Device for increasing depth of quench hardening layer of rail head of steel rail

By adopting two-stage induction heating technology in rail heat treatment, using preheating and heat transfer, combined with air spray cooling, the problem of insufficient hardened layer depth is solved, and the hardened layer depth is achieved without reducing production efficiency. Significantly increase and improve uniformity of metallographic structure.

CN221988634UActive Publication Date: 2024-11-12CHINA RAILWAY BAOJI BRIDGE GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420381926.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-28
Publication Date
2024-11-12
Estimated Expiration
2034-02-28

Smart Images

  • Figure CN221988634U_ABST
    Figure CN221988634U_ABST
Patent Text Reader

Abstract

The utility model relates to a device for increasing the depth of a quench hardening layer of a steel rail head. The device comprises a steel rail feeding system, a preheating induction heating system, a first infrared thermometer, a middle-stage induction heating system, a second infrared thermometer, a blast cooling system, a third infrared thermometer and an equipment supporting seat. The device is reasonable in conception, can effectively reduce the content of residual ferrite, can effectively increase the depth of a hardened layer of the rail head, and is suitable for off-line heat treatment of rail heads of various models.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the field of railway tracks, and in particular relates to a device for increasing the depth of a quenching hardened layer of a rail head. Background Art

[0002] At present, induction heating is widely used in industrial production. Its working principle is to place the workpiece in the inductor. When alternating current passes through the inductor, an alternating magnetic field is generated inside the inductor. The induced potential excited by the alternating magnetic field will produce eddy currents on the surface of the workpiece. Because the resistance of the workpiece material is very small, a small induced potential will cause a very strong eddy current, thereby releasing a large amount of Joule heat, causing the surface temperature of the workpiece to rise rapidly.

[0003] At present, domestic turnout manufacturers still use a one-stage medium-frequency induction heating process for offline heat treatment of hot-rolled rails. The advantages of this process are that it does not require overall heating, local heating can meet product requirements, the workpiece has small deformation, low power consumption, and fast heating speed, and the workpiece surface oxidation and decarburization is relatively light. However, there is a corresponding relationship between frequency and heat penetration in induction heating. Affected by the characteristics of induction heating, the temperature of the workpiece after heating is mainly concentrated on the surface of the rail, and the core cannot be completely heated through. After under-speed cooling, a deeper hardened layer depth cannot be obtained; if the hardened layer depth is increased, a heat transfer process is required. The one-stage heating surface temperature does not have time to transfer to the core and enters the air jet cooling stage. If low-power long-term heating is used, production efficiency cannot be guaranteed.

[0004] Under the condition of fixed equipment frequency, if the depth of rail head heating layer is increased, it can be achieved by adjusting equipment power and extending heating time, but this method will inevitably affect the production cycle of products, reduce production efficiency and increase energy waste. Due to the characteristics of induction heating, the heat penetration depth is about 500 / √f (f is frequency), so if the induction heating depth is increased, it can only be increased through heat transfer, but the time for the rail to pass through a one-stage induction heating is very short, and the heat does not have time to transfer to the center before entering the air jet cooling stage, so simply reducing power and extending heating time to increase the hardened layer is not effective. Utility Model Content

[0005] In view of the problems existing in the above-mentioned background technology, the utility model provides a heat treatment device for increasing the depth of the hardened layer of the rail head. The device has a reasonable design, can effectively reduce the residual ferrite content, can effectively increase the depth of the hardened layer of the rail head, and is suitable for offline heat treatment of various types of rail heads.

[0006] The technical solution of the utility model is as follows:

[0007] The above-mentioned device for increasing the depth of the quenching hardened layer of the rail head comprises a rail feeding system, a preheating induction heating system, a first infrared thermometer, a mid-term induction heating system, a second infrared thermometer, an air jet cooling system, a third infrared thermometer and an equipment support seat;

[0008] The rail feeding system is used to carry the rails forward, and comprises a rail feeding platform, a rail position lifting mechanism, a feeding platform forward motor and a lifting height adjustment motor; the rail position lifting mechanism is matched and arranged on the upper part of the rail feeding platform; the feeding platform forward motor is matched and arranged on the lower part of the rail feeding platform, and its power output end is matched and connected with the rail feeding platform; the rail feeding platform is driven to move by the feeding platform forward motor; the lifting height adjustment motor is matched and arranged on the rail feeding platform, and its power output end is matched and connected with the rail position lifting mechanism; the rails are placed on the rail position lifting mechanism and the height can be achieved by driving the height of the rail position lifting mechanism by the lifting height adjustment motor;

[0009] The equipment support seat is matched and arranged in front of the rail feeding platform in the advancing direction of the rail; a height adjustment motor is matched and arranged on the equipment support seat, and an induction coil height adjustment slide is matched and installed vertically on the side facing the preheating induction heating system;

[0010] The preheating induction heating system is matched and arranged above the rail feeding platform, and includes an initial preheating induction heating coil and an initial medium frequency induction heating control meter cabinet; the initial preheating induction heating coil is matched and slidably installed on the induction coil height adjustment slideway and matched and connected to the power output end of the height adjustment motor, and the initial preheating induction heating coil is driven by the height adjustment motor to move in the vertical direction along the induction coil height adjustment slideway; the initial preheating induction heating coil is electrically connected to the initial medium frequency induction heating control meter cabinet; the initial medium frequency induction heating control meter cabinet is installed in the device parameter control area, and adjusts the temperature of the rail after passing through the initial preheating induction heating coil by controlling its heating output power;

[0011] The mid-term induction heating system is matched and arranged in front of the initial preheating induction heating coil in the advancing direction of the rail, and includes a mid-term induction heating coil and a mid-term medium-frequency induction heating control cabinet; the mid-term induction heating coil is matched and slidably installed on the induction coil height adjustment slideway and matched and connected with the power output end of the height adjustment motor; the mid-term induction heating coil is driven by the height adjustment motor to move in the vertical direction along the induction coil height adjustment slideway; the mid-term induction heating coil is electrically connected to the mid-term medium-frequency induction heating control cabinet; the mid-term medium-frequency induction heating control cabinet is installed in the device parameter control area, and adjusts the temperature of the rail after passing through the mid-term induction heating coil by controlling its heating output power;

[0012] The air jet cooling system is composed of an air compression pressure vessel installed in the device parameter control area, an air jet pressure regulating device, and an air jet cooling bellows fixedly installed on the device support seat; the air compression pressure vessel is matched and connected with the air jet pressure regulating device; the height of the air jet cooling bellows from the rail tread can be driven and adjusted by the height regulating motor, and the air pressure of the air jet cooling bellows is adjusted by the air jet pressure regulating device;

[0013] The first infrared thermometer is matched and installed between the initial preheating induction heating coil and the mid-term induction heating coil in the forward direction of the rail; the measurement position of the first infrared thermometer is the rail tread;

[0014] The second infrared thermometer is matched and installed between the mid-term induction heating coil and the air jet cooling wind box in the traveling direction of the rail; the measuring position of the second infrared thermometer is the tread of the rail head;

[0015] The third infrared thermometer is matched and installed in front of the air jet cooling wind box in the forward direction of the rail; the measuring position of the third infrared thermometer is the top tread of the rail.

[0016] The device for increasing the depth of the quenching hardened layer of the rail head, wherein: the lower part of the rail feeding platform is matched with a platform moving wheel.

[0017] The device for increasing the depth of the quenching hardened layer of the rail head, wherein: roller-type rail position positioning fixtures are arranged at both ends of the initial preheating induction heating coil to ensure that the distance between the initial preheating induction heating coil and the rail head tread remains unchanged during the heat treatment of the rail; the initial medium-frequency induction heating control cabinet can increase the surface temperature of the rail from room temperature to above the austenite transformation temperature by adjusting its output power, and the preheating temperature is detected by the first infrared thermometer, and it is required that the surface temperature at this time is lower than the final heat treatment temperature.

[0018] The device for increasing the depth of the quenching hardened layer of the rail head, wherein: when the rail passes through the mid-term induction heating coil, low power is required to allow the rail temperature to continue to slowly increase to the temperature required by the process. This process can also allow heat to be continuously transferred to the center, effectively reducing the temperature difference between the center and the surface. The second infrared thermometer is used to detect the tread temperature of the rail head before the air jet cooling. At this time, the temperature should be controlled within the range required by the process.

[0019] The device for increasing the depth of the quenching hardened layer of the rail head, wherein: the gap between the air jet nozzle of the air jet cooling bellows and the rail top surface is 45mm-55mm. After the rail passes through the air jet cooling system, the temperature of the rail head after cooling is detected by the third infrared thermometer, and the temperature is required to be between 300℃ and 600℃ at this time. If the temperature after the air jet exceeds the process requirements, the air pressure should be adjusted in time.

[0020] A method for increasing the depth of the quenching hardened layer of a rail head, based on the device for increasing the depth of the quenching hardened layer of a rail head, mainly comprises the following steps:

[0021] 1) Quenching preparation

[0022] The rails to be heat treated are manually hoisted onto the rail feeding system, and the height is adjusted on the rail feeding system to place the rails at the specified position; the positions of the initial preheating induction heating coil, the mid-term induction heating coil and the air jet cooling system are adjusted to ensure that the rails meet the process requirements during the heating and cooling process;

[0023] 2) Initial warm-up

[0024] The speed of the rail feeding system 1 is adjusted to the process requirements, and the heating speed of the initial preheating induction heating coil connected thereto is controlled by adjusting the output power of the initial medium-frequency induction heating control cabinet. The heating temperature of the rail after preheating is detected by the first infrared temperature measurement. At this time, the heating temperature is required to be slightly higher than the austenite transformation temperature;

[0025] 3) Mid-term heating

[0026] After the rail passes through the initial preheating induction heating coil, it immediately enters the mid-term induction heating coil. The heating speed of the mid-term induction heating coil connected to it is controlled by adjusting the output power of the mid-term medium-frequency induction heating control cabinet. During this process, the rail temperature needs to continue to slowly increase to the process requirements. The heating temperature at this time is detected by the second infrared thermometer to monitor the heat treatment temperature of the rail before air spray cooling in real time.

[0027] 4) Air jet cooling

[0028] The cooling of the rail after heating is under-speed cooling. The temperature of the rail head after cooling is controlled by adjusting the air jet cooling pressure. This process requires a sufficient cooling rate to transform the metallographic structure into fine lamellar pearlite.

[0029] The method for increasing the depth of the quenching hardened layer of the rail head, wherein: in the step 2), medium frequency high power is used for heating in the initial preheating stage, so that the surface temperature of the rail is quickly increased to above the austenite transformation temperature, and the temperature is required to be controlled at 820°C to 880°C; the temperature of the rail head after preheating is monitored in real time by a first infrared induction temperature measuring instrument; after the temperature meets the requirements, the medium-term induction heating coil is passed, and at this time, the output power of the medium-term induction heating control meter cabinet is adjusted to make the surface temperature of the rail continue to slowly increase to the process requirement range. In this process, heat is continuously transferred to the core, and at the same time, the metallographic structure transformation is made more uniform.

[0030] The method for increasing the depth of the quenching hardened layer of the rail head, wherein: in the step 3), after the intermediate heating, the temperature before the air jet is detected by a second infrared thermometer, and the rail enters the air jet cooling system after the temperature meets the requirements, at which time the temperature of the rail head after cooling is controlled by adjusting the wind pressure, and a sufficient under-speed cooling rate is required here, so that the temperature of the rail head after air jet cooling is controlled at 300°C to 600°C, so that the metallographic structure of the rail head is transformed into fine lamellar pearlite, so as to achieve the purpose of deepening the depth of the hardened layer.

[0031] Beneficial effects:

[0032] The utility model discloses a heat treatment device for increasing the depth of the hardened layer of the rail head, which has a simple and reasonable structural design. It is a two-end induction heating treatment device, which can effectively increase the depth of the hardened layer of the rail head without affecting the heat treatment production rhythm. Through process verification, under the premise of the same driving speed, the depth of the tread hardened layer of the one-stage induction heating method can only reach about 15mm, while the depth of the hardened layer of the two-stage heating method can reach more than 30mm.

[0033] The utility model discloses a heat treatment method for increasing the depth of the hardened layer of the rail head, which is reasonably conceived and simple in process. It is an induction two-stage heating method, which achieves the purpose of increasing the depth of the hardened layer by means of heat penetration + heat transfer. The first preheating stage allows the surface temperature of the rail to quickly reach a temperature range that satisfies the metallographic structure transformation, and the second mid-term heat treatment stage allows the rail temperature to continue to increase slowly, while meeting the process requirements, allowing the heat to be transferred to the center as much as possible, which can effectively improve the uniformity of the structure and increase the heating depth. After the rail is heated, the final heat treatment is completed by air jet underspeed cooling, which can effectively increase the depth of the hardened layer of the rail head.

[0034] The utility model discloses a heat treatment method for increasing the depth of the hardened layer of a rail head, which increases the depth of the austenite transformation layer of the rail head through the process of preheating + heat transfer, and the metallographic structure is more fully transformed after air jet underspeed cooling, and the residual ferrite content can be effectively reduced. BRIEF DESCRIPTION OF THE DRAWINGS

[0035] Figure 1 This is a schematic diagram of the structure of a device for increasing the depth of the quenching hardened layer of a rail head according to the utility model;

[0036] Figure 2 The utility model is a schematic diagram of the process flow of the method for increasing the depth of the quenching hardening layer of the rail head. DETAILED DESCRIPTION

[0037] like Figure 1 As shown, the device for increasing the depth of the quenching hardened layer of the rail head of the utility model comprises a rail feeding system 1, a preheating induction heating system 2, a first infrared thermometer 3, a mid-term induction heating system 4, a second infrared thermometer 5, an air jet cooling system 6, a third infrared thermometer 7 and an equipment support seat 8.

[0038] The rail feeding system 1 is mainly used to carry the rails forward, and includes a rail feeding platform 11, a rail position lifting mechanism 12, a feeding platform forward motor, and a lifting height adjustment motor. The lower part of the rail feeding platform 11 is matched with a platform moving wheel; the rail position lifting mechanism 12 is matched with the upper part of the rail feeding platform 11; the feeding platform forward motor is matched with the lower part of the rail feeding platform 11, and its power output end is matched with the rail feeding platform 11; the overall movement of the rail feeding platform 11 is controlled by the feeding platform forward motor, and the driving distance and position can be accurately controlled, so that the rails carried on the rail feeding platform 11 pass through the initial and intermediate induction heating coils at a uniform speed; the lifting height adjustment motor is matched with the rail feeding platform 11, and its power output end is matched with the rail position lifting mechanism 12; the height of the rails placed on the rail position lifting mechanism 12 can be achieved by adjusting the height of the rail position lifting mechanism 12 by the lifting height adjustment motor.

[0039] The equipment support seat 8 is matched and arranged in front of the rail feeding platform 11 in the advancing direction of the rail; wherein, a height adjustment motor is matched and arranged on the equipment support seat 8 and an induction coil height adjustment slide 81 is vertically installed on the side facing the preheating induction heating system 2.

[0040] The preheating induction heating system 2 is matched and arranged above the rail feeding platform 11 of the rail feeding system 1, and includes an initial preheating induction heating coil 21 and an initial medium frequency induction control meter cabinet installed in the device parameter control area. The initial preheating induction heating coil 21 is slidably installed on the induction coil height adjustment slide 81 of the equipment support seat 8 and matched and connected with the power output end of the height adjustment motor. The initial preheating induction heating coil 21 is driven by the height adjustment motor to move in the vertical direction along the induction coil height adjustment slide 81; the initial preheating induction heating coil 2 is electrically connected to the initial medium frequency induction heating control meter cabinet. The height of the initial preheating induction heating coil 21 can be adjusted according to the height adjustment motor installed on the equipment support seat 8; roller-type rail position positioning tooling is set at both ends of the initial preheating induction heating coil 21 to ensure that the distance between the initial preheating induction heating coil 21 and the rail head tread remains unchanged during the heat treatment of the rail; the heating temperature of the rail after passing through the initial preheating induction heating coil 21 is adjusted by adjusting the output power of the initial medium-frequency induction heating control cabinet connected to the initial preheating induction heating coil 21; by controlling the output power of the initial medium-frequency induction heating control cabinet, the surface temperature of the rail can be quickly increased from room temperature to above the austenite transformation temperature, and the preheating temperature is detected by the first infrared thermometer 3, and the surface temperature is required to be lower than the final heat treatment temperature at this time.

[0041] The first infrared thermometer 3 is matched and installed between the initial preheating induction heating coil 21 of the preheating induction heating system 2 and the mid-term induction heating coil 41 of the mid-term induction heating system 4 in the forward direction of the rail, and the measurement position is required to be the rail tread.

[0042] The mid-term induction heating system 4 is matched and arranged in front of the initial preheating induction heating coil 21 of the preheating induction heating system 2 in the forward direction of the rail, and includes a mid-term induction heating coil 41 and a mid-term medium-frequency induction heating control cabinet. Among them, the mid-term induction heating coil 41 is slidably installed on the induction coil height adjustment slide 81 of the equipment support seat 8, and the height adjustment motor installed on the equipment support seat 8 drives the air along the induction coil height adjustment slide 81 to achieve up and down height adjustment; the mid-term induction heating coil 41 is connected to the mid-term medium-frequency induction heating control cabinet, and the heating output power is controlled by the mid-term medium-frequency induction heating control cabinet to adjust the temperature of the rail after passing through the mid-term induction heating coil 41. When the rail passes through the mid-term induction heating coil 41, low power should be used to make the rail temperature continue to slowly increase to the process required temperature. This process can also make the heat continuously transferred to the center, effectively reducing the temperature difference between the center and the surface. The second infrared thermometer 5 is used to detect the tread temperature before the rail head is sprayed with air to cool the rail head. At this time, the temperature should be controlled within the process requirement range.

[0043] The second infrared thermometer 5 is matched and installed between the mid-term induction heating coil 41 in the traveling direction of the rail and the air jet cooling wind box of the air jet cooling system 6, and the required measuring position is the tread of the rail head.

[0044] The air jet cooling system 6 is composed of an air compression pressure vessel installed in the device parameter control area, an air jet pressure control device and an air jet cooling bellows installed on the device support seat. The air pressure of the air jet cooling bellows can be adjusted by the air pressure control device connected to the air compression pressure vessel. Among them, the air jet cooling system 6 adjusts the air pressure according to the process requirements of different rail types; the air jet cooling bellows is fixed on the equipment support seat 8, and its height from the rail tread can be adjusted by the height adjustment motor installed on the equipment support seat 8. At this time, the gap between the air jet nozzle of the air jet cooling bellows and the top surface of the rail is required to be 45mm to 55mm. After the rail passes through the air jet cooling system 6, the temperature of the rail head after cooling is detected by the third infrared thermometer 7. The temperature is required to be between 300℃ and 600℃ at this time. If the temperature after the air jet exceeds the process requirements, the air pressure should be adjusted in time.

[0045] The third infrared thermometer 7 is matched and installed in front of the air jet cooling wind box in the forward direction of the rail, and the measurement position is required to be the top tread of the rail.

[0046] The utility model discloses a method for increasing the depth of the quenching hardened layer of a rail head, which is a two-stage induction heating method, that is, by adjusting the forward speed of a rail-bearing feeding platform 11, the rail is made to pass through an initial preheating induction heating coil 21, a first infrared induction thermometer 3, a mid-term induction heating coil 41, a second infrared induction thermometer 5, a spray cooling bellows of a spray cooling system 6 and a third infrared induction thermometer 7 in accordance with process requirements; in this process, the rail is preheated + heat transferred so that the temperature of the core of the rail head reaches the austenite transformation requirement, and the purpose of increasing the depth of the hardened layer is achieved after spray cooling; this heat treatment method can effectively increase the depth of the hardened layer without reducing the production cycle, and can ensure the uniformity of the metallographic structure of the rail head hardened layer at the same time.

[0047] like Figure 2 As shown, the method for increasing the depth of the quenching hardened layer of the rail head of the utility model is based on the above-mentioned device for increasing the depth of the quenching hardened layer of the rail head, and specifically comprises the following steps:

[0048] 1) Quenching preparation

[0049] The rails to be heat treated are manually hoisted onto the rail feeding system 1, and the height is adjusted on the rail feeding system 1 to place the rails at a specified position; the positions of the initial preheating induction heating coil 21, the mid-term induction heating coil 41 and the air jet cooling system 6 are adjusted to ensure that the rails meet the process requirements during the heating and cooling process;

[0050] 2) Initial warm-up

[0051] The speed of the rail feeding system 1 is adjusted to the process requirements, and the heating speed of the initial preheating induction heating coil 21 connected thereto is controlled by adjusting the output power of the initial medium-frequency induction heating control meter cabinet. The heating temperature of the rail after preheating is detected by the first infrared thermometer 3. At this time, the heating temperature is required to be slightly higher than the austenite transformation temperature;

[0052] 3) Mid-term heating

[0053] After the rail passes through the initial preheating induction heating coil 21 of the preheating induction heating system 2, it immediately enters the mid-term induction heating coil 41 of the mid-term induction heating system 4. The heating speed of the mid-term induction heating coil 41 connected thereto is controlled by adjusting the output power of the mid-term medium-frequency induction heating control meter cabinet, so that the surface temperature of the preheated rail continues to increase slowly. This process requires that the rail temperature continues to increase slowly to the process requirements, the purpose of which is to allow the surface temperature to have enough time to transfer to the core of the rail, reduce the temperature difference between the surface and the core of the rail head, and at the same time ensure that the metallographic structure is more fully transformed; the heating temperature at this time is detected by the second infrared thermometer 5, and the heat treatment temperature of the rail before air jet cooling is monitored in real time;

[0054] 4) Air jet cooling

[0055] The cooling of the rail after heating is under-speed cooling. The air jet pressure is adjusted by adjusting the air jet cooling system 6 to control the temperature of the rail head after cooling. This process requires a sufficient cooling rate to transform the metallographic structure into fine lamellar pearlite.

[0056] Based on the existing induction heating equipment, the utility model transforms the one-stage induction heating equipment into a two-stage induction heating device, that is, realizes the process of preheating + heat transfer; wherein the preheating induction heating coil and the mid-term induction heating coil are controlled by independent meter cabinets, and the heating power of each coil can be adjusted separately.

[0057] In the above step 2), medium frequency high power is used for heating in the initial preheating stage, so that the surface temperature of the rail is quickly raised to above the austenite transformation temperature (the temperature is required to be controlled at 820°C to 880°C); the temperature of the rail head after preheating is monitored in real time by the first infrared thermometer 3; after the temperature meets the requirement, the rail can pass through the medium-term induction heating coil 41, and at this time, the power of the medium-term medium frequency induction heating control cabinet is adjusted to make the rail temperature continue to slowly rise to the process requirement range. In this process, heat is continuously transferred to the core, and at the same time, the metallographic structure transformation is made more uniform.

[0058] After the final heating in step 3), the temperature before air jetting is detected by the second infrared thermometer 5. When the temperature meets the requirements, it enters the air jet cooling system 6. At this time, the temperature of the rail head after cooling is controlled by adjusting the wind pressure. Here, a sufficient under-speed cooling rate is required to control the temperature of the rail head after air jet cooling at 300°C to 600°C, so that the metallographic structure of the rail head is transformed into fine lamellar pearlite, thereby achieving the purpose of deepening the depth of the hardened layer.

[0059] The utility model can monitor the heat treatment production process in real time through three infrared induction temperature measurement systems. If the temperature at any place exceeds the tolerance, the on-site technicians will make adjustments and batch production will be carried out after the process is stabilized.

Claims

1. A device for increasing the depth of the quenching hardened layer of a rail head, characterized in that: The device comprises a rail feeding system (1), a preheating induction heating system (2), a first infrared thermometer (3), a mid-term induction heating system (4), a second infrared thermometer (5), an air jet cooling system (6), a third infrared thermometer (7) and an equipment support base (8); The rail feeding system (1) is used to carry rails forward, and comprises a rail feeding platform (11), a rail position lifting mechanism (12), a feeding platform forward motor and a lifting height adjustment motor; the rail position lifting mechanism (12) is matched and arranged on the upper part of the rail feeding platform (11); the feeding platform forward motor is matched and arranged on the lower part of the rail feeding platform (11), and its power output end is matched and connected with the rail feeding platform (11); the rail feeding platform (11) is driven to move by the feeding platform forward motor; the lifting height adjustment motor is matched and arranged on the rail feeding platform (11), and its power output end is matched and connected with the rail position lifting mechanism (12); the rail is placed on the rail position lifting mechanism (12), and the height can be achieved by the lifting height adjustment motor driving the rail position lifting mechanism (12) to move; The equipment support seat (8) is matched and arranged in front of the rail feeding platform (11) in the advancing direction of the rail; a height adjustment motor is matched and arranged on the equipment support seat (8), and an induction coil height adjustment slideway (81) is matched and installed vertically on the side facing the preheating induction heating system (2); The preheating induction heating system (2) is matched and arranged above the rail feeding platform (11), and comprises an initial preheating induction heating coil (21) and an initial medium frequency induction heating control cabinet; the initial preheating induction heating coil (21) is matched and slidably installed on the induction coil height adjustment slideway (81) and matched and connected to the power output end of the height adjustment motor, and the initial preheating induction heating coil (21) is driven by the height adjustment motor to move in the vertical direction along the induction coil height adjustment slideway (81); the initial preheating induction heating coil (21) is electrically connected to the initial medium frequency induction heating control cabinet; the initial medium frequency induction heating control cabinet is installed in the device parameter control area, and adjusts the temperature of the rail after passing through the initial preheating induction heating coil (21) by controlling its heating output power; The mid-term induction heating system (4) is matched and arranged in front of the initial preheating induction heating coil (21) in the advancing direction of the rail, and comprises a mid-term induction heating coil (41) and a mid-term medium-frequency induction heating control cabinet; the mid-term induction heating coil (41) is matched and slidably installed on the induction coil height adjustment slideway (81) and matched and connected to the power output end of the height adjustment motor; the mid-term induction heating coil (41) is driven by the height adjustment motor to move in the vertical direction along the induction coil height adjustment slideway (81); the mid-term induction heating coil (41) is electrically connected to the mid-term medium-frequency induction heating control cabinet; the mid-term medium-frequency induction heating control cabinet is installed in the device parameter control area, and adjusts the temperature of the rail after passing through the mid-term induction heating coil (41) by controlling its heating output power; The air jet cooling system (6) is composed of an air compression pressure vessel installed in the device parameter control area, an air jet pressure regulating device, and an air jet cooling wind box fixedly installed on the device support seat (8); the air compression pressure vessel is matched and connected with the air jet pressure regulating device; the height of the air jet cooling wind box from the rail tread can be driven and adjusted by the height adjustment motor, and the wind pressure of the air jet cooling wind box is adjusted by the air jet pressure regulating device; The first infrared thermometer (3) is matched and installed between the initial preheating induction heating coil (21) and the mid-term induction heating coil (41) in the advancing direction of the rail; the measuring position of the first infrared thermometer (3) is the tread of the rail; The second infrared thermometer (5) is matched and installed between the mid-term induction heating coil (41) and the air jet cooling wind box in the direction of travel of the rail; the measurement position of the second infrared thermometer (5) is at the tread of the rail head; The third infrared thermometer (7) is matched and installed in front of the air jet cooling wind box in the advancing direction of the rail; the measuring position of the third infrared thermometer (7) is the top tread of the rail.

2. The device for increasing the depth of the quenching hardened layer of the rail head according to claim 1, characterized in that: The lower part of the rail feeding platform (11) is matched with a platform moving wheel.

3. The device for increasing the depth of the quenching hardened layer of the rail head according to claim 1, characterized in that: Both ends of the initial preheating induction heating coil (21) are provided with roller-type rail positioning fixtures to ensure that the distance between the initial preheating induction heating coil (21) and the rail head tread remains unchanged during the heat treatment of the rail; the initial medium-frequency induction heating control cabinet can increase the surface temperature of the rail from room temperature to above the austenite transformation temperature by adjusting its output power, and the preheating temperature is detected by the first infrared thermometer (3), and it is required that the surface temperature at this time is lower than the final heat treatment temperature.

4. The device for increasing the depth of the quenching hardened layer of the rail head according to claim 1, characterized in that: When the rail passes through the mid-term induction heating coil (41), low power is required to allow the rail temperature to continue to slowly increase to the temperature required by the process. This process can also allow heat to be continuously transferred to the center, effectively reducing the temperature difference between the center and the surface. The second infrared thermometer (5) detects the tread temperature before the rail head is cooled by air jets. At this time, the temperature should be controlled within the range required by the process.

5. The device for increasing the depth of the quenching hardened layer of the rail head according to claim 1, characterized in that: The gap between the air jet nozzle of the air jet cooling wind box and the rail top surface is 45 mm to 55 mm. After the rail passes through the air jet cooling system (6), the third infrared thermometer (7) detects the temperature of the rail head after cooling. The temperature is required to be between 300° C. and 600° C. At this time, if the temperature after the air jet exceeds the process requirements, the air pressure should be adjusted in time.