Wire insulating layer extrusion die

By designing the wire insulation layer extrusion mold with through-slots, the problem of insufficient pressure caused by improper matching of the inner and outer mold angles is solved, ensuring that the insulation rubber adheres to the conductor, preventing the insulation layer from shrinking, and improving the extrusion quality of the wire insulation layer.

CN221913177UActive Publication Date: 2024-10-29LTK INDS HUIZHOU +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323255802.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-11-30
Publication Date
2024-10-29
Estimated Expiration
2033-11-30

AI Technical Summary

Technical Problem

The angles of the inner and outer molds of the existing wire insulation layer extrusion mold are not properly matched, resulting in insufficient pressure, low adhesion of the insulation layer, and prone to problems such as insulation shrinkage and exposed conductors.

Method used

Design a wire insulation layer extrusion mold that includes an outer mold and an inner mold. The outer mold has a through slot along the axial direction. The through slot is composed of a straight section, a first cone section and a second cone section. The inner mold faces the end of the outer mold. The part is in the shape of a frustum. A gap is formed at the connection between the first cone segment and the second cone segment. The conductor passes through the center. The insulating compound flows into the gap from the second cone segment and adheres through the first cone segment. The straight-through segment ensures The glue adheres to the conductor.

Benefits of technology

It improves the adhesion of the insulating glue on the conductor, prevents the insulation layer from shrinking and exposing the conductor, and improves the extrusion quality of the wire insulation layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221913177U_ABST
    Figure CN221913177U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of wire processing die design, in particular to a wire insulating layer extrusion die. A through groove is formed in an outer mold in the axial direction, the through groove comprises a straight-through section, a first conical surface section and a second conical surface section which are sequentially connected, the appearance of the end, facing the outer mold, of an inner mold is in a frustum shape, and a gap is formed between the joint of the first conical surface section and the second conical surface section and the end of the inner mold. And the insulating rubber material flows to the gap from the second conical surface section and the outer peripheral surface of the inner mold and then enters the first conical surface section of the outer mold from the gap, so that the insulating rubber material coats the conductor, the pressure during extrusion is improved, the insulating rubber material is attached to the conductor through the straight-through section, and the conductor can be extruded by adjusting the structures of the outer mold and the inner mold. The insulating rubber material is attached to the conductor with a certain pressure to form an insulating layer, so that after the conductor and the insulating layer leave the outer mold and the inner mold, the condition that the insulating layer retracts to expose the conductor is prevented, and the extrusion quality of the wire insulating layer is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of wire processing die design, and in particular to a wire insulation layer extrusion die. Background Art

[0002] In the manufacturing of wires, an insulating layer is required to be attached to the surface of the wires to isolate the wires and prevent people from getting injured by electric shock. In the existing 8-2AWG polyvinyl chloride wire production insulation layer, the angles of the inner and outer molds of the extruder are improperly matched, resulting in insufficient pressure between the inner and outer molds during the extrusion process. After the insulation is extruded, the adhesion between the conductor and the insulation layer is relatively small, resulting in the phenomenon of insulation shrinkage and exposed conductors after processing and use. Utility Model Content

[0003] In order to solve the above technical problems, the present application provides an electric wire insulation layer extrusion mold, including an outer mold and an inner mold, the outer mold is provided with a through groove along the axial direction, the through groove includes a straight section, a first conical section and a second conical section connected in sequence, the outer shape of the inner mold facing one end of the outer mold is in the shape of a cone, and the connection between the first conical section and the second conical section forms a gap with the end of the inner mold.

[0004] Preferably, the inner mold is provided with an inner wire outlet and a feed inlet along the axial direction, and the inner wire outlet and the feed inlet are connected to each other.

[0005] Preferably, the length of the straight-through section is 2 mm.

[0006] Preferably, the angle of the first conical surface segment is 6°.

[0007] Preferably, the angle of the second conical surface segment is 42-45°.

[0008] Preferably, a first mounting block is provided on the outer side surface of the inner mold.

[0009] Preferably, a second mounting block is provided on the end surface of the inner mold away from the outer mold.

[0010] Preferably, a recessed groove is provided on the end surface of the outer mold close to the straight-through section.

[0011] As can be seen from the above, the following beneficial effects can be obtained by applying the present application: the present application provides a through slot in the axial direction of the outer mold, the through slot includes a straight-through section, a first conical section and a second conical section connected in sequence, the outer shape of the inner mold facing the outer mold is in the shape of a cone, a gap is formed between the connection of the first conical section and the second conical section and the end of the inner mold, and the end of the inner mold is outside the first conical section. The wire conductor passes through the center of the outer mold and the inner mold, and then the insulating rubber flows from the second conical section and the outer peripheral surface of the inner mold to the gap, and then enters the first conical section of the outer mold from the gap, so that the insulating rubber is coated on the conductor, the pressure during extrusion is increased, and then the insulating rubber adheres to the conductor through the straight-through section. By adjusting the structure of the outer mold and the inner mold, the insulating rubber adheres to the conductor with a certain pressure to form an insulating layer, and then after the conductor and the insulating layer leave the outer mold and the inner mold, the situation of the insulating layer shrinking and exposing the bare conductor is prevented, thereby improving the extrusion quality of the wire insulating layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] In order to more clearly illustrate the technical solutions in the embodiments of the present application or the prior art, the drawings required for use in the description of the embodiments of the present application or the prior art are briefly introduced below. Obviously, the drawings described below are only part of the embodiments of the present application, and for ordinary technicians in this field, other drawings can be obtained based on these drawings without creative labor.

[0013] Figure 1 This is a schematic diagram of the structure of the wire insulation layer extrusion mold according to an embodiment of the present application. DETAILED DESCRIPTION

[0014] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0015] Example

[0016] In order to solve the above technical problems, this embodiment provides a wire insulation layer extrusion die, such as Figure 1As shown, it includes an outer mold 10 and an inner mold 20. The outer mold 10 is provided with a through groove along the axial direction. The through groove includes a straight section 11, a first conical section 12 and a second conical section 13 connected in sequence. The outer shape of the inner mold 20 facing one end of the outer mold 10 is in the shape of a frustum. A gap is formed between the connection between the first conical section 12 and the second conical section 13 and the end of the inner mold 20, and the end of the inner mold 20 is outside the first conical section 12. The wire conductor passes through the center of the outer mold 10 and the inner mold 20, and then the insulating rubber flows from the second conical section 13 and the outer peripheral surface of the inner mold 20 to the gap, and then enters the first conical section 12 of the outer mold 10 from the gap, so that the insulating rubber is coated on the conductor, increasing the pressure during extrusion, and then passes through the straight section 11 so that the insulating rubber adheres to the conductor. By adjusting the structure of the outer mold 10 and the inner mold 20, the insulating rubber adheres to the conductor with a certain pressure to form an insulating layer, and then after the conductor and the insulating layer leave the outer mold 10 and the inner mold 20, the situation of the insulating layer shrinking and exposing the conductor is prevented, thereby improving the extrusion quality of the wire insulation layer.

[0017] Furthermore, the angle of the second conical surface segment 13 is 42-45°, preferably, the angle of the second conical surface segment 13 is 45°, the angle of the first conical surface segment 12 is 6°, the outer shape of the end of the inner mold 20 facing the outer mold 10 is in the shape of a cone, and the end of the inner mold 20 in the shape of a cone is outside the first conical surface segment 12, preferably, the plane where the connection between the first conical surface segment 12 and the second conical surface segment 13 is located is in the same vertical plane as the end face of the inner mold 20, and then after the insulating rubber flows into the first conical surface segment 12 from the gap between the connection between the first conical surface segment 12 and the second conical surface segment 13 and the end of the inner mold 20, the second conical surface segment 13 and the first conical surface segment 12 cooperate with the inner mold 20 to increase the extrusion pressure, so that the insulating rubber adheres to the conductor.

[0018] Furthermore, the length of the straight-through section 11 is 2-4 mm. When the insulating rubber and the conductor pass through the straight-through section 11, the straight-through section 11 allows the insulating rubber to further adhere to the conductor.

[0019] Furthermore, the inner mold 20 is axially provided with an inner wire outlet 21 and a feed port 22 , which are interconnected. The conductor enters from the feed port 22 , and then passes through the inner wire outlet 21 and enters the first conical surface section 12 of the outer mold 10 .

[0020] A first mounting block 23 is provided on the outer side of the inner mold 20. A second mounting block 24 is provided on the end face of the inner mold 20 away from the outer mold 10. Exemplarily, an external thread is formed on the surface of the second mounting block 24, so that the second mounting block 24 can be installed on the extruder. At the same time, during installation, the first mounting block 23 is used for positioning to improve the accuracy of the position between the inner mold 20 and the outer mold 10. A sink groove 14 is provided on the end face of the outer mold 10 close to the straight-through section 11, so that when the outer mold 10 is installed on the extruder, the outer mold 10 can be positioned through the sink groove 14, thereby improving the accuracy of the position between the inner mold 20 and the outer mold 10, so that the inner mold 20 and the outer mold 10 are accurately matched.

[0021] In summary, the present application scheme is to open a through groove in the axial direction of the outer mold, and the through groove includes a straight-through section, a first conical section and a second conical section connected in sequence, and the outer shape of the inner mold facing the outer mold is in the shape of a cone, and a gap is formed between the connection of the first conical section and the second conical section and the end of the inner mold, and the end of the inner mold is outside the first conical section. The wire conductor passes through the center of the outer mold and the inner mold, and then the insulating rubber flows from the second conical section and the outer peripheral surface of the inner mold to the gap, and then enters the first conical section of the outer mold from the gap, so that the insulating rubber is coated on the conductor, increasing the pressure during extrusion, and then passing through the straight-through section so that the insulating rubber adheres to the conductor. By adjusting the structure of the outer mold and the inner mold, the insulating rubber adheres to the conductor with a certain pressure to form an insulating layer, and then after the conductor and the insulating layer leave the outer mold and the inner mold, the situation of the insulating layer shrinking and exposing the bare conductor is prevented, thereby improving the extrusion quality of the insulating layer of the wire.

[0022] The above-described implementation methods do not constitute a limitation on the protection scope of the technical solution. Any modification, equivalent replacement and improvement made within the spirit and principle of the above-described implementation methods shall be included in the protection scope of the technical solution.

Claims

1. A wire insulation layer extrusion die, characterized in that: The invention comprises an outer mold (10) and an inner mold (20), wherein the outer mold (10) is provided with a through groove along the axial direction, wherein the through groove comprises a straight section (11), a first conical section (12) and a second conical section (13) connected in sequence, and the outer shape of the inner mold (20) facing one end of the outer mold (10) is in the shape of a frustum, and the end of the inner mold (20) is located outside the first conical section (12), and a gap is formed between the connection between the first conical section (12) and the second conical section (13) and the end of the inner mold (20).

2. The wire insulation layer extrusion die according to claim 1, characterized in that: The inner mold (20) is provided with an inner wire outlet (21) and a material inlet (22) along the axial direction, and the inner wire outlet (21) and the material inlet (22) are communicated with each other.

3. The wire insulation layer extrusion die according to claim 1, characterized in that: The length of the straight-through section (11) is 2-4 mm.

4. The wire insulation layer extrusion die according to claim 2, characterized in that: The angle of the first conical surface segment (12) is 6°.

5. The wire insulation layer extrusion die according to claim 2, characterized in that: The angle of the second conical surface section (13) is 42-45°.

6. The wire insulation layer extrusion die according to claim 1, characterized in that: A first mounting block (23) is provided on the outer side surface of the inner mold (20).

7. The wire insulation layer extrusion die according to claim 1, characterized in that: A second mounting block (24) is provided on the end surface of the inner mold (20) away from the outer mold (10).