High-flux tube
By setting longitudinal grooves and inner wall protrusions on the outer surface of the high-flux tube base, or by designing a spliced split tube and outer sleeve, the problem of insufficient contact area of the porous layer is solved, the heat exchange effect is improved and maintenance is facilitated.
Patent Information
- Application Number
- CN202323298325.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-04
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-12-04
AI Technical Summary
The limited contact area between the porous layer and the base tube in existing high-flux tubes results in poor heat exchange performance.
Several longitudinal grooves are set along the axial direction on the outer surface of the base tube body, and a convex strip is formed on the inner wall of the microchannel tube to match the longitudinal grooves. Alternatively, the microchannel tube is designed as a spliced split part and fixed by a clamping component, or the microchannel tube is designed as an integrally formed outer sleeve that is fitted onto the outside of the base tube body.
It effectively increases the contact area between the microchannel tube and the outer surface of the base tube, improves the heat exchange effect, and facilitates disassembly and maintenance.
Smart Images

Figure CN221944992U_ABST
Abstract
Description
[Technical Field]
[0001] This utility model relates to the field of heat exchange tube technology, and in particular to a high-throughput tube. [Background Technology]
[0002] Shell-and-tube heat exchangers, also known as tubular heat exchangers, are indirect heat exchangers that use the walls of tube bundles enclosed in a shell as the heat transfer surface. Shell-and-tube heat exchangers are widely used in chemical, oil refining, petrochemical, power, and nuclear energy industries.
[0003] Traditional shell-and-tube heat exchangers typically use bare tubes, which have low heat exchange efficiency. To improve the heat exchange efficiency of shell-and-tube heat exchangers, high-efficiency heat exchange tubes have been developed. Currently, high-efficiency heat exchange tubes include corrugated tubes, finned tubes, and high-flux tubes, among which high-flux tubes exhibit the best heat exchange performance in boiling and condensation heat transfer. For example, Chinese utility model patent application CN201520595528.8 discloses a copper-nickel alloy high-flux tube, which includes a copper-nickel alloy base tube. The inner surface of the base tube has several integrally rolled longitudinal grooves along the axial direction, and the outer surface of the base tube has a porous layer of the same material as the base tube. This high-flux tube can be used in vertical heat exchangers with evaporation on the outer surface and condensation on the inner surface. However, the contact area between the porous layer and the base tube in existing high-flux tubes is limited, and the heat exchange effect still needs improvement. In view of the above-mentioned problems, the inventors of this case conducted in-depth research on this issue, resulting in this application. [Utility Model Content]
[0004] The technical problem to be solved by this utility model is to provide a high-throughput tube that can increase the contact area between the microchannel tube and the outer surface of the base tube body, thereby improving the heat exchange effect.
[0005] This invention is implemented as follows: a high-throughput tube includes a base tube body and a microchannel tube disposed outside the base tube body. Optical tube segments are provided at both ends of the base tube body. The outer surface of the base tube body is provided with a plurality of longitudinal grooves along the axial direction, and the inner wall of the microchannel tube has convex strips that match the longitudinal grooves.
[0006] Furthermore, the microchannel tube is a microchannel outer layer directly sintered onto the outside of the base tube body.
[0007] Furthermore, the microchannel tube includes at least two spliced components and at least two clamping members. Each spliced component is arranged around the outside of the base tube body, and the clamping members clamp and fix each spliced component to the outside of the base tube body.
[0008] Furthermore, the microchannel tube is an integrally formed outer sleeve, which is fitted over the outside of the base tube body.
[0009] Furthermore, the porosity of the microchannel tube is between 40% and 60%.
[0010] Furthermore, the longitudinal groove is located between the two optical tube segments.
[0011] Furthermore, the base tube body is made of stainless steel or carbon steel.
[0012] By adopting the technical solution of this utility model, at least the following beneficial effects are achieved:
[0013] 1. Several longitudinal grooves are set along the axial direction on the outer surface of the base tube body, and convex strips are formed on the inner wall of the microchannel tube to match the longitudinal grooves. This can effectively increase the contact area between the microchannel tube and the outer surface of the base tube body, thereby improving the heat exchange effect.
[0014] 2. The microchannel tube is designed to include at least two spliced components and at least two clamping components, with each spliced component being clamped and fixed to the outside of the base tube body by the clamping components; or the microchannel tube is designed as an integrally formed outer sleeve, which is fitted onto the outside of the base tube body. This allows for the use of longitudinal grooves and protrusions to increase the contact area between the microchannel tube and the base tube body, thereby improving the heat exchange effect. Furthermore, it allows for the disassembly and installation of the microchannel tube, facilitating replacement, maintenance, and other operations. [Attached Image Description]
[0015] The present invention will be further described below with reference to the accompanying drawings and embodiments.
[0016] Figure 1 This is an overall view of the high-throughput tube in Embodiment 1 of this utility model;
[0017] Figure 2 This is a cross-sectional view of the high-throughput tube in Embodiment 1 of this utility model;
[0018] Figure 3 This is an overall view of the high-throughput tube in Embodiment 2 of this utility model;
[0019] Figure 4 This is a cross-sectional view of the high-throughput tube in Embodiment 2 of this utility model;
[0020] Figure 5 This is an overall view of the high-throughput tube in Embodiment 3 of this utility model;
[0021] Figure 6 This is a cross-sectional view of the high-throughput tube in Embodiment 3 of this utility model;
[0022] Figure 7 This is a cross-sectional view of the base tube body in Embodiment 3 of this utility model;
[0023] Figure 8 This is a cross-sectional view of the microchannel tube in Embodiment 3 of this utility model.
[0024] Explanation of reference numerals in the attached figures:
[0025] High-throughput tube 100;
[0026] Base pipe body 1, light pipe section 11, longitudinal groove 12;
[0027] Microchannel tube 2, protrusion 21, microchannel outer layer 22, spliced split 23, outer tube 24;
[0028] Clamping component 3.
Detailed Implementation Methods
[0029] To better understand the technical solution of this utility model, the technical solution of this utility model will be described in detail below with reference to the accompanying drawings and specific embodiments.
[0030] It should be noted that the terms "center," "longitudinal," "lateral," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used solely for the convenience of describing these embodiments and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Furthermore, the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Therefore, a feature defined with "first," "second," etc., may explicitly or implicitly include one or more of that feature.
[0031] Example 1
[0032] Please see Figures 1 to 2 As shown, this utility model discloses a high-throughput tube 100, which includes a base tube body 1 and a microchannel tube 2 disposed outside the base tube body 1. Optical tube segments 11 are provided at both ends of the base tube body 1. Since the high-throughput tube 100 needs to be connected to a tube sheet (not shown) during installation, the optical tube segments 11 at both ends of the base tube body 1 facilitate connection to the tube sheet. Furthermore, to ensure a reliable connection between the high-throughput tube 100 and the tube sheet, the length of the optical tube segment 11 must be at least 30 mm greater than the thickness of the tube sheet.
[0033] The outer surface of the base tube body 1 is provided with a plurality of longitudinal grooves 12 along the axial direction, and the inner wall of the microchannel tube 2 has protrusions 21 that match the longitudinal grooves 12.
[0034] Because existing high-throughput tubes use metal powder directly sintered on the outer surface of the base tube to form a microchannel layer, and the area of the outer surface of the base tube is relatively limited. Therefore, this invention uses several longitudinal grooves 12 arranged along the axial direction on the outer surface of the base tube body 1, and forms protrusions 21 on the inner wall of the microchannel tube 2 that cooperate with the longitudinal grooves 12. This can effectively increase the contact area between the microchannel tube 2 and the outer surface of the base tube body 1, thereby improving the heat exchange effect.
[0035] In Embodiment 1 of this utility model, the microchannel tube 2 is a microchannel outer layer 22 directly sintered onto the outside of the base tube body 1. In a specific implementation of this utility model, metal powder can be evenly distributed on the outer wall surface and longitudinal groove 12 of the base tube body 1 before sintering, so that the microchannel outer layer 22 can cover the outer wall surface and longitudinal groove 12 of the base tube body 1, thereby increasing the contact area between the microchannel outer layer 22 and the base tube body 1; while the bare tube segments 11 at both ends of the base tube body 1 do not need to be sintered with metal powder.
[0036] In Embodiment 1 of this utility model, in order to ensure the heat exchange effect of the high-flux tube 100, the porosity of the microchannel tube 2 is between 40% and 60%. In specific implementations of this utility model, the porosity of the microchannel tube 2 can be set according to actual needs. For example, the porosity of the microchannel tube 2 can be set to any one of 40%, 45%, 50%, 55%, and 60%.
[0037] In Embodiment 1 of this utility model, the longitudinal groove 12 is located between the two optical tube segments 11, that is, the longitudinal groove 12 does not extend to the optical tube segment 11, so that the optical tube segment 11 can be better connected to the tube sheet.
[0038] In Embodiment 1 of this utility model, the base tube body 1 is made of stainless steel or carbon steel. However, this utility model is not limited to this; in specific implementations, the base tube body 1 can also be made of aluminum alloy, copper-nickel alloy, or other materials.
[0039] In Embodiment 1 of this utility model, the cross-section of the longitudinal groove 12 is an arc-shaped groove structure, a trapezoidal groove structure, or a triangular groove structure, and the cross-section of the protrusion 21 is an arc-shaped protrusion structure matching the arc-shaped groove structure, a trapezoidal protrusion structure matching the trapezoidal groove structure, or a triangular protrusion structure matching the triangular groove structure. Of course, this utility model is not limited to this, and other shapes of structures can be used in specific implementations.
[0040] Example 2
[0041] Please see Figures 3 to 4As shown, this utility model discloses a high-throughput tube 100, which includes a base tube body 1 and a microchannel tube 2 disposed outside the base tube body 1. Optical tube segments 11 are provided at both ends of the base tube body 1. Since the high-throughput tube 100 needs to be connected to a tube sheet (not shown) during installation, the optical tube segments 11 at both ends of the base tube body 1 facilitate connection to the tube sheet. Furthermore, to ensure a reliable connection between the high-throughput tube 100 and the tube sheet, the length of the optical tube segment 11 must be at least 30 mm greater than the thickness of the tube sheet.
[0042] The outer surface of the base tube body 1 is provided with a plurality of longitudinal grooves 12 along the axial direction, and the inner wall of the microchannel tube 2 has protrusions 21 that match the longitudinal grooves 12.
[0043] Because existing high-throughput tubes use metal powder directly sintered on the outer surface of the base tube to form a microchannel layer, and the area of the outer surface of the base tube is relatively limited. Therefore, this invention uses several longitudinal grooves 12 arranged along the axial direction on the outer surface of the base tube body 1, and forms protrusions 21 on the inner wall of the microchannel tube 2 that cooperate with the longitudinal grooves 12. This can effectively increase the contact area between the microchannel tube 2 and the outer surface of the base tube body 1, thereby improving the heat exchange effect.
[0044] In Embodiment 2 of this utility model, the microchannel tube 2 includes at least two spliced components 23 and at least two clamping members 3. Each spliced component 23 is arranged around the outside of the base tube body 1, and the clamping members 3 clamp and fix each spliced component 23 to the outside of the base tube body 1. The clamping members 3 can adopt various clamping structures in the prior art, as long as they can achieve the goal of clamping and fixing each spliced component 23 to the outside of the base tube body 1. Preferably, the microchannel tube 2 includes two spliced components 23 and two clamping members 3. The two spliced components 23 can form a cylindrical structure, and both ends of the two spliced components 23 are clamped and fixed to the outside of the base tube body 1 by the clamping members 3.
[0045] Because existing high-throughput tubes use metal powder directly sintered on the outer surface of the base tube to form a microchannel layer, the microchannel layer cannot be replaced as needed during use. Therefore, this utility model designs the microchannel tube 2 to include at least two spliced parts 23 and at least two clamping parts 3. The clamping parts 3 clamp and fix each spliced part 23 to the outside of the base tube body 1. This allows the longitudinal groove 12 and the protrusion 21 to increase the contact area between the microchannel tube 2 and the base tube body 1, thereby improving the heat exchange effect. Moreover, the microchannel tube 2 can be disassembled or installed, making it convenient for replacement, maintenance and other operations.
[0046] In Embodiment 2 of this utility model, in order to ensure the heat exchange effect of the high-flux tube 100, the porosity of the microchannel tube 2 is between 40% and 60%. In specific implementations of this utility model, the porosity of the microchannel tube 2 can be set according to actual needs. For example, the porosity of the microchannel tube 2 can be set to any one of 40%, 45%, 50%, 55%, and 60%.
[0047] In Embodiment 2 of this utility model, the longitudinal groove 12 is located between the two optical tube segments 11, that is, the longitudinal groove 12 does not extend to the optical tube segment 11, so that the optical tube segment 11 can be better connected to the tube sheet.
[0048] In Embodiment 2 of this utility model, the base tube body 1 is made of stainless steel or carbon steel. However, this utility model is not limited to this; in specific implementations, the base tube body 1 can also be made of aluminum alloy, copper-nickel alloy, or other materials.
[0049] In Embodiment 2 of this utility model, the cross-section of the longitudinal groove 12 is an arc-shaped groove structure, a trapezoidal groove structure, or a triangular groove structure, and the cross-section of the protrusion 21 is an arc-shaped protrusion structure matching the arc-shaped groove structure, a trapezoidal protrusion structure matching the trapezoidal groove structure, or a triangular protrusion structure matching the triangular groove structure. Of course, this utility model is not limited to this, and other shapes of structures can be used in specific implementations.
[0050] Example 3
[0051] Please see Figures 5 to 8 As shown, this utility model discloses a high-throughput tube 100, which includes a base tube body 1 and a microchannel tube 2 disposed outside the base tube body 1. Optical tube segments 11 are provided at both ends of the base tube body 1. Since the high-throughput tube 100 needs to be connected to a tube sheet (not shown) during installation, the optical tube segments 11 at both ends of the base tube body 1 facilitate connection to the tube sheet. Furthermore, to ensure a reliable connection between the high-throughput tube 100 and the tube sheet, the length of the optical tube segment 11 must be at least 30 mm greater than the thickness of the tube sheet.
[0052] The outer surface of the base tube body 1 is provided with a plurality of longitudinal grooves 12 along the axial direction, and the inner wall of the microchannel tube 2 has protrusions 21 that match the longitudinal grooves 12.
[0053] Because existing high-throughput tubes use metal powder directly sintered on the outer surface of the base tube to form a microchannel layer, and the area of the outer surface of the base tube is relatively limited. Therefore, this invention uses several longitudinal grooves 12 arranged along the axial direction on the outer surface of the base tube body 1, and forms protrusions 21 on the inner wall of the microchannel tube 2 that cooperate with the longitudinal grooves 12. This can effectively increase the contact area between the microchannel tube 2 and the outer surface of the base tube body 1, thereby improving the heat exchange effect.
[0054] In Embodiment 3 of this utility model, the microchannel tube 2 is an integrally formed outer sleeve 24, which is fitted onto the outside of the base tube body 1. In specific implementation, to facilitate fitting the outer sleeve 24 onto the outside of the base tube body 1, the outer diameters of the optical segments 11 at both ends of the base tube body 1 are designed to be different. The outer diameter of the optical segment 11 at the end used to fit the outer sleeve 24 is smaller, allowing the outer sleeve 24 to pass through this optical segment 11 and fit onto the position on the base tube body 1 where the longitudinal groove 12 is provided. Since the outer surface of the base tube body 1 has the longitudinal groove 12 along the axial direction, and the inner wall of the microchannel tube 2 has a protrusion 21 that cooperates with the longitudinal groove 12, during assembly, it is only necessary to align the protrusion 21 with one end of the longitudinal groove 12 and push the outer sleeve 24 inward to achieve fitting the outer sleeve 24 onto the outside of the base tube body 1.
[0055] Because existing high-throughput tubes use metal powder directly sintered on the outer surface of the base tube to form a microchannel layer, the microchannel layer cannot be replaced as needed during use. Therefore, this utility model designs the microchannel tube 2 as an integrally formed outer sleeve 24, which is fitted onto the outside of the base tube body 1. This allows for increased contact area between the microchannel tube 2 and the base tube body 1 using the longitudinal grooves 12 and protrusions 21, thereby improving heat exchange efficiency. Furthermore, it enables the microchannel tube 2 to be disassembled or installed, facilitating replacement and maintenance.
[0056] In Embodiment 3 of this utility model, in order to ensure the heat exchange effect of the high-flux tube 100, the porosity of the microchannel tube 2 is between 40% and 60%. In specific implementations of this utility model, the porosity of the microchannel tube 2 can be set according to actual needs. For example, the porosity of the microchannel tube 2 can be set to any one of 40%, 45%, 50%, 55%, and 60%.
[0057] In embodiment 3 of this utility model, the longitudinal groove 12 is located between the two optical tube segments 11, that is, the longitudinal groove 12 does not extend to the optical tube segment 11, so that the optical tube segment 11 can be better connected to the tube sheet.
[0058] In Embodiment 3 of this utility model, the base tube body 1 is made of stainless steel or carbon steel. However, this utility model is not limited to this; in specific implementations, the base tube body 1 can also be made of aluminum alloy, copper-nickel alloy, or other materials.
[0059] In embodiment 3 of this utility model, the cross-section of the longitudinal groove 12 is an arc-shaped groove structure or a trapezoidal groove structure, and the cross-section of the protrusion 21 is an arc-shaped protrusion structure that matches the arc-shaped groove structure or a trapezoidal protrusion structure that matches the trapezoidal groove structure. Of course, this utility model is not limited to this, and other shapes of structures can be used in specific implementations.
[0060] While specific embodiments of the present invention have been described above, those skilled in the art should understand that the specific embodiments described are merely illustrative and not intended to limit the scope of the present invention. Equivalent modifications and variations made by those skilled in the art in accordance with the spirit of the present invention should be covered within the scope of protection of the claims of the present invention.
Claims
1. A high flux tube, comprising a base tube body, wherein light tube segments are arranged at both ends of the base tube body; characterized in that: It also includes a microchannel tube arranged outside the base tube body; the outer surface of the base tube body is provided with a plurality of longitudinal grooves along the axial direction, and the inner wall of the microchannel tube has convex strips matching the longitudinal grooves.
2. A high flux tube as claimed in claim 1, characterized in that: The microchannel tube is a microchannel outer layer formed by direct sintering on the outside of the base tube body.
3. A high flux tube as claimed in claim 1, characterized in that: The microchannel tube comprises at least two spliced parts and at least two clamping parts. Each of the spliced parts is surrounded by the outside of the base tube body, and each of the spliced parts is clamped and fixed on the outside of the base tube body by the clamping parts.
4. A high flux tube as claimed in claim 1, characterized in that: The microchannel tube is an integrally formed outer sleeve, and the outer sleeve is sleeved on the outside of the base tube body.
5. A high flux tube according to any one of claims 2 to 4, characterized in that: The void ratio of the microchannel tube is between 40% and 60%.
6. A high flux tube as claimed in claim 1, characterized in that: The longitudinal groove is located between the two light pipe segments.
7. A high flux tube as claimed in claim 1, characterized in that: The base pipe body is a stainless steel body or a carbon steel body.
