Membrane clamping device for testing water absorption rate of membrane material

By designing a membrane jig containing frame and blessing parts, using cylinders and magnetic suction sheets to fix the film material, the problem of low water absorption test results and no repetition of the photoresist film is solved, and more accurate and reliable water absorption test.

CN222013872UActive Publication Date: 2024-11-15MINSEOA (BEIJING) ADVANCED MATERIALS DEV CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202323516164.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-22
Publication Date
2024-11-15
Estimated Expiration
2033-12-22

AI Technical Summary

Technical Problem

The lack of professional devices in the prior art to test the water absorption rate of the photoresist film, resulting in low results and no repetition. It is mainly because the film is prone to curl and adsorb on the cup wall, affecting the water absorption area and test accuracy.

Method used

A membrane jigator including a frame and a bracelet is designed, and the membrane material is fixed with cylinders and magnetic suction sheets to ensure that it is spread and fixed, avoid the impact of patching, and improve the accuracy and repeatability of the test data.

Benefits of technology

The cylindrical raised fixed film material improves the accuracy and repeatability of the test data, ensuring the reliability and consistency of the water absorption test.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222013872U_ABST
    Figure CN222013872U_ABST
Patent Text Reader

Abstract

The utility model discloses a membrane clamping device for testing the water absorption rate of a membrane material, which comprises frames and clamping pieces, the clamping pieces are arranged at the periphery and the central position of the frames, the two frames are oppositely arranged, and the clamping pieces are used for clamping the membrane material to be tested. The device disclosed by the utility model is simple and practical in structure, simple and convenient to operate and high in working efficiency, the test membrane material is spread and fixed through the cylindrical bulge, the influence of the sticking of the test membrane material on the water absorption rate is avoided, and the accuracy and data repeatability of test data are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of film material testing, in particular to a film clamping device for testing the water absorption rate of a film material. Background Art

[0002] During the research and development of polyimide photoresist, it is necessary to test the water absorption rate of the film after the glue liquid is cured, so as to infer the reliability of the photoresist in the device.

[0003] At present, there is no professional equipment for testing the water absorption rate of photoresist films. The laboratory puts the film into a beaker filled with water, then puts the beaker into a constant temperature bath for a certain period of time, takes it out and wipes the surface of the film dry, and calculates the water absorption rate by comparing the weight change before and after the test. However, polyimide film is easy to curl and adsorb on the wall of the cup, so the film cannot be fully stretched, and the water absorption area of ​​the film is reduced after being attached to the wall of the cup, so the water absorption rate result of the test is low. In addition, the degree of curling and the degree of adsorption of the film to the wall of the cup are different in each test, so the test data is not repeatable.

[0004] Therefore, there is an urgent need for a film clamp for testing the water absorption rate of film materials. Utility Model Content

[0005] The utility model aims to provide a film clamp for testing the water absorption rate of film materials, so as to solve the problems that the water absorption rate test result in the above-mentioned background technology is low and the batch test data cannot be repeated.

[0006] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0007] The utility model provides a film clamp for testing the water absorption rate of film materials, comprising a frame and a supporting member, wherein the supporting member is arranged around and at the center of the frame, two frames are arranged oppositely, and the supporting member is used for supporting the testing film material.

[0008] The film clamp for testing the water absorption rate of the film material, preferably, the supporting member includes a plurality of cylinders and a magnetic sheet, one end of the cylinder is connected to the frame, the plurality of cylinders do not contact each other, and the other end of the cylinder is provided with the magnetic sheet.

[0009] In the film clamp for testing the water absorption rate of film materials, preferably, the cylinders are distributed at the four corners of the frame and the center of the frame.

[0010] The film clamp for testing the water absorption rate of the film material, preferably, the surface area of ​​the frame is 16-64cm 2 .

[0011] In the film clamp for testing the water absorption rate of the film material, preferably, the sum of the surface areas of all the cylinders is 2%-3% of the surface area of ​​the frame.

[0012] In the film clamp for testing the water absorption rate of a film material, preferably, the height of the cylinder is 1-3 cm.

[0013] The utility model adopts the above technical solution, which has the following advantages:

[0014] The device of the utility model has a simple and practical structure, is easy to operate and has high working efficiency. The test film material is spread and fixed by the cylindrical protrusion, and the influence of the test film material application on the water absorption rate is avoided, thereby improving the accuracy and repeatability of the test data. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the use of the utility model;

[0016] Figure 2 It is a structural diagram of the framework.

[0017] Reference numerals in the figures:

[0018] 1. Frame; 2. Cylinder; 3. Magnetic sheet; 4. Test film. DETAILED DESCRIPTION

[0019] In order to make the purpose, technical solution and advantages of the utility model clearer, the technical solution of the utility model will be clearly and completely described below in conjunction with the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] In the description of the present invention, it should be noted that the terms "one end" and "the other end" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the system or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0021] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the term "provided with" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be an indirect connection through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0022] The utility model provides a film clamp for testing the water absorption rate of a film material. The utility model comprises a frame and a supporting member, wherein the supporting member is arranged around and at the center of the frame, and the supporting member is used to support the test film material. The device of the utility model has a simple and practical structure, is easy to operate, and has high working efficiency. The test film material is spread and fixed by a cylindrical protrusion, and the influence of the test film material application on the water absorption rate is avoided, thereby improving the accuracy and repeatability of the test data.

[0023] Below, a film clamp for testing the water absorption rate of a film material provided by an embodiment of the utility model is described in detail with reference to the accompanying drawings.

[0024] Reference Figure 1 A film clamp for testing the water absorption rate of a film material comprises a frame 1 and a supporting member. The supporting member is arranged around and at the center of the frame 1 and is used to support a test film material 4 .

[0025] Reference Figure 2 As shown, the support member includes a plurality of cylinders 2 and a magnetic sheet 3, one end of the cylinder 2 is connected to the frame 1, the plurality of cylinders 2 do not contact each other, and the other end of the cylinder 2 is provided with a magnetic sheet 3. Further, the cylinder 2 is provided at the four corners of the frame 1 and at the center point of the frame 1. The magnetic sheet 3 can be relatively adsorbed and is used to fix and support the test film 4.

[0026] Among them, the surface area of ​​frame 1 is 16-64cm 2 , ensuring that the circular area does not form sharp edges, that is, avoiding the frame 1 being too small, resulting in a small circular surface area of ​​the cylinder 2, a strong pressure, and easy damage to the film when clamping the film. Reduce the balance weighing error and ensure that the test film is a whole film, and have easy operation. The area of ​​the film clamping frame cannot be less than 5 square centimeters, in order to ensure that the circular area does not form sharp edges.

[0027] The adjacent cylinders 2 cannot touch each other to preserve the contact area between the membrane and water as much as possible. The total surface area of ​​the cylinders 2 is 2%-3% of the surface area of ​​the frame 1. If the circular surface area of ​​the cylinders is too large, it will affect the adsorption effect of the surface of the test membrane 4 on water and affect the test results. If the circular surface area of ​​the cylinders 2 is too small, it is easy to form sharp edges and damage the test membrane 4.

[0028] The height of the cylinder 2 is 1-3 cm to ensure that the test film 4 will not adhere to the frame 1, and at the same time ensure that the overall size of the film clamp is convenient for handholding and operation.

[0029] Furthermore, the frame 1 and the cylinder 2 are made of plastic material, which can eliminate the pollution of water by the device, for example, polytetrafluoroethylene, PP, PE.

[0030] The film clamp of the utility model is suitable for testing the water absorption rate below 100° C., and the film clamp of the utility model is suitable for testing the water absorption rate of the test film material 4 with a thickness of 10-100 μm.

[0031] Example 1

[0032] In this embodiment, the length of the frame 1 is 5 cm, the width of the frame 1 is 6 cm, and therefore the area of ​​the frame 1 is 30 square centimeters. The bottom radius of the cylinder 2 in the frame 1 is 0.2 cm, and the height of the cylinder 2 is 1.5 cm.

[0033] How to do it:

[0034] Take the first piece as an example:

[0035] S1: Cut the polyimide film as the test film material 4 into three pieces, each piece has a size of 5 cm*6 cm, and each piece weighs 28.90 mmg.

[0036] S2: Place the polyimide film between the two frames 1 and fix it via the magnetic sheet 3.

[0037] S3: Place the entire film holder with the polyimide film in a constant temperature water bath and keep it for 24 hours. After the soaking is completed, open the film holder and take out the polyimide film.

[0038] S4: Wipe the water off the surface of the polyimide film with dust-free paper and weigh 29.08 mg. The water absorption rate is calculated to be 0.62%.

[0039] According to the above operation method, the test was repeated. The second piece weighed 29.02 mg before the test and 29.20 mg after the test. The calculated water absorption was 0.68%.

[0040] According to the above operation method, the test was repeated. The third piece weighed 28.95 mg before the test and 29.14 mg after the test. The calculated water absorption was 0.65%.

[0041] Finally, the water absorption of the first, second, and third sheets was averaged, and it was confirmed that the water absorption of the polyimide adhesive film was 0.65%.

[0042] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the utility model.

Claims

1. A film clamp for testing the water absorption rate of a film material, characterized in that: It includes a frame and a supporting member, wherein the supporting member is arranged around and at the center of the frame, and two frames are arranged opposite to each other, and the supporting member is used to support the test film material; The supporting member includes a plurality of cylinders and a magnetic sheet. One end of the cylinder is connected to the frame, and the plurality of cylinders do not contact each other. The magnetic sheet is disposed at the other end of the cylinder.

2. The film clamp for testing the water absorption rate of a film material according to claim 1, characterized in that: The cylinders are distributed at the four corners of the frame and the center of the frame.

3. The film clamp for testing the water absorption rate of a film material according to claim 2, characterized in that: The surface area of ​​the frame is 16-64 cm 2 .

4. The film clamp for testing the water absorption rate of a film material according to claim 3, characterized in that: The sum of the surface areas of all the cylinders is 2%-3% of the surface area of ​​the frame.

5. The film clamp for testing the water absorption rate of a film material according to claim 4, characterized in that: The height of the cylinder is 1-3 cm.

Citation Information

Cited By

  • Pre-detection system and detection method for PDLC (Polymer Dispersed Liquid Crystal) membrane material

    CN120721752A