Pavement structure for asphalt road maintenance

By combining the emulsified asphalt bonding layer, thin cover layer and gravel seal wear-resistant layer on asphalt pavement, the problem of insufficient wear resistance of asphalt pavement in the prior art is solved, and more efficient pavement maintenance and Extended service life.

CN221989003UActive Publication Date: 2024-11-12JIANGSU SILMA ROAD ENVIRONMENTAL PROTECTION MATERIALS GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323490524.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-20
Publication Date
2024-11-12
Estimated Expiration
2033-12-20

AI Technical Summary

Technical Problem

The existing asphalt pavement has cracks, ruts, pits and other diseases under the influence of traffic loads, resulting in structural damage. The existing maintenance technology cannot make full use of the original pavement and has the problem of insufficient wear resistance.

Method used

Using a combined structure of emulsified asphalt bonding layer, thin-layer cover layer and gravel seal wear-resistant layer, the emulsified asphalt bonding layer bonds the thin-layer cover layer to the original asphalt pavement layer, the thin-layer cover layer and The wear-resistant layer of gravel seal improves the wear resistance of the road surface.

Benefits of technology

On the basis of making full use of the original pavement layer, improve the wear resistance of asphalt pavement, extend the service life, reduce maintenance costs, and enhance the wear resistance of the pavement.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221989003U_ABST
    Figure CN221989003U_ABST
Patent Text Reader

Abstract

The utility model discloses a pavement structure for asphalt road maintenance, which relates to the technical field of pavement structures and mainly comprises an original asphalt pavement layer, an emulsified asphalt bonding layer, a thin overlay layer and a rubble seal wear-resistant layer which are sequentially laid on the original asphalt pavement layer from bottom to top. The emulsified asphalt bonding layer is used for bonding the thin overlay layer to the original asphalt pavement layer, and the thin overlay layer is used for maintaining the original asphalt pavement layer. The thin overlay layer is adhered to the original asphalt pavement layer through the emulsified asphalt adhesive layer, and the rubble seal wear-resistant layer is paved on the thin overlay layer, so that the wear resistance of the asphalt pavement can be improved on the premise of fully utilizing the original asphalt pavement layer, and the maintenance effect of the thin overlay layer on the original asphalt pavement layer is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of pavement structures, in particular to a pavement structure for asphalt road maintenance. Background Art

[0002] With the increase in the service life of asphalt pavements in my country, the growth of transportation volume, and the combined effects of various climatic factors, asphalt pavements have developed defects such as cracking, rutting, and potholes. Rainwater and other factors can penetrate into the pavement structure through cracks, gradually causing structural damage under the action of traffic loads, seriously reducing the service life of asphalt pavements and increasing traffic hazards.

[0003] The occurrence of the above problems affects the quality of asphalt pavement and has become an important issue that needs to be solved urgently in the field of road maintenance. In the existing technology, the traditional practice is usually to dig out the original basic pavement structure and then lay a new pavement structure, but this practice cannot make full use of the original pavement and will cause waste of waste and environmental pollution; or spraying fog seal materials for covering treatment, but in the application of existing fog seal technology, due to the thin seal layer and weak wear resistance, the surface of the fog seal layer is worn and consumed in the road section where heavy-loaded vehicles are driving, resulting in a decrease in maintenance effect and a reduction in service life.

[0004] Therefore, it is urgent to provide a pavement structure for asphalt road maintenance to solve the above problems existing in the prior art. Utility Model Content

[0005] The purpose of the utility model is to provide a pavement structure for asphalt road maintenance to solve the problems existing in the above-mentioned prior art, to improve the wear resistance of the asphalt pavement while making full use of the original asphalt pavement layer, and to ensure the maintenance effect of the thin layer overlay on the asphalt pavement.

[0006] To achieve the above purpose, the utility model provides the following solutions:

[0007] The utility model provides a pavement structure for asphalt road maintenance, comprising an original asphalt pavement layer, an emulsified asphalt bonding layer, a thin overlay layer and a chip seal wear-resistant layer, wherein the emulsified asphalt bonding layer, the thin overlay layer and the chip seal wear-resistant layer are sequentially laid on the original asphalt pavement layer from bottom to top, the emulsified asphalt bonding layer is used to bond the thin overlay layer to the original asphalt pavement layer, and the thin overlay layer is used to maintain the original asphalt pavement layer.

[0008] Preferably, the emulsified asphalt bonding layer is a polymer-modified emulsified asphalt bonding layer.

[0009] Preferably, the polymer-modified emulsified asphalt bonding layer is a cationic SBS-modified emulsified asphalt bonding layer.

[0010] Preferably, the spraying amount of the emulsified asphalt bonding layer is 200g / m 2 ~350g / m 2 .

[0011] Preferably, the chip seal wear-resistant layer is a wear-resistant layer formed by paving a chip seal binder.

[0012] Preferably, the thin layer of overlay is a thin layer of overlay formed by paving an asphalt binder.

[0013] Preferably, the thickness of the thin layer cover is between 10 mm and 25 mm.

[0014] Compared with the prior art, the utility model has achieved the following technical effects:

[0015] The utility model provides a pavement structure for asphalt road maintenance. A thin overlay layer is bonded to an original asphalt pavement layer through an emulsified asphalt bonding layer, which can play a good maintenance role on the original asphalt pavement. The crushed stone seal wear-resistant layer laid on the thin overlay layer improves the wear resistance of the asphalt pavement and enhances the maintenance effect on the asphalt pavement. The utility model can improve the wear resistance of the asphalt pavement while making full use of the original asphalt pavement layer, and ensure the maintenance effect of the thin overlay layer on the asphalt pavement. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0017] Figure 1 A schematic diagram of a pavement structure for asphalt road maintenance provided by the utility model.

[0018] In the figure: 1-original asphalt pavement layer; 2-emulsified asphalt bonding layer; 3-thin layer of overlay; 4-chip seal wear layer. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] The purpose of the utility model is to provide a pavement structure for asphalt road maintenance to solve the problems existing in the above-mentioned prior art, to improve the wear resistance of the asphalt pavement while making full use of the original asphalt pavement layer, and to ensure the maintenance effect of the thin layer overlay on the asphalt pavement.

[0021] In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0022] like Figure 1 As shown, in an embodiment of the utility model, a pavement structure for asphalt road maintenance is provided, comprising an original asphalt pavement layer 1, an emulsified asphalt bonding layer 2, a thin layer overlay layer 3 and a chip seal wear-resistant layer 4, wherein the emulsified asphalt bonding layer 2, the thin layer overlay layer 3 and the chip seal wear-resistant layer 4 are sequentially laid on the original asphalt pavement layer 1 from bottom to top, the emulsified asphalt bonding layer 2 is used to bond the thin layer overlay layer 3 to the original asphalt pavement layer 1, and the thin layer overlay layer 3 is used to maintain the original asphalt pavement layer 1.

[0023] In this embodiment, the thin layer of overlay 3 is bonded to the original asphalt pavement layer 1 through the emulsified asphalt bonding layer 2, which can play a good maintenance role on the original asphalt pavement layer 1. The gravel seal wear-resistant layer 4 laid on the thin layer of overlay 3 improves the wear resistance of the original asphalt pavement layer 1 and enhances the maintenance effect on the original asphalt pavement layer 1. The utility model can improve the wear resistance of the original asphalt pavement layer 1 while fully utilizing the original asphalt pavement layer 1, and ensure the maintenance effect of the thin layer of overlay 3 on the original asphalt pavement layer 1.

[0024] In this embodiment, the emulsified asphalt bonding layer 2 is a polymer modified emulsified asphalt bonding layer, and the polymer modified emulsified asphalt bonding layer is a cationic SBS modified emulsified asphalt bonding layer. Before spraying the emulsified asphalt bonding layer 2, the surface of the original asphalt pavement layer 1 should be cleaned, and the dust on the surface should be blown away with a fan, and then the emulsified asphalt bonding layer 2 should be sprayed. The spraying amount of the emulsified asphalt bonding layer 2 is 200-350g / m 2 The specific spraying amount can be 300g / m 2 , to meet the bonding strength, which increases the pavement bonding strength and extends the service life of the road.

[0025] In this embodiment, the thin layer of overlay 3 is a thin layer of overlay 3 formed by paving an asphalt binder. The asphalt binder is a combination of asphalt and aggregate. The aggregate includes coarse aggregate and mineral powder. Specifically, the asphalt can be rubber asphalt, SMC or high-viscosity SBS modified asphalt, the coarse aggregate is basalt or diabase, and can also contain some milling materials. The mineral powder can be limestone powder. The oil-stone ratio of asphalt and aggregate is controlled at 4% to 6%; the coarse aggregate with a particle size of 0-3mm accounts for 20% to 30% of the aggregate, the coarse aggregate with a particle size of 5-10mm accounts for 10% to 40%, and the coarse aggregate with a particle size of 10-20mm accounts for 10%. Coarse aggregate accounts for 30% to 60%, and mineral powder accounts for 2% to 7%. Among them, the thickness of the thin overlay layer 3 is 10 to 25 mm. The thin overlay layer 3 can improve the original flatness of the original asphalt pavement layer 1. At the same time, the thickness is only 1 / 3 to 1 / 2 of the thickness of the traditional wear layer, saving 30% to 40% of the construction and maintenance costs, reducing the consumption of resources and energy, and at the same time increasing the load and shear stress that the road surface can withstand. The traffic interruption time during construction is short, and the impact on traffic flow is small. The thin overlay layer 3 can play a better maintenance role on the original asphalt pavement layer 1, and enhances the maintenance effect of the original asphalt pavement layer 1.

[0026] In this embodiment, the chip seal wear layer 4 is a wear layer formed by laying a chip seal binder, and the chip seal binder is composed of wear-resistant aggregate and fast-cracking or medium-cracking emulsified asphalt. Specifically, the wear-resistant aggregate is 10-20 mesh corundum, and the spraying amount of emulsified asphalt is 0.7-1.1 kg / m 2 After the spraying is completed, the road is compacted and traffic can be opened after drying. The chip seal wear layer 4 improves the wear resistance of the original asphalt pavement layer 1 and enhances the maintenance effect of the original asphalt pavement layer 1.

[0027] Specifically, the pavement structure paving process of asphalt road maintenance in this embodiment is as follows:

[0028] First, clean the surface of the original asphalt pavement layer 1 with a fan, and then spray the emulsified asphalt bonding layer 2. The spraying amount of the emulsified asphalt bonding layer 2 is 200g / m 2 ~350g / m 2 , and then the hot paving thin layer surface layer 3 is constructed. The thickness of the thin layer surface layer 3 is 1.0 to 2.5 cm. After the emulsified asphalt bonding layer 2 is completely dry, the thin layer surface layer 3 is laid.

[0029] After the thin overlay layer 3 is completely dried and formed, the chip seal wear layer 4 is evenly laid on the thin overlay layer 3 by a synchronous chip seal vehicle. The wear-resistant aggregate selected for the chip seal wear layer 4 is 10-20 mesh corundum, bonded with fast-cracking or medium-cracking emulsified asphalt, and the spraying amount of emulsified asphalt is 0.7-1.1 kg / m 2After spraying, compact it and wait for it to dry before opening it to traffic. The chip seal wear layer 4 improves the wear resistance of the asphalt pavement and has a good maintenance effect on the original asphalt pavement layer 1.

[0030] The present invention uses specific examples to illustrate the principle and implementation of the present invention. The above examples are only used to help understand the method and core idea of ​​the present invention. At the same time, for those skilled in the art, according to the idea of ​​the present invention, there will be changes in the specific implementation and application scope. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A pavement structure for asphalt road maintenance, Features: It includes an original asphalt pavement layer, an emulsified asphalt bonding layer, a thin overlay layer and a chip seal wear-resistant layer. The emulsified asphalt bonding layer, the thin overlay layer and the chip seal wear-resistant layer are laid on the original asphalt pavement layer from bottom to top in sequence. The emulsified asphalt bonding layer is used to bond the thin overlay layer to the original asphalt pavement layer. The thin overlay layer is used to maintain the original asphalt pavement layer.

2. The pavement structure for asphalt road maintenance according to claim 1, Features: The emulsified asphalt bonding layer is a polymer modified emulsified asphalt bonding layer.

3. The pavement structure for asphalt road maintenance according to claim 2, Features: The polymer modified emulsified asphalt bonding layer is a cationic SBS modified emulsified asphalt bonding layer.

4. The pavement structure for asphalt road maintenance according to any one of claims 1 to 3, Features: The spraying amount of the emulsified asphalt bonding layer is 200g / m 2 ~350g / m 2 .

5. The pavement structure for asphalt road maintenance according to claim 1, Features: The chip seal wear-resistant layer is a wear-resistant layer formed by laying chip seal binder.

6. The pavement structure for asphalt road maintenance according to claim 1, Features: The thin overlay layer is a thin overlay layer formed by paving an asphalt binder.

7. The pavement structure for asphalt road maintenance according to claim 4, Features: The thickness of the thin layer cover is 10 mm to 25 mm.