Low-stress MEMS chip packaging structure

By arranging a thermal stress buffer plate and an adhesive layer between the MEMS chip and the organic substrate, the impact of stress changes on the MEMS chip during the high-temperature packaging process is solved, thereby reducing the stress impact and improving stability during the packaging process.

CN221836755UActive Publication Date: 2024-10-15HUNAN YUEMO ADVANCED SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420093020.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-15
Publication Date
2024-10-15
Estimated Expiration
2034-01-15

AI Technical Summary

Technical Problem

During the high-temperature sealing and plastic packaging process using organic substrates to connect MEMS chips, the MEMS chips are affected by large stress changes, threatening performance stability.

Method used

A thermal stress buffer plate is provided between the MEMS chip and the organic substrate, and an adhesive layer is provided between the thermal stress buffer plate and the organic substrate and between the MEMS chip and the thermal stress buffer plate. The thermal expansion coefficient of the thermal stress buffer plate is between that of the MEMS chip. Between the thermal stress buffer plate and the organic substrate, a thermal stress buffer plate made of glass or silicon is used, and conductive or insulating silver paste is used in the bonding layer. The surface of the thermal stress buffer plate has protrusions that enhance horizontal resistance.

Benefits of technology

It significantly reduces the stress effect of the organic substrate on the MEMS chip, enhances the stability between the chip and the substrate, and simplifies the structural design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221836755U_ABST
    Figure CN221836755U_ABST
Patent Text Reader

Abstract

The utility model discloses a low-stress MEMS chip packaging structure, which is characterized in that a thermal stress buffer plate is arranged between an MEMS chip and an organic substrate, and adhesive layers are respectively arranged between the thermal stress buffer plate and the organic substrate and between the MEMS chip and the thermal stress buffer plate. The thermal expansion coefficient of the thermal stress buffer plate is larger than that of the MEMS chip and smaller than that of the organic substrate. And the thermal stress buffer plate is made of a glass material with an optional thermal expansion coefficient. The method has the advantages that the influence of the organic substrate with large stress change on the MEMS chip can be obviously reduced in the packaging process; the stability between the MEMS chip and the organic substrate along the plane direction of the substrate can be enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a low-stress MEMS chip packaging structure, belonging to the technical field of chip packaging. Background Art

[0002] MEMS packaging usually uses ceramic substrates. The advantage of ceramic substrates is that the CTE (coefficient of thermal expansion) value of the ceramic substrate is close to the CTE value of the chip, the stress generated during the packaging process is low, and the performance of the packaged MEMS sensor is stable; the disadvantage of ceramic substrates is that the packaging cost is too high and the production efficiency is low. In order to reduce production costs, some MEMS sensors use organic substrate packaging.

[0003] MEMS sensors packaged with organic substrates usually contain two chips, one is a MEMS chip and the other is an ASIC control chip. The two chips can be packaged side by side or in a stacked manner. Unlike ASIC control chips, MEMS chips have built-in acceleration sensors. The chip has extremely small mechanical structures and has components that can change position and produce displacement when accelerating or decelerating.

[0004] Both the MEMS chip and the ASIC chip are arranged on the same substrate. No matter the two chips are arranged side by side or stacked, the MEMS chip must be connected to the substrate. The following describes the problem of connecting and packaging the MEMS chip with the organic substrate.

[0005] The packaging of MEMS chips and ASIC chips is carried out at a high temperature of nearly 175 degrees Celsius or even 250 degrees Celsius. Before the MEMS chip is sealed, the MEMS chip is first connected to the organic substrate through silver paste or bonding glue. Since the silver paste layer or bonding glue layer between the MEMS chip and the organic substrate is very thin, during the high-temperature packaging and subsequent cooling process, the thermal stress change of the MEMS chip will be directly affected by the thermal stress change of the organic substrate. Due to the large difference between the CTE value of the MEMS chip and the CTE value of the organic substrate, the large stress deformation generated by the organic substrate will directly cause the MEMS chip to generate corresponding stress deformation, while the micromechanical structure in the MEMS chip does not allow such large deformation to occur, otherwise it will seriously affect the sensing effect and even make the MEMS chip scrapped. Utility Model Content

[0006] The technical problem to be solved by the utility model is: how to reduce the influence of the organic substrate with large stress changes on the MEMS chip during the process of high-temperature sealing and plastic sealing by connecting the organic substrate with the MEMS chip.

[0007] In view of the above problems, the technical solution proposed by the utility model is:

[0008] A low-stress MEMS chip packaging structure, a thermal stress buffer plate is provided between the MEMS chip and an organic substrate, adhesive layers are provided between the thermal stress buffer plate and the organic substrate and between the MEMS chip and the thermal stress buffer plate, respectively, the thermal expansion coefficient of the thermal stress buffer plate is greater than the thermal expansion coefficient of the MEMS chip but less than the thermal expansion coefficient of the organic substrate.

[0009] Furthermore, the thermal stress buffer plate is made of glass material with a selectable thermal expansion coefficient.

[0010] Furthermore, the thermal stress buffer plate is made of silicon.

[0011] Furthermore, the adhesive layer is a conductive silver paste with adhesive strength.

[0012] Furthermore, the adhesive layer is an insulating adhesive with adhesive strength.

[0013] Furthermore, the upper surface and the lower surface of the thermal stress buffer plate have protrusions for enhancing horizontal resistance. Beneficial Effects

[0014] 1. It can significantly reduce the impact of organic substrates with large stress changes on MEMS chips during the packaging process;

[0015] 2. It can enhance the stability between the MEMS chip and the organic substrate along the substrate plane direction;

[0016] 3. Simple structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a schematic plan view of the low-stress MEMS chip packaging structure before packaging according to the first embodiment, in which WB is a wire connecting the MEMS chip to the substrate;

[0018] Figure 2 This is a schematic plan view of the low-stress MEMS chip packaging structure before packaging according to the second embodiment, where WB is a wire connecting the MEMS chip to the substrate.

[0019] In the figure: 1. MEMS chip; 2. organic substrate; 3. thermal stress buffer plate; 301. protrusion; 4. adhesive layer. DETAILED DESCRIPTION

[0020] The utility model is further described below in conjunction with the accompanying drawings: Embodiment 1

[0021] like Figure 1As shown, a low stress MEMS chip packaging structure is provided, wherein a thermal stress buffer plate 3 is provided between the MEMS chip 1 and the organic substrate 2, and adhesive layers 4 are provided between the thermal stress buffer plate 3 and the organic substrate 2 and between the MEMS chip 1 and the thermal stress buffer plate 3, respectively. The thermal expansion coefficient of the thermal stress buffer plate 3 is greater than the thermal expansion coefficient of the MEMS chip 1 but less than the thermal expansion coefficient of the organic substrate 2. That is, the thermal expansion coefficient of the thermal stress buffer plate 3 is between the thermal expansion coefficient of the MEMS chip 1 and the thermal expansion coefficient of the organic substrate 2. In this way, the stress difference between the MEMS chip 1 and the thermal stress buffer plate 3 after the thermal stress buffer plate 3 is provided is compared with the stress difference between the MEMS chip 1 and the organic substrate 2 without the thermal stress buffer plate 3, and the stress difference between the MEMS chip 1 and the thermal stress buffer plate 3 becomes smaller, thereby reducing the influence of the organic substrate with large stress changes on the MEMS chip during the packaging process.

[0022] Preferably, the thermal stress buffer plate 3 is made of glass with selectable thermal expansion coefficient. Thus, glass with suitable thermal expansion coefficient can be selected as the thermal stress buffer plate 3 as needed to reduce the influence of the organic substrate with large stress changes on the MEMS chip during the packaging process to an allowable range.

[0023] Optionally, the thermal stress buffer plate 3 is made of silicon.

[0024] As required, the adhesive layer 4 is a conductive silver paste with adhesive strength.

[0025] As required, the adhesive layer 4 is an insulating adhesive with adhesive strength. Embodiment 2

[0026] like Figure 2 As shown, the difference from the first embodiment is that the upper and lower surfaces of the thermal stress buffer plate 3 have protrusions 301 for enhancing horizontal resistance, which can effectively resist the shear force formed between the MEMS chip and the organic substrate and enhance the stability between the MEMS chip and the organic substrate along the substrate plane direction.

[0027] The above embodiments are only used to more clearly describe the present invention and cannot be regarded as limiting the protection scope of the present invention. Any modifications in equivalent forms should be regarded as falling within the protection scope of the present invention.

Claims

1. A low stress MEMS chip packaging structure, characterized in that: A thermal stress buffer plate (3) is provided between the MEMS chip (1) and the organic substrate (2), and an adhesive layer (4) is provided between the thermal stress buffer plate (3) and the organic substrate (2) and between the MEMS chip (1) and the thermal stress buffer plate (3), respectively; the thermal expansion coefficient of the thermal stress buffer plate (3) is greater than the thermal expansion coefficient of the MEMS chip (1) but less than the thermal expansion coefficient of the organic substrate (2).

2. The low stress MEMS chip packaging structure according to claim 1, characterized in that: The thermal stress buffer plate (3) is made of glass material with a selectable thermal expansion coefficient.

3. The low stress MEMS chip packaging structure according to claim 1, characterized in that: The thermal stress buffer plate (3) is made of silicon.

4. The low stress MEMS chip packaging structure according to claim 1, characterized in that: The adhesive layer (4) is a conductive silver paste with adhesive strength.

5. The low stress MEMS chip packaging structure according to claim 1, characterized in that: The adhesive layer (4) is an insulating adhesive with adhesive strength.

6. The low stress MEMS chip packaging structure according to any one of claims 1 to 5, characterized in that: The upper surface and the lower surface of the thermal stress buffer plate (3) have protrusions (301) for enhancing horizontal resistance.