Carbonization and drying system for nano calcium carbonate
Through temperature-controlled carbonization and surface activation modification, combined with spray drying technology, the particle size instability and agglomeration problems caused by the complexity of nano-calcium carbonate carbonation and drying process parameters are solved, and the stable production and dispersion of nano-scale particles are achieved, promoting the promotion of nano-scale particles. The application development of nano calcium carbonate.
Patent Information
- Application Number
- CN202420521987.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-18
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2034-03-18
AI Technical Summary
The carbonization and drying process parameters of nano calcium carbonate are complex and difficult to control, resulting in unstable particle size and particle agglomeration, limiting its application development.
The temperature-controlled carbonization system is used to take away the reaction heat through the jacket and coil, control the carbonization reaction temperature, and perform surface activation modification after carbonization, and combine it with a spray drying system to ensure particle dispersion.
The nano-calcium carbonate particle size is effectively controlled within the nanoscale range, inhibiting the particle growth rate, avoiding agglomeration, and improving the dispersion and stability of the product.
Smart Images

Figure CN221933076U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a production device for calcium carbonate powder, in particular to a carbonization and drying system for nano calcium carbonate. Background Art
[0002] Nano calcium carbonate is a new type of ultrafine solid powder material developed in the 1980s. Due to the ultrafineness of nano calcium carbonate particles, its crystal structure and surface electronic structure change, resulting in quantum size effect, small size effect, surface effect and macro quantum effect that ordinary calcium carbonate does not have. Compared with ordinary light calcium carbonate products, its product quality and performance have been greatly improved, so that it can play a role in strengthening and toughening in many application fields such as rubber, plastics, papermaking, coatings, adhesives, inks, etc., and change the processability, usability and appearance of the application products. It can partially replace expensive raw materials such as carbon black, white carbon black and titanium dioxide, so that product costs are reduced and quality is greatly improved. Therefore, as soon as nano calcium carbonate appeared, it showed a wide range of applicability and a relatively strong market demand.
[0003] Carbonization is a common method for chemically preparing light calcium carbonate. The main process is to first calcine limestone to obtain quicklime and kiln gas containing carbon dioxide. The quicklime is digested and reacted with water to obtain calcium hydroxide slurry. Then, purified kiln gas is introduced into the calcium hydroxide slurry to obtain calcium carbonate slurry. After dehydration and drying, the finished calcium carbonate product is obtained. Compared with the ordinary light calcium carbonate preparation process, the biggest difference in the preparation of nano calcium carbonate lies in the control of carbonization and drying process. The carbonization reaction is the most critical process step in the production process of nano calcium carbonate. The control of reaction conditions determines the particle size and distribution of the product. Improper operation of the drying process can also easily lead to the agglomeration and compaction of nano calcium carbonate. However, the current nano calcium carbonate carbonization and drying equipment requires many and strict process parameters to be controlled, and the product quality is difficult to stably control, which seriously restricts the application and development of nano calcium carbonate. Utility Model Content
[0004] In order to solve the above technical problems, the utility model proposes a carbonization and drying system for nano calcium carbonate. Aiming at the problem that the heat released by the carbonization reaction causes the temperature of the carbonization reaction system to rise, the reaction speed is accelerated, and the particle size of the calcium carbonate particles is difficult to control, a jacket and a coil are added to the carbonization kettle to take away the heat generated by the carbonization reaction, thereby controlling the temperature of the carbonization reaction system, inhibiting the growth rate of the calcium carbonate particles, and controlling the particle size of the generated calcium carbonate particles to be within the nanometer range; in order to prevent the agglomeration of the nano particles, a modification device is provided after the carbonization to perform surface modification on the nano calcium carbonate particles; in view of the problem that the conventional light calcium carbonate dehydration-drum drying-air cannon dispersion drying process easily causes the particles to be compacted and difficult to disperse, the modified nano calcium carbonate particle slurry is directly dried by spray drying to ensure the dispersibility of the particles.
[0005] In order to achieve the above object, the technical solution of the utility model is as follows:
[0006] A carbonization and drying system for nano calcium carbonate; comprising a temperature-controlled carbonization system A, a surface activation modification system B, and a spray drying system C;
[0007] The core device of the temperature-controlled carbonization system A is a carbonization tank, the outer layer of the carbonization tank is a cooling jacket, and a cooling coil is arranged inside. The cooling jacket and the cooling coil are connected to the cooling liquid storage tank through inlet and outlet pipes, and the cooling liquid storage tank is connected to the refrigerator;
[0008] The bottom of the carbonization tank is connected to the surface activation modification system B through a pipeline;
[0009] The spray drying system C is connected to the surface modification system B through a pipeline via a clinker slurry pump.
[0010] Furthermore, a slurry feed port, a stirring motor, a temperature probe and a pH probe are arranged on the top of the carbonization tank; a hollow stirring rod with a paddle is arranged at the center of the carbonization tank, and kiln air is passed through the stirring rod.
[0011] Furthermore, a rotating ultrasonic atomizing nozzle is provided at the bottom of the stirring rod.
[0012] Furthermore, the surface activation modification system B includes a modification tank, a modified stirring motor and a stirring paddle.
[0013] Furthermore; the spray drying system C includes a spray drying tower, a spray nozzle, an air intake fan, an air heating device, a cyclone separator, a fan and a dust collector; a spray nozzle is arranged in the inner cavity of the spray drying tower, the spray nozzle is connected to the clinker slurry pump, the spray drying tower is also connected to the cyclone separator, and the cyclone separator is connected to the dust collector through a fan and a pipeline.
[0014] Furthermore, in the temperature-controlled carbonization system A, the raw material slurry is pumped into the carbonization tank from the feed port, and the kiln gas enters the carbonization tank from the rotating ultrasonic atomizing nozzle through the stirring rod via the stirring motor to carry out carbonization reaction with the raw material slurry under stirring; the heat generated by the carbonization reaction enters the coolant through the cooling coil and the cooling jacket for heat exchange, and the coolant absorbs the heat of the carbonization reaction system and enters the coolant storage tank, and returns to the coolant storage tank after being cooled by the refrigerator, and is pumped into the cooling coil and the cooling jacket by the freezing liquid pump again for heat exchange with the carbonization reaction system; the temperature and pH value of the slurry in the carbonization tank are monitored by the temperature probe and the pH probe. When the pH value drops to a certain value, the reaction is stopped, and the slurry is placed in the surface modification tank after stirring for a period of time.
[0015] In the spray drying system C, the clinker slurry is pumped out from the surface modification tank by the clinker slurry pump and enters the interior of the spray drying tower through the spray nozzle, and the air is sucked into the spray drying tower by the air intake fan through the air heating device; the dried nano calcium carbonate material is discharged from the material discharge port at the bottom of the spray drying tower, and the gas is separated from the material by the cyclone separator and discharged into the atmosphere after passing through the fan and dust collector.
[0016] The beneficial effects of the utility model are as follows: the utility model adds a jacket and a coil in the carbonization kettle to take away the heat generated by the carbonization reaction, thereby realizing the temperature control of the carbonization reaction system, overcoming the problem that the carbonization reaction releases heat and causes the carbonization reaction system to heat up, and the reaction speed is accelerated, resulting in the difficulty in controlling the particle size of calcium carbonate particles. The growth rate of calcium carbonate particles can be inhibited, and the particle size of the generated calcium carbonate particles can be controlled within the nanometer range; the rotating ultrasonic atomizing nozzle at the bottom of the carbonization kettle can make the kiln gas enter the carbonization kettle in the form of finer bubbles. Due to the enlarged gas-liquid mass transfer area and countercurrent contact, coupled with the mechanical With the help of mechanical stirring, the microscopic mixing degree between gas and liquid is extremely high, so the kiln gas and slurry react more fully; after carbonization, a modification device is set to modify the surface of the nano calcium carbonate particles, which can alleviate the agglomeration problem of the nano particles in the subsequent drying, packaging and transportation processes; the modified nano calcium carbonate particle slurry is directly dried by spray drying to ensure the dispersion of the particles. On the one hand, it simplifies the conventional light calcium carbonate dehydration-drum drying-air cannon dispersion drying process, and on the other hand, it avoids the problem of calcium carbonate particles being compacted and difficult to disperse that is easily caused by the existing process. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a structural schematic diagram of the carbonization and drying system of nano calcium carbonate of the utility model;
[0018] Among them: 1. Carbonization tank, 2. Cooling coil, 3. Cooling jacket, 4. Stirring rod with paddle, 5. Slurry feed port, 6. Stirring motor, 7. Temperature probe, 8. pH probe, 9. Rotary ultrasonic atomizing nozzle, 10. Refrigerator, 11. Coolant pump, 12. Coolant storage tank, 13. Modification tank, 14. Modified stirring motor and stirring paddle, 15. Clinker slurry pump, 17. Spray nozzle, 18. Inlet fan, 19. Air heating device, 20. Cyclone separator, 21. Fan, 22. Dust collector. DETAILED DESCRIPTION
[0019] The utility model is further described in detail below in conjunction with specific implementation methods.
[0020] like Figure 1 As shown; the present application provides a carbonization and drying system of nano calcium carbonate, which can be implemented in the following manner; it includes a temperature-controlled carbonization system A, a surface modification system B, and a spray drying system C; the core device of the temperature-controlled carbonization system A is a carbonization tank 1, and a slurry feed port 5, a stirring motor 6, a temperature probe 7, and a pH probe 8 are arranged on the top of the carbonization tank 1; a hollow stirring rod is arranged at the center of the carbonization tank 1, and the stirring rod has a paddle 4, and kiln air is passed through the stirring rod. A rotating ultrasonic atomizing nozzle 9 is arranged at the bottom of the stirring rod; the outer layer of the carbonization tank 1 is a reducing The temperature jacket 3 has a cooling coil 2 arranged inside, the cooling jacket 3 and the cooling coil 2 are connected to the cooling liquid storage tank 12 through inlet and outlet pipes, and the cooling liquid storage tank 12 is connected to the refrigerator 10; the surface modification system B includes a modification tank 13 and a modification stirring motor and a stirring paddle 14; the spray drying system C is connected to the surface modification system B through a pipeline via a clinker slurry pump 15; the spray drying system C includes a spray drying tower 16, a spray nozzle 17, an air intake fan 18, an air heating device 19, a cyclone separator 20, a fan 21, and a dust collector 22.
[0021] The working process of the utility model is as follows: the raw material slurry is pumped into the carbonization tank 1 from the feed port, and the kiln gas enters the carbonization tank 1 from the rotating ultrasonic atomizing nozzle 5 through the stirring rod while the stirring motor 6 drives the stirring rod with the paddle 4 to perform a carbonization reaction with the raw material slurry; the heat generated by the carbonization reaction enters the cooling liquid through the cooling coil 2 and the cooling jacket 3 through heat exchange, and the cooling liquid absorbs the heat of the carbonization reaction system and enters the cooling liquid storage tank 10, and returns to the cooling liquid storage tank 10 after being cooled by the refrigerator 9, and is pumped into the cooling coil 2 and the cooling jacket 3 by the freezing liquid pump 11 again to perform a heat exchange with the carbonization reaction system; the temperature probe 7 and the pH value are measured by ... The probe 8 monitors the temperature and pH value of the slurry in the carbonization tank 1. When the pH value drops to a certain value, the reaction is stopped. After stirring for a period of time, the slurry is placed in the surface modification tank 12. After the clinker slurry is activated and modified in the modification tank 13, it is pumped out from the surface modification tank 12 by the clinker slurry pump 15 and enters the spray drying tower 16 through the spray nozzle 17. The air is sucked into the spray drying tower 16 by the air intake fan 18 through the air heating device 19. The dried nano calcium carbonate material is discharged from the material discharge port at the bottom of the spray drying tower 16. The gas is separated by the cyclone separator 20 and then discharged into the atmosphere through the fan 21 and the dust collector 22.
[0022] The above description of the disclosed embodiments enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A carbonization and drying system for nano calcium carbonate, characterized in that; It includes temperature-controlled carbonization system A, surface activation modification system B, and spray drying system C; The core device of the temperature-controlled carbonization system A is a carbonization tank (1), the outer layer of the carbonization tank (1) is a cooling jacket (3), a cooling coil (2) is arranged inside, the cooling jacket (3) and the cooling coil (2) are connected to a cooling liquid storage tank (12) through inlet and outlet pipes, and the cooling liquid storage tank (12) is connected to a refrigerator (10); The bottom of the carbonization tank (1) is connected to the surface activation modification system B through a pipeline; The spray drying system C is connected to the surface modification system B through a pipeline via a clinker slurry pump (15).
2. A carbonization and drying system for nano-calcium carbonate according to claim 1, characterized in that: The top of the carbonization tank (1) is provided with a slurry feed port (5), a stirring motor (6), a temperature probe (7) and a pH probe (8); a hollow stirring rod is arranged at the center of the carbonization tank (1), the stirring rod has a paddle (4), and kiln air is passed through the stirring rod.
3. A carbonization and drying system for nano-calcium carbonate according to claim 2, characterized in that: A rotating ultrasonic atomizing nozzle (9) is arranged at the bottom of the stirring rod.
4. A carbonization and drying system for nano-calcium carbonate according to claim 1, characterized in that: The surface activation modification system B comprises a modification tank (13) and a modification stirring motor and a stirring paddle (14).
5. A carbonization and drying system for nano-calcium carbonate according to claim 1, characterized in that: The spray drying system C comprises a spray drying tower (16), a spray nozzle (17), an air intake fan (18), an air heating device (19), a cyclone separator (20), a fan (21) and a dust collector (22); the spray nozzle (17) is arranged in the inner cavity of the spray drying tower (16), the spray nozzle (17) is connected to the clinker slurry pump (15), the spray drying tower (16) is also connected to the cyclone separator (20), and the cyclone separator (20) is connected to the dust collector (22) through the fan (21) and a pipeline.