Partitioned doped high-voltage-resistant groove silicon carbide VDMOS (Vertical Double-diffused Metal Oxide Semiconductor)

By designing partitioned doping and protection zones, the problems of electric field concentration and insufficient voltage withstand capability of trench gate silicon carbide VDMOS devices are solved, achieving a combination of high voltage withstand, low resistance, and high reliability, thus improving the overall performance of the device.

CN222051773UActive Publication Date: 2024-11-22GLOBAL POWER TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420725630.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-09
Publication Date
2024-11-22
Estimated Expiration
2034-04-09

AI Technical Summary

Technical Problem

The reliability issues and insufficient withstand voltage caused by the electric field concentration at the gate corner of trench-gate silicon carbide VDMOS devices make it difficult to combine low on-resistance and high withstand voltage, thus limiting the expansion of device applications.

Method used

A high-voltage trench silicon carbide VDMOS structure with partitioned doping is adopted, including a partitioned doped drift layer and a protection zone. Combined with the trench gate structure, the reverse breakdown voltage of the device is improved by the partitioned doped drift layer, and the protection zone is built at the gate corner to alleviate electric field concentration.

Benefits of technology

It achieves a combination of high withstand voltage, low resistance, and high reliability, improving device performance, solving the problems of electric field concentration and insufficient withstand voltage of trench gate silicon carbide VDMOS, and optimizing the on-resistance and reliability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222051773U_ABST
    Figure CN222051773U_ABST
Patent Text Reader

Abstract

The utility model provides a partitioned doped high-voltage-resistant groove silicon carbide VDMOS. The partitioned doped high-voltage-resistant groove silicon carbide VDMOS is characterized in that the lower side surface of a first drift layer is connected to the upper side surface of a silicon carbide substrate; the lower side face of the second drift layer is connected to the upper side face of the first drift layer, a groove is formed in the second drift layer, and protection areas are arranged on the two sides of the bottom of the groove respectively; the gate dielectric layer is arranged on the groove, and a groove is formed in the gate dielectric layer; the well region is connected to the upper side face of the second drift layer, a source region is arranged in the well region, and one side face of the well region and one side face of the source region are connected to the side face of the gate dielectric layer; a gate metal layer, wherein the gate metal layer is arranged in the groove; the source electrode metal layer is respectively connected with the well region and the source region; and the drain electrode metal layer is connected to the lower side surface of the silicon carbide substrate, so that high voltage resistance, low resistance and high reliability are realized at the same time, and the performance of the device is excellent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a zone-doped high-voltage trench silicon carbide VDMOS. Background Art

[0002] Silicon carbide (VDMOS), a representative silicon carbide power device, is widely used in electric vehicles, aerospace, power conversion, and other fields. Trench-gate silicon carbide VDMOS has attracted much attention for its advantages such as low on-resistance and low drive charge. However, it suffers from gate reliability issues caused by electric field concentration at the gate corners. Furthermore, the device's withstand voltage is lower than that of a planar-gate VDMOS structure with the same epitaxial layer thickness. This makes it difficult for trench gates to achieve both low on-resistance and high withstand voltage, limiting further expansion of device applications. Utility Model Content

[0003] The technical problem to be solved by the utility model is to provide a partition-doped high-voltage trench silicon carbide VDMOS, which achieves high voltage resistance, low resistance and high reliability, so that the device performance is excellent.

[0004] The utility model is implemented as follows: a high-voltage trench silicon carbide VDMOS with partitioned doping, comprising:

[0005] Silicon carbide substrate,

[0006] a first drift layer, wherein a lower side of the first drift layer is connected to an upper side of the silicon carbide substrate;

[0007] a second drift layer, wherein a lower side of the second drift layer is connected to an upper side of the first drift layer, a groove is provided on the second drift layer, and protection zones are provided on both sides of a bottom of the groove;

[0008] a gate dielectric layer, the gate dielectric layer being disposed on the groove, and a trench being disposed in the gate dielectric layer;

[0009] a well region, the well region being connected to the upper side of the second drift layer, a source region being provided in the well region, and a side surface of the well region and a side surface of the source region being connected to a side surface of the gate dielectric layer;

[0010] a gate metal layer, the gate metal layer being disposed in the trench;

[0011] a source metal layer, the source metal layer being connected to the well region and the source region respectively;

[0012] and a drain metal layer connected to the lower side of the silicon carbide substrate.

[0013] The advantages of the present invention are:

[0014] 1. The device adopts a partitioned doped drift layer structure, which can effectively improve the reverse withstand voltage of the device;

[0015] 2. The device adopts a trench gate structure to ensure that the device can achieve low resistance conduction;

[0016] 3. The device has a protection zone, which alleviates the electric field concentration problem at the corner of the trench gate, effectively protects the device gate, and improves device reliability;

[0017] 4. The overall device structure achieves high voltage resistance, low resistance and high reliability, making the device have excellent performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] The present invention will be further described below with reference to the accompanying drawings and embodiments.

[0019] Figure 1 This is a schematic diagram of a high-voltage trench silicon carbide VDMOS with partitioned doping according to the present invention.

[0020] Figure 2 The present invention provides a flow chart of a method for preparing a zone-doped high-voltage trench silicon carbide VDMOS.

[0021] Figure 3 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 1 .

[0022] Figure 4 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 2 .

[0023] Figure 5 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 3 .

[0024] Figure 6 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 4 .

[0025] Figure 7 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 5 .

[0026] Figure 8 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 6 .

[0027] Figure 9This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 7 .

[0028] Figure 10 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 8 .

[0029] Figure 11 This is a cross-sectional view of the process of a high-voltage trench silicon carbide VDMOS with partitioned doping in this utility model. Figure 9 . DETAILED DESCRIPTION

[0030] To facilitate understanding of the present application, the present application will be described more fully below with reference to the accompanying drawings. The accompanying drawings provide embodiments of the present application. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided to make the disclosure of the present application more thorough and comprehensive.

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art to which this application pertains. The terms used herein in the specification of this application are for the purpose of describing specific embodiments only and are not intended to limit this application.

[0032] It should be understood that when an element or layer is referred to as being "on," "adjacent to," "connected to," or "coupled to" another element or layer, it may be directly on, adjacent to, connected to, or coupled to the other element or layer, or there may be intervening elements or layers. Conversely, when an element is referred to as being "directly on," "in contact with," "directly connected to," or "directly coupled to" another element or layer, there are no intervening elements or layers. It should be understood that although the terms first, second, third, etc. may be used to describe various elements, components, regions, layers, doping types, and / or portions, these elements, components, regions, layers, doping types, and / or portions should not be limited by these terms. These terms are merely used to distinguish one element, component, region, layer, doping type, or portion from another element, component, region, layer, doping type, or portion. Therefore, without departing from the teachings of the present invention, the first element, component, region, layer, doping type, or portion discussed below may be represented as a second element, component, region, layer, or portion.

[0033] Spatially relative terms such as "under," "beneath," "beneath," "under," "above," "above," etc., may be used herein to describe the relationship of one element or feature to other elements or features depicted in the figures. It should be understood that, in addition to the orientations depicted in the figures, spatially relative terms also encompass different orientations of the device in use and operation. For example, if the device in the figures is flipped over, an element or feature described as "under" or "beneath" or "beneath" the other elements would be oriented "over" the other elements or features. Thus, the exemplary terms "under" and "under" may encompass both the upper and lower orientations. Additionally, the device may also include alternative orientations (e.g., rotated 90 degrees or other orientations), and the spatial descriptors used herein are to be interpreted accordingly.

[0034] As used herein, the singular forms "a," "an," and "the" may also include the plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "include," "comprising," "having," and the like specify the presence of stated features, integers, steps, operations, components, parts, or combinations thereof, but do not preclude the presence or addition of one or more other features, integers, steps, operations, components, parts, or combinations thereof. Also, in this specification, the term "and / or" includes any and all combinations of the relevant listed items.

[0035] like Figure 1 As shown, the embodiment of the present application provides a high-voltage trench silicon carbide VDMOS with partitioned doping, including:

[0036] Silicon carbide substrate 1,

[0037] a first drift layer 2, wherein the lower side of the first drift layer 2 is connected to the upper side of the silicon carbide substrate 1;

[0038] a second drift layer 3, wherein the lower side of the second drift layer 3 is connected to the upper side of the first drift layer 2, a groove 31 is provided on the second drift layer 3, and protection zones 32 are provided on both sides of the bottom of the groove 31;

[0039] a gate dielectric layer 4 , the gate dielectric layer 4 being disposed on the groove 31 , and having a trench 41 therein;

[0040] a well region 5, the well region 5 being connected to the upper side of the second drift layer 3, a source region 51 being provided in the well region 5, and a side surface of the well region 5 and a side surface of the source region 51 being connected to a side surface of the gate dielectric layer 4;

[0041] a gate metal layer 6 disposed in the trench 41;

[0042] a source metal layer 7, the source metal layer 7 being connected to the well region 5 and the source region 51 respectively;

[0043] and a drain metal layer 8 , wherein the drain metal layer 8 is connected to the lower side of the silicon carbide substrate 1 .

[0044] The first drift layer 2 has a thickness of 1 μm, the second drift layer 3 has a thickness of 2 μm, the doping concentration of the first drift layer 2 is equal to the doping concentration of the protection zone 32, and the doping concentration of the first drift layer 2 is greater than the doping concentration of the second drift layer 3. The silicon carbide substrate 1, the first drift layer 2, the second drift layer 3 and the source region 51 are all N-type; the protection zone 32 and the well region 5 are both P-type.

[0045] The device adopts a partitioned doped drift layer structure. The first drift layer 2 adopts a high doping concentration to withstand high voltage with a smaller thickness near the drain layer of the device, so as to reduce the influence of the drain-source electric field on the gate structure of the device and reduce the on-resistance of the device. The doping concentration is excessive with the silicon carbide substrate 1 to avoid sudden changes in the internal resistance of the device and affect the device characteristics. The second drift layer 3 adopts a lower doping concentration to use a thicker space charge region to withstand the reverse voltage when the device is reversely withstand voltage, reduce the internal pressure of the device, and achieve a transition from the high concentration of the silicon carbide substrate. The partitioned doping structure can effectively improve the reverse withstand voltage of the device.

[0046] Since the doping concentration of the second drift layer 3 of the device is low, it has a certain ability to alleviate the electric field concentration at the corner of the device gate compared to the high doping situation, so the electric field concentration at the bottom of the device gate has little effect. However, the gate reliability of the device cannot be guaranteed at the gate corner. In this case, a p-type protection zone is constructed to further enhance the reliability of the device gate. In order not to affect the conduction characteristics of the device, the protection zone 32 is set below the gate dielectric layer and does not affect the electron flow channel from the source region 51 to the drain. The overall structure of the device adopts partitioned doping and p-type protection zone structure, which reduces the device's maximum on-resistance, improves the device's withstand voltage, ensures the device's gate reliability, and has excellent device performance.

[0047] like Figures 1 to 11 As shown, the method for preparing the silicon carbide VDMOS obtained by the above manufacturing method includes the following steps:

[0048] Step 1: Deposit metal on one side of the silicon carbide substrate 1 to form a drain metal layer 8, and deposit and grow a first drift layer 2 on the other side of the silicon carbide substrate 1. Then, grow a second drift layer 3 on the first drift layer 2. The first drift layer 2 is 1 μm thick, and the second drift layer 3 is 2 μm thick.

[0049] Step 2: depositing a barrier layer a above the second drift layer 3, etching the barrier layer a to form a through hole, and performing ion implantation into the second drift layer 3 to form a protection zone 32 at a depth of 900 nm to 1200 nm in the middle of the second drift layer 3.

[0050] Step 3: remove the barrier layer a and form a well region 5 by ion implantation into the second drift layer 3. The ion implantation energy is 10-200 keV and the depth is 600 nm.

[0051] Step 4: Re-form the barrier layer a, etch to form a through hole, and perform ion implantation into the well region 5 through the through hole to form a source region 51. The implantation energy is 10-100 keV and the depth is 300 nm.

[0052] Step 5: remove the original barrier layer a, re-form the barrier layer a, etch to form a source metal deposition area, perform metal deposition, and form a source metal layer 7;

[0053] Step 6: Remove the original barrier layer a, re-form the barrier layer a, etch the barrier layer a, the well region 5, and the second drift layer 3 to form a through hole and a groove 31. The etching depth is 1000 nm. After etching, dry oxygen oxidation is performed to form a gate dielectric layer 4.

[0054] Step 7: remove the original barrier layer a, re-form the barrier layer a, etch the barrier layer a and the gate dielectric layer 4 to form a through hole and a trench 41, deposit metal in the trench 41 through the through hole to form a gate metal layer 6; remove the barrier layer a, and complete the manufacturing.

[0055] The silicon carbide substrate 1, the first drift layer 2, the second drift layer 3 and the source region 51 are all N-type; the protection region 32 and the well region 5 are all P-type, and the doping concentration of the silicon carbide substrate 1 is 2e18cm -3 The doping concentration of the first drift layer 2 is 1e17cm -3 The doping concentration of the second drift layer 3 is 1e16cm-3, the doping concentration of the protection zone 32 is 2e17cm-3, and the doping concentration of the source region 51 is 2e18cm-3. -3 The doping concentration of the well region 5 is 3e17 cm -3 .

[0056] The gate dielectric layer 4 is silicon dioxide, and the doping concentration of the silicon carbide substrate 1 is to form an ohmic contact with the drain metal layer 8 while reducing the drain contact resistance; since the partitioned doping structure formed by the first drift layer 2 and the second drift layer 3 can ensure the voltage resistance characteristics of the device, the doping concentration of the first drift layer 2 is mainly intended to reduce the on-resistance of the device, the doping concentration of the second drift layer 3 is intended to improve the voltage resistance of the device, the doping concentration of the protection zone 32 is intended to achieve electric field concentration relief at the gate corner with a smaller doping area, the doping concentration of the well region 5 is intended to achieve effective shutdown of the device and reduce the gate-source capacitance to increase the switching speed of the device, and the doping concentration of the source region 51 is intended to form an ohmic contact with the source metal layer to reduce the on-resistance of the device.

[0057] Although the specific implementation methods of the present invention are described above, those skilled in the art should understand that the specific embodiments described are merely illustrative and are not intended to limit the scope of the present invention. Equivalent modifications and changes made by those skilled in the art in accordance with the spirit of the present invention should be included within the scope of protection of the claims of the present invention.

Claims

1. A high-voltage trench silicon carbide VDMOS with partitioned doping, characterized in that: include: Silicon carbide substrate, A first drift layer, wherein a lower side of the first drift layer is connected to an upper side of the silicon carbide substrate; a second drift layer, wherein the lower side of the second drift layer is connected to the upper side of the first drift layer, the second drift layer is provided with a groove, and protection areas are respectively provided on both sides of the bottom of the groove; a gate dielectric layer, wherein the gate dielectric layer is disposed on the groove, and a groove is disposed in the gate dielectric layer; A well region, the well region is connected to the upper side of the second drift layer, a source region is arranged in the well region, and one side of the well region and one side of the source region are connected to the side of the gate dielectric layer; A gate metal layer, wherein the gate metal layer is disposed in the groove; A source metal layer, the source metal layer is connected to the well region and the source region respectively; and a drain metal layer connected to the lower side of the silicon carbide substrate.

2. The high-voltage trench silicon carbide VDMOS with zone doping according to claim 1, characterized in that: The doping concentration of the first drift layer is equal to the doping concentration of the protection zone.

3. The high-voltage trench silicon carbide VDMOS with zone doping according to claim 1, characterized in that: The doping concentration of the first drift layer is greater than the doping concentration of the second drift layer.

4. The high-voltage trench silicon carbide VDMOS with zone doping according to claim 1, characterized in that: The thickness of the first drift layer is 1 μm, and the thickness of the second drift layer is 2 μm.

5. The high-voltage trench silicon carbide VDMOS with zone doping according to claim 1, characterized in that: The silicon carbide substrate, the first drift layer, the second drift layer and the source region are all N-type; the protection region and the well region are all P-type.