Wafer clamping and fixing device

By designing a clamping thimble and ring structure with support and limit functions, combined with the monitoring of pressure sensors, the problem of rupture caused by thermal stress and deviation in laser annealing equipment is solved, and the stable fixation of the wafer is achieved and precise processing reduces the risk of damage.

CN222071921UActive Publication Date: 2024-11-26HUBEI YANGTZE PILOT-LINE SERVICES CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420774167.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-15
Publication Date
2024-11-26
Estimated Expiration
2034-04-15

AI Technical Summary

Technical Problem

During semiconductor manufacturing, wafers are broken due to uneven thermal stress in laser annealing equipment, and the wear and lifting and movement of the support thimble lead to smooth deviation of the wafer, which is difficult to accurately measure and increase the probability of damage.

Method used

Design a wafer clamping fixing device, including a bracket, an adsorption chuck and a plurality of clamping thimbles. The clamping thimble has a support part and a limiting part, and provides upward support force through the support part, and the limiting part and the side of the wafer The gap between the limit part and the wafer can be preset. The clamping thimble passes through the through hole to lift the clamping wafer, and a ring is arranged above the wafer to cover the edge. The pressure sensor is used to monitor the clamping thimble. Pressure to ensure stable and stable wafer fixation.

Benefits of technology

It effectively avoids the offset and rupture of the wafer during heat treatment, improves the stability and fixation accuracy of the wafer, reduces the probability of damage, and ensures the safety and reliability of laser heat treatment through real-time monitoring of the pressure sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222071921U_ABST
    Figure CN222071921U_ABST
Patent Text Reader

Abstract

The utility model provides a wafer clamping and fixing device, and relates to the technical field of semiconductor manufacturing, the clamping and fixing device comprises a support, an adsorption chuck and a plurality of clamping thimbles, the adsorption chuck is used for adsorbing a wafer, and the adsorption chuck is provided with a through hole; the support supports the clamping ejector pin, and the clamping ejector pin can penetrate through the through hole to jack and clamp the wafer. Wherein the clamping ejector pin comprises a supporting part and a limiting part, the supporting part is used for supporting a wafer, and the side face of at least part of the limiting part can make contact with the side face of the wafer and is used for clamping the wafer. Through the improvement of the structure, the problem of wafer slip can be effectively avoided, so that the wafer is prevented from being damaged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of semiconductor manufacturing, in particular to a wafer clamping and fixing device. Background Art

[0002] In semiconductor manufacturing, wafers need to undergo various surface treatments, such as etching, cleaning, polishing, material deposition, etc. When performing surface treatment on the wafer, the wafer needs to be fixed.

[0003] At present, when using DSA laser annealing equipment for heat treatment, due to the high-energy characteristics of the laser, the laser directly hits the edge of the wafer. Due to the existence of thermal stress, the thermal stress on both sides of the wafer is inconsistent, which may cause the wafer to crack. At the same time, considering that the support pins support the wafer through long-term lifting and lowering movements, the support pins may be worn. When using the support to lift the wafer, it may cause the wafer to slide and deflect, and the offset cannot be accurately measured. If the offset exceeds the threshold, it is more likely to hit the edge of the wafer during laser heat treatment, increasing the probability of wafer damage. Utility Model Content

[0004] The utility model provides a wafer clamping and fixing device to solve the technical problem of how to avoid the wafer from being offset during surface treatment, thereby reducing the probability of wafer damage.

[0005] An embodiment of the utility model provides a wafer clamping and fixing device, which comprises: a bracket; an adsorption chuck for adsorbing the wafer, and the adsorption chuck has a through hole; a plurality of clamping ejectors, the bracket supports the clamping ejectors, and the clamping ejectors can pass through the through holes to lift and clamp the wafer; wherein the clamping ejectors comprise a supporting portion and a limiting portion, the supporting portion is used to support the wafer, and at least part of the side surface of the limiting portion can contact the side surface of the wafer for clamping the wafer.

[0006] Furthermore, the clamping and fixing device also includes a plurality of pressure sensors, and the pressure sensors are respectively arranged between the clamping ejector pins and the bracket, and the pressure sensors can obtain the weight of the clamping ejector pins and the wafer.

[0007] Furthermore, the side surface of the limiting portion is an arc-shaped surface.

[0008] Furthermore, the supporting portion supports the wafer, and a gap is provided between part of the limiting portion and the wafer.

[0009] Furthermore, the maximum gap between the limiting portion and the wafer is 0.5 mm.

[0010] Furthermore, the clamping and fixing device also includes a circular ring, the inner diameter of the circular ring is 296 mm, the outer diameter of the circular ring is 336 mm, the diameter of the wafer is 300 mm, and the circular ring is arranged above the wafer to cover the wafer.

[0011] Furthermore, the diameter of the adsorption chuck is 330 mm, and the through hole is in an annular area, which is an area formed by the overlapping position of the circular ring and the adsorption chuck in the lifting direction of the clamping ejector pin.

[0012] Furthermore, the number of the through holes and the number of the clamping ejector pins are both three, and the through holes are circumferentially spaced apart on the adsorption chuck.

[0013] Furthermore, the number of the through holes and the number of the clamping ejector pins are both four, and the through holes are circumferentially spaced apart on the adsorption chuck.

[0014] Furthermore, the through holes are evenly spaced in the circumferential direction of the adsorption chuck.

[0015] The utility model provides a wafer clamping and fixing device, which comprises a bracket, an adsorption chuck and a plurality of clamping ejectors, wherein the adsorption chuck is used for adsorbing the wafer, and the adsorption chuck has a through hole; the bracket supports the clamping ejectors, and the clamping ejectors can pass through the through holes to lift and clamp the wafer; wherein the clamping ejectors comprise a supporting portion and a limiting portion, wherein the supporting portion is used for supporting the wafer, and at least part of the side surfaces of the limiting portions can contact with the side surfaces of the wafer for clamping the wafer. Through a new structural design, the position of the traditional clamping pin is moved from the center of the adsorption chuck to the edge of the adsorption chuck, thereby improving the stability of the clamping pin in supporting the wafer. At the same time, the structural design of the clamping pin is also changed. The clamping pin includes a supporting part and a limiting part. The limiting part protrudes from the supporting part. The supporting part is used to provide an upward supporting force for the wafer. At the same time, part of the limiting part contacts the side of the wafer. The limiting part is used to limit the wafer so that the wafer is clamped between multiple limiting parts. The gap between the limiting part and the wafer can be pre-set to avoid excessive horizontal displacement of the wafer as much as possible, thereby avoiding damage to the wafer during heat treatment. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 A schematic structural diagram of a wafer clamping and fixing device provided in an embodiment of the utility model;

[0017] Figure 2 A schematic diagram of the exploded structure of the clamping and fixing device provided in an embodiment of the utility model;

[0018] Figure 3 A top view of a wafer clamping and fixing device provided in an embodiment of the utility model;

[0019] Figure 4 A side view of a wafer clamping and fixing device provided by an embodiment of the utility model;

[0020] Figure 5 A schematic diagram of the structure of a clamping ejector pin provided in an embodiment of the utility model;

[0021] Figure 6 A schematic diagram of the structure of another clamping ejector pin provided in an embodiment of the utility model;

[0022] Figure 7 A schematic structural diagram of another wafer clamping and fixing device provided in an embodiment of the utility model;

[0023] Figure 8 for Figure 7 Schematic diagram of the local enlarged structure of part A.

[0024] Description of Reference Numerals

[0025] 100, clamping and fixing device; 110, bracket; 120, adsorption chuck; 121, through hole; 130, clamping pin; 131, supporting part; 132, limiting part; 1321, side of limiting part; 140, ring; 150, pressure sensor; 200, wafer; D1, diameter of wafer; D2, diameter of adsorption chuck; D3, inner diameter of ring; D4, outer diameter of ring; D5, gap between limiting part and wafer. DETAILED DESCRIPTION

[0026] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.

[0027] The various specific technical features described in the specific embodiments can be combined in any suitable manner without contradiction, for example, different embodiments and technical solutions can be formed by combining different specific technical features. In order to avoid unnecessary repetition, the various possible combinations of the specific technical features in the utility model will not be described separately.

[0028] In the following description, the terms "first\second\..." are only used to distinguish different objects, and do not mean that the objects have the same or related points. It should be understood that the directions "above", "below", "outside" and "inside" are all directions in normal use, and the directions "left" and "right" refer to the left and right directions shown in the specific corresponding schematic diagrams, which may or may not be the left and right directions in normal use.

[0029] It should be noted that the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, an element defined by the sentence "comprising a ..." does not exclude the presence of other identical elements in the process, method, article or device including the element. The term "connected" includes both direct and indirect connections unless otherwise specified.

[0030] In a specific embodiment, the clamping and fixing device is suitable for any clamping and fixing that requires wafer processing. For example, the clamping and fixing device can be used to clamp and fix the wafer so as to clean the surface of the wafer; for example, the clamping and fixing device can be used to clamp and fix the wafer so as to perform laser heat treatment on the surface of the wafer; for the sake of ease of explanation, the following is an exemplary explanation using the example of clamping and fixing the wafer by the clamping and fixing device so as to perform laser annealing on the surface of the wafer.

[0031] To facilitate understanding, let's first give a brief introduction to laser annealing. The main purpose of wafer laser annealing is to improve the microstructure of the wafer surface by using high-energy lasers to quickly heat and cool the material, thereby improving the performance and characteristics of the material. Specifically, laser annealing can effectively repair ion implantation damage, reduce grain boundaries and lattice defects, and improve the crystallization quality of the wafer and the order of the crystal. In addition, it can increase the light absorption rate on the wafer surface, improve the photoelectric conversion efficiency, and activate dopant ions, thereby improving the performance and reliability of semiconductor devices. Laser annealing technology has the following advantages over traditional annealing methods: heating is limited to the local surface layer and will not affect the physical properties of surrounding components; it can form a hemispherical deep contact area; because the laser beam can be shaped to be very fine, it provides the possibility for micro-area thin layer annealing.

[0032] At present, in the process of annealing by laser, the laser has the particularity of high energy, which directly hits the edge of the wafer. Due to the problem of thermal stress, the thermal stress on both sides of the wafer is inconsistent, which may cause the wafer to break. During use, a circular ring structure can be used to block the edge of the wafer to ensure that the laser does not directly act on the edge of the wafer during operation. However, considering the wear of the support pin, the transportation of the manipulator and the up and down movement of the support pin may cause the wafer to shift. Due to the high operating temperature of the laser as high as 250 ° C and the particularity of the laser, the machine cannot detect the offset of the wafer through the sensor inside. The existing method injects GE ions into the wafer, anneals it normally with laser, and observes its edge. Due to the GE ion injection into the wafer, the unannealed area will form a white edge characteristic. By measuring the size of the edge, it is ensured that the wafer is in a reasonable annealing range, and the wafer position is adjusted according to the offset, and the GE ions are injected again to repeat the operation. This method is complicated and cumbersome, and there is a deviation in manual measurement. Based on the above problems, the present application provides a wafer clamping and fixing device.

[0033] In some embodiments, Figures 1 to 4 As shown, the clamping and fixing device 100 includes a support 110, an adsorption chuck 120 and a plurality of clamping ejector pins 130. The adsorption chuck 120 is used to adsorb the wafer 200, and the adsorption chuck 120 has a through hole 121; the support 110 supports the clamping ejector pins 130, and the clamping ejector pins 130 can pass through the through hole 121 to lift and clamp the wafer 200; wherein, the clamping ejector pins 130 include a supporting portion 131 and a limiting portion 132, the supporting portion 131 is used to support the wafer 200, and at least part of the side surface of the limiting portion 132 can contact the side surface of the wafer 200, and is used to clamp the wafer 200.

[0034] Specifically, the size of the wafer 200 is different, and the size of the corresponding clamping structure is also different. For the sake of convenience, the diameter of the wafer 200 is defined as D1, and the diameter D1 of the wafer 200 is 300 mm for example. The wafer 200 is located above the adsorption chuck 120, and the adsorption chuck 120 is used to adsorb the wafer 200. The diameter size of the adsorption chuck 120 is defined as D2. The size of D2 is not specifically limited and can be determined according to actual needs. For example, the diameter D2 of the adsorption chuck 120 is 330 mm. When the wafer 200 is placed above the adsorption chuck 120, the edge of the adsorption chuck 120 protrudes from the edge of the wafer 200. The adsorption chuck 120 is provided with a plurality of through holes 121, and the number and size of the through holes 121 are related to the clamping ejector pin 130. Each through hole 121 corresponds to a clamping ejector pin 130, and the clamping ejector pin 130 can pass through the through hole 121, that is, the size of the through hole 121 should be slightly larger than the size of the clamping ejector pin 130. For example, the clamping ejector pin 130 is a cylindrical structure, and the through hole 121 can also be a circular through hole.

[0035] One end of the clamping ejector pin 130 contacts the wafer 200, and the other end of the clamping ejector pin 130 contacts the bracket 110. The bracket 110 provides support for the clamping ejector pin 130. The specific structure of the bracket 110 is not limited, and it only needs to play a supporting role. Each clamping ejector pin 130 can be provided with a bracket 110 separately, or multiple clamping ejectors 130 can share a bracket 110. Considering the need for the clamping ejector pin 130 to be lifted and lowered, the side of the clamping ejector pin 130 close to the bracket 110 is connected to the motor, and the operation of the motor drives the clamping ejector pin 130 to rise and fall. The specific process is that the wafer 200 is adsorbed on the adsorption chuck 120, the motor starts to run, the clamping ejector pin 130 passes through the through hole 121 from the bottom of the through hole 121 to the top, contacts the wafer 200, and lifts the wafer 200 to the corresponding position, so as to use the laser to heat treat the wafer 200. In order to prevent the laser from directly hitting the edge of the wafer 200 and causing the wafer 200 to break, the clamping and fixing device 100 also includes a ring 140. The ring 140 is located directly above the wafer 200. Here, directly above means that the center of the ring 140 and the center of the wafer 200 are in the same vertical direction. The ring 140 can be a ceramic structure. The inner diameter of the ring 140 is defined as D3, and the outer diameter of the ring 140 is defined as D4. For example, the inner diameter D3 of the ring 140 is 296 mm, and the outer diameter D4 of the ring 140 is 336 mm. The ring 140 can cover the 2 mm area of ​​the edge of the wafer 200, thereby preventing the laser from directly hitting the 2 mm area of ​​the edge.

[0036] In order to improve the stability of the wafer 200, the clamping pin 130 is designed to be a structure that can perform dual functions of support and clamping. The clamping pin 130 includes a supporting portion 131 and a limiting portion 132. The limiting portion 132 protrudes from the upper surface of the supporting portion 131. For example, the supporting portion 131 is a cylindrical structure, and the limiting portion 132 is also a cylindrical structure. One end of the limiting portion 132 is connected to the upper surface of the supporting portion 131. The cross-sections of the supporting portion 131 and the limiting portion 132 perpendicular to the vertical direction are both circular. The circular cross-section size of the limiting portion 132 is smaller than the circular cross-section size of the supporting portion 131. The circular upper surface of the supporting portion 131 is used to contact the wafer 200 to support the wafer 200, and the cylindrical side surface of the limiting portion 132 is used to contact the side surface of the wafer 200, so as to limit the movement of the wafer 200 in the horizontal direction. For example, the supporting portion 131 is a cubic structure, and the limiting portion 132 is also a cubic structure. One end of the limiting portion 132 is connected to the upper surface of the supporting portion 131. The cross-sections of the supporting portion 131 and the limiting portion 132 perpendicular to the vertical direction are both square. The square cross-section size of the limiting portion 132 is smaller than the square cross-section size of the supporting portion 131. The upper surface of the supporting portion 131 in the positive direction is used to contact the wafer 200 to support the wafer 200, and the cubic side surface of the limiting portion 132 is used to contact the side surface of the wafer 200, so as to limit the movement of the wafer 200 in the horizontal direction.

[0037] It should be noted that the clamping ejector pins 130 need both support and clamping, so the diameter of the circle formed by the limiting parts 132 of the multiple clamping ejector pins 130 should be equal to or slightly larger than the diameter of the wafer 200. For example, when the diameter of the circle formed by the limiting parts 132 is equal to the diameter of the wafer 200, the side surfaces of all the limiting parts 132 can contact the side surfaces of the wafer 200 to clamp the wafer 200. The wafer 200 cannot be offset when surrounded by the limiting parts 132 and is in a completely fitted state. For example, when the diameter of the circle formed by the limiting parts 132 is slightly larger than the diameter of the wafer 200, the side surfaces of some limiting parts 132 can contact the side surfaces of the wafer 200, and there is a gap between the side surfaces of another part of the limiting parts 132 and the side surfaces of the wafer 200, and the wafer 200 can move within the range of the gap when surrounded by the limiting parts 132. A specific embodiment of the gap movement will be given later. Therefore, the through hole 121 corresponding to the clamping ejector pin 130 should be arranged in the annular area formed by the overlapping position of the ring 140 and the adsorption chuck 120 in the lifting direction of the clamping ejector pin 130 .

[0038] The utility model provides a wafer clamping and fixing device, which comprises a bracket, an adsorption chuck and a plurality of clamping ejectors, wherein the adsorption chuck is used for adsorbing the wafer, and the adsorption chuck has a through hole; the bracket supports the clamping ejectors, and the clamping ejectors can pass through the through holes to lift and clamp the wafer; wherein the clamping ejectors comprise a supporting portion and a limiting portion, wherein the supporting portion is used for supporting the wafer, and at least part of the side surfaces of the limiting portions can contact with the side surfaces of the wafer for clamping the wafer. Through a new structural design, the position of the traditional clamping pin is moved from the center of the adsorption chuck to the edge of the adsorption chuck, thereby improving the stability of the clamping pin in supporting the wafer. At the same time, the structural design of the clamping pin is also changed. The clamping pin includes a supporting part and a limiting part. The limiting part protrudes from the supporting part. The supporting part is used to provide an upward supporting force for the wafer. At the same time, part of the limiting part contacts the side of the wafer. The limiting part is used to limit the wafer so that the wafer is clamped between multiple limiting parts. The gap between the limiting part and the wafer can be pre-set to avoid excessive horizontal displacement of the wafer as much as possible, thereby avoiding damage to the wafer during heat treatment.

[0039] In some embodiments, Figure 1 and Figure 2 As shown, the clamping and fixing device 100 also includes a plurality of pressure sensors 150, which are respectively arranged between the clamping ejector pins 130 and the bracket 110, and the pressure sensors 150 can obtain the weight of the clamping ejector pins 130 and the wafer 200. Specifically, in order to further ensure the reliability during laser heat treatment, the wafer 200 is kept in a horizontal position as much as possible so that the surface of the wafer 200 can be heat treated uniformly, and a pressure sensor 150 is also installed between each clamping ejector pin 130 and the bracket 110. The pressure sensor 150 is used to obtain the weight of the clamping ejector pin 130 and the wafer 200 above the clamping ejector pin 130. Under normal circumstances, the weight displayed by each pressure sensor 150 should be the same, or very close. Here, very close can be understood as the mass error obtained by different pressure sensors 150 is within 5%. If the pressure displayed by a certain pressure sensor 150 is abnormal, the landing position of the surface wafer 200 is abnormal, or the wafer 200 does not land on the clamping ejector pin 130 above the pressure sensor 150. In abnormal situations, the laser heat treatment can be stopped in time to ensure the safety and integrity of the wafer 200. Considering that the clamping ejector pin 130 needs to be raised and lowered, the motor can drive the pressure sensor 150 to be connected to the clamping ejector pin 130 and rise and fall together. As long as the clamping ejector pin 130 lands on the pressure sensor 150, the landing point placement information of the clamping ejector pin 130 and the wafer 200 can be obtained.

[0040] In some embodiments, Figure 5 and Figure 6As shown, considering that the limiting portion 132 is used to limit the wafer 200 in the horizontal direction, the side surface 1321 of the limiting portion will inevitably contact the edge of the wafer 200. In order to avoid damage to the wafer 200 caused by bumps as much as possible, the side surface 1321 of the limiting portion is set to an arc surface, thereby avoiding edges and corners and achieving better contact with the wafer 200. For example, Figure 5 As shown, the limiting portion 132 is a cylinder, and the side surface 1321 of the limiting portion is an arc-shaped curved surface. The side surface of the cylinder does not have edges and corners, which can avoid the limiting portion 132 from damaging the wafer 200 as much as possible. Figure 6 As shown, the limiting portion 132 is a fan ring body, which is a part of a circular ring cut into a fan shape. The fan ring body is a cube with a fan ring end face. The inner ring of the fan ring can be directly the same as the diameter of the wafer 200, so that the side surface 1321 of the limiting portion can better fit with the side surface of the wafer 200. The limiting portion 132 of this structure can increase the contact area with the wafer 200, avoid tip force, etc., and provide better protection for the wafer 200.

[0041] In some embodiments, Figure 7 and Figure 8As shown, the support portion 131 supports the wafer 200, and there is a gap between the part of the limiting portion 132 and the wafer 200. Specifically, any product will inevitably have a dimensional error. If the error of the product is within the specified range, the product is considered to be in compliance with the marking, and there will also be corresponding installation errors in the installation of the product. For example, for the laser heat treatment of the wafer 200, the center of the wafer 200 should be in the same vertical direction as the center of the adsorption chuck 120. However, if the error between the center of the wafer 200 and the center of the adsorption chuck 120 is within the allowable range, the laser heat treatment of the wafer 200 will not be affected. Based on the considerations of dimensional error and installation convenience, without affecting the normal annealing heat treatment of the wafer 200 by the laser, the diameter of the circle surrounded by the limiting parts 132 of the multiple clamping pins 130 can be slightly larger than the diameter of the wafer 200, so that the wafer 200 is placed on the supporting part 131 and is directly stuck in the limited position of the limiting part 132. When some limiting parts 132 are in contact with the wafer 200, some limiting parts 132 are not in contact with the wafer 200. The distance between the limiting part 132 and the wafer 200 is an active gap. Within the set active gap range, no matter which limiting part 132 the wafer 200 is close to, the working range of the laser will not cause damage to the wafer 200 during laser annealing heat treatment. The gap between the limiting portion 132 and the wafer 200 is defined as D5. The specific numerical value of the movable gap D5 is not limited and can be determined according to actual conditions. For example, the maximum gap D5 between the limiting portion 132 and the wafer 200 is 0.5 mm, and the range in which the wafer 200 can move relative to the limiting portion 132 is between 0 and 0.5 mm. For example, the number of through holes 121 and the number of clamping pins 130 are both 2, and the through holes 121 are symmetrically arranged on both sides of the adsorption chuck 120 with the center of the circle of the adsorption chuck 120 as the center. If the limiting portion 132 of one of the clamping pins 130 contacts the wafer 200, the limiting portion 132 of the other clamping pin 130 is spaced 0.5 mm from the wafer 200.

[0042] In some embodiments, Figure 1 and Figure 3As shown, the number of through holes 121 and clamping pins 130 are both three, and the through holes 121 are arranged at intervals circumferentially on the adsorption chuck 120. Specifically, the clamping pins 130 pass through the through holes 121 to support and clamp the wafer 200. In order to improve the stability of the support and clamping, three through holes 121 can be arranged circumferentially on the adsorption chuck 120, so as to be matched with three clamping pins 130 accordingly. The three clamping pins 130 are used to support and clamp the wafer 200. The three through holes 121 can be arranged evenly or unevenly on the adsorption chuck 120. For example, if the three through holes 121 are evenly spaced in the circumferential direction of the adsorption chuck 120, the angle between two adjacent through holes 121 and the center of the adsorption chuck 120 is 120 degrees. If a pressure sensor 150 is installed, the pressure value of each pressure sensor 150 should also be the same, so as to facilitate the judgment of whether the wafer 200 is placed stably. For example, the three through holes 121 are unevenly arranged in the circumferential direction of the adsorption chuck 120, wherein the angle between two of the through holes 121 and the center of the adsorption chuck 120 is 90 degrees, and the angle between the remaining through hole 121 and the other through holes 121 and the center of the adsorption chuck 120 is 135 degrees. It should be emphasized that in the case of uneven arrangement, the three clamping pins 130 must not tilt or flip over during the process of lifting the wafer 200.

[0043] In some embodiments, the number of through holes 121 and clamping pins 130 are both four, and the through holes 121 are arranged circumferentially at intervals on the adsorption chuck 120. Specifically, the clamping pins 130 pass through the through holes 121 to support and clamp the wafer 200. In order to improve the stability of the support and clamping, four through holes 121 can be arranged circumferentially at intervals on the adsorption chuck 120, so as to be matched with four clamping pins 130 accordingly. The four clamping pins 130 are used to support and clamp the wafer 200. The four through holes 121 can be arranged evenly or unevenly on the adsorption chuck 120. For example, if the four through holes 121 are evenly spaced in the circumferential direction of the adsorption chuck 120, the angle between two adjacent through holes 121 and the center of the adsorption chuck 120 is 90 degrees. If a pressure sensor 150 is installed, the pressure value of each pressure sensor 150 should also be the same, so as to facilitate the judgment of whether the wafer 200 is placed stably. For example, the four through holes 121 are unevenly arranged in the circumferential direction of the adsorption chuck 120, and the angles formed between the four through holes 121 and the center of the adsorption chuck 120 are 70 degrees, 80 degrees, 100 degrees and 110 degrees respectively. Similarly, in the case of uneven arrangement, it is necessary to ensure that the four clamping ejector pins 130 cannot tilt or flip when lifting the wafer 200.

[0044] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention.

Claims

1. A wafer clamping and fixing device, characterized in that: include: Bracket; An adsorption chuck, used for adsorbing the wafer, and the adsorption chuck has a through hole; A plurality of clamping ejectors, the bracket supports the clamping ejectors, and the clamping ejectors can pass through the through holes to lift and clamp the wafer; The clamping ejector pin comprises a supporting portion and a limiting portion, wherein the supporting portion is used to support the wafer, and at least a part of the side surface of the limiting portion can contact the side surface of the wafer for clamping the wafer.

2. The clamping and fixing device according to claim 1, characterized in that: The clamping and fixing device further comprises a plurality of pressure sensors, wherein the pressure sensors are respectively arranged between the clamping ejector pins and the bracket, and the pressure sensors can obtain the weight of the clamping ejector pins and the wafer.

3. The clamping and fixing device according to claim 1, characterized in that: The side surface of the limiting portion is an arc-shaped surface.

4. The clamping and fixing device according to claim 1 or 3, characterized in that: The supporting portion supports the wafer, and a gap is formed between part of the limiting portion and the wafer.

5. The clamping and fixing device according to claim 4, characterized in that: The maximum gap between the limiting portion and the wafer is 0.5 mm.

6. The clamping and fixing device according to claim 1, characterized in that: The clamping and fixing device also includes a circular ring, the inner diameter of the circular ring is 296 mm, the outer diameter of the circular ring is 336 mm, the diameter of the wafer is 300 mm, and the circular ring is arranged above the wafer to cover the wafer.

7. The clamping and fixing device according to claim 6, characterized in that: The diameter of the adsorption chuck is 330 mm, and the through hole is in an annular area, which is an area formed by the overlapping position of the circular ring and the adsorption chuck in the lifting direction of the clamping ejector pin.

8. The clamping and fixing device according to claim 1, characterized in that: The number of the through holes and the number of the clamping ejector pins are both three, and the through holes are circumferentially spaced on the adsorption chuck.

9. The clamping and fixing device according to claim 1, characterized in that: The number of the through holes and the number of the clamping ejector pins are both four, and the through holes are circumferentially spaced on the adsorption chuck.

10. The clamping and fixing device according to claim 8 or 9, characterized in that: The through holes are evenly spaced in the circumferential direction of the adsorption chuck.

Citation Information

Cited By

  • Electrostatic chuck

    CN120809658A