Evaporation equipment

By using mask plates and cooling pipelines in the evaporation equipment, the problem of exposure of the inner metal conductive layer during cutting of the composite fluid collection blank is solved, the quality and life of the lithium battery are ensured, and the composite fluid collection is realized. Efficient manufacturing.

CN222064648UActive Publication Date: 2024-11-26ADVANCED MATERIALS TECH (BEIJING) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420646211.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-29
Publication Date
2024-11-26
Estimated Expiration
2034-03-29

AI Technical Summary

Technical Problem

When the composite fluid-collection blank produced by existing evaporation equipment is cut, the cut end face is prone to expose the inner metal conductive layer, resulting in electrochemical reaction and quality problems.

Method used

An evaporation device including an evaporation device, a baffle mechanism, a mask plate and a film carrier roller were designed. Through the removable installation and cooling pipeline of the mask plate, the outer metal conductive layer is ensured to fully cover the inner layer and avoid cutting. When exposed.

Benefits of technology

It effectively prevents the exposure of the inner metal conductive layer, improves the quality and life of the lithium battery, and ensures the conductivity and energy density of the composite liquid collector.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222064648U_ABST
    Figure CN222064648U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of battery manufacturing, and particularly relates to evaporation equipment. The evaporation equipment comprises an evaporation device, a baffle plate mechanism, a mask plate and a film carrying roller, the evaporation device is provided with an open cavity and used for containing, heating and evaporating materials to be evaporated. The film carrying roller is located on the open side of the open cavity and wound around the current to-be-evaporated part of the base material layer. The baffle mechanism is connected to the evaporation device and located on the open side of the open cavity, and the mask plate is located between the baffle mechanism and the film carrying roller and is detachably installed; the baffle mechanism is used for opening and closing the opening cavity so as to be matched with the mask plate to form a target pattern plating layer on the base material layer. The evaporation equipment can be applied to manufacturing of a composite current collector with a plurality of metal conducting layers formed on the surface of the same side of the base material layer, it is ensured that the metal conducting layer on the outer side completely covers the metal conducting layer on the inner side, and therefore after cutting, the end face of a notch cannot expose the metal conducting layer on the inner side.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application belongs to the field of battery manufacturing technology, and in particular, relates to an evaporation device. Background Art

[0002] With the rapid development of the new energy industry, lithium-ion batteries, as one of the main ways of electrochemical energy storage, have developed rapidly. The market has put forward higher requirements for the use of lithium-ion batteries, and improving energy density is the main direction. In order to improve the energy density of lithium-ion batteries and reduce the weight of batteries, composite current collector materials are used.

[0003] The composite current collector is a multi-layer composite structure, with a polymer layer as the inner layer and metal conductive layers on both sides of the inner layer. Generally speaking, composite aluminum foil is used as a positive electrode current collector to replace aluminum foil in lithium-ion batteries, and composite copper foil is used as a negative electrode current collector to replace copper foil.

[0004] Evaporation coating process (abbreviated as evaporation) is a commonly used method for making composite current collector materials. Evaporation is a process in which the material to be coated is heated under vacuum conditions to evaporate it onto the substrate film and form a coating on the substrate film.

[0005] In order to realize the evaporation on a large area of ​​substrate film, a rewinding device is generally configured. The rewinding device is used to unwind the substrate film on one reel and rewind it onto another reel. In this way, the substrate film can be unwound while the evaporation is being performed, which greatly improves production efficiency and reduces costs.

[0006] It should be noted that for some composite current collectors, one side of the substrate film has multiple metal conductive layers. The composite current collector blank with multiple metal conductive layers on one side produced by the evaporation equipment equipped with a rewinding device has the same pattern formed on each metal conductive layer on the same side of the composite current collector blank, resulting in the inner conductive metal layer being exposed at the end surface of the cut when the composite current collector blank is cut.

[0007] However, some inner conductive metal layers can react with battery materials, thereby reducing the quality and life of battery products. Utility Model Content

[0008] The present application provides an evaporation device to solve the technical problem that when a composite current collector blank produced by an existing evaporation device is cut, an inner metal layer is exposed at the end surface of the cut.

[0009] According to one aspect of the present application, a vapor deposition device is provided, including an evaporation device, a baffle mechanism, a mask plate and a carrier roller; the evaporation device is provided with an open chamber and is used to receive, heat and evaporate the material to be evaporated; the carrier roller is located on the opening side of the open chamber and is surrounded by a portion of the substrate layer currently to be evaporated; the baffle mechanism is connected to the evaporation device and is located on the opening side of the open chamber, the mask plate is located between the baffle mechanism and the carrier roller and is arranged to be detachably installed; the baffle mechanism is used to open and close the open chamber to cooperate with the mask plate to form a target pattern coating on the substrate layer.

[0010] In an optional solution of the present application, the projection enclosed range of the mask plate on the evaporation device covers the opening of the open chamber.

[0011] In an optional solution of the present application, the mask plate includes a plate body, which is provided with a plurality of evaporation holes arranged at intervals; the evaporation holes are used for allowing the vapor formed by the material to be evaporated to pass through, so as to form a target pattern coating on the substrate layer.

[0012] In an optional solution of the present application, the plate body is an arc-shaped structure; the diameter of the arc surface of the plate body facing the film-carrying roller is smaller than the diameter of the arc surface of the plate body away from the film-carrying roller.

[0013] In an optional solution of the present application, the plate body and the film-carrying roller are arranged in parallel and at intervals.

[0014] In an optional solution of the present application, the mask plate further includes a cooling pipeline, the cooling pipeline is connected to the plate body, and the cooling pipeline is configured to allow a cooling medium to pass through to cool the plate body.

[0015] In an optional solution of the present application, the cooling pipeline includes multiple first pipeline sections and multiple second pipeline sections, each second pipeline section connects two adjacent first pipeline sections; multiple evaporation holes are arranged in an array, and at least one row of evaporation holes is located between two adjacent first pipeline sections.

[0016] In an optional solution of the present application, the plate body is formed with a plurality of thinning areas arranged side by side, and each thinning area is provided with at least one row of evaporation holes.

[0017] In an optional solution of the present application, the baffle mechanism includes a baffle and a driving mechanism; the driving mechanism is connected to the evaporation device, and the baffle is connected to the driving mechanism; the driving mechanism is used to drive the baffle to move linearly to open and close the opening of the open chamber.

[0018] In an optional solution of the present application, the evaporation device includes an evaporation container and a heating structure; the evaporation container is provided with an open chamber to accommodate the material to be evaporated, and the heating structure is arranged in the evaporation container to heat and evaporate the material to be evaporated.

[0019] In summary, the evaporation device provided by the present application has at least the following beneficial effects:

[0020] In the evaporation equipment provided in the present application, the evaporation device can heat the material to be evaporated to form steam. When the baffle mechanism opens the open chamber, the steam can pass through the opening of the open chamber and through the mask plate to condense on the current evaporated part of the substrate layer on the carrier roller to form a coating.

[0021] The mask plate is arranged to be detachably mounted. In a specific application, the desired first pattern coating can be accurately formed on the substrate layer through the mask plate when the mask plate is installed. When the mask plate is removed, a second pattern coating that completely covers the first pattern coating can be formed on the substrate layer without the shielding of the mask plate, and the second pattern coating is located outside the first pattern coating.

[0022] Specifically, the evaporation equipment can be used to manufacture a composite current collector with multiple metal conductive layers formed on the same side surface of the substrate layer, ensuring that the outer metal conductive layer completely covers the inner metal conductive layer, so that after cutting, the cut end surface will not expose the inner metal conductive layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the specific implementation of the present application or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the specific implementation or the prior art description. Obviously, the drawings described below are some implementations of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.

[0024] Figure 1 A partial schematic diagram of an evaporation device provided according to one embodiment of the present application;

[0025] Figure 2 A partial schematic diagram of a vapor deposition device provided with a rewinding device according to one embodiment of the present application;

[0026] Figure 3 A schematic diagram of a mask provided according to one embodiment of the present application at a viewing angle;

[0027] Figure 4 for Figure 3 A schematic diagram of the mask in another viewing angle;

[0028] Figure 5 for Figure 3 Schematic diagram of the mask plate in another viewing angle;

[0029] Figure 6 A schematic diagram of a process for preparing a composite current collector according to one embodiment of the present application;

[0030] Figure 7A partial schematic diagram of a copper-aluminum composite current collector blank is shown.

[0031] The reference numerals are as follows:

[0032] 1000. Evaporation equipment;

[0033] 100. Evaporation device; 110. Evaporation container; 120. Heating structure;

[0034] 200, baffle mechanism; 210, baffle; 220, driving mechanism;

[0035] 300, mask plate; 310, plate body; 320, cooling pipeline; 321, first pipeline section; 322, second pipeline section;

[0036] 400, film-carrying roller;

[0037] 500, rewinding device;

[0038] 600, substrate layer;

[0039] 700, copper-aluminum composite current collector blank; 710, inner aluminum layer; 720, outer copper layer;

[0040] H1, evaporation hole; S, thinning area; R, open chamber. DETAILED DESCRIPTION

[0041] In the description of the present application, it should be understood that if terms such as "upper", "lower", "top", "bottom", "inside", "outside", "circumferential" and the like appear to indicate orientation or positional relationships, unless otherwise specified, they are understood to be based on the orientation or positional relationships shown in the drawings, which are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0042] In addition, if there is a feature defined as "first" or "second", it is only used for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Features defined as "first" or "second" may explicitly or implicitly include at least one of the defined features. If there is a description of "plurality", the general meaning is to include at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0043] In this application, unless otherwise clearly specified and limited, the terms such as "installed", "connected", "connected", "fixed" and so on should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection, it can be a direct connection, or it can be an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For those skilled in the art, the specific meanings of the above terms in this application can be understood according to the specific circumstances.

[0044] In the description of this specification, if the terms "one embodiment", "some embodiments", "example", "specific example", or "some examples" appear, it means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present application. In this specification, the schematic representations of the above terms do not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described may be combined in any one or more embodiments or examples in a suitable manner. In addition, those skilled in the art may combine and combine the different embodiments or examples described in this specification and the features of the different embodiments or examples, unless they are contradictory.

[0045] A composite current collector blank having multiple metal conductive layers on one side produced by existing evaporation equipment has the same pattern formed by each metal conductive layer on the same side of the composite current collector blank.

[0046] The inventors found that when the composite current collector blank is cut, each metal conductive layer on the cut end surface will be exposed. For some application scenarios, the composite current collector cannot expose the inner metal conductive layer.

[0047] It should be noted that since metallic aluminum will undergo an electrochemical reaction with lithium, which will consume lithium ions and is also accompanied by a large volume effect, it will eventually become pulverized under the action of stress and its surface structure will be destroyed. Therefore, aluminum metal cannot be directly used as a current collector for the negative electrode of a lithium-ion battery.

[0048] During the battery charging and discharging process, copper metal has only a small lithium insertion capacity and has high chemical and electrochemical stability, and can be used as a current collector for the negative electrode of lithium-ion batteries.

[0049] Since the price of aluminum is about 30% of that of copper and the density of aluminum is about 30% of that of copper, at present, the copper-aluminum composite current collector formed by replacing part of the copper with aluminum as the negative electrode composite current collector can not only ensure the conductivity of the current collector, but also improve the energy density of the lithium-ion battery, and save a lot of material costs.

[0050] However, when the copper-aluminum composite current collector produced by existing evaporation equipment is cut, the inner aluminum metal conductive layer will be exposed on the cut end surface. Therefore, the cut end surface needs to be protected to avoid electrochemical reaction between the aluminum metal conductive layer and lithium ions to ensure the quality and life of the lithium battery product.

[0051] For this purpose, the present application provides an evaporation device 1000 . Figure 1 It is a partial schematic diagram of an evaporation device 1000 provided according to one embodiment of the present application. Figure 2 FIG. 1 is a partial schematic diagram of a vapor deposition device 1000 provided with a rewinding device 500 according to one embodiment of the present application. Figure 1 and Figure 2 The evaporation equipment 1000 includes an evaporation device 100 , a baffle mechanism 200 , a mask plate 300 and a film carrier roller 400 .

[0052] The evaporation device 100 is provided with an open chamber R and is used to receive, heat and evaporate the material to be evaporated. The film carrier roller 400 is located at the opening side of the open chamber R and surrounds the current evaporated portion of the substrate layer 600.

[0053] The baffle mechanism 200 is connected to the evaporation device 100 and is located at the opening side of the open chamber R. The mask plate 300 is located between the baffle mechanism 200 and the film carrier roller 400. The baffle mechanism 200 is used to open and close the open chamber R to cooperate with the mask plate 300 to form a target pattern coating on the substrate layer 600.

[0054] In this embodiment, the material to be evaporated can be loaded into the open chamber R in the evaporation device 100 and heated to the required temperature for evaporation in the evaporation device 100. The evaporation device 100 is fixedly installed with a baffle mechanism 200, which is located at the opening side of the open chamber R to open and close the open chamber R.

[0055] The mask plate 300 and the film-carrying roller 400 are both located at the opening side of the open chamber R of the evaporation device 100 . The mask plate 300 is located between the film-carrying roller 400 and the baffle mechanism 200 and is configured to be detachably installed.

[0056] The carrier roller 400 is used to load the substrate layer 600 . The portion of the substrate layer 600 to be evaporated can be wrapped around a portion of the outer circumference of the carrier roller 400 and located between the mask plate 300 and the carrier roller 400 .

[0057] The steam flowing out of the evaporation device 100 must first pass through the mask plate 300 before it can be deposited on the current portion of the substrate layer 600 to be evaporated, so as to form a coating on the current portion of the substrate layer 600 to be evaporated. The mask plate 300 is used to block part of the vapor of the material to be evaporated to limit the coating pattern formed on the substrate layer 600.

[0058] It should be understood that when the baffle mechanism 200 opens the open chamber R, steam can be allowed to flow out from the opening of the open chamber R and reach the current portion of the substrate layer 600 to be evaporated on the carrier roller 400 through the mask plate 300 to form a target pattern coating on the substrate layer 600.

[0059] When the baffle mechanism 200 closes the open chamber R, the steam cannot flow out from the opening of the open chamber R, and thus cannot be deposited on the substrate layer 600 on the film carrier roller 400 .

[0060] It should be noted that the mask plate 300 is configured to be detachably installed, and specifically, it can be detachably fixed by means of screws, hooks, etc. In the process of producing the copper-aluminum composite current collector, when the aluminum layer is evaporated on the substrate layer 600, the mask plate 300 blocks part of the aluminum vapor to form an evaporated aluminum layer on one side surface of the substrate layer 600, and the evaporated aluminum layer can be formed on the substrate layer 600 as a patterned coating having a plurality of image element blocks arranged at intervals.

[0061] When a copper layer is evaporated on the surface of the substrate layer 600 having the evaporated aluminum layer, the mask plate 300 is removed. Without the shielding of the mask plate 300, the evaporated copper layer formed on the substrate layer 600 is a patterned coating with continuous image elements and completely covers the evaporated aluminum layer.

[0062] In this way, when cutting, the end face of the cut will only expose the outer vapor-deposited copper layer, and the inner vapor-deposited aluminum layer will be completely covered, so that the end face of the copper-aluminum composite current collector can be used as the negative electrode of the lithium battery without protective treatment, thereby ensuring the quality and life of the lithium battery product.

[0063] It should be noted that the substrate layer 600 here refers to a polymer material film layer, including, for example, a polyethylene terephthalate film layer, a polypropylene film layer, and a polyimide film layer.

[0064] See also Figure 2 The substrate layer 600 can be fed through the rewinding device 500, and the rewinding device 500 includes at least two rollers, one of which is used for receiving the material and the other for feeding the material. The mask plate 300 and the film carrier roller 400 are located above the evaporation device 100, specifically above the opening side of the open chamber R. The vapor of the material to be evaporated formed in the open chamber R can move upward to reach the current portion of the substrate layer 600 to be evaporated.

[0065] The film carrier roller 400 keeps the current part of the substrate layer 600 to be evaporated in a taut state to ensure the quality of the coating on the surface of the substrate layer 600. In addition, the film carrier roller 400 also has a cooling function to ensure that the steam is quickly cooled down and deposited to form a coating on the current part of the substrate layer 600 to be evaporated, thereby ensuring the quality of the coating and avoiding the substrate layer 600 from being melted due to excessively high steam temperature.

[0066] In a further optional embodiment, the area enclosed by the projection pattern of the mask plate 300 on the evaporation device 100 covers the opening of the open chamber R.

[0067] It should be understood that the steam coverage formed by the material to be evaporated is determined by the opening size of the open chamber R. The area enclosed by the pattern formed by the projection of the mask plate 300 on the evaporation device 100 completely covers the opening of the open chamber R. Only in this way can the steam coverage formed by the material to be evaporated be completely covered, thereby preventing the steam from forming a coating outside the current part to be evaporated of the substrate layer 600.

[0068] In some optional embodiments, the baffle mechanism 200 includes a baffle 210 and a driving mechanism 220. The driving mechanism 220 is connected to the evaporation device 100, and the baffle 210 is connected to the driving mechanism 220. The driving mechanism 220 is used to drive the baffle 210 to move linearly to open the opening of the chamber R.

[0069] In this embodiment, the baffle mechanism 200 is composed of a baffle 210 and a driving mechanism 220. The driving mechanism 220 is fixedly installed at the opening of the evaporation device 100 and is used to drive the baffle 210 to move linearly, thereby opening or closing the opening of the opening chamber R.

[0070] exist Figure 1 and Figure 2 In the illustrated embodiment, the baffle 210 is a flat plate, and the drive mechanism 220 is a linear motor to drive the baffle 210 to move linearly. Of course, the baffle mechanism 200 is not limited to the illustrated embodiment, for example, the drive mechanism 220 may be a linear module driven by a motor. The baffle 210 is not limited to a flat plate, and may be designed according to the shape of the opening.

[0071] In a specific application, the baffle 210 should be made of high temperature resistant material, and the driving mechanism 220 should be fixedly installed on opposite sides of the opening of the open chamber R, so as to ensure the stability of the baffle 210 during movement and ensure that the translation is maintained.

[0072] In an optional embodiment, the evaporation device 100 includes an evaporation container 110 and a heating structure 120. The evaporation container 110 is provided with an open chamber R for receiving the material to be evaporated, and the heating structure 120 is disposed in the evaporation container 110 to heat and evaporate the material to be evaporated.

[0073] In this embodiment, the evaporation container 110 is formed with the above-mentioned open chamber R, and the heating structure 120 can heat the material to be evaporated in the open chamber R and heat the material to be evaporated to the required evaporation temperature, so that the material to be evaporated melts and forms steam.

[0074] exist Figure 1 and Figure 2 In the illustrated embodiment, the evaporation container 110 is a rectangular container, and the open chamber R is a rectangular chamber with an open top. Of course, the structural shapes of the evaporation container 110 and the open chamber R are not limited to the illustrated embodiment.

[0075] In specific applications, the evaporation container 110 should be made of high temperature resistant material, at least able to withstand the melting point temperature of the material to be evaporated. The heating structure 120 includes an evaporation boat, which has a high melting point and can load solid materials to be evaporated. Generally, heat energy can be transferred to the evaporation boat by resistance heating or electron beam heating, so as to heat the material to be evaporated to the evaporation temperature.

[0076] Figure 3 The figure is a schematic diagram of a mask plate 300 provided according to one embodiment of the present application at a certain viewing angle. Figure 4 for Figure 3 FIG. 3 is a schematic diagram of the mask plate 300 at another viewing angle. Figure 5 for Figure 3 FIG. 3 is a schematic diagram of the mask plate 300 in another viewing angle.

[0077] See also Figures 3 to 5 In some optional embodiments, the mask plate 300 includes a plate body 310 , and the plate body 310 is provided with a plurality of evaporation holes H1 arranged at intervals. The evaporation holes H1 are used to allow the vapor formed by the material to be evaporated to pass through, so as to form a target pattern coating on the substrate layer 600 .

[0078] In this embodiment, the plate body 310 of the mask plate 300 is formed with a plurality of evaporation holes H1, which allow the vapor formed by the material to be evaporated to pass through and reach the substrate layer 600 on the carrier roller 400. In other words, the projection of each evaporation hole H1 on the current portion to be evaporated of the substrate layer 600 can form a corresponding coating.

[0079] Thus, when the mask plate 300 is assembled, the baffle mechanism 200 cooperates with the mask plate 300 to form a target pattern coating having a plurality of spaced-apart image element blocks. Here, the image element block is a coating formed corresponding to one evaporation hole H1.

[0080] It should be understood that the projection enclosed range of the mask plate 300 on the evaporation device 100 covers the projections of all the evaporation holes H1 on the evaporation device 100 .

[0081] In a specific application, a plurality of evaporation holes H1 can be integrally processed on the plate body 310 . The evaporation holes H1 are independent of each other, and their shapes and sizes can be processed according to the size specifications of the composite current collector.

[0082] In an optional embodiment, the plurality of evaporation holes H1 include any one or more combinations of circular through holes, polygonal through holes, elliptical through holes, and waist-shaped through holes, and are not limited to the rectangular through holes in the illustrated embodiment, and can be designed according to the required shape of the composite current collector.

[0083] In a further optional embodiment, the mask plate 300 further includes a cooling pipeline 320 , which is connected to the plate body 310 , and the cooling pipeline 320 is configured to allow a cooling medium to pass through to cool the plate body 310 .

[0084] It should be understood that the area on the plate body 310 where the evaporation holes H1 are not provided is a shielding area, which can prevent the vapor formed by the material to be evaporated from passing through, that is, part of the vapor formed by the material to be evaporated is deposited in the shielding area. It should be noted that the evaporation material deposited in the shielding area of ​​the plate body 310 has the risk of falling off.

[0085] In this embodiment, by providing a cooling pipe 320 through which a cooling medium can flow on the plate body 310, the plate body 310 can be cooled quickly and fully, and the adhesion effect between the evaporation material and the shielding area in the plate body 310 is improved, and the risk of the evaporation material on the shielding area falling off is reduced. Here, the cooling medium can be water or other liquids capable of heat exchange.

[0086] In a further optional embodiment, the surface of the plate 310 close to the evaporation device 100 is a rough surface to further improve the bonding force between the evaporation material and the plate 310, so as to further reduce the risk of the evaporation material falling off on the shielding area. In a specific application, the surface of the plate 310 close to the evaporation device 100 can be formed into the above-mentioned rough surface by processes such as sandblasting or chemical etching.

[0087] In some optional embodiments, the plate body 310 is an arc-shaped structure, and the diameter of the arc surface of the plate body 310 facing the film-carrying roller 400 is smaller than the diameter of the arc surface of the plate body 310 away from the film-carrying roller 400 .

[0088] In this embodiment, the plate body 310 is an arc-shaped plate body, and the center of the arc-shaped plate body and the center of the film-carrying roller 400 are located on the same side of the plate body 310, that is, the side of the plate body 310 with a smaller radius is close to the film-carrying roller 400, and the side with a larger radius is close to the evaporation device 100. It should be understood that the above-mentioned shielding area is located on the arc surface of the plate body 310 away from the film-carrying roller 400, that is, the arc surface of the plate body 310 close to the evaporation device 100 can be set to a rough surface.

[0089] In a further optional embodiment, the plate 310 is arranged parallel to the film-carrying roller 400. In other words, the plate 310 and the film-carrying roller 400 are arranged concentrically, so that the gap formed between the plate 310 and the film-carrying roller 400 is uniform, that is, the gap between the arc surface of the plate 310 and the outer peripheral surface of the film-carrying roller 400 is consistent.

[0090] In a specific application, the gap between the location of each evaporation hole H1 in the plate body 310 and the film carrier roller 400 is 5 mm to 10 mm. In other words, the diameter of the plate body 310 is 10 mm to 20 mm larger than the diameter of the film carrier roller 400.

[0091] In a further optional embodiment, the center normal of each evaporation hole H1 is perpendicular to the outer peripheral surface of the film carrier roller 400. It can be understood that the current portion to be evaporated of the substrate layer 600 is closely attached to the outer peripheral surface of the film carrier roller 400, and the center normal of each evaporation hole H1 is perpendicular to the outer peripheral surface of the film carrier roller 400, which is equivalent to the center line normal of each evaporation hole H1 being perpendicular to the current portion to be evaporated of the substrate layer 600, ensuring that the incident angle of the vapor to be evaporated through the evaporation hole H1 into the current portion to be evaporated of the substrate layer 600 is the same, thereby ensuring the uniformity of the coating.

[0092] In some optional embodiments, the cooling pipeline 320 includes a plurality of first pipeline sections 321 and a plurality of second pipeline sections 322, each second pipeline section 322 connecting two adjacent first pipeline sections 321. The plurality of evaporation holes H1 are arranged in an array, and at least one row of evaporation holes H1 is located between two adjacent first pipeline sections 321.

[0093] In this embodiment, the cooling pipeline 320 is composed of a plurality of first pipeline sections 321 and a plurality of second pipeline sections 322 connected in sequence, wherein two adjacent first pipeline sections 321 are connected in series via one second pipeline section 322 .

[0094] In addition, the plurality of evaporation holes H1 on the plate body 310 are arranged in an array, that is, the plurality of evaporation holes H1 form a plurality of evaporation hole rows, and the plurality of evaporation hole rows are arranged side by side.

[0095] In the illustrated embodiment, only one row of evaporation holes H1 is provided between two adjacent first pipeline sections 321, so that the cooling pipeline 320 covers a wider range to ensure the cooling effect on the shielding area. Of course, it is not limited to the illustrated embodiment, and two or three rows of evaporation holes H1 can also be provided between two adjacent first pipeline sections 321. In other words, at least one row of evaporation holes H1 is provided between two adjacent first pipeline sections 321.

[0096] In the illustrated embodiment, three rows of evaporation holes H1 are formed on the plate body 310, the number of the first pipeline sections 321 is four and they are arranged side by side at intervals, and two adjacent first pipeline sections 321 are connected by a second pipeline section 322, forming a cooling pipeline 320 that extends in a circuitous manner and is arranged on the outside of each row of evaporation holes H1.

[0097] In a further optional embodiment, the plate body 310 is formed with a plurality of thinning regions S arranged side by side, and each thinning region S is provided with at least one row of evaporation holes H1.

[0098] In this embodiment, the location of the evaporation hole H1 is thinned to form a thinning area S. Accordingly, the depth of each evaporation hole H1 is reduced, which can reduce the shielding of the evaporation material by the hole wall and reduce material waste.

[0099] In the illustrated embodiment, each thinning area S is provided with only one row of evaporation holes H1, and first pipeline sections 321 are arranged on opposite sides of each thinning area S. Of course, it is not limited to the illustrated embodiment, and illustratively, each thinning area S may be provided with two or three rows of evaporation holes H1, which may be designed according to requirements.

[0100] To sum up, in the evaporation equipment 1000 provided in the present application, the evaporation device 100 can heat the material to be evaporated to form steam. When the baffle mechanism 200 opens the open chamber R, the steam can pass through the opening of the open chamber R and through the mask plate 300 to condense the current evaporated part of the substrate layer 600 on the carrier roller 400 to form a coating.

[0101] The mask plate 300 is configured to be detachably installed. In a specific application, the mask plate 300 can be installed to accurately form the desired first pattern coating on the substrate layer 600 through the mask plate 300. When the mask plate 300 is removed, a second pattern coating that completely covers the first pattern coating can be formed on the substrate layer 600 because there is no shielding by the mask plate 300. The second pattern coating is located outside the first pattern coating.

[0102] Specifically, the evaporation device 1000 can be used to manufacture a composite current collector that forms multiple metal conductive layers on the same side surface of the substrate layer 600, ensuring that the outer metal conductive layer completely covers the inner metal conductive layer, so that after cutting, the cut end surface will not expose the inner metal conductive layer.

[0103] Another aspect of the present application further provides a method for preparing a composite current collector, which can be applied to the above-mentioned evaporation device 1000 . Figure 6 A schematic diagram of a process for preparing a composite current collector according to one embodiment of the present application is shown in FIG. Figure 6As shown, the composite current collector preparation method may include but is not limited to the following steps:

[0104] S11, sending the first material to be evaporated and the substrate layer 600 into the evaporation device 1000, and evaporating the first patterned coating layer composed of the first material to be evaporated on the surface of the substrate layer 600 through the mask plate 300;

[0105] S12, removing the mask plate 300;

[0106] S13 , sending the second material to be evaporated and the substrate layer 600 formed with the first evaporation pattern into the evaporation equipment 1000 , so as to form a second pattern coating layer on the surface of the substrate layer 600 , which covers the first pattern coating layer and is composed of the second material to be evaporated.

[0107] In S11, the first material to be evaporated is fed into the evaporation device 100 in the evaporation device 1000, and the substrate layer 600 is fed onto the film carrier roller 400 in the evaporation device 1000. When the mask plate 300 is assembled, a first pattern coating is formed on one side of the substrate layer 600. The first pattern coating is formed by the steam formed by heating the first material to be evaporated in the evaporation device 100, and condensing on the substrate layer 600 after passing through the mask plate 300.

[0108] After the evaporation of the first to-be-evaporated material is completed, S12 may be performed, ie, the mask plate 300 is removed.

[0109] In S13, the second material to be evaporated is fed into the evaporation device 100 in the evaporation device 1000, and the substrate layer 600 is fed onto the film carrier roller 400 in the evaporation device 1000. In the absence of the mask plate 300, a second pattern coating is formed on the same side surface of the substrate layer 600, and the second pattern coating is formed by condensing the steam formed by heating the second material to be evaporated in the evaporation device 100 on the substrate layer 600.

[0110] Since the vapor formed by the second material to be evaporated is not blocked by the mask plate 300 , the second pattern coating formed on the same side surface of the substrate layer 600 is located outside the first pattern coating and completely covers the first pattern coating.

[0111] It can be seen that through the above-mentioned composite current collector preparation method, two coating layers stacked along the thickness direction can be formed on the surface of the substrate layer 600, the inner coating layer is composed of the first material to be evaporated and forms a first pattern coating layer, and the outer coating layer is composed of the second material to be evaporated and forms a second pattern coating layer, and the second pattern coating layer completely covers the first pattern coating layer.

[0112] It should be understood that when cutting the substrate layer 600 having the above-mentioned coating, the position of the cutting seam can be appropriately set so that only the coating layer formed by the second material to be evaporated is exposed on the end surface of the cutting seam.

[0113] It should be noted that the first material to be evaporated and the second material to be evaporated are both made into filament structures for easy melting, and can be fed into the open chamber R in the evaporation device 100 through a wire feeding device, specifically on the heating structure 120 in the open chamber R, so as to be heated on the heating structure 120 to form steam. The wire feeding device here can be a rotary wire feeding device, a vibrating wire feeding device, etc., which can be selected according to needs.

[0114] The substrate layer 600 can be fed to the film carrier roller 400 through the rewinding device 500, and the portion of the substrate layer 600 located on the outer circumference of the film carrier roller 400 is the portion to be evaporated. It should be noted that, for the two rollers in the rewinding device 500, one of them is used as a feeder in S11, and then the roller is used as a reel in S13; the other is used as a reel in S11, and then the roller is used as a feeder in S13. In this way, the first pattern coating and the second pattern coating stacked in the thickness direction can be formed on the same surface of the substrate layer 600.

[0115] In a specific application, the first material to be evaporated and the second material to be evaporated are both conductive metals, for example, copper, aluminum, silver, etc.

[0116] In some optional embodiments, S11, feeding the first material to be evaporated and the substrate layer 600 into the evaporation device 1000, and evaporating the first pattern coating layer composed of the first material to be evaporated on the surface of the substrate layer 600 through the mask plate 300, may include:

[0117] S111, when the first material to be evaporated in the open chamber R is in a stable evaporation state, the target portion to be evaporated of the substrate layer 600 is fed to the film carrier roller 400;

[0118] S112, opening the baffle mechanism 200, so as to allow the vapor formed by the first material to be evaporated in the open chamber R to be deposited on the target portion to be evaporated after passing through the mask plate 300;

[0119] S113, when the opening time of the baffle mechanism 200 reaches a preset time, closing the baffle mechanism 200 to form a pattern coating segment composed of the first material to be evaporated in the target portion to be evaporated;

[0120] S114, sending the vapor-deposited portion of the substrate layer 600 out of the film carrier roller 400, and sending the next vapor-deposited portion of the substrate layer 600 as the target vapor-deposited portion into the film carrier roller 400;

[0121] S115, return to open the baffle mechanism 200 to allow the vapor formed by the first material to be evaporated in the open chamber R to be deposited on the target part to be evaporated after passing through the mask plate 300, until the entire surface of the substrate layer 600 is formed with multiple pattern coating segments to constitute a first pattern coating.

[0122] In S111, the stable evaporation state means that the material to be evaporated can stably form a certain amount of vapor. After the first material to be evaporated reaches the stable evaporation state, part of the substrate layer 600 can be sent to the outer peripheral surface of the carrier roller 400 through the rewinding device 500. This part of the substrate layer 600 is the target part to be evaporated.

[0123] In S112 , the first material to be evaporated is in a stable evaporation state and can continuously provide steam. The baffle mechanism 200 is controlled to open the opening of the opening chamber R so that the steam can pass through the mask plate 300 and condense and deposit on the target portion to be evaporated on the substrate layer 600 .

[0124] In S113, the baffle mechanism 200 is controlled to be opened for a preset time and then closed, so that the steam can form a coating layer of a certain thickness on the target portion to be evaporated of the substrate layer 600 within the preset time period. These coating layers are formed by the first material to be evaporated and form a patterned coating segment on the target portion to be evaporated.

[0125] It should be understood that the opening time of the baffle mechanism 200 is one of the main factors affecting the thickness of the coating. In a specific application, the opening time of the baffle mechanism 200 is controlled to be 3 to 10 seconds.

[0126] In S114, the part of the substrate layer 600 that has completed vapor deposition refers to the target part to be vapor deposited that has completed vapor deposition in S113. The part of the substrate layer 600 that has completed vapor deposition can be sent out of the carrier roller 400 by the rewinding device 500, and the next part of the substrate layer 600 to be vapor deposited can be sent into the carrier roller 400 at the same time. The next part of the substrate layer 600 to be vapor deposited at the position of the carrier roller 400 serves as the current target part to be vapor deposited.

[0127] In S115 , the process returns to S113 to perform vapor deposition on the next portion to be vapor deposited. This cycle can form patterned coating segments on each target portion to be vapor deposited on the substrate layer 600 . These patterned coating segments constitute a first patterned coating.

[0128] In some optional embodiments, in S111, when the first material to be evaporated in the open chamber R is in a stable evaporation state, before the target portion to be evaporated of the substrate layer 600 is fed to the film carrier roller 400, the composite current collector preparation method may further include:

[0129] Obtaining a start signal to evacuate the environment where the evaporation device 1000 is located, and obtaining vacuum degree information;

[0130] When the vacuum degree information reaches the vacuum degree threshold, the evaporation device 100 is started to heat up to a first preset temperature to heat the first material to be evaporated;

[0131] Determine whether the first material to be evaporated in the open chamber R reaches a stable evaporation state.

[0132] It should be noted that the evaporation process needs to maintain a certain vacuum environment to avoid oxidation, prevent impurity contamination, and improve condensation deposition efficiency. Therefore, the evaporation device 1000 is generally set in a sealed environment, and the sealed environment is evacuated to allow the entire evaporation process to be carried out in a vacuum environment.

[0133] The start signal here can be a signal from the start button being pressed, or a signal from the host computer input device. The vacuum information can be obtained through the air pressure sensor. In specific applications, the vacuum threshold is generally set at 5×10 -2 pa to 5×10 -3 pa, can be adjusted according to needs.

[0134] In addition, the first preset temperature here is set according to the first material to be evaporated. It should be understood that the first preset temperature cannot be lower than the melting point of the first material to be evaporated.

[0135] Under the condition that the sealed environment meets the vacuum degree, the first material to be evaporated is heated to above its melting point, so that the first material to be evaporated is melted and generates steam.

[0136] It should be noted that the stable evaporation state can be determined manually or by collecting image data through an image acquisition device. When the first material to be evaporated is in a stable evaporation state, the first material to be evaporated is in a liquid state and basically does not generate bubbles. Whether it is in a stable evaporation state can be determined by observing the bubbles generated by the liquid first material to be evaporated.

[0137] It can be understood that the above steps disclose the preparation work before performing S111, that is, how to implement and ensure that the first material to be evaporated is in a stable evaporation state.

[0138] It should be noted that the first material to be evaporated in the above steps can be metal aluminum, and can be applied Figures 3 to 5 The mask plate 300 is shown. Each evaporation hole H1 on the mask plate 300 can form an aluminum coating block at a corresponding position on the substrate layer 600, and these aluminum coating blocks are arranged in an array to form a first pattern coating.

[0139] It should be additionally explained that, before performing S12 , the environment where the evaporation device 1000 is located needs to be switched to an atmospheric environment, so that the mask plate 300 can be removed.

[0140] In some optional embodiments, S13, the second material to be evaporated and the substrate layer 600 formed with the first evaporation pattern are fed into the evaporation device 1000 to form a second pattern coating layer covering the first evaporation pattern and composed of the second material to be evaporated on the surface of the substrate layer 600, including:

[0141] S131, when the second material to be evaporated in the open chamber R is in a stable evaporation state, opening the baffle mechanism 200;

[0142] S132, the substrate layer 600 is continuously transferred to the film-carrying roller 400, so that the vapor formed by the second material to be evaporated in the open chamber R is deposited on the surface of the substrate layer 600 formed with the first pattern coating, until the entire surface of the substrate layer 600 is formed with the second pattern coating covering the first pattern coating.

[0143] In S131, when the second material to be evaporated can stably form steam, the baffle mechanism 200 is controlled to open the open chamber R to allow the steam formed by the second material to be evaporated to flow out and reach the substrate layer 600 on the carrier roller 400, and condense and deposit on the substrate layer 600 to form a coating layer composed of the second material to be evaporated.

[0144] It should be noted that the coating formed by the second material to be evaporated and the coating formed by the first material to be evaporated are located on the same side surface of the substrate layer 600. Since there is no mask plate 300 to block it, the coating formed by the second material to be evaporated can completely cover the coating formed by the first material to be evaporated.

[0145] In S132, the substrate layer 600 can be continuously transferred to the carrier roller 400 by the rewinding device 500, and factors such as the transfer speed of the substrate layer 600 and the feeding speed of the second material to be evaporated can be controlled to form a second pattern coating with a certain thickness that completely covers the first pattern coating on the substrate layer 600.

[0146] It should be understood that the first pattern coating on the substrate layer 600 may be a discontinuous pattern coating due to the shielding of the mask plate 300. The second pattern coating on the substrate layer 600 may be a continuous pattern coating due to the absence of the shielding of the mask plate 300.

[0147] In some optional embodiments, in S131, when the second material to be evaporated in the open chamber R is in a stable evaporation state, before opening the baffle mechanism 200, the composite current collector preparation method further includes:

[0148] Obtaining a start signal to evacuate the environment where the evaporation device 1000 is located, and obtaining vacuum degree information;

[0149] When the vacuum degree information reaches the vacuum degree threshold, the evaporation device 100 is started to heat up to a second preset temperature to heat the second material to be evaporated;

[0150] Determine whether the second material to be evaporated in the open chamber R reaches a stable evaporation state.

[0151] It is understandable that the above steps disclose the preparation work before S131, that is, how to achieve and ensure that the second material to be evaporated is in a stable evaporation state. The above steps are similar to the preparation work before S111, except that the second preset temperature is different. It should be understood that heating to the preset temperature is determined by the melting point of the material to be evaporated. In specific applications, the first preset temperature and the second preset temperature are both 1000°C to 2000°C.

[0152] It should be noted that the second material to be evaporated in the above steps can be metallic copper. Since there is no mask plate 300 to block it, a continuous copper plating layer can be covered on the surface of the substrate layer 600, and this copper plating layer can completely cover the plating layer composed of the first material to be evaporated.

[0153] It can be understood that, through the above composite collective preparation method, two coating layers can be stacked along the thickness direction on the same side surface of the substrate layer 600, and the outer coating layer completely covers the inner coating layer. Repeating the above steps can form two coating layers with the same pattern on the other side surface of the substrate layer 600, thereby forming the composite current collector blank, and cutting the composite current collector blank can obtain a composite current collector that meets the size requirements.

[0154] Figure 7 A partial schematic diagram of a copper-aluminum composite current collector blank 700 is shown. Figure 7 The copper-aluminum composite current collector blank 700 can be manufactured by the above-mentioned evaporation equipment and the above-mentioned preparation method. The same pattern coating is formed on both sides of the substrate layer 600, and the single-side surface of the substrate layer 600 is stacked with an inner aluminum layer 710 and an outer copper layer 720, wherein the inner aluminum layer 710 is a pattern coating arranged in an array of multiple aluminum layer tiles, and the outer copper layer 720 completely covers the inner aluminum layer 710.

[0155] It should be understood that when the copper-aluminum composite current collector blank 700 is cut, the cut is set between two adjacent inner aluminum layer blocks, so that the inner aluminum layer 710 is not exposed at the end surface of the cut, and the copper-aluminum composite current collector can be used as the negative electrode of a lithium battery. Of course, the above-mentioned composite current collector preparation method in combination with the evaporation device 1000 is not limited to the preparation of copper-aluminum composite current collectors.

[0156] The optional embodiments of the present invention are described in detail above in conjunction with the accompanying drawings. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the embodiments of the present invention, a variety of simple modifications can be made to the technical solutions of the embodiments of the present invention, and these simple modifications all belong to the protection scope of the embodiments of the present invention.

[0157] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. To avoid unnecessary repetition, the embodiments of the present invention will not further describe various possible combinations.

[0158] Those skilled in the art will understand that all or part of the steps in the above-mentioned implementation methods can be completed by instructing the relevant hardware through a program, and the program is stored in a storage medium, including several instructions for making a single-chip microcomputer, a chip or a processor (processor) perform all or part of the steps of the methods described in each embodiment of the present invention. The aforementioned storage medium includes: U disk, mobile hard disk, read-only memory (ROM, Read-Only Memory), random access memory (RAM, Random Access Memory), disk or optical disk and other media that can store program codes.

[0159] In addition, various embodiments of the present invention may be arbitrarily combined, and as long as they do not violate the concept of the embodiments of the present invention, they should also be regarded as the contents disclosed by the present invention.

[0160] Although the embodiments of the present application have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations on the present application. Those skilled in the art can change, modify, replace and modify the above embodiments within the scope of the present application.

Claims

1. A vapor deposition device, characterized in that: It comprises an evaporation device (100), a baffle mechanism (200), a mask plate (300) and a film-carrying roller (400); The evaporation device (100) is provided with an open chamber (R) and is used to receive, heat and evaporate the material to be evaporated; The film-carrying roller (400) is located at the opening side of the open chamber (R) and is wound around the portion of the substrate layer (600) currently to be evaporated; The baffle mechanism (200) is connected to the evaporation device (100) and is located at the opening side of the open chamber (R); the mask plate (300) is located between the baffle mechanism (200) and the film carrier roller (400) and is configured to be detachably installed; The baffle mechanism (200) is used to open and close the open chamber (R) to cooperate with the mask plate (300) to form a target pattern coating on the substrate layer (600).

2. The evaporation device according to claim 1, characterized in that: The projection enclosed range of the mask plate (300) on the evaporation device (100) covers the opening of the open chamber (R).

3. The evaporation device according to claim 1, characterized in that: The mask plate (300) comprises a plate body (310), wherein the plate body (310) is provided with a plurality of evaporation holes (H1) arranged at intervals; The evaporation holes (H1) are used to allow the vapor formed by the material to be evaporated to pass through, so as to form a target pattern coating on the substrate layer (600).

4. The evaporation device according to claim 3, characterized in that: The plate body (310) is an arc-shaped structure; The diameter of the arc surface of the plate body (310) facing the film-carrying roller (400) is smaller than the diameter of the arc surface of the plate body (310) facing away from the film-carrying roller (400).

5. The evaporation device according to claim 3, characterized in that: The plate body (310) and the film-carrying roller (400) are arranged in parallel and at intervals.

6. The evaporation device according to claim 3, characterized in that: The mask plate (300) further comprises a cooling pipeline (320), wherein the cooling pipeline (320) is connected to the plate body (310), and the cooling pipeline (320) is configured to allow a cooling medium to pass through so as to cool the plate body (310).

7. The evaporation device according to claim 6, characterized in that: The cooling pipeline (320) comprises a plurality of first pipeline sections (321) and a plurality of second pipeline sections (322), and each of the second pipeline sections (322) connects two adjacent first pipeline sections (321); The plurality of evaporation holes (H1) are arranged in an array, and at least one row of the evaporation holes (H1) is located between two adjacent first pipeline sections (321).

8. The evaporation device according to claim 7, characterized in that: The plate body (310) is formed with a plurality of thinning areas (S) arranged side by side, and each of the thinning areas (S) is provided with at least one row of the vapor deposition holes (H1).

9. The evaporation device according to claim 1, characterized in that: The baffle mechanism (200) comprises a baffle (210) and a driving mechanism (220); The driving mechanism (220) is connected to the evaporation device (100), and the baffle (210) is connected to the driving mechanism (220); The driving mechanism (220) is used to drive the baffle (210) to move linearly to open and close the opening of the open chamber (R).

10. The evaporation device according to claim 1, characterized in that: The evaporation device (100) comprises an evaporation container (110) and a heating structure (120); The evaporation container (110) is provided with the open chamber (R) for accommodating the material to be evaporated, and the heating structure (120) is arranged in the evaporation container (110) for heating and evaporating the material to be evaporated.