Chip packaging structure
By arranging annular bumps in the glue bonding layer of the chip packaging structure, the problem of poor air tightness caused by polymer bonding is solved, the air tightness performance and reliability of the chip packaging are improved, and the cost and process complexity are reduced.
Patent Information
- Application Number
- CN202420152895.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-22
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-01-22
AI Technical Summary
The polymer bonding method in chip packaging results in poor airtightness of the cavity, resulting in low reliability of the chip packaging structure.
An annular bump is provided in the glue bonding layer. The annular bump is located in the bonding area and within the glue bonding layer. The height and width of the annular bump are not higher than the thickness and width of the glue bonding layer, forming a gap to delay Penetration of gas molecules.
The airtight performance and reliability of the chip packaging structure are significantly improved, the time for gas molecules to penetrate into the functional area is delayed, and the cost and process complexity are reduced.
Smart Images

Figure CN221861634U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of chip packaging, and in particular relates to a chip packaging structure. Background Art
[0002] Wafer-level airtight bonding generally adopts dielectric-free bonding, metal dielectric bonding or polymer bonding. Among them, dielectric-free bonding, such as silicon-silicon, silicon oxide-silicon oxide or anodic bonding, etc., all have extremely high flatness and cleanliness requirements for the two wafers to be bonded, so expensive pre-treatment processes and bonding equipment are required to ensure the bonding effect. Metal bonding, such as aluminum germanium or gold-gold, gold-tin, etc., all require the surfaces of the two wafers to be bonded to have nanometer-level flatness, and pre-place two metals for bonding on the flat surfaces of the two wafers. The bonding pre-treatment is complicated and the bonding requires high temperature and pressure. Although polymer bonding has low cost and low requirements for wafer surface flatness, it can fill some concave and convex morphologies on the wafer surface. However, because the high molecular components of the polymer itself are difficult to isolate the penetration of small molecules, it is easy to cause the cavity formed by it to have poor airtightness.
[0003] Figure 1 and Figure 2 It is a chip packaging structure after two polymers are bonded. Please refer to Figure 1 As shown, the chip packaging structure includes a chip 1, a cover plate 2, a cofferdam 3 and a glue bonding layer 4 disposed between the chip 1 and the cover plate 2. Since the cofferdam 3 and the glue bonding layer 4 are both polymers, the air tightness of the cavity enclosed by them is poor, wherein the arrows indicate the permeation path of the gas. Figure 1 It is to penetrate from the outside to the inside, of course, it can also penetrate from the inside to the outside. Please refer to Figure 2 As shown, the chip packaging structure includes a chip 1', a cover plate 2' and a glue bonding layer 4' disposed between the chip 1' and the cover plate 2'. Since the glue bonding layer 4' is a polymer, the air tightness of the cavity is poor, wherein the arrows indicate the permeation path of the gas. Figure 2 In order to penetrate from the outside to the inside, it is also possible to penetrate from the inside to the outside. Figure 2 In the structure, since the side wall of the cavity is part of the cover plate 2', the gas can only penetrate into the cavity through the glue bonding layer 4', so the airtightness is better than Figure 1 The structure is good.
[0004] However, the above chip packaging structure still has the problem of poor cavity airtightness.
[0005] The information disclosed in this background technology section is only intended to increase the understanding of the overall background of the present invention, and should not be regarded as acknowledging or suggesting in any form that the information constitutes the prior art already known to a person skilled in the art. Utility Model Content
[0006] The utility model aims to provide a chip packaging structure, which can improve the airtightness and reliability of the chip packaging structure packaged in a polymer bonding manner.
[0007] In order to achieve the above purpose, the technical solution provided by a specific embodiment of the utility model is as follows:
[0008] A chip packaging structure, comprising:
[0009] A chip has a first surface, wherein the first surface has a functional area and a first bonding area, and the first bonding area is arranged around the functional area;
[0010] A cover plate, disposed on the first surface of the chip, the cover plate having a second bonding area bonded to the first bonding area;
[0011] a glue bonding layer, disposed between the first bonding area and the second bonding area; and
[0012] An annular bump is arranged on the first bonding area and / or the second bonding area and is located in the glue bonding layer, and the functional area is located in the annular bump.
[0013] In one or more embodiments of the present invention, the height of the annular protrusion is not higher than the thickness of the glue bonding layer.
[0014] In one or more embodiments of the present invention, the width of the annular protrusion is not greater than the width of the glue bonding layer.
[0015] In one or more embodiments of the present invention, the annular protrusion is selected from a metal protrusion.
[0016] In one or more embodiments of the present invention, the number of the annular protrusions is one circle, the annular protrusions are arranged on the first bonding area, a gap is formed between the annular protrusions and the second bonding area, and the gap is filled with glue.
[0017] In one or more embodiments of the present invention, the number of the annular protrusions is one circle, the annular protrusions are arranged on the second bonding area, a gap is formed between the annular protrusions and the first bonding area, and the gap is filled with glue.
[0018] In one or more embodiments of the present invention, the number of the annular protrusions is multiple circles, and the multiple circles of annular protrusions are arranged on the first bonding area and distributed in concentric rings. A gap is formed between the annular protrusions and the second bonding area, and the gap is filled with glue.
[0019] In one or more embodiments of the present invention, the number of the annular protrusions is multiple circles, and the multiple circles of annular protrusions are arranged on the second bonding area and distributed in concentric rings. A gap is formed between the annular protrusions and the first bonding area, and the gap is filled with glue.
[0020] In one or more embodiments of the present invention, the number of the annular bumps is multiple circles, wherein some of the annular bumps are arranged on the first bonding area, and the remaining annular bumps are arranged on the second bonding area, and the annular bumps arranged on the first bonding area and the annular bumps arranged on the second bonding area are staggered or alternately staggered.
[0021] In one or more embodiments of the present invention, a groove is provided on the surface of the cover plate facing the chip, the groove is surrounded by the second bonding area, and the groove corresponds to and covers the functional area.
[0022] Compared with the prior art, the chip packaging structure of the present invention greatly delays the penetration of gas molecules into the functional area by setting an annular protrusion in the glue bonding layer, thereby improving the airtightness of the chip packaging structure and improving the reliability of the chip packaging structure.
[0023] Compared with a packaging structure formed by dielectric-free bonding and metal bonding, the chip packaging structure of the utility model has the advantages of low cost and simple process. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0025] Figure 1 It is a chip packaging structure in the prior art;
[0026] Figure 2 This is another chip packaging structure in the prior art.
[0027] Figure 3 The chip packaging structure in the first embodiment of the utility model;
[0028] Figure 4 This is a distribution diagram of the annular protrusions in the first embodiment of the utility model;
[0029] Figure 5 for Figure 3 A magnified view of part A;
[0030] Figure 6 It is a partial detail diagram of the chip packaging structure in the second embodiment of the utility model;
[0031] Figure 7 The chip packaging structure in the third embodiment of the present invention;
[0032] Figure 8 This is a distribution diagram of the annular protrusions in the third embodiment of the utility model;
[0033] Fig. 9 for Figure 7 A magnified view of part B;
[0034] Fig.10 It is a partial detail diagram of the chip packaging structure in the fourth embodiment of the utility model;
[0035] Fig.11 It is a partial detail diagram of the chip packaging structure in the fifth embodiment of the present utility model;
[0036] Fig.12 It is a partial detail diagram of the chip packaging structure in the sixth embodiment of the present invention;. DETAILED DESCRIPTION
[0037] In order to enable those skilled in the art to better understand the technical solutions in the present invention, the following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present invention.
[0038] As mentioned in the background technology, among the wafer-level airtight bonding methods, polymer bonding has the advantage of low cost compared to dielectric bonding and metal dielectric bonding. At the same time, because polymer bonding can fill some concave and convex morphologies on the wafer surface, the requirement for wafer surface flatness is also low. However, because the high molecular components of the polymer itself are difficult to isolate the penetration of small molecules, it is easy to cause the cavity formed by it to have poor airtightness, which in turn leads to low reliability of the chip packaging structure encapsulated by polymer bonding.
[0039] In order to solve the above technical problems, the utility model provides a chip packaging structure. By setting an annular protrusion in the glue bonding layer in the area where the cover plate and the chip are bonded, the penetration of gas molecules into the area where the chip functional area is located can be delayed, the airtightness of the chip packaging structure can be improved, and the reliability of the chip packaging structure can be improved.
[0040] The chip packaging structure of the utility model comprises a chip, a cover plate, a glue bonding layer and an annular bump. The chip has a first surface, the first surface has a functional area and a first bonding area, and the first bonding area is arranged around the functional area. The cover plate is arranged on the first surface of the chip, and the cover plate has a second bonding area bonded to the first bonding area. The glue bonding layer is arranged between the first bonding area and the second bonding area. And, the annular bump is arranged on the first bonding area and / or the second bonding area and is located in the glue bonding layer, and the functional area is located in the annular bump.
[0041] The chip packaging structure of the utility model can improve the air tightness and reliability of the chip packaging structure packaged in a polymer bonding manner by arranging an annular protrusion in the glue bonding layer.
[0042] refer to Figures 3 to 5 As shown, the chip packaging structure in the first embodiment of the present invention includes a chip 10 , a cover plate 20 , a glue bonding layer 30 and a circle of annular bumps 40 .
[0043] The chip 10 has a first surface 10 a . The first surface 10 a has a functional region X and a first bonding region Y. The first bonding region Y is disposed around the functional region X.
[0044] The cover plate 20 has a second surface 20a, the second surface 20a has a second bonding area Z, and a groove 21 surrounded by the second bonding area Z is formed on the second surface 20a. The second surface 20a of the cover plate 20 is arranged in contact with the first surface 10a of the chip 10, the groove 21 corresponds to and covers the functional area X, and the second bonding area Z is bonded to the first bonding area Y.
[0045] The glue bonding layer 30 is disposed between the first bonding area Y and the second bonding area Z.
[0046] A circle of annular bumps 40 is arranged on the first bonding area Y and is located in the glue bonding layer 30, and the functional area X is located in the annular bumps 40. Among them, the height of the annular bumps 40 is not higher than the thickness of the glue bonding layer 30, and the width of the annular bumps 40 is not greater than the width of the glue bonding layer 30. Exemplarily, a gap is formed between the annular bumps 40 and the second bonding area Z, and the gap is filled with glue (the glue bonding layer 30 is formed after the glue is cured). This is because, during bonding, due to the pressure and the fluidity of the glue, the glue in the annular bump 40 area is pushed out to the surroundings, and only a small thickness is retained.
[0047] In a preferred embodiment, the annular protrusion 40 is selected from a metal protrusion to further improve the airtightness.
[0048] The chip packaging structure in the second embodiment of the present invention is different from that in the first embodiment only in that the annular bump 40 is disposed at a different position.
[0049] refer to Figure 6 As shown, in the second embodiment, a circle of annular bumps 40 is disposed on the second bonding area Z. The height of the annular bumps 40 is not higher than the thickness of the glue bonding layer 30, and the width of the annular bumps 40 is not greater than the width of the glue bonding layer 30. Exemplarily, a gap is formed between the annular bumps 40 and the first bonding area Y, and the gap is filled with glue (the glue bonding layer 30 is formed after the glue is cured). This is because, during bonding, due to the pressure and the fluidity of the glue, the glue in the annular bump 40 area is pushed out to the surroundings, and only a small thickness is retained.
[0050] In a preferred embodiment, the annular protrusion 40 is selected from a metal protrusion to further improve the airtightness.
[0051] refer to Figures 7 to 9 As shown, the chip packaging structure in the third embodiment of the present invention includes a chip 10 , a cover plate 20 , a glue bonding layer 30 and three ring-shaped bumps 40 .
[0052] The chip 10 has a first surface 10 a . The first surface 10 a has a functional region X and a first bonding region Y. The first bonding region Y is disposed around the functional region X.
[0053] The cover plate 20 has a second surface 20a, the second surface 20a has a second bonding area Z, and a groove 21 surrounded by the second bonding area Z is formed on the second surface 20a. The second surface 20a of the cover plate 20 is arranged in contact with the first surface 10a of the chip 10, the groove 21 corresponds to and covers the functional area X, and the second bonding area Z is bonded to the first bonding area Y.
[0054] The glue bonding layer 30 is disposed between the first bonding area Y and the second bonding area Z.
[0055] Two circles of annular bumps 40 are both arranged on the first bonding area Y and located in the glue bonding layer 30. The two circles of annular bumps 40 are spaced apart in concentric rings, and the functional area X is located in the annular bumps 40. Another circle of annular bumps 40 is arranged on the second bonding area Z and located in the glue bonding layer 30. The annular bumps 40 arranged on the first bonding area Y and the annular bumps 40 arranged on the second bonding area Z are mutually staggered or alternately staggered.
[0056] Exemplarily, the annular bump 40 arranged on the second bonding area Z is located between the two circles of annular bumps 40 arranged on the first bonding area Y; or, the annular bump 40 arranged on the second bonding area Z is located on the periphery of the two circles of annular bumps 40 arranged on the first bonding area Y; or, the annular bump 40 arranged on the second bonding area Z is located inside the two circles of annular bumps 40 arranged on the first bonding area Y.
[0057] Among them, the height of each circle of annular bumps 40 is not higher than the thickness of the glue bonding layer 30, and the sum of the widths of multiple circles of annular bumps 40 is not greater than the width of the glue bonding layer 30. Exemplarily, a gap is formed between the annular bumps 40 arranged on the second bonding area Z and the first bonding area Y, and the gap is filled with glue (the glue bonding layer 30 is formed after the glue is cured); a gap is formed between the two circles of annular bumps 40 arranged on the first bonding area Y and the second bonding area Z, and the gap is filled with glue (the glue bonding layer 30 is formed after the glue is cured). This is because, during bonding, due to the pressure and the fluidity of the glue, the glue in the annular bump 40 area is pushed out to the surroundings, and only a small thickness is retained.
[0058] In a preferred embodiment, the annular protrusion 40 is selected from a metal protrusion to further improve the airtightness.
[0059] The chip packaging structure in the fourth embodiment of the present invention is different from that in the third embodiment only in that the annular bump 40 is disposed at a different position.
[0060] refer to Fig.10 As shown, in the fourth embodiment, two circles of annular bumps 40 are both arranged on the second bonding area Z and located in the glue bonding layer 30, and the two circles of annular bumps 40 are spaced apart in concentric rings. Another circle of annular bumps 40 is arranged on the first bonding area Y and located in the glue bonding layer 30. The annular bumps 40 arranged on the first bonding area Y and the annular bumps 40 arranged on the second bonding area Z are mutually staggered or alternately staggered.
[0061] In a preferred embodiment, the annular protrusion 40 is selected from a metal protrusion to further improve the airtightness.
[0062] In the third embodiment and the fourth embodiment, the annular protrusions are distributed in different bonding areas, and the annular protrusions on different bonding areas are staggered, which can further extend the penetration time of gas molecules.
[0063] The chip packaging structure in the fifth embodiment of the present invention is different from that in the third embodiment only in that the annular bump 40 is disposed at a different position.
[0064] refer to Fig.11As shown, in the fifth embodiment, three circles of annular bumps 40 are all arranged on the second bonding area Z and located in the glue bonding layer 30, and the three circles of annular bumps 40 are distributed in concentric rings. Among them, the height of each circle of annular bumps 40 is not higher than the thickness of the glue bonding layer 30, and the sum of the widths of multiple circles of annular bumps 40 is not greater than the width of the glue bonding layer 30. Exemplarily, a gap is formed between the multiple circles of annular bumps 40 and the first bonding area Y, and the gap is filled with glue (the glue bonding layer 30 is formed after the glue is cured). This is because, during bonding, due to the pressure and the fluidity of the glue, the glue in the annular bump 40 area is pushed out to the surroundings, and only a small thickness is retained.
[0065] In a preferred embodiment, the annular protrusion 40 is selected from a metal protrusion to further improve the airtightness.
[0066] The chip packaging structure in the sixth embodiment of the present invention is different from that in the third embodiment only in that the annular bump 40 is disposed at a different position.
[0067] refer to Fig.12 As shown, in the sixth embodiment, three circles of annular bumps 40 are all arranged on the first bonding area Y and located in the glue bonding layer 30, and the three circles of annular bumps 40 are distributed in concentric rings. Among them, the height of each circle of annular bumps 40 is not higher than the thickness of the glue bonding layer 30, and the sum of the widths of multiple circles of annular bumps 40 is not greater than the width of the glue bonding layer 30. Exemplarily, a gap is formed between the multiple circles of annular bumps 40 and the second bonding area Z, and the gap is filled with glue (the glue bonding layer 30 is formed after the glue is cured). This is because, during bonding, due to the pressure and the fluidity of the glue, the glue in the annular bump 40 area is pushed out to the surroundings, and only a small thickness is retained.
[0068] In a preferred embodiment, the annular protrusion 40 is selected from a metal protrusion to further improve the airtightness.
[0069] In the fifth and sixth embodiments described above, by providing multiple circles of annular protrusions, the penetration time of gas molecules can also be further prolonged.
[0070] The chip packaging structure of the present invention can be manufactured by the following process (taking three-circle annular bump as an example):
[0071] First, two circles of annular protrusions are made in the first bonding area of the chip. Then, a groove is etched on the cover plate and a circle of annular protrusions is made in the second bonding area. Next, glue is applied on the first bonding area of the chip or on the second bonding area of the cover plate, and the first bonding area of the chip is bonded to the second bonding area of the cover plate. Among them, the annular protrusions on the cover plate are located between the annular protrusions on the chip, and the grooves cover the functional area of the chip. Furthermore, the above structure is wafer thinned, and through holes, insulation layers, wiring, solder resists, solder balls are made, and finally the chip packaging is completed by cutting.
[0072] Compared with the prior art, the chip packaging structure of the present invention greatly delays the penetration of gas molecules into the functional area by setting an annular protrusion in the glue bonding layer, thereby improving the airtightness of the chip packaging structure and improving the reliability of the chip packaging structure.
[0073] Compared with a packaging structure formed by dielectric-free bonding and metal bonding, the chip packaging structure of the utility model has the advantages of low cost and simple process.
[0074] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.
[0075] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. A chip packaging structure, characterized in that: include: A chip has a first surface, wherein the first surface has a functional area and a first bonding area, and the first bonding area is arranged around the functional area; A cover plate, disposed on the first surface of the chip, the cover plate having a second bonding area bonded to the first bonding area; a glue bonding layer, disposed between the first bonding area and the second bonding area; and An annular bump is arranged on the first bonding area and / or the second bonding area and is located in the glue bonding layer, and the functional area is located in the annular bump.
2. The chip packaging structure according to claim 1, characterized in that: The height of the annular protrusion is not higher than the thickness of the glue bonding layer.
3. The chip packaging structure according to claim 1, characterized in that: The width of the annular protrusion is not greater than the width of the glue bonding layer.
4. The chip packaging structure according to claim 1, characterized in that: The annular bump is selected from metal bumps.
5. The chip packaging structure according to claim 1, characterized in that: The number of the annular bumps is one circle. The annular bumps are arranged on the first bonding area. A gap is formed between the annular bumps and the second bonding area. The gap is filled with glue.
6. The chip packaging structure according to claim 1, characterized in that: The number of the annular bumps is one circle. The annular bumps are arranged on the second bonding area. A gap is formed between the annular bumps and the first bonding area. The gap is filled with glue.
7. The chip packaging structure according to claim 1, characterized in that: The number of the annular protrusions is multiple, and the multiple circles of annular protrusions are arranged on the first bonding area and distributed in concentric rings. A gap is formed between the annular protrusions and the second bonding area, and the gap is filled with glue.
8. The chip packaging structure according to claim 1, characterized in that: The number of the annular protrusions is multiple, and the multiple circles of annular protrusions are arranged on the second bonding area and distributed in concentric rings. A gap is formed between the annular protrusions and the first bonding area, and the gap is filled with glue.
9. The chip packaging structure according to claim 1, characterized in that: The number of the annular bumps is multiple circles, wherein some of the annular bumps are arranged on the first bonding area, and the remaining annular bumps are arranged on the second bonding area, and the annular bumps arranged on the first bonding area and the annular bumps arranged on the second bonding area are staggered or alternately staggered.
10. The chip packaging structure according to claim 1, characterized in that: A groove is arranged on the surface of the cover plate facing the chip, the groove is surrounded by the second bonding area, and the groove corresponds to and covers the functional area.
Citation Information
Cited By
Semiconductor wafer level package method and package structure
WO2026041074A1