CFG etching device

By using the built-in electric heating element of the metal liner in the CFG etching device to accelerate the etching of the middle thinning area, the problems of complex processes and large tape consumables in the existing technology are solved, CFG preparation of uniform thickness is achieved, and the yield of finished products is improved. and user experience.

CN221917812UActive Publication Date: 2024-10-29CHENGDU TOMI SHUANG DU OPTOELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323540274.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-25
Publication Date
2024-10-29
Estimated Expiration
2033-12-25

AI Technical Summary

Technical Problem

The existing CFG production process is complex, and the tape consumables are large and easy to fall off, resulting in poor etching and thickness differences, affecting the finished product yield and user experience.

Method used

A metal lining plate is used with a built-in electric heating element in the middle thinned area. The etching is accelerated by heating to achieve CFG preparation with a thin middle and thick ends, simplifying the process and reducing the use of tape.

Benefits of technology

It solves the thickness gap problem, improves the yield of finished products, avoids bad etching caused by acid seepage at the edge of the tape, simplifies the process and saves tape consumables.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221917812U_ABST
    Figure CN221917812U_ABST
Patent Text Reader

Abstract

The utility model discloses a CFG etching device which comprises a metal lining plate for bearing glass to be etched, a mounting hole arranged on the side surface of the metal lining plate, an electric heating element and a temperature sensor which are arranged in the mounting hole, a plugging piece arranged on the mounting hole, and a temperature controller electrically connected with the electric heating element and the temperature sensor, wherein the electric heating element and the temperature sensor which are arranged in the mounting hole correspond to the middle thinning area of the glass to be etched. According to the utility model, the CFG etching process is improved through the structural design, the etching process of the middle thinned area is promoted by heating, the surface of the etched glass presents a uniform gentle slope without mutation, the problem of thickness offset in the traditional process is solved, the use process of the adhesive tape in the etching process is reduced, the production cost is reduced, and the production efficiency is improved. The cost of adhesive tape consumables is saved, the technological process is simplified, and the problem of poor etching caused by acid seepage of the edge of the adhesive tape in the traditional process is effectively solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a CFG (Center Folded Glass, center bendable glass) preparation device, in particular to a CFG etching device. Background Art

[0002] With the development of display technology, the performance requirements for the screen in display devices are gradually increasing. And with the expansion of application scenarios, ultra-thin glass-based flexible display panels can be applied to foldable mobile phones, laptops and various curled display devices.

[0003] Foldable glass is divided into two categories: overall bendable glass UTG and center bendable glass CFG. UTG is thin overall due to the overall thinning process, and has poor impact resistance. It is easily damaged when impacted by external forces. The impact resistance can only be improved by film or coating. If the film is applied, the middle part is prone to whitening after too many bends. If the coating method is used, the improvement in impact resistance is average. Both methods cause the UTG surface to have plastic characteristics, poor touch, and poor wear resistance. CFG is thick on both sides and thin in the middle. It has better overall impact resistance than UTG and is not easy to break. It can be used directly as the outer layer of the screen without film. It has good touch and scratch resistance, and there is no whitening when bent.

[0004] The production process of CFG is mainly to thin the middle part of the glass, which is roughly as follows: firstly, a large plate glass 11 of standard thickness (generally 400um) is attached to a plastic liner 12, and the non-bending area 13 is protected by tape, and the bending area 14 is exposed. Figure 1 As shown; then the glass together with the plastic liner is placed in the etching solution for middle etching, and the bending area is etched to a specified thickness (generally 40-100um) according to the etching time and the etching solution concentration; then the large plate of glass is removed, cleaned, and placed in hydrofluoric acid for overall etching to the required thickness, and then the glass is cut into specified sizes by laser cutting; finally, the required CFG (generally 70-130um at both ends and 20-50um in the middle) is obtained after cleaning and strengthening.

[0005] The above-mentioned CFG production process has the following problems: First, the production process is relatively complicated, and it is necessary to stick tape over a large area before etching, and the tape needs to be torn off after etching, resulting in a large amount of tape consumables; secondly, the edges of the tape sometimes fall off after being soaked in hydrofluoric acid, causing poor etching and resulting in low yield of finished products; and because the tape-protected position cannot be etched, after etching the exposed position, a thickness difference will occur between the two positions, and after subsequent coating, light and shadow will appear due to the difference in refractive index, affecting the user experience. Utility Model Content

[0006] In view of the problems existing in the above-mentioned prior art, the utility model provides a CFG etching device, which adopts a metal lining plate and has a built-in electric heating element in the middle thinning area. When etching a large plate of glass as a whole, the etching of the middle thinning area is accelerated by heating, thereby obtaining a CFG that is thin in the middle and thick at both ends.

[0007] In order to achieve the above purpose, the technical solution adopted by the utility model is as follows:

[0008] A CFG etching device comprises a metal lining plate made of a hydrofluoric acid resistant material, a mounting hole arranged on the side of the metal lining plate, an electric heating element and a temperature sensor arranged in the mounting hole, a plugging piece arranged at the opening of the mounting hole on the metal lining plate, and a temperature controller electrically connected to the electric heating element and the temperature sensor, wherein the metal lining plate is used to carry glass to be etched, and the electric heating element and the temperature sensor arranged in the mounting hole correspond to the middle thinning area of ​​the glass to be etched.

[0009] Specifically, the upper surface of the metal backing plate used for supporting the glass to be etched is coated with a flexible thermally conductive polyurethane coating, which avoids rigid contact between the glass and the metal backing plate while maintaining thermal conductivity.

[0010] Specifically, the four sides and the back of the metal lining plate are coated with an anti-corrosion coating to protect the metal lining plate. The anti-corrosion coating can be an epoxy or unsaturated polyester coating.

[0011] Specifically, the four sides and the back of the metal lining are provided with tightly fitting anti-corrosion frames to protect the metal lining, and the anti-corrosion frames can be made of plastic material.

[0012] Specifically, the metal backing plate is also provided with an anti-corrosion clamp for clamping the glass to be etched.

[0013] Specifically, the electric heating element is configured as a long U-shaped electric heating wire, the long side of which matches the length of the middle thinning area of ​​the glass to be etched, and a long temperature sensor is placed between the two long sides of the U-shaped electric heating wire to improve the accuracy of temperature detection feedback.

[0014] Specifically, the mounting hole is filled with potting glue, so that the electric heating element and the temperature sensor are spaced apart from the metal lining plate, so as to protect the electric heating element and the temperature sensor and transfer heat evenly to the metal lining plate.

[0015] Furthermore, a plurality of mounting holes are arranged side by side on the metal lining plate, and an electric heating element and a temperature sensor are placed in each mounting hole and sealed with a blocking member. The temperature controller can be configured for independent control or unified control.

[0016] Compared with the prior art, the utility model has the following beneficial effects:

[0017] The utility model improves the CFG etching process through structural design, and uses heating to promote the etching process of the middle thinning area, so as to achieve the effect of different etching thicknesses in different areas. At the same time, since the temperature from the direct heating area to the non-heating area changes linearly, the etching thickness from the middle thinning area to the two side areas changes linearly. After the glass is etched, the surface presents a uniform gentle slope without mutation, which solves the thickness difference problem in the traditional process and ensures that there is no light and shadow after the CFG coating is applied. In addition, the use of the utility model simplifies the use of the tape in the etching process, saves the cost of tape consumables, simplifies the process flow, and effectively solves the problem of poor etching caused by acid seepage at the edge of the tape in the traditional process. The utility model is simple and ingenious in design, easy to use, low in cost, and suitable for application in CFG preparation. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of the structure after sticking tape on the glass surface in the existing etching process.

[0019] Figure 2 It is a schematic diagram of the overall structure of an embodiment of the utility model.

[0020] Figure 3 This is a circuit principle block diagram of an embodiment of the utility model.

[0021] Figure 4 It is a schematic diagram of the cross-sectional structure of the metal lining plate part in the embodiment of the utility model.

[0022] In the above drawings, the component names corresponding to the reference numerals are as follows:

[0023] 1-metal lining, 2-electric heating element, 3-temperature sensor, 4-temperature controller, 5-mounting hole, 6-sealing piece, 7-potting glue, 8-flexible thermal conductive polyurethane coating, 9-anti-corrosion coating, 10-anti-corrosion frame, 11-large plate glass, 12-plastic lining, 13-non-bending area, 14-bending area. DETAILED DESCRIPTION

[0024] The present invention is further described below in conjunction with the accompanying drawings and embodiments. The implementation methods of the present invention include but are not limited to the following embodiments.

[0025] Example

[0026] like Figures 2 to 4As shown, the CFG etching device mainly includes components such as a metal lining plate 1, an electric heating element 2, a temperature sensor 3 and a temperature controller 4. Among them, the metal lining plate 1 is made of hydrofluoric acid resistant materials such as copper-nickel alloy and monel alloy, and is used to carry the glass to be etched and conduct heat transfer; the metal lining plate is provided with a mounting hole 5 from one side to the opposite side, which is used to place the electric heating element 2 and the temperature sensor 3. The length of the mounting hole 5 and the electric heating element 2 and the temperature sensor 3 placed therein in this direction are matched with the middle thinning area of ​​the glass to be etched to ensure that the direct heating position and the temperature detection position are both corresponding to the middle thinning area. The mounting hole 5 can be a through hole or a blind hole, which can be directly cast or opened separately. The two end openings or the single end opening of the mounting hole 5 are provided with a plugging piece 6 to protect the components in the hole. The mounting hole can also be filled with potting glue 7 to protect and fix the electric heating element and the temperature sensor, and keep the electric heating element and the temperature sensor spaced from the metal lining to ensure that the heat is evenly transferred to the upper surface of the metal lining. The connecting wires of the electric heating element and the temperature sensor extend through the plugging piece to the outside to connect to the external temperature controller, and the surface of the wire can also be provided with an anti-corrosion coating. After the temperature controller 4 is powered on, it controls the electric heating element 2 to heat to the process set temperature, such as 30-50°C. The temperature sensor 3 is used to detect the temperature of the metal lining part close to the electric heating element and feed it back to the temperature controller for temperature calibration and compensation. The electric heating element 2 can specifically adopt a long U-shaped electric heating wire, the long side of which matches the length of the middle thinning area of ​​the glass to be etched, and the long strip temperature sensor is placed between the two long sides of the U-shaped electric heating wire. In this embodiment, the electric heating elements 2 and the temperature sensors 3 are configured into three groups, and the corresponding mounting holes 5 are set as three parallel ones, so that three different designated areas on the large plate glass can be etched at the same time. After the etching process, the large plate glass can be cut to obtain multiple groups of CFG, thereby improving the preparation efficiency.

[0027] Furthermore, the upper surface of the metal lining plate 1 for supporting the glass to be etched is coated with a flexible thermally conductive polyurethane coating 8, which prevents the glass from rigidly contacting the metal lining plate while maintaining thermal conductivity. The four sides and the back of the metal lining plate 1 are coated with an anti-corrosion coating 9 or a tightly fitting anti-corrosion frame 10 is provided to protect the metal lining plate. The anti-corrosion coating 9 and the anti-corrosion frame 10 can also be configured at the same time, wherein the anti-corrosion coating can be epoxy or unsaturated polyester coating, and the anti-corrosion frame can be made of plastic materials such as PPS, PS, etc.

[0028] In order to facilitate the process, an anti-corrosion clamp for clamping the glass to be etched on the metal backing plate can also be configured.

[0029] The CFG etching process of the utility model is as follows:

[0030] First, a large glass plate with a thickness of 400um is tightly attached to the metal lining plate, and anti-corrosion clamps are used to clamp the metal lining plate on all sides. Then, the temperature controller is turned on. When the temperature stabilizes, the glass and the metal lining plate are placed in the etching solution for etching. Due to the heating effect of the electric heating element, the closer the glass temperature is to the electric heating element, the closer it is to the set temperature, and the faster it is etched. The etching depth of the glass surface is controlled by controlling parameters such as etching temperature, etching time, and etching solution concentration to 40-100um.

[0031] After etching, remove the glass, clean it, and then put it into the etching solution for overall etching until the glass thickness in the non-bending area is 70-130um. At this time, the glass thickness in the bending area is 20-50um. Then use laser cutting to cut the glass into specified sizes. Finally, after cleaning and strengthening, you can get the middle bendable glass CFG with a thickness of 70-130um at both ends and 20-50um in the middle.

[0032] The above embodiments are only preferred embodiments of the present utility model and are not intended to limit the protection scope of the present utility model. Any changes that adopt the design principles of the present utility model and are made through non-creative labor on this basis should fall within the protection scope of the present utility model.

Claims

1. A CFG etching device, characterized in that: The invention comprises a metal lining plate (1) made of a hydrofluoric acid resistant material, a mounting hole (5) arranged on the side of the metal lining plate (1), an electric heating element (2) and a temperature sensor (3) arranged in the mounting hole (5), a blocking member (6) arranged at the opening of the mounting hole (5) on the metal lining plate (1), and a temperature controller (4) electrically connected to the electric heating element (2) and the temperature sensor (3), wherein the metal lining plate (1) is used to carry glass to be etched, and the electric heating element (2) and the temperature sensor (3) arranged in the mounting hole (5) correspond to the middle thinning area of ​​the glass to be etched.

2. The CFG etching device according to claim 1, characterized in that: The upper surface of the metal lining plate (1) used for supporting the glass to be etched is coated with a flexible heat-conductive polyurethane coating (8).

3. The CFG etching device according to claim 1, characterized in that: The four sides and the back of the metal lining plate (1) are coated with an anti-corrosion coating (9).

4. The CFG etching device according to claim 1, characterized in that: The four side surfaces and the back surface of the metal lining plate (1) are provided with tightly fitting anti-corrosion frames (10).

5. The CFG etching device according to claim 1, characterized in that: The metal lining plate (1) is also provided with an anti-corrosion clamp for clamping the glass to be etched.

6. The CFG etching device according to any one of claims 1 to 5, characterized in that: The electric heating element (2) is configured as a long U-shaped electric heating wire, the long side of which matches the length of the middle thinning area of ​​the glass to be etched, and the long temperature sensor (3) is arranged between the two long sides of the U-shaped electric heating wire.

7. The CFG etching device according to claim 6, characterized in that: The mounting hole (5) is filled with potting glue (7) so that the electric heating element (2) and the temperature sensor (3) are spaced apart from the metal lining plate (1).

8. The CFG etching device according to any one of claims 1 to 5, characterized in that: A plurality of mounting holes (5) are arranged side by side on the metal lining plate (1), and each mounting hole (5) is provided with an electric heating element (2) and a temperature sensor (3) and is sealed with a blocking member (6).