Test structure for vertical cavity surface emitting laser

By designing a test structure including a first ohmic contact layer, a first reflector layer, an active layer, an oxidation confinement layer and a second reflector layer in a vertical cavity surface emitting laser, two photolithography steps were used to obtain the lateral oxide portion and The flow-blocking part solves the problem of low efficiency in evaluating the photoelectric characteristics of epitaxial wafers in the existing technology, and realizes fast and efficient evaluation of the photoelectric characteristics.

CN221928883UActive Publication Date: 2024-10-29ZHEJIANG BERXEL PHOTONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420286186.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-06
Publication Date
2024-10-29
Estimated Expiration
2034-02-06

AI Technical Summary

Technical Problem

The manufacturing process of vertical cavity surface emitting lasers requires 7-10 photolithography steps and multiple passivation layers, resulting in low efficiency in evaluating the photoelectric properties of epitaxial wafers and affecting processing time.

Method used

A test structure is provided, including a stacked first ohmic contact layer, a first reflector layer, an active layer, an oxidation confinement layer, a second reflector layer and a second ohmic contact layer, with lateral oxidation obtained by two photolithography steps The second ohmic contact layer is located in the blocking part and surrounds the emission hole, which is suitable for quickly evaluating the optoelectronic characteristics of the epitaxial wafer.

Benefits of technology

The lateral oxidation part and the large-area second ohmic contact layer are quickly obtained through two photolithography steps, which improves the efficiency of evaluating the photoelectric properties of the epitaxial wafer and significantly shortens the processing time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221928883U_ABST
    Figure CN221928883U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of photoelectric testing, and provides a testing structure for a vertical cavity surface emitting laser. The test structure comprises a first ohmic contact layer, a first reflector layer, an active layer, an oxidation limiting layer, a second reflector layer and a second ohmic contact layer which are stacked, the first reflector layer is an N-type Bragg reflector layer, the second reflector layer is a P-type Bragg reflector layer, and a detection area is arranged on the second ohmic contact layer; a transverse oxidation part and a flow blocking part surrounding the transverse oxidation part are distributed around the emission hole of the oxidation limiting layer; the second ohmic contact layer is located in a closed ring formed by the flow blocking part, at least surrounds a part of the emission hole and does not cover the transverse oxidation part. By adopting the test structure disclosed by the invention, the photoelectric characteristics of the epitaxial wafer can be efficiently evaluated, and the processing efficiency is greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure generally relates to the field of optoelectronic testing technology, and more particularly to a testing structure for vertical cavity surface emitting lasers. Background Art

[0002] Over the years, many advances have been made in the manufacturing process of Vertical Cavity Surface Emitting Laser (VCSEL), such as the development of optimized processes for various applications such as LiDAR, 3D sensing and high-speed optical interconnects to achieve a balance between optimal performance, device reliability and low cost.

[0003] At present, the manufacturing process of vertical cavity surface emitting lasers in related technologies requires 7-10 lithography steps and the deposition of multiple passivation layers, which consumes several weeks of processing time and seriously affects the efficiency of evaluating the optoelectronic properties of laser epitaxial wafers. Utility Model Content

[0004] In view of the above-mentioned defects or deficiencies in the related art, it is desirable to provide a test structure for a vertical cavity surface emitting laser, which can quickly evaluate the optoelectronic characteristics of an epitaxial wafer and improve processing efficiency.

[0005] The present disclosure provides a test structure for a vertical cavity surface emitting laser, the test structure comprising a first ohmic contact layer, a first reflector layer, an active layer, an oxidation restriction layer, a second reflector layer and a second ohmic contact layer which are stacked, the first reflector layer is an N-type Bragg reflector layer, the second reflector layer is a P-type Bragg reflector layer, and a detection area is arranged on the second ohmic contact layer;

[0006] A lateral oxidation portion and a blocking portion surrounding the lateral oxidation portion are distributed around the emission hole of the oxidation restriction layer; the second ohmic contact layer is located in a closed circle formed by the blocking portion, and surrounds at least a portion of the emission hole without covering the lateral oxidation portion.

[0007] Optionally, the distance between the second ohmic contact layer and the emission hole ranges from 1 μm to 5 μm.

[0008] Optionally, the first ohmic contact layer is an N-type contact layer, and the second ohmic contact layer is a P-type contact layer.

[0009] Optionally, the distance between the lateral oxidation portion and the flow blocking portion is at most twice the lateral oxidation distance.

[0010] Optionally, along a direction perpendicular to the emitted light, a cross-sectional shape of the lateral oxidation portion includes at least one of a straight line segment and a curved line segment.

[0011] Optionally, the flow blocking portion is an annular groove or an annular table.

[0012] Optionally, the diameter of the detection area ranges from 10 μm to 60 μm.

[0013] Optionally, the active layer is a single quantum well layer or a multi-quantum well layer.

[0014] It can be seen from the above technical solutions that the embodiments of the present disclosure have the following advantages:

[0015] The disclosed embodiment provides a test structure for a vertical cavity surface emitting laser, which can quickly obtain a lateral oxidation portion and a blocking portion for lateral oxidation and a large-area second ohmic contact layer that is convenient for direct detection by a standard wafer-level testing machine through two photolithography steps. The manufactured test structure can then be used to efficiently evaluate the optoelectronic properties of an epitaxial wafer, thereby greatly improving processing efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Other features, objects and advantages of the present disclosure will become more apparent from the detailed description of non-limiting embodiments made with reference to the following drawings:

[0017] Figure 1 A schematic diagram of a side view of a test structure for a vertical cavity surface emitting laser provided in an embodiment of the present disclosure;

[0018] Figure 2 A schematic diagram of a top view of a test structure for a vertical cavity surface emitting laser provided in an embodiment of the present disclosure;

[0019] Figure 3 A schematic top view of another test structure for a vertical cavity surface emitting laser provided in an embodiment of the present disclosure;

[0020] Figure 4 A schematic diagram of a lateral oxidation process provided in an embodiment of the present disclosure, wherein Figure 4 (a) is a schematic diagram of the top view of the structure when the lateral oxidation is 5 μm. Figure 4 (b) is a schematic diagram showing the top view of the structure when the lateral oxidation is 10 μm, and Figure 4 (c) Schematic diagram of the top view of the structure when the lateral oxidation is 15 μm;

[0021] Figure 5 A top view schematic diagram of another test structure for a vertical cavity surface emitting laser provided in an embodiment of the present disclosure, wherein Figure 5 (a) is a schematic diagram showing a top view of a structure having an annular groove, and Figure 5 (b) is a schematic diagram showing a top view of a structure having an annular table;

[0022] Figure 6 A basic flow chart of a test structure manufacturing method provided by an embodiment of the present disclosure;

[0023] Figure 7 A specific example of a test structure manufacturing method provided in an embodiment of the present disclosure.

[0024] Reference numerals:

[0025] 10 - test structure, 101 - first ohmic contact layer, 102 - first reflector layer, 103 - active layer, 104 - oxidation restriction layer, 1041 - emission hole, 1042 - lateral oxidation part, 1043 - blocking part, 105 - second reflector layer, 1051 - detection area, 106 - second ohmic contact layer. DETAILED DESCRIPTION

[0026] In order to enable those skilled in the art to better understand the disclosed solution, the technical solution in the disclosed embodiment will be clearly and completely described below in conjunction with the drawings in the disclosed embodiment. Obviously, the described embodiment is only a part of the disclosed embodiment, not all of the embodiments. Based on the embodiments in the disclosed embodiment, all other embodiments obtained by ordinary technicians in the field without creative work are within the scope of protection of the disclosed embodiment.

[0027] The terms "first", "second", "third", "fourth", etc. (if any) in the specification and claims of the present disclosure and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the numbers used in this way can be interchanged where appropriate, so that the embodiments of the present disclosure described can be implemented in sequences other than those illustrated or described herein.

[0028] In addition, the terms "include" and "have" and any variations thereof are intended to cover non-exclusive inclusions. For example, a process, method, system, product, or apparatus that includes a series of steps or modules is not necessarily limited to those steps or modules explicitly listed, but may include other steps or modules not explicitly listed or inherent to these processes, methods, products, or apparatuses.

[0029] For ease of understanding and explanation, the following Figures 1 to 7 The test structure for a vertical cavity surface emitting laser and the manufacturing method thereof provided by the embodiments of the present disclosure are described in detail.

[0030] Please refer to Figure 1, which is a side view schematic diagram of a test structure for a vertical cavity surface emitting laser provided by an embodiment of the present disclosure, wherein the test structure 10 comprises a first ohmic contact layer 101, a first reflector layer 102, an active layer 103, an oxidation restriction layer 104, a second reflector layer 105 and a second ohmic contact layer 106 which are stacked. Figure 2 As shown, a lateral oxidation portion 1042 and a blocking portion 1043 surrounding the lateral oxidation portion 1042 are distributed around the emission hole 1041 of the oxidation restriction layer 104, and a detection area 1051 is arranged on the second ohmic contact layer 105. The second ohmic contact layer 106 is located in a closed circle formed by the blocking portion 1043, and surrounds at least a part of the emission hole 1041 and does not cover the lateral oxidation portion 1042.

[0031] It should be noted that the size of the lateral current and light field limiting emission aperture in the vertical cavity surface emitting laser depends on the overall performance design of the device, which will affect key parameters such as the threshold current and peak power of the device. The vertical cavity surface emitting laser of the embodiment of the present disclosure includes but is not limited to the top emission structure and the bottom emission structure, etc., which are not limited to this, wherein the first ohmic contact layer 101 in the top emission structure is below the substrate layer, the first reflector layer 102, the active layer 103, the oxidation restriction layer 104, the second reflector layer 105, the second ohmic contact layer 106 and the passivation layer are stacked in sequence above the substrate layer, and the first ohmic contact layer 101 and the passivation layer in the bottom emission structure are below the substrate layer, and the first reflector layer 102, the active layer 103, the oxidation restriction layer 104, the second reflector layer 105 and the second ohmic contact layer 106 are stacked in sequence above the substrate layer. In addition, since the test structure 10 of the embodiment of the present disclosure can quickly evaluate the optoelectronic characteristics of the vertical cavity surface emitting laser epitaxial wafer to be manufactured, the test structure 10 is not a complete vertical cavity surface emitting laser structure.

[0032] For example, in the embodiment of the present disclosure, the distance between the second ohmic contact layer 106 and the emission hole 1041 ranges from 1 μm to 5 μm, and can further be 1.5 μm to 2.2 μm, so that the second ohmic contact layer 106 can be closer to the emission hole 1041 without blocking the emission hole 1041, and limit the resistance caused by the lateral current diffusing from the second ohmic contact layer 106 to the center of the device. For example, in the embodiment of the present disclosure, the first ohmic contact layer 101 can be an N-type contact layer, and the second ohmic contact layer 106 can be a P-type contact layer. For gallium arsenide (GaAs) devices, the P-type contact layer is usually Ti / Au or Ti / Pt / Au, and is deposited by evaporation or sputtering. In addition, compared to Figure 2 The second ohmic contact layer 106 is a complete ring-shaped layer. Figure 3The blank areas are interconnected and not covered by the P-type contact layer, thereby facilitating a lift-off process for the P-type contact layer. Meanwhile, the P-type contact layer can uniformly surround the emission hole 1041 from most sides.

[0033] For another example, in the embodiment of the present disclosure, the distance between the lateral oxidation portion 1042 and the flow blocking portion 1043 is at most twice the lateral oxidation distance, thereby ensuring that the area between the lateral oxidation portion 1042 and the flow blocking portion 1043 can be completely oxidized laterally. Figure 4 As shown, it is a schematic diagram of a lateral oxidation process provided by an embodiment of the present disclosure, Figure 4 (a) is a schematic diagram of the top view of the structure when the lateral oxidation is 5 μm. Figure 4 (b) is a schematic diagram showing the top view of the structure when the lateral oxidation is 10 μm, and Figure 4 (c) is a schematic diagram of the top view of the structure when the lateral oxidation is 15 μm. It can be seen from the figure that after 15 μm of lateral oxidation, the diameter of the emission hole 1041 located at the center of the device reaches the designed 16 μm. According to actual needs, further oxidation can reduce the aperture size to produce a device with a smaller aperture.

[0034] Optionally, in the embodiment of the present disclosure, along the direction perpendicular to the emitted light, the cross-sectional shape of the lateral oxidation portion 1042 may include at least one of a straight line segment and a curved line segment. For example, the lateral oxidation portion 1042 is a trench, and the cross-sectional shape of the trench may be a triangle, a quadrilateral, or a complex figure including both straight line segments and curved line segments. There is no limitation on this, as long as the emission hole 1041 can be generated after lateral oxidation at the center of the device. In addition, the number of lateral oxidation portions 1042 may be 2, 3, 4, or 5, etc., and up to 10 may be meaningful depending on the size of the oxide aperture. At the same time, since the P-type contact layer needs to enter between the trenches to approach the emission hole 1041, the lateral oxidation portion 1042 is not a continuous trench.

[0035] Optionally, in the embodiment of the present disclosure, the flow blocking portion 1043 may be an annular groove or an annular table, for example Figure 5 (a) is a schematic diagram of a top view of a structure having an annular groove, Figure 5(b) is a schematic diagram of a top view of a structure with an annular table. Among them, the blocking portion 1043 needs to be a continuous groove, so as to prevent the lateral current from diffusing to the outside of the device, and the corresponding closed circle area is appropriate, which is convenient for setting the second ohmic contact layer 106 and subsequent direct detection on the one hand, and on the other hand, it ensures that the area between the lateral oxidation portion 1042 and the blocking portion 1043 can be completely oxidized laterally. In addition, the blocking portion 1043 and the second ohmic contact layer 106 are not located in the same plane, that is, the blocking portion 1043 is located on the surface of the semiconductor, and the etching depth at least ensures that the lateral oxidation can form the emission hole 1041, generally reaching the first reflector layer 102, and the second ohmic contact layer 106 is located above the semiconductor surface.

[0036] For example, in the embodiment of the present disclosure, the diameter of the detection area 1051 ranges from 10 μm to 60 μm, and can further be 15 μm to 30 μm. The reason for this setting is that the detection area 1051 is covered by the P-type contact layer and has a suitable area, which is convenient for direct detection by an electrical probe head that provides measurement voltage or current stimulation.

[0037] For example, in the embodiment of the present disclosure, the active layer 103 is a single quantum well layer or a multiple quantum well (MQW) layer, which is used to emit light when powered on. The first reflector layer 102 and the second reflector layer 105 may include any one of an N-type reflector layer and a P-type reflector layer, for example, the first reflector layer 102 is an N-type Bragg reflector (DBR) layer, and the second reflector layer 105 is a P-type Bragg reflector layer.

[0038] The test structure for a vertical cavity surface emitting laser provided in the embodiment of the present disclosure can quickly obtain a lateral oxidation portion and a blocking portion for lateral oxidation and a large-area second ohmic contact layer that is convenient for direct detection by a standard wafer-level test machine through two photolithography steps. The manufactured test structure can then be used to efficiently evaluate the optoelectronic properties of the epitaxial wafer, thereby greatly improving the processing efficiency.

[0039] Based on the above examples, please refer to Figure 6 , which is a basic flow chart of a test structure manufacturing method provided by an embodiment of the present disclosure. The manufacturing method can be applied to Figure 1 to Figure 5 The test structure 10 of the corresponding embodiment specifically includes the following steps:

[0040] S101 , providing an epitaxial structure, wherein the epitaxial structure includes a first reflector layer, an active layer, an oxidation restriction layer, and a second reflector layer that are stacked.

[0041] For example, the embodiment of the present disclosure may adopt metal organic chemical vapor deposition (MOCVD) or molecular beam epitaxy (MBE) and other technologies to periodically and alternately grow a first reflector layer 102 and a light-emitting layer on a substrate layer, and periodically and alternately grow a second reflector layer 105, wherein the first reflector layer 102 is an N-type Bragg reflector layer, the second reflector layer 105 is a P-type Bragg reflector layer, and the light-emitting layer may include Al 0.98 Ga 0.02 As high aluminum composition active layer 103 and oxidation restriction layer 104.

[0042] S102, photolithography is performed downward along the direction from the second reflector layer to the first reflector layer to expose at least the oxidation restriction layer, so as to obtain a lateral oxidation portion and a flow blocking portion.

[0043] For example, Figure 7 As shown, the embodiment of the present disclosure can obtain the mesa pattern by photolithography, and obtain the mesa and remove the photoresist of the groove by inductively coupled plasma (ICP) etching to expose the Al 0.98 Ga 0.02 The etching depths of the oxidation limiting layer 104 , the lateral oxidation portion 1042 and the blocking portion 1043 of the As high aluminum component may be the same.

[0044] S103, performing transverse oxidation on the oxidation limiting layer through the transverse oxidation part and the blocking part to obtain an emission hole.

[0045] For example, Figure 7 As shown, the embodiment of the present disclosure can perform pre-oxidation cleaning before oxidation, and then obtain the current limiting emission hole 1041 by wet oxidation. The emission hole 1041 is located in the Al 0.98 Ga 0.02 As is located in the middle of the oxidation restriction layer 104 of the high aluminum component.

[0046] S104, after depositing a passivation layer on the upper surface of the second reflector layer, photoetching the passivation layer downward, and depositing to form a second ohmic contact layer.

[0047] For example, Figure 7As shown, in the embodiment of the present disclosure, a passivation layer may be deposited on the upper surface of the second reflector layer 105, and the passivation layer includes but is not limited to a SiN layer, an Al2O3 layer or a SiO2 layer, which is used as an insulating protection and an exit window protection. Since the second ohmic contact layer 106 is generated after the passivation layer is applied, it is necessary to remove the passivation layer in the area where the second ohmic contact layer 106 should contact the semiconductor surface. Further, the passivation layer in the open area is first etched, and then the second ohmic contact layer 106 is evaporated using the same photoresist pattern, which ensures the natural alignment of the passivation layer etching and the second ohmic contact layer 106 evaporation, and the P-type contact layer corresponding to the second ohmic contact layer 106 is obtained by magnetron sputtering and a stripping process.

[0048] S105 , after depositing a first ohmic contact layer on the lower surface of the first reflector layer, annealing is performed to obtain a test structure.

[0049] For example, Figure 7 As shown, the embodiment of the present disclosure can obtain an N-type contact layer corresponding to the first ohmic contact layer 101 through an electrode evaporation process, and then place the entire test structure 10 into a rapid annealing furnace for annealing to achieve the purpose of alloying, so that a good ohmic contact can be formed between the contact layer and the semiconductor material, thereby improving the electrical properties of the device.

[0050] It should be noted that, for the description of the same steps and the same contents in this embodiment as those in other embodiments, reference can be made to the description in other embodiments and will not be repeated here.

[0051] The test structure manufacturing method for a vertical cavity surface emitting laser provided in the embodiment of the present disclosure can quickly obtain a lateral oxidation portion and a blocking portion for lateral oxidation and a large-area second ohmic contact layer that is convenient for direct detection by a standard wafer-level testing machine through two photolithography steps. The manufactured test structure can then be used to efficiently evaluate the optoelectronic properties of the epitaxial wafer, thereby greatly improving the processing efficiency.

[0052] The above embodiments are only used to illustrate the technical solutions of the present disclosure, rather than to limit them. Although the present disclosure has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present disclosure.

Claims

1. A test structure for a vertical cavity surface emitting laser, characterized in that: The test structure includes a first ohmic contact layer, a first reflector layer, an active layer, an oxidation restriction layer, a second reflector layer and a second ohmic contact layer which are stacked, wherein the first reflector layer is an N-type Bragg reflector layer, the second reflector layer is a P-type Bragg reflector layer, and a detection area is arranged on the second ohmic contact layer; A lateral oxidation portion and a blocking portion surrounding the lateral oxidation portion are distributed around the emission hole of the oxidation restriction layer; the second ohmic contact layer is located in a closed circle formed by the blocking portion, and surrounds at least a portion of the emission hole without covering the lateral oxidation portion.

2. The test structure according to claim 1, characterized in that: The distance between the second ohmic contact layer and the emission hole is in the range of 1 μm to 5 μm.

3. The test structure according to claim 2, characterized in that: The first ohmic contact layer is an N-type contact layer, and the second ohmic contact layer is a P-type contact layer.

4. The test structure according to claim 1, characterized in that: The maximum distance between the lateral oxidation portion and the flow blocking portion is twice the lateral oxidation distance.

5. The test structure according to claim 4, characterized in that: Along the direction perpendicular to the emitted light, the cross-sectional shape of the lateral oxidation portion includes at least one of a straight line segment and a curved line segment.

6. The test structure according to claim 4, characterized in that: The flow blocking portion is an annular groove or an annular table.

7. The test structure according to any one of claims 1 to 6, characterized in that: The diameter of the detection area ranges from 10 μm to 60 μm.

8. The test structure according to claim 7, characterized in that: The active layer is a single quantum well layer or a multi-quantum well layer.