Kiln capable of preventing furnace bottom from being bonded
By arranging auxiliary components at the bottom of the kiln, airflow and vibration are used to prevent ceramic materials from adhering to the bottom of the furnace, thereby solving the adhesion problem of ceramic materials in the kiln and extending the service life of the kiln.
Patent Information
- Application Number
- CN202420424789.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-05
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-03-05
AI Technical Summary
During the use of existing kilns, ceramic materials are prone to adhere to the furnace bottom, which affects the refractory performance and reduces the service life.
A kiln is designed to prevent the bonding of the furnace bottom. By arranging auxiliary components at the bottom of the kiln, including connecting frames, partitions, corrugated plates, air ducts, support rods and arc blocks, airflow and vibration are used to prevent ceramic materials. Adhered to the bottom of the furnace.
By reducing the contact area between ceramic products and the furnace bottom and using air flow isolation and vibration to prevent adhesion, the probability of adhesion between ceramic products and the furnace bottom is significantly reduced and the service life of the kiln is extended.
Smart Images

Figure CN221859225U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of kilns, in particular to a kiln capable of preventing the bottom of the kiln from being adhered. Background Art
[0002] A kiln is a device used to fire ceramics at high temperatures, but in the current existing technology, kilns may become sticky during use. This is mainly because the residual ceramic materials in the kiln crystallize and solidify at high temperatures, or chemically react with the kiln wall and refractory materials, causing the ceramic materials to stick to the bottom of the kiln. The sticking ceramic materials will affect the refractory performance of the bottom of the kiln, affect the use effect, and reduce the service life of the kiln. Utility Model Content
[0003] The utility model aims to provide a kiln capable of preventing the bottom of the kiln from sticking, so as to solve the problems raised in the above-mentioned background technology.
[0004] In order to achieve the above purpose, the utility model provides the following technical solutions:
[0005] A kiln for preventing the bottom of the furnace from sticking comprises a kiln, wherein a base is arranged at the bottom of the kiln, an auxiliary component for preventing the bottom of the furnace from sticking is arranged inside the base, the auxiliary component comprises a connecting frame arranged on one side of the base, two partitions are arranged on the inner wall of the base, three chambers are separated by the two partitions, corrugated plates are arranged inside the three chambers, a plurality of air slots are arranged inside the two partitions, support rods and arc blocks are arranged inside the plurality of air slots, and a vibration block is arranged on the top of the arc block.
[0006] As a preferred solution of the utility model, the kiln is located on the top of the base and connected to the base by bolts, the connecting frame is connected to one side of the base by bolts, and a plurality of fan blades are installed inside the connecting frame to blow air into the base.
[0007] As a preferred solution of the utility model, the two partitions are integrally formed with the inner wall of the base, the corrugated plate is connected to the inner wall of the chamber by welding, and the protruding part of the corrugated plate is flush with the partition and the base.
[0008] As a preferred solution of the utility model, the air grooves inside the two partitions are connected to the chamber, and the connecting frame is connected to the chamber. The airflow generated in the connecting frame can flow in the recessed part of the corrugated plate and pass through the air grooves of the partitions, so that the airflow can pass through the three chambers in sequence.
[0009] As a preferred solution of the utility model, the multiple air slots in the two partitions are matched with the concave positions of the corrugated plates, and the support rods are located in the air slots and connected to the inner walls of the air slots by bolts.
[0010] As a preferred solution of the utility model, the arc block is located in the air duct and is slidably connected to the inner wall of the air duct through a slide rail, the support rod passes through the arc block, and the vibration block is connected to the outer wall of the arc block through bolts. When the airflow passes through the air duct, the arc block is pushed to rise upward.
[0011] Compared with the prior art, the beneficial effects of the utility model are as follows: in response to the problems raised in the background technology, the present application adopts an auxiliary component, which can reduce the contact area between the fired ceramic products and the furnace bottom by setting a corrugated structure on the furnace bottom, and when airflow is generated, the airflow flows in the grooves of the corrugated plate, so that the ceramic products are isolated from the furnace bottom. At the same time, when the airflow passes through, the arc block hits the corrugated plate to produce slight vibrations, which again prevents the ceramic products from sticking to the furnace bottom, thereby reducing the probability of the ceramic products sticking to the furnace bottom, ensuring the surface integrity of the furnace bottom, protecting the kiln, and increasing the service life.
[0012] The utility model can isolate the ceramic product from the furnace bottom by reducing the contact area, isolating the airflow and vibrating, thereby protecting the kiln, reducing the probability of adhesion of the furnace bottom and increasing the service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 This is the appearance structure diagram of the kiln of the utility model;
[0014] Figure 2 This is the appearance structure diagram of the partition of the utility model;
[0015] Figure 3 This is the appearance structure diagram of the arc block of the utility model.
[0016] In the figure: 1, kiln; 2, base; 201, connection frame; 3, partition; 4, chamber; 401, corrugated plate; 5, air trough; 6, support rod; 7, arc block; 701, vibration block. DETAILED DESCRIPTION
[0017] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the embodiments of the present invention.
[0018] Example
[0019] See also Figure 1-3The utility model provides a technical solution: a kiln for preventing the bottom of the furnace from sticking, comprising a kiln 1, a base 2 is arranged at the bottom of the kiln 1, an auxiliary component for preventing the bottom of the furnace from sticking is arranged inside the base 2, and the auxiliary component comprises a connecting frame 201 arranged on one side of the base 2, and a fan blade is installed in the connecting frame 201, which can generate airflow and transport the airflow to the chamber 4 of the base 2, and circulate in the concave part of the corrugated plate 401, and the airflow circulates in the groove of the corrugated plate 401 to isolate the ceramic product from the bottom of the furnace, and the inner wall of the base 2 is provided with two partitions 3 for dividing the base 2 to form three chambers 4, and the three chambers 4 are separated by the two partitions 3, and the three chambers 4 can be used for multiple ceramic products During firing, the three chambers 4 are each provided with a corrugated plate 401, the raised portion of the corrugated plate 401 can lift and support the ceramic product, and due to the corrugated structure, the contact area of the ceramic product is reduced, thereby reducing the area of adhesion at the bottom of the furnace, and the two partitions 3 are each provided with a plurality of air grooves 5 for allowing the air flow to pass through the partitions 3 and flow into the three chambers 4, and the plurality of air grooves 5 are each provided with a support rod 6 and an arc block 7, when the air flow passes through the arc block 7, the air flow will follow the arc surface and flow to the bottom of the arc block 7, thereby blowing and lifting the arc block 7, and a vibration block 701 is provided on the top of the arc block 7, and when the arc block 7 is raised, the vibration block 701 on the top abuts against the inner wall of the air groove 5, thereby causing the chamber 4 to vibrate.
[0020] In this embodiment, all electrical components are controlled by conventional controllers.
[0021] For example, please refer to Figure 1-3The kiln 1 is located on the top of the base 2 and is connected to the base 2 by bolts. The connecting frame 201 is connected to one side of the base 2 by bolts. A plurality of fan blades are installed inside the connecting frame 201 to blow air into the base 2. The two partitions 3 are integrally formed with the inner wall of the base 2. The corrugated plate 401 is connected to the inner wall of the chamber 4 by welding. The protruding part of the corrugated plate 401 is flush with the partition 3 and the base 2. The air grooves 5 inside the two partitions 3 are connected to the chamber 4. The connecting frame 201 is connected to the chamber 4. The airflow generated in the connecting frame 201 The air can circulate in the concave part of the corrugated plate 401, and pass through the air slot 5 of the partition 3, so that the air flow can pass through the three chambers 4 in sequence. The multiple air slots 5 in the two partitions 3 are matched with the concave positions of the corrugated plate 401. The support rod 6 is located in the air slot 5 and is connected to the inner wall of the air slot 5 by bolts. The arc block 7 is located in the air slot 5 and is slidably connected to the inner wall of the air slot 5 by a slide rail. The support rod 6 passes through the arc block 7, and the vibration block 701 is connected to the outer wall of the arc block 7 by bolts. When the air flow passes through the air slot 5, the arc block 7 is pushed to rise upward. When in use, first place the ceramic product and the loading furnace in different chambers 4 at the bottom of the kiln 1 and place them on the corrugated plate 401. During the firing process, the fan blades inside the connection frame 201 are operated by the PLC controller to generate airflow, and the airflow is blown into the corrugated plate 401 in the chamber 4, and circulates in the grooves of the corrugated plate 401. At the same time, the airflow is circulated in the three chambers 4 in sequence through the air grooves 5 of the partition 3. When passing through the air grooves 5, the arc block 7 can be blown up in accordance with the arc surface angle outside the arc block 7, and the vibration block 701 abuts against the partition 3 to generate vibration. By reducing the contact area, isolating the airflow and vibrating, the ceramic product is isolated from the furnace bottom, the kiln is protected, the probability of adhesion of the furnace bottom is reduced, and the service life is increased.
[0022] The working process of the utility model: when in use, firstly place the ceramic product and the loading furnace in different chambers 4 of the bottom of the kiln 1 and place them on the corrugated plate 401. During the firing process, the fan blades inside the connection frame 201 are operated by the PLC controller to generate airflow, and the airflow is blown into the corrugated plate 401 in the chamber 4, and circulates in the grooves of the corrugated plate 401. At the same time, the airflow is circulated in the three chambers 4 in sequence through the air grooves 5 of the partition 3. When passing through the air grooves 5, the arc block 7 can be blown up in accordance with the arc surface angle outside the arc block 7, so that the vibration block 701 abuts against the partition 3 to generate vibration. By reducing the contact area, isolating the airflow and vibration, the ceramic product is isolated from the bottom of the furnace, the kiln is protected, the probability of adhesion of the bottom of the furnace is reduced, and the service life is increased.
[0023] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A kiln for preventing the bottom of the kiln from sticking, comprising a kiln (1), wherein a base (2) is arranged at the bottom of the kiln (1), and an auxiliary component for preventing the bottom of the kiln from sticking is arranged inside the base (2), characterized in that: The auxiliary component comprises a connection frame (201) arranged on one side of the base (2); two partitions (3) are arranged on the inner wall of the base (2); three chambers (4) are separated by the two partitions (3); a corrugated plate (401) is arranged inside each of the three chambers (4); a plurality of air ducts (5) are arranged inside each of the two partitions (3); a support rod (6) and an arc block (7) are arranged inside each of the plurality of air ducts (5); a vibration block (701) is arranged on the top of the arc block (7).
2. A kiln for preventing furnace bottom adhesion according to claim 1, characterized in that: The kiln (1) is located on the top of the base (2) and is connected to the base (2) by bolts. The connection frame (201) is connected to one side of the base (2) by bolts. A plurality of fan blades are installed inside the connection frame (201) to blow air into the base (2).
3. A kiln for preventing furnace bottom adhesion according to claim 1, characterized in that: The two partitions (3) are integrally formed with the inner wall of the base (2); the corrugated plate (401) is connected to the inner wall of the chamber (4) by welding; and the protruding portion of the corrugated plate (401) is flush with the partition (3) and the base (2).
4. A kiln for preventing furnace bottom adhesion according to claim 1, characterized in that: The air grooves (5) inside the two partitions (3) are in communication with the chamber (4), and the connection frame (201) is in communication with the chamber (4). The airflow generated in the connection frame (201) can flow through the inner recess of the corrugated plate (401) and pass through the air grooves (5) of the partitions (3), so that the airflow can pass through the three chambers (4) in sequence.
5. A kiln for preventing furnace bottom adhesion according to claim 1, characterized in that: The multiple air slots (5) in the two partitions (3) are matched with the concave positions of the corrugated plate (401), and the support rod (6) is located in the air slot (5) and connected to the inner wall of the air slot (5) by bolts.
6. A kiln for preventing furnace bottom adhesion according to claim 1, characterized in that: The arc block (7) is located in the air duct (5) and is slidably connected to the inner wall of the air duct (5) via a slide rail; the support rod (6) passes through the arc block (7); the vibration block (701) is connected to the outer wall of the arc block (7) via bolts; when the airflow passes through the air duct (5), the arc block (7) is pushed to rise upward.