealed by waterproof sealing paste 27 .
[0037] A standard maintenance box 17 and a test tool cabinet 18 are provided in the operating room 1.
[0038] The operation room 1 and the maintenance room 2 are assembled structures. The wall panels 29 of the operation room 1 and the maintenance room 2 are composed of double-layer color steel plates 19, light steel keels 20 and rock wool 21. The light steel keels 20 and rock wool 21 are located between the double-layer color steel plates 19. The floors of the operation room 1 and the maintenance room 2 are paved with fine stone concrete. The operation room 1 is provided with a first door 22 leading to the outside, and a second door 23 is provided between the operation room 1 and the maintenance room 2. Both the operation room 1 and the maintenance room 2 are provided with anti-fog lights 32.
[0039] The heating device 7 is an electric heating coil, which is arranged in the heating insulation layer 10.
[0040] The connecting pipe 11 is a galvanized pipe.
[0041] During maintenance, water is added to the water supply tank 4 through an external water pipe. The test blocks to be maintained are placed on the test block placement rack 3, and the water pump 8 is turned on. The water pump transports water to the spray water pipe 6 and sprays it through the atomizing nozzle 28. The water mist permeates the maintenance room 2, providing the test blocks with the humidity conditions required for maintenance. After condensation, the water mist flows into the drainage ditch 9 and then into the sedimentation tank 5. The upper layer of clear water after sedimentation flows back to the water supply tank 4 through the connecting pipe 11. The spray water is recycled, and the debris in the sedimentation tank 5 is cleaned regularly.
[0042] When the temperature in the curing room 2 is low, the water in the water supply tank 4 can be heated by the heating device 7, so that the curing room 2 is heated by spraying, and the temperature and humidity in the curing room 2 are made to meet the standard curing conditions by using water vapor.
[0043] A humidity and heat sensor 31 is arranged in the curing room 2, and the humidity and heat sensor 31 can be connected to a mobile phone, so that the staff can check the indoor humidity and temperature at any time through the mobile phone.
[0044] The heating device 7 is separately arranged in the heating interlayer 10, and is separated from the moisture in the curing room 2, so as to avoid electrical short circuit and eliminate safety hazards.
[0045] The utility model device is convenient to operate, easy to control, and improves construction efficiency. The utility model device can easily achieve the humidity and temperature conditions required by the specification, and the cured test block has good compressive strength and stable quality.
[0046] The utility model adopts an assembled structure and can be used repeatedly, thus reducing the project construction cost.
Claims
1. A construction site test block standard curing room, characterized by: It includes an operation room (1) and a curing room (2). In the curing room (2), there are test block placement racks (3), a water supply pool (4), a spray water pipe (6) and a heating device (7). A water pump (8) is provided in the water supply pool (4). The water outlet end of the water pump (8) is connected to the spray water pipe (6). The spray water pipe (6) is arranged in the top space of the curing room (2). A plurality of atomizing nozzles (28) are provided on the spray water pipe (6). A heating partition layer (10) is provided at the bottom of the water supply pool (4). The heating device (7) is arranged in the heating partition layer (10).
2. The construction site test block standard curing room according to claim 1 is characterized in that: The spray water pipe (6) is arranged in a cross shape.
3. The construction site test block standard curing room according to claim 1 or 2, characterized in that: A humidity and temperature sensor (31) is provided in the curing room (2).
4. The construction site test block standard curing room according to claim 3 is characterized by: A sedimentation pool (5) and a drainage ditch (9) are provided in the curing room (2). The drainage ditch (9) is arranged around the perimeter of the ground of the curing room (2). One end of the drainage ditch (9) is connected to the sedimentation pool (5). The sedimentation pool (5) and the water supply pool (4) are connected by a connecting pipe (11). The connecting pipe (11) is located above the sedimentation pool (5).
5. The construction site test block standard curing room according to claim 4 is characterized in that: The drainage ditch (9) has a slope. The sedimentation pool (5) is connected to the low end of the drainage ditch (9).
6. The construction site test block standard curing room according to claim 5 is characterized by: The top of the drainage ditch (9) is flush with the ground of the curing room (2). A drainage ditch grate (14) is provided on the top of the drainage ditch (9).
7. The construction site test block standard curing room according to claim 6, characterized in that: The top of the water supply pool (4) and the top of the sedimentation pool (5) are flush with the ground of the curing room (2). A first grate (12) and a second grate (13) are respectively provided on the tops of the water supply pool (4) and the sedimentation pool (5).
8. The construction site test block standard curing room according to claim 7, characterized in that: A sleeve (24) is provided outside the connecting pipe (11). A fixed wing ring (25) is provided on the periphery of the sleeve (24). Asbestos cement (26) is filled between the sleeve (24) and the connecting pipe (11). Both ends of the asbestos cement (26) are sealed by a waterproof sealant (27).
9. The construction site test block standard curing room according to claim 8, characterized in that: A standard curing box (17) and a test tool cabinet (18) are provided in the operation room (1).
10. The construction site test block standard curing room according to claim 9, characterized in that: The operation room (1) and the curing room (2) are of a prefabricated structure. The wall panels (29) of the operation room (1) and the curing room (2) are composed of double-layer color steel plates (19), light steel keels (20) and rock wool (21). The light steel keels (20) and the rock wool (21) are located between the double-layer color steel plates (19).
Citation Information
Cited By
Concrete test block standard curing chamber
CN223456216U