Heatable die sleeve for extruding magnesium alloy and hard aluminum alloy profiles
By designing a heatable die sleeve for the extrusion die, the problem of the die temperature decreasing during the extrusion process of magnesium alloy and duralumin alloy is solved, the stable control of the die temperature is achieved, and the production efficiency and product quality are improved.
Patent Information
- Application Number
- CN202420343674.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-23
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-02-23
AI Technical Summary
During the extrusion process, magnesium alloys and duralumin alloys have difficulty in deformation due to their close-packed structure and high hardness, and the mold temperature decreases rapidly, resulting in production interruption and mold damage, which reduces production efficiency.
Design a heatable mold sleeve, including a shell, a heating component and a temperature control component. The shell is divided into a mold sleeve lining and an outer shell, with embedded heating components and temperature-control thermocouples, and is monitored and adjusted in real time through the temperature control module. Heating to keep the mold temperature stable.
It extends the continuous extrusion time of the mold, reduces the frequency of mold changes, improves product quality and production efficiency, and prevents the mold from being damaged due to lower temperature.
Smart Images

Figure CN221848235U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of alloy profile extrusion processing, in particular to a heatable die sleeve for extruding magnesium alloy and hard aluminum alloy profiles. Background Art
[0002] Magnesium and its alloys have the advantages of low density, high specific strength and specific stiffness, good damping and shock absorption, good thermal conductivity, good electromagnetic shielding effect, excellent machining performance, and easy recycling. However, the mechanical properties of magnesium alloy castings are not ideal, there are certain limitations and they are prone to structural defects, which greatly limits the practicality and application scope of magnesium alloys.
[0003] Extrusion refers to a pressure processing method that applies pressure to one end of the ingot placed in the extrusion barrel to make it pass through the extrusion die to achieve plastic deformation. Compared with forging and rolling processes, extrusion has a more severe three-dimensional compressive stress state than forging and rolling, and the metal can exert its maximum plasticity; the extrusion process has great flexibility and is easy to operate; the product has high dimensional accuracy and good surface quality.
[0004] For magnesium alloy extrusion molding, due to the close-packed hexagonal structure of magnesium alloy itself, there are fewer slip systems during deformation, deformation is difficult, and deformation largely depends on twinning, which will increase the probability of cracking of large materials and reduce the formability and mechanical properties of the material. Even if the magnesium alloy is heated to a certain temperature, deformation is still difficult to carry out, so the extrusion speed of magnesium alloy must be reduced during extrusion; for hard aluminum alloy, the reason is the same. Hard aluminum alloy (such as 2 series, 7 series, etc.) is too hard and the speed is slow during extrusion, but the too slow extrusion speed makes the extrusion die cool down faster. Because the extrusion speed is too slow, the heat loss of the die is much greater than the heat generated by friction, and the reduction of the die temperature will also be transferred to the billet, which reduces the billet temperature and increases the resistance to extrusion deformation, which in turn leads to production interruption. At the same time, it also increases the risk of mold damage, and reheating the billet and replacing the mold takes a lot of time, which reduces production efficiency.
[0005] Therefore, the present application designs a heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles to solve the above technical problems. Utility Model Content
[0006] To achieve the above-mentioned purpose, the utility model provides a heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles, which supports and provides heating and heat preservation for a conventional cylindrical extrusion die, and comprises a shell sleeved outside the extrusion die, a heating component is arranged in the shell, and the heating component is electrically connected to a temperature control component;
[0007] The housing comprises a coaxially arranged die sleeve liner and a die sleeve outer shell, the die sleeve liner is sleeved on the extrusion die, and the heating assembly is arranged between the die sleeve liner and the die sleeve outer shell;
[0008] The temperature control component includes a temperature control thermocouple inserted in the inner lining of the mold sleeve, the temperature control thermocouple extends out of the mold sleeve shell and is electrically connected to an electrode of the temperature control module, and the other electrode of the temperature control module is electrically connected to the heating component.
[0009] Preferably, a ring-shaped heating chamber is provided on the inner lining of the mold sleeve, and the heating component is embedded and fixed in the heating chamber.
[0010] Preferably, the heating assembly comprises a heating element embedded and fixed in the heating chamber, and the heating element is electrically connected to an electrode of the temperature control module.
[0011] Preferably, the outer jacket of the heating element is provided with heat-insulating cotton for heat preservation, and the heat-insulating cotton is arranged in contact with the inner wall of the mold sleeve shell.
[0012] Preferably, the mold sleeve liner is matched with the extrusion die in radial clearance.
[0013] Preferably, the mold sleeve inner lining is reserved with a first cylindrical hole adapted to the temperature-controlling thermocouple, and the temperature-controlling thermocouple is embedded and clamped in the first cylindrical hole.
[0014] Preferably, a second cylindrical hole corresponding to the first cylindrical hole is formed through the mold sleeve shell, and the temperature-controlling thermocouple passes through the second cylindrical hole.
[0015] Compared with the prior art, the utility model has the following advantages and technical effects: the utility model discloses a heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles, which is mainly used to support and provide heating and heat preservation for the traditional cylindrical extrusion die; the shell sleeve with the heating component embedded inside is arranged outside the extrusion die, and the temperature control component is used to monitor the problems of the shell and the extrusion die. During the extrusion process, when the temperature of the extrusion die drops, the heating component starts heating to increase the temperature of the extrusion die, so that the extrusion die is maintained at a suitable extrusion temperature, the temperature drop of the die during the extrusion process is reduced, the continuous extrusion time of a single set of extrusion dies is increased, and the extrusion time is reduced. The mold changing frequency ensures product quality and production efficiency; the shell is divided into a coaxial mold sleeve outer shell and a mold sleeve lining. The double-layer structure design can be used to fix the heating component to ensure stable heating and prevent damage to the heating component caused by the force of the extrusion mold during the extrusion molding process, thereby ensuring the constant temperature of the extrusion process; the temperature-controlled thermocouple is plugged into the mold sleeve lining and close to the extrusion mold, which can monitor the temperature of the extrusion mold in real time, and then control the operation of the heating component through the temperature control module to achieve temperature control of the extrusion mold, ensure the stability of the temperature of the extrusion mold, facilitate the extrusion of the alloy, and ensure the efficiency and quality of the alloy extrusion molding.
[0016] The utility model has a simple structure and is easy to use, and can effectively solve the problems of excessive extrusion pressure, extrusion interruption or damage to the mold or extrusion equipment caused by the reduction of mold temperature during the extrusion process of magnesium alloy and hard aluminum alloy profiles, thereby realizing continuous extrusion of magnesium alloy and hard aluminum alloy profiles and improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The drawings constituting a part of the present application are used to provide a further understanding of the present application. The illustrative embodiments and descriptions of the present application are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0018] Figure 1 This is a schematic diagram of the structure of a heatable die sleeve for extruding magnesium alloy and hard aluminum alloy profiles of the utility model;
[0019] In the figure: 1. Extrusion die; 2. Die sleeve lining; 3. Heating chamber; 4. Heating components; 5. Insulation cotton; 6. Die sleeve shell; 7. Temperature control thermocouple; 8. Temperature control module. DETAILED DESCRIPTION
[0020] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0021] In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.
[0022] Reference Figure 1 As shown, this embodiment provides a heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles, which supports and provides heating and heat preservation for a conventional cylindrical extrusion die 1, and comprises a shell sleeved outside the extrusion die 1, a heating component is arranged in the shell, and the heating component is electrically connected to a temperature control component;
[0023] The housing comprises a coaxially arranged die sleeve liner 2 and a die sleeve outer shell 6, the die sleeve liner 2 is sleeved on the extrusion die 1, and the heating component is arranged between the die sleeve liner 2 and the die sleeve outer shell 6;
[0024] The temperature control component includes a temperature control thermocouple 7 inserted in the mold sleeve lining 2. The temperature control thermocouple 7 extends out of the mold sleeve shell 6 and is electrically connected to one electrode of the temperature control module 8. The other electrode of the temperature control module 8 is electrically connected to the heating component.
[0025] The utility model discloses a heatable die sleeve for extruding magnesium alloy and hard aluminum alloy profiles, which is mainly used for supporting and providing heating and heat preservation for a traditional cylindrical extrusion die 1; a shell with a heating component embedded inside is sleeved outside the extrusion die 1, and a temperature control component is used to monitor problems of the shell and the extrusion die 1; during the extrusion process, when the temperature of the extrusion die 1 decreases, the heating component starts heating to increase the temperature of the extrusion die 1, so that the extrusion die 1 is maintained at a suitable extrusion temperature, the temperature drop of the die during the extrusion process is reduced, the continuous extrusion time of a single set of extrusion die 1 is increased, and the die change time of the extrusion die 1 is reduced frequency, ensuring product quality and production efficiency; the shell is divided into a coaxially sleeved mold shell and a mold sleeve lining 2, and the double-layer structure design can be used to fix the heating component to ensure stable heating, prevent the heating component from being damaged due to the force on the extrusion mold 1 during the extrusion molding process, and ensure the constant temperature of the extrusion process; the temperature-controlled thermocouple 7 is plugged into the mold sleeve lining 2 and is close to the extrusion mold 1, and can monitor the temperature of the extrusion mold 1 in real time, and then control the operation of the heating component through the temperature control module 8 to achieve temperature control of the extrusion mold 1, ensure the stability of the temperature of the extrusion mold 1, and facilitate the extrusion of the alloy. The utility model has a simple structure and is easy to use. It can effectively solve the problems of excessive extrusion pressure, extrusion interruption or damage to the mold or extrusion equipment caused by the reduction of mold temperature during the extrusion of magnesium alloy and hard aluminum alloy profiles, realize the continuous extrusion of magnesium alloy and hard aluminum alloy profiles, and improve production efficiency.
[0026] In a further optimized solution, a ring-shaped heating chamber 3 is provided on the die sleeve inner liner 2, and the heating component is embedded and fixed in the heating chamber 3. The heating chamber 3 is used to fix the heating component, improve the stability of the heating component, and prevent the instability caused by the shaking of the heating component; at the same time, the concave heating chamber 3 can also make the heating component closer to the extrusion die 1, accelerate the heat transfer efficiency, and reduce the heat loss.
[0027] In a further optimized solution, the heating assembly includes a heating element 4 embedded and fixed in the heating chamber 3, and the heating element 4 is electrically connected to the electrode of the temperature control module 8. As a heating device, the heating element 4 can mainly heat under the control of the temperature control module 8, and continuously transfer the heat to the extrusion die 1.
[0028] In a further optimized solution, the outer cover of the heating element 4 is provided with a heat-insulating cotton 5 for heat preservation, and the heat-insulating cotton 5 is arranged in contact with the inner wall of the mold sleeve shell 6. The heat-insulating cotton 5 is sleeved on the outer periphery of the heating element 4 to reduce the heat loss to the side away from the extrusion die 1, and can also be used as an extrusion pad to contact the mold sleeve shell 6, play a role in fixing the heating element 4, and also avoid the wear caused by the contact between the heating element 4 and the inner wall of the mold sleeve shell 6, thereby extending the service life.
[0029] Furthermore, the heating element 4 and the heat-insulating cotton 5 do not extend beyond the surface of the heating chamber 3 , thereby avoiding being damaged by the mold sleeve shell 6 .
[0030] Further optimizing the scheme, the die sleeve liner 2 is matched with the radial clearance of the extrusion die 1. The die sleeve liner 2 is matched with the radial clearance of the extrusion die 1, which is conducive to the installation and disassembly of the extrusion die 1 and the device.
[0031] Furthermore, the gap between the mold sleeve lining 2 and the extrusion die 1 should be appropriate and not too large, otherwise the extrusion die 1 will be unstable and the heat of the mold sleeve lining 2 will be difficult to effectively transfer to the die itself.
[0032] Furthermore, the mold sleeve outer shell 6 should fit well with the mold sleeve inner liner 2 and be fastened together with bolts to avoid relative displacement and damage to the heating element 4 and the temperature-controlling thermocouple 7.
[0033] Further optimization scheme, the mold sleeve lining 2 is reserved with a first cylindrical hole adapted to the temperature control thermocouple 7, and the temperature control thermocouple 7 is embedded and clamped in the first cylindrical hole; the mold sleeve shell 6 is penetrated with a second cylindrical hole corresponding to the first cylindrical hole, and the temperature control thermocouple 7 passes through the second cylindrical hole. The first cylindrical hole and the second cylindrical hole are coaxial and have the same diameter, and the temperature control thermocouple 7 can be smoothly inserted into the cylindrical hole of the mold sleeve lining 2 and the through hole of the mold sleeve shell 6, and effectively contact the mold sleeve lining 2.
[0034] Furthermore, the temperature control module 8 can effectively connect the temperature-controlling thermocouple 7 and the heating chamber 3, and timely adjust the heating power of the heating element 4 according to the feedback signal of the temperature-controlling thermocouple 7 to ensure that the extrusion die 1 is within a certain temperature range.
[0035] In the description of the present invention, it should be understood that the terms "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.
[0036] The embodiments described above are only descriptions of the preferred methods of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should fall within the protection scope determined by the claims of the present invention.
Claims
1. A heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles, which supports a conventional cylindrical extrusion die (1) and provides heating and heat preservation, and is characterized by: It comprises a shell sleeved outside the extrusion die (1), a heating component is arranged inside the shell, and the heating component is electrically connected to a temperature control component; The shell comprises a coaxially arranged die sleeve liner (2) and a die sleeve outer shell (6), the die sleeve liner (2) being sleeved on the extrusion die (1), and the heating component being arranged between the die sleeve liner (2) and the die sleeve outer shell (6); The temperature control component comprises a temperature control thermocouple (7) inserted into the mold sleeve lining (2); the temperature control thermocouple (7) extends out of the mold sleeve shell (6) and is electrically connected to an electrode of the temperature control module (8); and the other electrode of the temperature control module (8) is electrically connected to the heating component.
2. The heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles according to claim 1, characterized in that: The mold sleeve inner lining (2) is provided with an annular heating chamber (3), and the heating component is embedded and fixed in the heating chamber (3).
3. The heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles according to claim 2, characterized in that: The heating assembly comprises a heating element (4) embedded and fixed in the heating chamber (3); the heating element (4) is electrically connected to an electrode of the temperature control module (8).
4. The heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles according to claim 3 is characterized in that: The outer jacket of the heating element (4) is provided with heat-insulating cotton (5) for heat preservation, and the heat-insulating cotton (5) is arranged in contact with the inner wall of the mold sleeve shell (6).
5. The heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles according to claim 1, characterized in that: The die sleeve liner (2) and the extrusion die (1) are matched with radial clearance.
6. The heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles according to claim 1, characterized in that: The mold sleeve lining (2) is reserved with a first cylindrical hole adapted to the temperature-controlling thermocouple (7), and the temperature-controlling thermocouple (7) is embedded and clamped in the first cylindrical hole.
7. The heatable die sleeve for extrusion of magnesium alloy and hard aluminum alloy profiles according to claim 6, characterized in that: The mold sleeve shell (6) is provided with a second cylindrical hole corresponding to the first cylindrical hole, and the temperature-controlling thermocouple (7) passes through the second cylindrical hole.