Photovoltaic module and photovoltaic system

By introducing stretchable glue into the photovoltaic module and using disassembled immersion liquid, the problem of low recycling efficiency of photovoltaic modules in the prior art is solved, and the adhesive force of glass to the adhesive film and back plate is removed in a short time, thereby improving the improvement of Recycling efficiency.

CN222106734UActive Publication Date: 2024-12-03JIANGXI MUBON HI TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420496262.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-14
Publication Date
2024-12-03
Estimated Expiration
2034-03-14

AI Technical Summary

Technical Problem

When recycling glass and back panels in existing photovoltaic modules, since the glass and back panel are not easy to separate from the adhesive film, it takes a long time of chemical soaking to remove the adhesive force, resulting in low recycling efficiency.

Method used

The photovoltaic module is introduced and is arranged between the glass and the packaging film and between the back plate and the packaging film. The bonding structure is partially separated by pulling out the binding adhesive, and the contact is increased by using the disassembled immersion liquid. Area, shorten the soaking time.

Benefits of technology

Through the combined action of easy-twist glue and disassembled immersion liquid, the immersion time of photovoltaic modules is significantly shortened, the recycling efficiency of glass and back plate is improved, and the recycling process is simple and efficient.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222106734U_ABST
    Figure CN222106734U_ABST
Patent Text Reader

Abstract

The utility model discloses a photovoltaic assembly and a photovoltaic system, and belongs to the technical field of photovoltaic products. The photovoltaic module comprises upper glass, an upper packaging adhesive film, a battery piece, a lower packaging adhesive film and a lower packaging piece which are sequentially arranged from top to bottom; the photovoltaic module further comprises easy-to-pull glue, and the easy-to-pull glue is arranged between the upper glass and the upper packaging glue film and / or between the lower packaging glue film and the lower packaging piece. The easy-to-pull adhesive is of a long-strip-shaped structure, a plurality of pieces of easy-to-pull adhesive are arranged between the upper glass and the upper packaging adhesive film and / or between the lower packaging adhesive film and the lower packaging piece, and the plurality of pieces of easy-to-pull adhesive are arranged in the length direction of the photovoltaic module at intervals. According to the photovoltaic module provided by the utility model, under the combined action of the easy-to-pull glue and the disassembly soaking solution, the bonding force between the upper glass and the upper packaging glue film and / or the bonding force between the lower packaging glue film and the lower packaging piece can be removed in a short time, so that the recovery of the upper glass and the lower packaging piece can be realized in a short time.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of photovoltaic products, in particular to a photovoltaic component and a photovoltaic system. Background Art

[0002] like Figure 1 As shown, the photovoltaic module mainly includes an upper glass 1', an upper packaging film 2', a battery cell 3', a lower packaging film 4' and a lower packaging member 5' (which can be a lower glass or a back plate) arranged in sequence from top to bottom; wherein, the upper packaging film 2' and the lower packaging film 4' can seal the battery cell 3', and can tightly bond the glass and the back plate to the battery cell 3' respectively.

[0003] At present, when the glass and back panel need to be recycled, since the glass and back panel are not easy to be separated from the adhesive film respectively, the entire photovoltaic module is usually immersed in a disassembly soaking liquid. After a certain soaking time, the adhesion between the glass and back panel and the adhesive film respectively can be released, so that the glass and back panel can be smoothly recycled.

[0004] However, in the above-mentioned chemical immersion recycling method, since the contact area between the disassembly immersion liquid and the adhesive film is small, a long immersion time is required to release the adhesion between the glass and the back panel and the adhesive film respectively, and the recycling efficiency is low. Utility Model Content

[0005] The purpose of the utility model is to provide a photovoltaic module and a photovoltaic system, which can release the adhesion between the upper glass and the upper packaging film, and / or between the lower packaging film and the lower packaging component in a relatively short time by disassembling the immersion effect of the immersion liquid, so that the upper glass and the lower packaging component can be recycled in a relatively short time.

[0006] To achieve this purpose, the utility model adopts the following technical solutions:

[0007] A photovoltaic module, comprising an upper glass, an upper packaging film, a battery cell, a lower packaging film and a lower packaging member arranged in sequence from top to bottom, and the photovoltaic module also includes:

[0008] Easy-to-pull adhesive, the easy-to-pull adhesive is arranged between the upper glass and the upper packaging adhesive film, and / or between the lower packaging adhesive film and the lower packaging member;

[0009] The easy-to-pull adhesive is in a long strip structure, and a plurality of the easy-to-pull adhesives are arranged between the upper glass and the upper packaging adhesive film, and / or between the lower packaging adhesive film and the lower packaging component. The plurality of easy-to-pull adhesives are arranged at intervals in the length direction of the photovoltaic module.

[0010] As an optional solution, the sum of the surface areas of the individual stretch adhesives between the upper glass and the upper packaging film is 30%-60% of the surface area of ​​the upper glass, and the sum of the surface areas of the individual stretch adhesives between the lower packaging film and the lower packaging component is 30%-60% of the surface area of ​​the lower packaging component.

[0011] As an optional solution, the easy-to-pull adhesive is provided between the upper glass and the upper packaging film, and between the lower packaging member and the lower packaging film.

[0012] As an optional solution, the easy-to-pull adhesive includes:

[0013] substrate layer;

[0014] Adhesive layers are respectively disposed on opposite end surfaces of the substrate layer, and in the width direction of the photovoltaic module, the lengths of the adhesive layers are respectively equal to the widths of the upper glass and the lower packaging component.

[0015] As an optional solution, in the width direction of the upper glass, at least one end portion of the substrate layer protrudes from the adhesive layer.

[0016] As an optional solution, the bonding force between the adhesive layer and the upper glass and the upper packaging film, and the bonding force between the adhesive layer and the lower packaging member and the lower packaging film, respectively, are both smaller than the bonding force between the substrate layer and the adhesive layer.

[0017] As an optional solution, the lower packaging component is a lower glass or a back panel.

[0018] A photovoltaic system comprises the photovoltaic module described above.

[0019] The beneficial effects of the utility model are:

[0020] The photovoltaic module of the utility model is provided with an easy-to-pull adhesive between the upper glass and the upper packaging adhesive film, and / or between the lower packaging adhesive film and the lower packaging member; when the upper glass and / or the lower packaging member are recovered, the easy-to-pull adhesive is directly pulled out, and since the upper glass and the upper packaging adhesive film, and / or the lower packaging adhesive film and the lower packaging member can be partially separated after the easy-to-pull adhesive is pulled out, the adhesive force between the adhesive film and the upper glass and the lower packaging member is small, thereby shortening the subsequent immersion time of the photovoltaic module; when the photovoltaic module after the easy-to-pull adhesive is pulled out is immersed in a disassembly immersion liquid, the disassembly immersion liquid can flow into the photovoltaic module. At the gap position after the easy-pull adhesive is pulled out; that is, the disassembly soaking liquid can flow into between the upper glass and the upper packaging adhesive film, and / or between the lower packaging adhesive film and the lower packaging component, so as to increase the contact area between the disassembly soaking liquid and the upper packaging adhesive film and the lower packaging adhesive film, respectively, so as to shorten the soaking time of the photovoltaic module; that is, through the joint action of the easy-pull adhesive and the disassembly soaking liquid, it is possible to release the adhesion between the upper glass and the upper packaging adhesive film, and / or between the lower packaging adhesive film and the lower packaging component in a shorter time, so that the upper glass and the lower packaging component can be recovered in a shorter time.

[0021] Furthermore, by providing a plurality of easy-to-pull adhesives, a plurality of gap positions can be left after the easy-to-pull adhesives are pulled out, so that the disassembly immersion liquid can flow into the plurality of gap positions after the easy-to-pull adhesives are pulled out, further increasing the contact area between the disassembly immersion liquid and the upper packaging adhesive film and the lower packaging adhesive film, respectively, thereby better shortening the immersion time of the photovoltaic module; at the same time, since a plurality of easy-to-pull adhesives are provided, most of the structures between the upper glass and the upper packaging adhesive film, and / or between the lower packaging adhesive film and the lower packaging component can be separated after the easy-to-pull adhesives are pulled out, so that the adhesion between the adhesive film and the upper glass and the lower packaging component, respectively, is smaller, thereby shortening the subsequent immersion time of the photovoltaic module, and thus enabling more efficient recovery of the upper glass and the lower packaging component.

[0022] The photovoltaic system of the utility model, because it includes the above-mentioned photovoltaic components, can realize the recycling of the upper glass and the lower packaging components in the photovoltaic components in a relatively short time, and the recycling operation is simple, convenient and efficient. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the structure of a photovoltaic module in the prior art;

[0024] Figure 2 It is a schematic cross-sectional view of a photovoltaic module provided by the utility model (with easy-to-pull adhesives respectively disposed on the upper glass and the lower packaging member) in a direction perpendicular to the length of the easy-to-pull adhesive;

[0025] Figure 3 yes Figure 2 Schematic diagram of the structure after the easy-to-pull adhesive is pulled out;

[0026] Figure 4 It is a schematic cross-sectional view of a photovoltaic module provided by the utility model (with easy-to-pull adhesives respectively disposed on the upper glass and the lower packaging member) in a direction parallel to the length of the easy-to-pull adhesive;

[0027] Figure 5 yes Figure 4 Schematic diagram of the structure after the easy-to-pull adhesive is pulled out;

[0028] Figure 6 It is a structural schematic diagram of the easy-to-pull adhesive provided by the utility model;

[0029] Figure 7 It is a schematic cross-sectional view of the photovoltaic module (only the pull-out adhesive is provided at the lower packaging member) provided by the utility model in a direction perpendicular to the length of the pull-out adhesive;

[0030] Figure 8 It is a schematic cross-sectional view of the photovoltaic module provided by the utility model (only the pull-out adhesive is provided at the lower packaging member) in the direction parallel to the length of the pull-out adhesive;

[0031] Fig. 9 It is a schematic diagram of the process of the photovoltaic module disassembly method provided by the utility model.

[0032] Description of reference numerals:

[0033] 1'-upper glass; 2'-upper packaging film; 3'-cell; 4'-lower packaging film; 5'-lower packaging piece;

[0034] 1-upper glass; 2-upper packaging film; 3-cell; 4-lower packaging film; 5-lower packaging component;

[0035] 6-easy-to-pull adhesive; 61-base material layer; 611-protruding portion; 62-adhesive layer;

[0036] 7- Gap position. DETAILED DESCRIPTION

[0037] All features disclosed in this specification, or steps in all methods or processes disclosed, except mutually exclusive features and / or steps, can be combined in any manner.

[0038] Any feature disclosed in this specification, unless otherwise stated, may be replaced by other equivalent or alternative features having similar purposes. That is, unless otherwise stated, each feature is only an example of a series of equivalent or similar features. Throughout the specification, the same reference numerals indicate the same elements.

[0039] In order to make the technical problems solved by the present invention, the technical solutions adopted and the technical effects achieved more clearly, the technical solutions of the present invention are further explained below with reference to the accompanying drawings and through specific implementation methods.

[0040] Embodiment 1

[0041] In this embodiment, a photovoltaic module and a photovoltaic system including the photovoltaic module are proposed. The photovoltaic module can be disassembled and recycled in a short time, and the disassembly and recycling method is simple and efficient. The working principle of the photovoltaic module is the same as the photovoltaic working principle in the prior art, and the working principle of the photovoltaic module is not described in detail here.

[0042] Specifically, Figures 2 to 5 As shown, the photovoltaic module includes an upper glass 1, an upper packaging film 2, a battery cell 3, a lower packaging film 4 and a lower packaging component 5, which are arranged in sequence from top to bottom. The upper packaging film 2 and the lower packaging film 4 can seal the battery cell 3, and can tightly bond the upper glass 1 to the battery cell 3 through the upper packaging film 2, and can tightly bond the lower packaging component 5 to the battery cell 3 through the lower packaging film 4; and the photovoltaic module also includes an easy-to-pull adhesive 6, and the easy-to-pull adhesive 6 is arranged between the upper glass 1 and the upper packaging film 2, and / or between the lower packaging film 4 and the lower packaging component 5. When the photovoltaic module after pulling out the easy-to-pull adhesive 6 is immersed in a disassembly soaking liquid, the disassembly soaking liquid can flow into the gap position 7 after the easy-to-pull adhesive 6 is pulled out.

[0043] Compared with the prior art, the photovoltaic module in this embodiment has an additional easy-to-pull adhesive 6, and the easy-to-pull adhesive 6 is made to cooperate with the disassembly soaking liquid; by arranging the easy-to-pull adhesive 6 between the upper glass 1 and the upper packaging adhesive film 2, and / or between the lower packaging adhesive film 4 and the lower packaging component 5; when the upper glass 1 and / or the lower packaging component 5 are recovered, the easy-to-pull adhesive 6 is directly pulled out, because after the easy-to-pull adhesive 6 is pulled out, the upper glass 1 and the upper packaging adhesive film 2, and / or the lower packaging adhesive film 4 and the lower packaging component 5 can be partially separated, so that the adhesion between the adhesive film and the upper glass 1 and the lower packaging component 5 is relatively small, thereby shortening the subsequent soaking time of the photovoltaic module; and then soaking the photovoltaic module after the easy-to-pull adhesive 6 is pulled out When in the disassembly soaking liquid, the disassembly soaking liquid can flow into the gap position 7 after the easy-pull adhesive 6 is pulled out; that is, the disassembly soaking liquid can flow between the upper glass 1 and the upper packaging film 2, and / or between the lower packaging film 4 and the lower packaging component 5, so as to increase the contact area between the disassembly soaking liquid and the upper packaging film 2 and the lower packaging film 4, respectively, so as to shorten the soaking time of the photovoltaic module; that is, through the joint action of the easy-pull adhesive 6 and the disassembly soaking liquid, it is possible to achieve the release of the adhesion between the upper glass 1 and the upper packaging film 2, and / or between the lower packaging film 4 and the lower packaging component 5 in a shorter time, so that the upper glass 1 and the lower packaging component 5 can be recovered in a shorter time.

[0044] Among them, the above-mentioned disassembly immersion liquid can be specifically the immersion solution for photovoltaic modules in the prior art. The specific composition of the disassembly immersion liquid is not limited here, as long as the upper glass 1 and the upper packaging film 2, as well as the lower packaging film 4 and the lower packaging component 5 can be completely separated by immersion in the disassembly immersion liquid.

[0045] It is worth mentioning that the utility model in this embodiment focuses on the smooth recycling of the upper glass 1 and the lower packaging component 5. The mutual connection method and the working process of the upper glass 1, the upper packaging film 2, the battery cell 3, the lower packaging film 4 and the lower packaging component 5 in the photovoltaic module are not described in detail here, and reference can be made to the photovoltaic modules in the prior art.

[0046] It is worth noting that the above-mentioned soaking of photovoltaic modules specifically refers to the photovoltaic modules after the easy-to-pull adhesive 6 is pulled out, that is, the easy-to-pull adhesive 6 will not be immersed in the disassembly soaking liquid; the easy-to-pull adhesive 6 specifically refers to a polymer material with ductility and elasticity, which can be used to bond paper, plastic, metal, glass and other materials. The easy-to-pull adhesive 6 usually does not contain solvents, is environmentally friendly and non-toxic, and has almost no residue after drying, and will not damage the bonded glass, adhesive film and other materials; the easy-to-pull adhesive 6 is ready to use when used, and can be easily pulled off without leaving any glue stains when removed, making it easy to clean.

[0047] Specifically, since the upper glass 1 located on the front of the photovoltaic module needs to receive light, the front of the photovoltaic module needs to be set as a transparent upper glass 1; and the lower packaging component 5 located on the back of the photovoltaic module can be set according to photovoltaic requirements, that is, the lower packaging component 5 can be set as a lower glass or a back plate, which is not specifically limited here. In this embodiment, the lower packaging component 5 is set as a lower glass.

[0048] Furthermore, if Figures 2 to 6 As shown, the adhesive 6 is in a long strip structure, and the length direction of the adhesive 6 is parallel to the width direction of the photovoltaic module, so that the adhesive 6 in the long strip structure can be directly pulled out, making it easier to pull out the adhesive 6. Figure 4 As shown by the arrow A in FIG. 1 , correspondingly, the length direction of the easy-to-pull adhesive 6 is as follows Figure 4 As shown by arrow A in FIG.

[0049] Specifically, Figures 2 to 5 As shown, a plurality of easy-to-pull adhesives 6 are arranged between the upper glass 1 and the upper packaging film 2, and / or between the lower packaging film 4 and the lower packaging member 5, and the plurality of easy-to-pull adhesives 6 are arranged at intervals in the length direction of the photovoltaic module. Figure 2 As shown by arrow B in FIG.

[0050] It is worth noting that the spacing setting of the multiple easy-to-pull adhesives 6 mentioned above specifically refers to that the multiple easy-to-pull adhesives 6 between the upper glass 1 and the upper packaging film 2 are spaced apart in the length direction of the photovoltaic module, and the multiple easy-to-pull adhesives 6 between the lower packaging film 4 and the lower packaging component 5 are spaced apart in the length direction of the photovoltaic module.

[0051] By providing a plurality of easy-to-pull adhesives 6, a plurality of gap positions 7 can be left after the easy-to-pull adhesives 6 are pulled out, so that the disassembly soaking liquid can flow into the plurality of gap positions 7 after the easy-to-pull adhesives 6 are pulled out, further increasing the contact area between the disassembly soaking liquid and the upper packaging adhesive film 2 and the lower packaging adhesive film 4, respectively, thereby better shortening the soaking time of the photovoltaic module; at the same time, since a plurality of easy-to-pull adhesives 6 are provided, most of the structures between the upper glass 1 and the upper packaging adhesive film 2, and / or between the lower packaging adhesive film 4 and the lower packaging component 5 can be separated after the easy-to-pull adhesives 6 are pulled out, so that the adhesion between the adhesive film and the upper glass 1 and the lower packaging component 5, respectively, is smaller, thereby shortening the subsequent soaking time of the photovoltaic module, and thus the upper glass 1 and the lower packaging component 5 can be recovered more efficiently.

[0052] In this embodiment, Figures 2 to 5 As shown, an easy-to-pull adhesive 6 is provided between the upper glass 1 and the upper packaging film 2, and between the lower packaging component 5 and the lower packaging film 4, and a plurality of easy-to-pull adhesives 6 are provided. Among them, four easy-to-pull adhesives 6 are provided between the upper glass 1 and the upper packaging film 2, and four easy-to-pull adhesives 6 are provided between the lower packaging component 5 and the lower packaging film 4. The number of easy-to-pull adhesives 6 is not limited here.

[0053] In other embodiments, the pull-out adhesive 6 may be provided only between the upper glass 1 and the upper packaging film 2, or Figure 7 and Figure 8 As shown, only the pull-out adhesive 6 is arranged between the lower packaging component 5 and the lower packaging adhesive film 4. There is no limitation on the specific arrangement position of the pull-out adhesive 6, which needs to be determined according to specific recycling requirements.

[0054] Furthermore, the sum of the surface areas of the individual adhesives 6 between the upper glass 1 and the upper packaging film 2 is 30%-60% of the surface area of ​​the upper glass 1; on the one hand, it can avoid the cumbersome operation of pulling out the adhesives 6 due to too many adhesives 6, making the pulling out operation of the adhesives 6 simpler and faster; on the other hand, it can avoid too few gap positions 7 due to too few adhesives 6, so that an appropriate number of gap positions 7 can be formed, so that the contact area between the disassembly soaking liquid and the upper packaging film 2 is sufficient, which is conducive to better shortening the soaking time. In this embodiment, the sum of the surface areas of the individual adhesives 6 between the upper glass 1 and the upper packaging film 2 is 50% of the surface area of ​​the upper glass 1.

[0055] Specifically, the sum of the surface areas of the individual stretch adhesives 6 between the lower packaging film 4 and the lower packaging member 5 is 30%-60% of the surface area of ​​the lower packaging member 5; while the pulling operation of the stretch adhesive 6 is relatively simple and fast, an appropriate number of gap positions 7 can be formed, so that the contact area between the disassembly soaking liquid and the lower packaging film 4 is sufficient, which is conducive to better shortening the soaking time. In this embodiment, the sum of the surface areas of the individual stretch adhesives 6 between the lower packaging member 5 and the lower packaging film 4 is 50% of the surface area of ​​the lower packaging member 5.

[0056] It is worth mentioning that, since the upper packaging film 2 and each easy-pull adhesive 6 are all bonded to the upper glass 1, sufficient bonding strength between the upper glass 1 and the upper packaging film 2 can be guaranteed; and, the number of easy-pull adhesives 6 will not affect the bonding effect on the upper glass 1; that is, when too few easy-pull adhesives 6 are provided, the upper packaging film 2 will be bonded to the upper glass 1 more correspondingly; when too many easy-pull adhesives 6 are provided, the upper packaging film 2 will be bonded to the upper glass 1 less correspondingly, thereby being able to ensure the bonding strength between the upper glass 1 and the upper packaging film 2 through the upper packaging film 2 and the easy-pull adhesives 6; similarly, the number of easy-pull adhesives 6 will not affect the bonding effect between the lower packaging film 4 and the lower packaging component 5.

[0057] Furthermore, if Figures 2 to 6 As shown, the easy-to-pull adhesive 6 includes a substrate layer 61 and an adhesive layer 62; wherein, the adhesive layer 62 is respectively arranged on the opposite end surfaces of the substrate layer 61, that is, the adhesive layer 62 is arranged on the front and back surfaces of the substrate layer 61, and the adhesive layer 62 can be used to bond to the upper glass 1, the upper packaging film 2, the lower packaging film 4 or the lower packaging component 5; and in the width direction of the photovoltaic module, the length of the adhesive layer 62 is equal to the width of the upper glass 1 and the width of the lower packaging component 5, that is, the adhesive layer 62 runs through the entire width of the upper glass 1 to ensure that the adhesive layer 62 and the upper glass 1 have a better bonding effect; correspondingly, the adhesive layer 62 runs through the entire width of the lower packaging component 5 to ensure that the adhesive layer 62 and the lower packaging component 5 have a better bonding effect.

[0058] Specifically, Figure 4 and Figure 6 As shown, in the width direction of the photovoltaic module, at least one end of the substrate layer 61 protrudes from the adhesive layer 62, that is, the length of the substrate layer 61 is longer than the length of the adhesive layer 62, so that a protruding portion 611 can be formed at the end of the substrate layer 61, so that the entire easy-to-pull adhesive 6 can be pulled out by directly pulling the protruding portion 611 at the end of the substrate layer 61, so that the pulling operation of the easy-to-pull adhesive 6 is relatively simple and convenient, saving time and effort. In this embodiment, one end of the substrate layer 61 protrudes from the adhesive layer 62. In other embodiments, both ends of the substrate layer 61 can also be arranged to protrude from the adhesive layer 62, so that the pulling operation of the substrate layer 61 can be more convenient and flexible.

[0059] Specifically, the bonding forces between the adhesive layer 62 and the upper glass 1 and the upper packaging film 2, as well as the bonding forces between the adhesive layer 62 and the lower packaging component 5 and the lower packaging film 4, are all smaller than the bonding forces between the substrate layer 61 and the adhesive layer 62; so that in the process of pulling up the easy-to-pull adhesive 6, it is ensured that the adhesive layer 62 can be detached from the upper glass 1, the upper packaging film 2, the lower packaging film 4 and the lower packaging component 5, respectively, without causing the adhesive layer 62 to be detached from the substrate layer 61, thereby ensuring that the easy-to-pull adhesive 6 can be pulled out smoothly.

[0060] Embodiment 2

[0061] This embodiment proposes a photovoltaic module disassembly method, based on the photovoltaic module in the first embodiment, such as Fig. 9 As shown, the following steps are included:

[0062] S1: Pull out the easy-pull adhesive 6 between the upper glass 1 and the upper packaging film 2, and / or between the lower packaging film 4 and the lower packaging member 5, so as to partially separate the upper glass 1 and the upper packaging film 2, and / or between the lower packaging film 4 and the lower packaging member 5, and leave a gap 7 after the easy-pull adhesive 6 is pulled out;

[0063] S2: The photovoltaic module with the easy-to-pull adhesive 6 pulled out is placed in a disassembly soaking liquid for soaking, so that the disassembly soaking liquid can flow into the gap position 7. After soaking for a preset time, the upper glass 1 and the upper packaging film 2, and / or the lower packaging component 5 and the lower packaging film 4 are completely separated.

[0064] The photovoltaic module disassembly method in this embodiment, by using the easy-to-pull adhesive 6 and the disassembly soaking liquid in combination, can make the recycling of the upper glass 1 and the lower packaging component 5 in the photovoltaic module simpler and more convenient, and can shorten the recycling time.

[0065] The specific disassembly process of the photovoltaic module disassembly method in this embodiment is as follows:

[0066] First, the four easy-pull adhesives 6 between the upper glass 1 and the upper packaging film 2, and the four easy-pull adhesives 6 between the lower packaging film 4 and the lower packaging component 5 are pulled out to partially separate the upper glass 1 and the upper packaging film 2, and the lower packaging film 4 and the lower packaging component 5, and leave a gap position 7 after the eight easy-pull adhesives 6 are pulled out.

[0067] Then, the photovoltaic module with the easy-to-pull adhesive 6 pulled out is placed in the disassembly soaking liquid for soaking, so that the disassembly soaking liquid can flow into the eight gap positions 7, thereby increasing the contact area between the disassembly soaking liquid and the upper packaging film 2 and the lower packaging film 4, respectively, to shorten the soaking time.

[0068] Finally, after soaking for a preset time, under the action of the disassembly soaking liquid, the upper glass 1 and the upper packaging film 2 are completely separated, and the lower packaging component 5 and the lower packaging film 4 are completely separated, and the upper glass 1 and the lower packaging component 5 can be recycled.

[0069] It is worth noting that the above preset time is much shorter than the soaking time of the photovoltaic module when the easy-to-pull adhesive 6 is not provided in the prior art, that is, the upper glass 1 and the lower packaging member 5 can be recovered in a shorter time. Here, the specific time of the preset time is not limited and needs to be determined according to the actual working conditions.

[0070] The photovoltaic module disassembly method in this embodiment first pulls out each easy-to-pull adhesive 6 to reduce the adhesion between the upper glass 1 and the upper packaging film 2, and between the lower packaging component 5 and the lower packaging film 4, and to leave a gap position 7; then the disassembly soaking liquid is allowed to flow into the gap position 7 after the easy-to-pull adhesive 6 is pulled out of the photovoltaic module, so as to increase the contact area between the disassembly soaking liquid and the upper packaging film 2 and the lower packaging film 4, respectively, thereby shortening the soaking time, making the recovery of the upper glass 1 and the lower packaging component 5 simpler and more efficient.

[0071] The above contents are only preferred embodiments of the present invention. For ordinary technicians in this field, according to the concept of the present invention, there will be changes in the specific implementation methods and application scopes. The contents of this specification should not be understood as limiting the present invention.

Claims

1. A photovoltaic module, comprising an upper glass (1), an upper packaging film (2), a battery cell (3), a lower packaging film (4) and a lower packaging member (5) arranged in sequence from top to bottom, characterized in that: The photovoltaic module further comprises: Easy-to-pull adhesive (6), the easy-to-pull adhesive (6) being arranged between the upper glass (1) and the upper packaging adhesive film (2), and / or between the lower packaging adhesive film (4) and the lower packaging member (5); The easy-to-pull adhesive (6) is in the form of a long strip, and a plurality of the easy-to-pull adhesives (6) are arranged between the upper glass (1) and the upper packaging adhesive film (2), and / or between the lower packaging adhesive film (4) and the lower packaging member (5), and the plurality of the easy-to-pull adhesives (6) are arranged at intervals in the length direction of the photovoltaic module.

2. The photovoltaic module according to claim 1, characterized in that: The sum of the surface areas of the individual stretch adhesives (6) between the upper glass (1) and the upper packaging film (2) is 30%-60% of the surface area of ​​the upper glass (1), and the sum of the surface areas of the individual stretch adhesives (6) between the lower packaging film (4) and the lower packaging component (5) is 30%-60% of the surface area of ​​the lower packaging component (5).

3. The photovoltaic module according to claim 1, characterized in that: The easy-to-pull adhesive (6) is provided between the upper glass (1) and the upper packaging film (2), and between the lower packaging component (5) and the lower packaging film (4).

4. The photovoltaic module according to any one of claims 1 to 3, characterized in that: The easy-to-pull adhesive (6) comprises: A substrate layer (61); An adhesive layer (62) is provided on opposite end surfaces of the substrate layer (61), and the length of the adhesive layer (62) in the width direction of the photovoltaic module is respectively equal to the width of the upper glass (1) and the width of the lower packaging component (5).

5. The photovoltaic module according to claim 4, characterized in that: In the width direction of the upper glass (1), at least one end portion of the substrate layer (61) protrudes from the adhesive layer (62).

6. The photovoltaic module according to claim 5, characterized in that: The bonding force between the adhesive layer (62) and the upper glass (1) and the upper packaging film (2), respectively, and the bonding force between the adhesive layer (62) and the lower packaging component (5) and the lower packaging film (4), respectively, are both smaller than the bonding force between the substrate layer (61) and the adhesive layer (62).

7. The photovoltaic module according to any one of claims 1 to 3, characterized in that: The lower packaging component (5) is a lower glass or a back plate.

8. A photovoltaic system, characterized in that: The invention comprises a photovoltaic module as claimed in any one of claims 1 to 7.