SMP welding hole structure
By designing the sinking tin groove, guide groove and air chamber in the SMP solder hole structure, the solder movement is guided, and the problem of solder flowing into the hole wall is solved, and the RF quality and ease of plugging and unplugging are improved.
Patent Information
- Application Number
- CN202323467981.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-19
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2033-12-19
AI Technical Summary
During SMP welding, solder easily flows into the hole wall, resulting in difficulty in plugging and unplugging, increasing losses, and affecting RF quality.
Design an SMP welding hole structure, including a sinking tin groove, a guide groove and an air chamber. The sinking tin groove is located at the opening of the upper surface of the cavity, and the guide groove is in communication with the air chamber, which is used to guide the solder to move along the sinking tin groove to avoid flow in. In the SMP connector, an arch head structure is formed to improve the RF quality.
It effectively avoids solder flow into the hole wall, reduces losses, improves RF quality, and solves plug-in and unplugging problems.
Smart Images

Figure CN222052109U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of microwave communications, in particular to an SMP welding hole structure. Background Art
[0002] SMP connectors are widely used in high-frequency and high-speed modules of matrix antennas, artificial satellites, military radars, and airborne equipment due to their high shielding, compact size, fast connection, and excellent RF performance.
[0003] like Figure 4 As shown, when the SMP is inserted into the cavity for sintering, the solder tends to flow into the hole wall and accumulate on the cavity surface, making it difficult to plug and unplug and increasing the loss. During sintering, it is not easy to add solder and voids are likely to occur, affecting the RF quality. Utility Model Content
[0004] In view of the above problems, the utility model provides a SMP welding hole structure.
[0005] The technical solution adopted is: an SMP welding hole structure, including a tin sinking tank, a guide groove and an air cavity, wherein the tin sinking tank, the guide groove and the air cavity are all arranged in the cavity;
[0006] The tin sinking tank is located at the opening of the upper surface of the cavity, and the bottom of the tin sinking tank is connected to the guide groove;
[0007] The guide groove is located between the tin sink and the air cavity;
[0008] The air cavity is communicated with the bottom of the guide groove.
[0009] Further, the tin sink is used to pre-place one of a solder ring, a solder wire and a solder paste.
[0010] Optionally, the depth of the tinning bath is twice the diameter of the solder wire.
[0011] Optionally, there is a gap between the guide groove and the inserted SMP.
[0012] Optionally, an air cavity is used to simulate and match the standing waves of the module.
[0013] Optionally, the tin sink has a diameter of 5.3mm and a depth of 0.3mm;
[0014] The guide groove has a diameter of 4.3 mm and a depth of 3.2 mm;
[0015] The air cavity has a diameter of 2.6 mm and a depth of 4.7 mm.
[0016] Optionally, the tin sinking tank is a truncated cone structure, and the diameter of the tin sinking tank at the opening of the cavity is larger than the diameter of the tin sinking tank at the connection with the guide groove.
[0017] The beneficial effects of the present utility model include at least one of the following:
[0018] 1. By opening a tin sink tank on the cavity, the solder can move along the tin sink tank toward the air cavity, and will not flow into the SMP connector to form structures such as arch heads. Compared with the existing welding hole structure, the RF quality is improved and the loss is reduced.
[0019] 2. The existing SMP welding hole structure is solved. When the SMP is inserted into the cavity for sintering, the solder tends to flow into the hole wall and accumulate on the cavity surface, making it difficult to plug and unplug and increasing losses. During sintering, it is not easy to add solder and voids are likely to occur, affecting the RF quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 A schematic diagram of a SMP welding hole structure;
[0021] Figure 2 It is a schematic diagram of another SMP welding hole structure;
[0022] Figure 3 A schematic diagram of a SMP welding hole structure from another perspective;
[0023] Figure 4 It is a schematic diagram of the existing SMP welding hole structure;
[0024] Figure 5 This is a physical picture of an SMP welding hole structure;
[0025] The reference numerals are as follows: 1 is a cavity, 2 is a tin sink, 3 is a guide groove, and 4 is an air cavity. DETAILED DESCRIPTION
[0026] The following describes the implementation of the present invention through specific examples. Those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific implementations, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the following embodiments and features in the embodiments can be combined with each other without conflict.
[0027] It should be noted that the illustrations provided in the following embodiments are only schematic illustrations of the basic concept of the present invention. The drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0028] like Figures 1 to 3As shown, an SMP soldering hole structure includes a tin sink 2, a guide groove 3 and an air cavity 4, wherein the tin sink 2, the guide groove 3 and the air cavity 4 are all arranged in a cavity 1;
[0029] The tin sinking tank 2 is located at the opening of the upper surface of the cavity 1, and the bottom of the tin sinking tank 2 is connected to the guide groove 3;
[0030] The guide groove 3 is located between the tin sink 2 and the air cavity 4;
[0031] The air cavity 4 is communicated with the bottom of the guide groove 3 .
[0032] The purpose of this design is to open a tin sinking tank on the cavity so that the solder can move along the tin sinking tank toward the guide groove, and will not flow into the SMP connector to form a structure such as an arch head. Compared with the existing soldering hole structure, the RF quality is improved and the loss is reduced. The existing SMP soldering hole structure solves the problem that when the SMP is inserted into the cavity for sintering, the solder easily flows into the hole wall and accumulates on the surface of the cavity, making it difficult to plug and unplug and increasing the loss. During sintering, it is not easy to add solder material, and voids are likely to occur, affecting the RF quality.
[0033] The specific sintering steps adapted thereto are:
[0034] 1.1 Inspection
[0035] 1.1.1 Appearance inspection:
[0036] According to "GJB 548B-2005 Microelectronic Device Test Methods and Procedures" Method 2009.1 External Visual Inspection 3.3.8 Glass Seal.
[0037] 1.1.2 Seal inspection:
[0038] According to "GJB548B-2005 Method 1014.2 Sealing---Failure Condition A4", the measured leakage rate is at least less than 1×10-9 (Pa.m3) / S (the tracer gas is helium), generally on the order of -10.
[0039] 1.1.3 Weldability test:
[0040] The inner and outer conductors of the insulators shall not have any excess material, blackening, oxidation, etc. For the solderability test of electronic components, see "GJB548B-2005 Microelectronic Device Test Methods and Procedures 2003.1 Solderability", and the tinning rate shall be at least 95%.
[0041] 1.1.4 High temperature resistance test:
[0042] Under the conditions of 270±5℃, 5min, no vitreous cracking shall occur.
[0043] 1.2 Trial Installation
[0044] The fit between the SMP outer conductor and the hole wall should not be an interference fit or a clearance fit.
[0045] 1.3 Gold removal
[0046] ① Apply an appropriate amount of flux on the surface of the connector where tinning is required;
[0047] ② Put the connector into the de-goldening tin pot and tin it. The temperature of the tin pot should be 230℃±5℃ and the time should not exceed 3s;
[0048] 1.4 Cleaning
[0049] Clean the SMP and cavity to be sintered with plate-cleaning water.
[0050] 1.5 Sintering
[0051] 1.5.1 Coating
[0052] Brush paste flux into the SMP hole to be sintered, then place the cavity on the preheating table and preheat for 3min to 5min depending on the size of the cavity.
[0053] 1.5.2 Filling
[0054] Use tweezers to place the SMP and solder ring into the insulator hole to be sintered in sequence.
[0055] 1.5.3 Preheating
[0056] Preheating table temperature: Set the preheating table temperature to 100℃±10℃ according to the solder composition.
[0057] Sintering hot plate temperature: T hot plate temperature = T solder melting point + 30°C.
[0058] 1.5.4 Welding
[0059] ① Feed solder wire into the tin sink until the solder flows completely from the outside of the pore to the other side of the pore. The solder needs to completely fill the tin sink and be flush with the cavity surface;
[0060] ② Apply a layer of liquid flux on the tin sink to prevent sintering voids;
[0061] ③ Use tweezers to remove the sintered component and place it on the heat dissipation platform. After it returns to room temperature, clean off the flux with board washing water and let it dry naturally.
[0062] 1.5.5 Organize
[0063] Remove excess solder that overflows from the tin sink and cavity wall, and clean the semi-finished products.
[0064] 1.5.6 Inspection
[0065] ① The solder in the tinning bath should be smooth and full, and the voids should not exceed 20%;
[0066] ② The lead wire is not deformed or damaged, and the root is not subjected to stress;
[0067] ③ The cracks on the glass seal surface meet the requirements of "GJB 548B-2005 Test Methods and Procedures for Microelectronic Devices" Method 2009.1 External Visual Inspection 3.3.8 Glass Seal;
[0068] ④ There is no solder contamination or accumulation in non-welding areas (no excess solder overflows from the tin sink);
[0069] ⑤ After the SMP connector is sintered, the internal gold-plated surface is contaminated by solder, and there is no obvious solder protrusion around the weld.
[0070] ⑥ For SMP sintering with airtightness requirements, an airtightness inspection should be carried out after sintering, and the leakage rate should meet the relevant requirements of GJB 548B-2005 Method 1014.
[0071] ⑦ The conductor inside the SMP cannot be short-circuited.
[0072] In this embodiment, the tin sinking tank 2 is used to pre-place one of a solder ring, a solder wire and a solder paste, and the depth of the tin sinking tank 2 is twice the diameter of the solder wire.
[0073] The purpose of this design is to pre-place a solder ring or solder paste before soldering. When soldering, the liquid solder is guided to flow to the tin sink and guide groove, and the solder becomes solid and acts as a seal.
[0074] In this embodiment, there is a gap between the guide groove 3 and the inserted SMP.
[0075] The purpose of this design is to guide the SMP to the correct position before welding. During welding, the liquid solder fills the gap between the guide groove and the SMP. After welding, the solder changes from liquid to solid to act as a seal. The tolerance of the guide groove diameter is 0.04mm to 0.08mm.
[0076] In this embodiment, the air cavity 4 is used to simulate and match the standing wave of the module.
[0077] In actual use, the tolerance of the air slot diameter is 0.04mm to 0.08mm.
[0078] In this embodiment, specific dimensions of the SMP soldering holes in actual use are provided: the diameter of the tin sink 2 is 5.3 mm, and the depth is 0.3 mm; the diameter of the guide groove 3 is 4.3 mm, and the depth is 3.2 mm; the diameter of the air cavity 4 is 2.6 mm, and the depth is 4.7 mm.
[0079] like Figure 2 As shown, in this embodiment, another tin sinking tank structure is provided, wherein the tin sinking tank 2 is a truncated cone structure, and the groove diameter of the tin sinking tank 2 at the opening of the cavity 1 is larger than the groove diameter at the connection between the tin sinking tank 2 and the guide groove 3.
[0080] Meanwhile, the cavity 1 is usually made of an aluminum structural member, and the welding hole structure is opened on the aluminum structural member.
[0081] Finally, it should be noted that the above are only preferred embodiments of the present invention and are not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A SMP welding hole structure, characterized in that: It comprises a tin sinking tank (2), a guide groove (3) and an air cavity (4), wherein the tin sinking tank (2), the guide groove (3) and the air cavity (4) are all arranged in the cavity body (1); The tin sinking tank (2) is located at the opening of the upper surface of the cavity (1), and the bottom of the tin sinking tank (2) is connected to the guide groove (3); The guide groove (3) is located between the tin sink (2) and the air cavity (4); The air cavity (4) is in communication with the bottom of the guide groove (3).
2. The SMP welding hole structure according to claim 1, characterized in that: The tin sink (2) is used for pre-setting one of a solder ring, a solder wire and a solder paste.
3. The SMP welding hole structure according to claim 2, characterized in that: The depth of the tin sink (2) is twice the diameter of the solder wire.
4. The SMP welding hole structure according to claim 1, characterized in that: There is a gap between the guide groove (3) and the inserted SMP.
5. The SMP welding hole structure according to claim 1, characterized in that: The air cavity (4) is used to simulate and match the standing wave of the module.
6. The SMP welding hole structure according to claim 1, characterized in that: The tin sink (2) has a diameter of 5.3 mm and a depth of 0.3 mm; The guide groove (3) has a diameter of 4.3 mm and a depth of 3.2 mm; The air cavity (4) has a diameter of 2.6 mm and a depth of 4.7 mm.
7. The SMP welding hole structure according to claim 1, characterized in that: The tin sinking tank (2) is a truncated cone structure, and the diameter of the tin sinking tank (2) at the opening of the cavity (1) is larger than the diameter of the tin sinking tank (2) at the connection with the guide groove (3).
Citation Information
Cited By
Sintering resistance welding process method for SMP radio frequency connector
CN121097468A