Mechanism for adjusting plastic filling flow balance
The balancing mechanism in plastic molds addresses the challenge of producing varied product sizes with consistent glue volumes by using a positioning groove and adjusting plate to stabilize flow channels, allowing for simultaneous production of multiple products with balanced glue amounts.
Patent Information
- Application Number
- CN202323460094.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-19
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2033-12-19
AI Technical Summary
Existing plastic molds struggle to produce multiple products of different sizes simultaneously due to unbalanced plastic flow, leading to inconsistent glue volumes, and current adjustment mechanisms are prone to slipping and twisting off, complicating the process.
A balancing mechanism with a positioning groove and adjusting plate, connected via a screw, allows for adjustable flow channels in the mold, enabling precise control of glue volume in each channel to accommodate various product sizes.
Enables simultaneous production of multiple products with balanced glue volumes by adjusting flow sizes through the positioning groove and adjusting plate, stabilizing the adjustment process and maintaining consistent product quality.
Smart Images

Figure CN222096847U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of plastic molds, in particular to a mechanism for adjusting plastic filling flow balance. Background Art
[0002] When plastic products are produced, they are injection molded through molds. During the production process, when the products are formed, small products are fully formed first, and large products are only half formed, resulting in unbalanced products. Currently, molds mostly use throttle valve screws to adjust the flow rate. The throttle valve screws often slip when adjusted, and are prone to twisting off when too much force is applied, causing certain losses.
[0003] The plastic mold in the prior art 201821553242.3 is pressed on one side of the baffle by a pressure cover, and the elastic member abuts against the other side of the baffle. The pressure cover is rotated, and the pressure cover pushes the baffle to move together with the latch. During the movement process, the latch is always pressed on the pressure cover by the elastic member, and the end of the latch away from the baffle is in the flow channel. The movement of the latch realizes the adjustment of the flow channel opening, and the trial mold does not need to disassemble the mold during the flow channel adjustment process.
[0004] The above structure can adjust the size of the flow channel, but the adjustment steps are relatively complicated, and multiple products of different sizes cannot be produced simultaneously in a set of molds, resulting in unbalanced glue volume control. Utility Model Content
[0005] In view of this, the purpose of the utility model is to provide a mechanism for adjusting the flow balance of plastic filling to solve the problem that a plurality of products of different sizes cannot be produced simultaneously in a set of molds, resulting in unbalanced control of the amount of plastic.
[0006] Based on the above purpose, the utility model provides a balancing mechanism for adjusting plastic filling flow, comprising a mold body and an upper demolding mold installed on the mold body, an injection port is provided on the top of the upper demolding mold, a plurality of flow channels are provided in the mold body and the upper demolding mold, the flow channels are connected to the injection port, and a balancing mechanism is provided outside the flow channel, and the balancing mechanism is used to adjust the amount of flow channel glue;
[0007] The balancing mechanism comprises a positioning groove provided in the mold body, an adjusting plate is slidably installed in the positioning groove, a through hole matching the flow channel is provided inside the adjusting plate, and the adjusting plate is connected to the positioning groove via a fixing member.
[0008] Preferably, the fixing member is a screw, a long screw hole is provided inside the adjusting plate, and the screw passes through the long screw hole provided in the adjusting plate.
[0009] Preferably, the long screw hole is a waist-shaped hole, and the screw and the long screw hole are used to fasten the connection between the adjustment plate and the positioning groove.
[0010] Preferably, the length of the positioning groove is greater than the length of the adjustment plate, and the adjustment plate moves inside the positioning groove to adjust the flow size.
[0011] Preferably, the width of the perforation is adapted to the width of the flow channel, and the perforation is arranged as a U-shaped groove.
[0012] The beneficial effects of the utility model are as follows: after the upper demoulding and the mold body are combined, when the amount of glue in a separate flow channel needs to be adjusted, the adjustment plate is moved in the positioning groove to change the space between the perforation of the adjustment plate and the flow channel. After adjustment, the balancing mechanism is fixed by the fixing part, and then injection molding is performed through the injection port and the flow channel. The flow size is adjusted according to demand to maintain the balance of the product glue amount, so that multiple products can be produced simultaneously with a set of molds. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] In order to more clearly illustrate the technical solutions in the present invention or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only for the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0014] Figure 1 It is a structural schematic diagram of the balancing mechanism of the utility model;
[0015] Figure 2 It is a schematic diagram of the half-section structure of the mold body of the utility model;
[0016] Figure 3 It is a schematic diagram of the structure of the utility model after the upper demoulding and the mold body are disassembled.
[0017] The markings in the figure are: 1. Mold body; 2. Upper demoulding; 3. Injection port; 4. Runner; 5. Balancing mechanism; 6. Adjustment plate; 7. Positioning groove; 8. Screw; 9. Screw long hole; 10. Perforation. DETAILED DESCRIPTION
[0018] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with specific embodiments.
[0019] like Figure 1 , Figure 2 and Figure 3 As shown, a plastic filling flow balancing mechanism comprises a mold body 1 and an upper demolding mold 2 installed on the mold body 1, an injection port 3 is provided on the top of the mold body 1, a plurality of flow channels 4 are provided in the mold body 1 and the upper demolding mold 2, the flow channels 4 are connected to the injection port 3, and a balancing mechanism 5 is provided outside the flow channels 4, and the balancing mechanism 5 is used to adjust the amount of glue in the flow channels 4;
[0020] The balancing mechanism 5 includes a positioning groove 7 provided in the mold body 1 , in which an adjusting plate 6 is slidably installed, and inside the adjusting plate 6 a through hole 10 matching the flow channel 4 is provided, and the adjusting plate 6 is connected to the positioning groove 7 via a fixing member.
[0021] In this embodiment, after the upper demolding 2 and the mold body 1 are combined, when it is necessary to adjust the amount of glue in a separate flow channel 4 to become smaller, the adjustment plate 6 is moved in the positioning groove 7, and the space between the perforation 10 of the adjustment plate 6 and the flow channel 4 becomes smaller, thereby reducing the amount of glue in the flow channel 4. When it is necessary to adjust the amount of glue in a separate flow channel 4 to become larger, the adjustment plate 6 is moved in the positioning groove 7, and the space between the perforation 10 of the adjustment plate 6 and the flow channel 4 is completely overlapped and becomes larger. After adjustment, the balancing mechanism 5 is fixed by the fixing part, and then injection molding is performed through the injection port 3 and the flow channel 4. The flow size is adjusted according to demand to maintain the balance of the product glue amount, thereby being able to produce multiple products at the same time with a set of molds.
[0022] As an implementation method, Figure 1 and Figure 3 As shown, the fixing member is a screw 8 , a long screw hole 9 is provided inside the adjusting plate 6 , and the screw 8 passes through the long screw hole 9 provided in the adjusting plate 6 .
[0023] In this embodiment, by moving the adjustment plate 6 in the positioning groove 7, the space between the through hole 10 of the adjustment plate 6 and the flow channel 4 changes. When adjusted, the adjustment plate 6 is fixed by the screw 8 and the screw long hole 9. The adjustment plate 6 is fixed to achieve the purpose of changing the amount of glue in the flow channel 4.
[0024] As an implementation method, Figure 1 and Figure 3 As shown, the long screw hole 9 is a waist-shaped hole, and the screw 8 and the long screw hole 9 are used to fasten the connection between the adjustment plate 6 and the positioning groove 7.
[0025] In this embodiment, the screw long hole 9 in the adjusting plate 6 moves outside the screw 8, so that the adjusting plate 6 can move stably in the positioning groove 7, and the screw 8 is used to fix the adjusted adjusting plate 6 at the same time.
[0026] As an implementation method, Figure 3 As shown, the length of the positioning groove 7 is greater than the length of the adjustment plate 6, and the adjustment plate 6 moves inside the positioning groove 7 to adjust the flow size.
[0027] In this embodiment, by stably moving the adjustment plate 6 in the positioning groove 7 , the through holes 10 in the adjustment plate 6 and the flow channel 4 are interlaced, thereby changing the distance between the flow channel 4 and the through holes 10 , thereby changing the flow size in the flow channel 4 .
[0028] As an implementation method, Figure 1As shown, the width of the through hole 10 is adapted to the width of the flow channel 4, and the through hole 10 is arranged as a U-shaped groove.
[0029] In this embodiment, after the perforation 10 is completely matched with the flow channel 4, the flow amount in the flow channel 4 reaches the maximum, and the flow size is adjusted according to actual needs to maintain the balance of the product glue amount.
[0030] Working principle: When in use, after separating the upper demolding 2 and the mold body 1, when it is necessary to adjust the amount of glue in a separate flow channel 4 to become smaller, the adjustment plate 6 is moved in the positioning groove 7, and the space between the perforation 10 of the adjustment plate 6 and the flow channel 4 becomes smaller, thereby reducing the amount of glue in the flow channel 4. When it is necessary to adjust the amount of glue in a separate flow channel 4 to become larger, the adjustment plate 6 is moved in the positioning groove 7, and the space between the perforation 10 of the adjustment plate 6 and the flow channel 4 that completely overlaps becomes larger. After adjustment, the adjustment plate 6 is fixed by screws 8 and screw long holes 9. The adjustment plate 6 is fixed to achieve the purpose of changing the amount of glue in the flow channel 4. After the upper demolding 2 and the mold body 1 are combined, injection molding is performed at the injection port 3 and the flow channel 4. The flow size is adjusted according to demand to maintain the balance of product glue amount, thereby being able to produce multiple products simultaneously with a set of molds.
[0031] Those skilled in the art should understand that the discussion of any of the above embodiments is merely illustrative and is not intended to imply that the scope of the present invention (including the claims) is limited to these examples. Under the concept of the present invention, the technical features in the above embodiments or different embodiments may be combined, the steps may be implemented in any order, and there are many other variations of the different aspects of the present invention as described above, which are not provided in detail for the sake of simplicity.
[0032] The utility model is intended to cover all such substitutions, modifications and variations that fall within the broad scope of the appended claims. Therefore, any omissions, modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the utility model should be included in the scope of protection of the utility model.
Claims
1. A mechanism for adjusting plastic filling flow balance, comprising a mold body (1) and an upper demolding mold (2) mounted on the mold body (1), wherein an injection port (3) is provided at the top of the upper demolding mold (2), and a plurality of flow channels (4) are provided in the mold body (1) and the upper demolding mold (2), wherein the flow channels (4) are connected to the injection port (3), and characterized in that: A balancing mechanism (5) is arranged outside the flow channel (4), and the balancing mechanism (5) is used to adjust the amount of glue in the flow channel (4); The balancing mechanism (5) comprises a positioning groove (7) provided in the mold body (1), an adjusting plate (6) being slidably mounted in the positioning groove (7), a through hole (10) matching the flow channel (4) being provided inside the adjusting plate (6), and the adjusting plate (6) and the positioning groove (7) being connected via a fixing member.
2. A plastic filling flow balancing mechanism according to claim 1, characterized in that: The fixing member is a screw (8), a long screw hole (9) is provided inside the adjusting plate (6), and the screw (8) passes through the long screw hole (9) provided in the adjusting plate (6).
3. A plastic filling flow balancing mechanism according to claim 2, characterized in that: The long screw hole (9) is a waist-shaped hole, and the screw (8) and the long screw hole (9) are used to fasten the connection between the adjustment plate (6) and the positioning groove (7).
4. The mechanism for adjusting plastic filling flow balance according to claim 1, characterized in that: The length of the positioning groove (7) is greater than the length of the adjustment plate (6), and the adjustment plate (6) moves inside the positioning groove (7) to adjust the flow size.