Device for pre-lithiation of silicon-based negative electrode

By using a closed system of reaction chamber, mixing chamber and heating chamber in the prelithiation device of silicon-based negative electrode material, combined with CVD method and stirring heating treatment, the problem of poor prelithiation quality of silicon-based negative electrode material in traditional processes is solved, and the problem of poor prelithiation quality of silicon-based negative electrode material in traditional processes is realized. High-quality carbon coating and secondary treatment have been used to significantly improve the performance of the finished product.

CN222111772UActive Publication Date: 2024-12-06SICHUAN FUFU NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420065950.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-11
Publication Date
2024-12-06
Estimated Expiration
2034-01-11

AI Technical Summary

Technical Problem

The prelithiation process of traditional silicon-based negative electrode materials is of poor quality and cannot effectively improve the quality of the finished product.

Method used

A closed system including a reaction chamber, a mixing chamber and a heating chamber is designed. Carbon coating and secondary carbon coating are carried out through the CVD method, combined with stirring and heating treatment, ensuring uniform reaction and gas distribution of the materials at different levels. Improve the sedimentary quality.

Benefits of technology

The finished product quality of silicon-based negative electrode materials is significantly improved, and the consistency of material density and gas utilization efficiency are ensured through carbon coating and heating treatment, and the prelithiation effect is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222111772U_ABST
    Figure CN222111772U_ABST
Patent Text Reader

Abstract

The utility model discloses a device for pre-lithiation of a silicon-based negative electrode, which comprises a reaction chamber, a mixing chamber and a heating chamber, the reaction chamber, the mixing chamber and the heating chamber form a closed system, a reaction zone is arranged at the upper part in the reaction chamber, an upper gas mixing zone is arranged above the reaction zone, and a lower gas mixing zone is arranged below the reaction chamber; a material mixing funnel, a stirring paddle and a material receiver are arranged in the mixing chamber; the first conveying device is used for conveying materials into the mixing chamber from the reaction chamber, the second conveying device is used for conveying materials into the reaction chamber from the mixing chamber, the two ends of the first conveying device and the two ends of the second conveying device are located in the reaction chamber and the mixing chamber, and the heating chamber is located in the middle section of the second conveying device. The carbon coating device can be used for sequentially carrying out carbon coating treatment, mixed high-temperature treatment and secondary carbon coating treatment on materials, and the finished product effect is good.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of silicon-based negative electrode material preparation, in particular to a device for pre-lithiation of silicon-based negative electrodes. Background Art

[0002] Lithium-ion batteries are the mainstream of energy storage batteries today. The positive and negative electrodes of lithium-ion batteries are important components of their structure. Silicon-based negative electrode materials have become the best choice for the new generation of negative electrode materials due to their high capacity and low cost.

[0003] The basic principle of pre-lithiation of silicon-based negative electrode materials is to embed lithium ions into the silicon-based negative electrode materials in advance to form a stable lithium-silicon alloy phase.

[0004] The traditional pre-lithiation process for silicon-based negative electrode materials is to directly mix lithium powder into the silicon-based negative electrode materials, resulting in poor quality of the finished product. Utility Model Content

[0005] The utility model aims to provide a device for pre-lithiation of silicon-based negative electrodes, which can sequentially perform carbon coating treatment, mixed high-temperature treatment, and secondary carbon coating treatment on materials, and the finished product has a good effect.

[0006] In order to solve the above technical problems, the utility model adopts the following solutions:

[0007] A device for pre-lithiation of a silicon-based negative electrode comprises a reaction chamber, a mixing chamber and a heating chamber, wherein the reaction chamber, the mixing chamber and the heating chamber form a closed system.

[0008] A reaction zone is provided above the reaction chamber, an upper gas mixing zone is provided above the reaction zone, and a lower gas mixing zone is provided below the reaction chamber;

[0009] The mixing chamber is provided with a mixing funnel, a stirring paddle and a material receiver;

[0010] It also includes a first transport device for transporting materials from the reaction chamber to the mixing chamber and a second transport device for transporting materials from the mixing chamber to the reaction chamber. Both ends of the first transport device and the second transport device are located in the reaction chamber and the mixing chamber, and the heating chamber is located in the middle section of the second transport device. Its function is that, through the arrangement of the reaction chamber, the mixing chamber, the heating chamber, the first transport device and the second transport device, the material can be placed on the first transport device in the reaction chamber first, and the reaction gas is introduced into the reaction chamber, and carbon-coated silicon is prepared by CVD method. After the carbon-coated silicon is moved to the mixing chamber through the first transport device, the carbon-coated silicon is transported to the mixing funnel, and the carbon-coated silicon is stirred and mixed with the lithium salt by the stirring paddle and then poured into the receiving device on the second transport device. The second transport device first transports the carbon-coated silicon mixed with the lithium salt to the heating chamber for heating, and then the material after the heating treatment is subjected to secondary carbon coating, and the finished product has good quality.

[0011] Furthermore, the upper gas mixing zone is connected with a first air inlet pipe, and the lower gas mixing zone is connected with a second air inlet pipe, and both the first air inlet pipe and the second air inlet pipe are provided with a stop valve. The function of the stop valve is that, through the setting of the first air inlet pipe, the reaction gas of the first CVD can be introduced into the upper gas mixing zone for mixing; through the setting of the second air inlet pipe, the reaction gas of the second CVD can be introduced into the lower gas mixing zone for mixing, and through the setting of the stop valve, the other air inlet pipe can be controlled to be closed during the ventilation process.

[0012] Furthermore, the reaction chamber is provided with an upper splitter plate and a lower splitter plate from top to bottom, the upper gas mixing zone and the reaction zone are separated by the upper splitter plate, the lower gas mixing zone and the reaction zone are separated by the lower splitter plate, and both the upper splitter plate and the lower splitter plate are provided with vents. The function of the vents is to allow the gas in the upper gas mixing zone and the lower gas mixing zone to enter the reaction zone through the vents through the arrangement of the upper splitter plate, the lower splitter plate and the vents.

[0013] Furthermore, the vent holes are evenly distributed in at least two layers of concentric rings on the upper and lower manifold plates, and the inner diameters of the vent holes in different layers gradually increase from the inside to the outside. The purpose is to make the material density of the inner and outer layers tend to be consistent through the design of the distribution and size of the vent holes, avoiding a large density gradient between different layers.

[0014] Furthermore, the intersection of the central axes of the vent holes on the upper and lower manifold plates is located above the upper manifold plate, and the intersection of the central axes of the vent holes on the lower manifold plate is located below the lower manifold plate. Its function is that, through the design of the inclination direction of the upper manifold plate and the inclination direction of the lower manifold plate, the gas in the upper gas mixing zone and the lower gas mixing zone can enter the reaction zone with a diffusion trend, so as to be able to fully react with the material in the reaction zone.

[0015] Furthermore, the inclination angles of the vents distributed on the upper and lower manifold plates with respect to the vertical direction gradually increase from the inner layer to the outer layer. The effect is that the gas entering the deposition chamber can be evenly distributed through the change of the inclination angles of the vents in different layers, thereby improving the utilization efficiency of the source gas and significantly improving the deposition quality.

[0016] Furthermore, support rings for supporting the upper diverter plate or the lower diverter plate are provided on the bottom surfaces of the upper diverter plate and the lower diverter plate.

[0017] Furthermore, an air pump is connected to the side wall of the reaction chamber, and its function is to extract the gas from the last reaction in the furnace body through the setting of the air pump.

[0018] Furthermore, a sealing door is provided on the side wall of the reaction chamber, and its function is to place materials into the reaction chamber and take out finished products from the reaction chamber through the setting of the sealing door.

[0019] Furthermore, a gate valve is provided on the mixing funnel, and its function is to control the opening and closing of the mixing funnel through the setting of the gate valve.

[0020] The utility model has the beneficial effects:

[0021] Through the arrangement of the reaction chamber, the mixing chamber, the heating chamber, the first transport device and the second transport device, the material can be first placed on the first transport device in the reaction chamber, the reaction gas is introduced into the reaction chamber, carbon-coated silicon is prepared by the CVD method, the carbon-coated silicon is moved into the mixing chamber through the first transport device, the carbon-coated silicon is transported to the mixing funnel, stirred and mixed with the lithium salt by a stirring paddle, and then poured into the receiver on the second transport device, the second transport device transports the carbon-coated silicon mixed with the lithium salt to the heating chamber for heating, and then the heated material is subjected to secondary carbon coating, so that the finished product has good quality. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 This is a schematic diagram of the structure of Example 1.

[0023] Figure numerals: 1. reaction chamber; 2. mixing chamber; 3. heating chamber; 4. reaction zone; 5. upper gas mixing zone; 6. lower gas mixing zone; 7. mixing funnel; 8. stirring paddle; 9. material receiver; 10. first transport device; 11. second transport device; 12. first air inlet pipe; 13. second air inlet pipe; 14. stop valve; 15. upper diverter plate; 16. lower diverter plate; 17. vent; 18. support ring; 19. air pump; 20. sealing door; 21. gate valve. DETAILED DESCRIPTION

[0024] The present invention will be further described in detail below in conjunction with the embodiments and drawings, but the implementation manner of the present invention is not limited thereto.

[0025] In the description of the present utility model, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "longitudinal", "lateral", "horizontal", "inside", "outside", "front", "back", "top", "bottom", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings, or are the directions or positional relationships in which the utility model product is usually placed when in use. They are only for the convenience of describing the present utility model and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present utility model.

[0026] In the description of the present invention, it is also necessary to explain that, unless otherwise clearly specified and limited, the terms "set", "open", "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0027] Example 1

[0028] A device for pre-lithiation of silicon-based negative electrodes, such as Figure 1 As shown, it includes a reaction chamber 1, a mixing chamber 2 and a heating chamber 3, wherein the reaction chamber 1, the mixing chamber 2 and the heating chamber 3 form a closed system.

[0029] A reaction zone 4 is provided at the top of the reaction chamber 1, an upper gas mixing zone 5 is provided above the reaction zone 4, and a lower gas mixing zone 6 is provided at the bottom of the reaction chamber 1;

[0030] The mixing chamber 2 is provided with a mixing funnel 7, a stirring paddle 8 and a material receiver 9;

[0031] It also includes a first transport device 10 for transporting materials from the reaction chamber 1 to the mixing chamber 2 and a second transport device 11 for transporting materials from the mixing chamber 2 to the reaction chamber 1. Both ends of the first transport device 10 and the second transport device 11 are located in the reaction chamber 1 and the mixing chamber 2, and the heating chamber 3 is located in the middle section of the second transport device 11. Its function is that, through the arrangement of the reaction chamber 1, the mixing chamber 2, the heating chamber 3, the first transport device 10 and the second transport device 11, the material can be first placed on the first transport device 10 in the reaction chamber 1, the reaction gas is introduced into the reaction chamber 1, and the carbon-coated silicon is prepared by the CVD method. The carbon-coated silicon is moved to the mixing chamber 2 through the first transport device 10, and the carbon-coated silicon is transported to the mixing funnel 7. After being stirred and mixed with the lithium salt by the stirring paddle 8, the carbon-coated silicon is poured into the receiver 9 on the second transport device 11. The second transport device 11 first transports the carbon-coated silicon mixed with the lithium salt to the heating chamber 3 for heating, and then the material after the heat treatment is subjected to secondary carbon coating, so that the finished product has good quality.

[0032] Specifically, Figure 1As shown, the upper gas mixing zone 5 is connected to a first gas inlet pipe 12, and the lower gas mixing zone 6 is connected to a second gas inlet pipe 13. Both the first gas inlet pipe 12 and the second gas inlet pipe 13 are provided with a stop valve 14. Its function is that, through the setting of the first gas inlet pipe 12, the reaction gas of the first CVD can be introduced into the upper gas mixing zone 5 for mixing; through the setting of the second gas inlet pipe 13, the reaction gas of the second CVD can be introduced into the lower gas mixing zone 6 for mixing, and through the setting of the stop valve 14, the first gas inlet pipe 12 or the second gas inlet pipe 13 can be controlled to be closed during the ventilation process.

[0033] Specifically, Figure 1 As shown, the reaction chamber 1 is provided with an upper manifold plate 15 and a lower manifold plate 16 from top to bottom, the upper gas mixing zone 5 and the reaction zone 4 are separated by the upper manifold plate 15, and the lower gas mixing zone 6 and the reaction zone 4 are separated by the lower manifold plate 16, and the upper manifold plate 15 and the lower manifold plate 16 are both provided with vents 17. The function is that, through the arrangement of the upper manifold plate 15, the lower manifold plate 16, and the vents 17, the gas in the upper gas mixing zone 5 and the lower gas mixing zone 6 can enter the reaction zone 4 through the vents 17.

[0034] Specifically, Figure 1 As shown, the vent holes 17 are evenly distributed in at least two layers of concentric rings on the upper manifold plate 15 and the lower manifold plate 16, and the inner diameters of the vent holes 17 in different layers gradually increase from the inside to the outside. The purpose is to make the material density of the inner and outer layers tend to be consistent through the design of the distribution and size of the vent holes 17, so as to avoid a large density gradient in different layers.

[0035] Specifically, Figure 1 As shown, the intersection of the central axes of the vent holes 17 on the upper manifold 15 and the lower manifold 16 is located above the upper manifold 15, and the intersection of the central axes of the vent holes 17 on the lower manifold 16 is located below the lower manifold 16. Its function is that, through the design of the inclination direction of the upper manifold 15 and the inclination direction of the lower manifold 16, the gas in the upper gas mixing zone 5 and the lower gas mixing zone 6 can enter the reaction zone 4 with a diffusion trend, so as to be able to react comprehensively with the materials in the reaction zone 4.

[0036] Specifically, Figure 1 As shown, the inclination angles of the vent holes 17 distributed on the upper manifold plate 15 and the lower manifold plate 16 with respect to the vertical direction gradually increase from the inner layer to the outer layer. The function is that the gas entering the deposition chamber can be evenly distributed through the change of the inclination angles of the vent holes 17 in different layers, thereby improving the utilization efficiency of the source gas and significantly improving the deposition quality.

[0037] Specifically, Figure 1As shown, a support ring 18 for supporting the upper splitter plate 15 or the lower splitter plate 16 is provided on the bottom surface of the upper splitter plate 15 and the lower splitter plate 16 .

[0038] Specifically, Figure 1 As shown, an air pump 19 is connected to the side wall of the reaction chamber 1, and a three-way valve is provided between the air pump 19 and the reaction chamber 1. Its function is that the gas of the last reaction in the furnace body can be extracted through the setting of the air pump 19.

[0039] Specifically, Figure 1 As shown, a sealing door 20 is provided on the side wall of the reaction chamber 1. Its function is to place materials into the reaction chamber 1 and take out finished products from the reaction chamber 1 through the setting of the sealing door 20.

[0040] Specifically, Figure 1 As shown, a gate valve 21 is provided on the mixing funnel 7. Its function is to control the opening and closing of the mixing funnel 7 through the setting of the gate valve 21.

[0041] Specifically, Figure 1 As shown, the material receiver 9 is in the shape of a box with an open top, the first transport device 10 is arranged above the second transport device 11, the stirring paddle 8 is coaxially arranged with the mixing funnel 7, and a feeding channel for introducing lithium salt from top to bottom into the mixing funnel 7 is provided on the side wall of the mixing chamber 2, and a gate valve 21 is provided on the feeding channel.

[0042] The heating chamber 3 is provided with a heating device using the prior art, the stirring paddle 8 and the gate valve 21 are common prior art, the first transport device 10 and the second transport device 11 both use conveyor belts in the prior art, and the belt body of the conveyor belt uses a mesh belt with good air permeability, which will not be described in detail.

[0043] The working principle of this embodiment is described as follows: first, open the sealing door 20, place the material on the first transportation device 10 in the reaction chamber 1, close the sealing door 20, close the stop valve 14 on the second air inlet pipe 13, open the stop valve 14 on the first air inlet pipe 12, introduce the reaction gas into the gas mixing zone 5 through the first air inlet pipe 12, and then close the stop valve 14 on the first air inlet pipe 12. The reaction gas diffuses through the upper diverter plate 15 and enters the reaction zone 4 to react with the material. After the material is prepared into carbon-coated silicon by CVD, start the first transportation device 10, transport the carbon-coated silicon into the mixing chamber 2 and introduce it into the mixing funnel 7. The gate valve 21 in the mixing funnel 7 is in a closed state, and then the mixing funnel is fed into the mixing funnel through the feed channel. Lithium salt is poured into the funnel 7, and the stirring paddle 8 is started to stir the carbon-coated silicon and lithium salt. After the stirring is completed, the gate valve 21 at the bottom of the mixing funnel 7 is opened to allow the material to fall into the receiver 9 below the mixing funnel 7, and the second transportation device 11 is started to transport the receiver 9 to the heating chamber 3 to heat the material in the receiver 9. The stirring and heating is the pre-lithium treatment, and then the receiver 9 is transported to the reaction chamber 1, and the stop valve 14 on the second air inlet pipe 13 is opened. The reaction gas is introduced into the gas mixing zone 6 through the second air inlet pipe 13, and then the stop valve 14 on the second air inlet pipe 13 is closed. The gas of the second reaction diffuses through the lower diverter plate 16 and enters the reaction zone 4 to react with the material. The material is carbon-coated for the second time to prepare a finished product.

[0044] After the first carbon coating is completed, the reaction gas in the reaction chamber 1 is pumped out by the gas pump 19 .

[0045] The above is only a preferred embodiment of the utility model and does not limit the utility model in any form. According to the technical essence of the utility model, within the spirit and principles of the utility model, any simple modification, equivalent replacement and improvement made to the above embodiment still falls within the protection scope of the technical solution of the utility model.

Claims

1. A device for pre-lithiation of silicon-based negative electrodes, characterized in that: The invention comprises a reaction chamber (1), a mixing chamber (2) and a heating chamber (3), wherein the reaction chamber (1), the mixing chamber (2) and the heating chamber (3) form a closed system. A reaction zone (4) is provided at the top of the reaction chamber (1), an upper gas mixing zone (5) is provided above the reaction zone (4), and a lower gas mixing zone (6) is provided below the reaction chamber (1); A mixing funnel (7), a stirring paddle (8) and a material receiver (9) are provided in the mixing chamber (2); The heating chamber (3) further comprises a first transport device (10) for transporting materials from the reaction chamber (1) to the mixing chamber (2) and a second transport device (11) for transporting materials from the mixing chamber (2) to the reaction chamber (1). Both ends of the first transport device (10) and the second transport device (11) are located in the reaction chamber (1) and the mixing chamber (2), and the heating chamber (3) is located in the middle section of the second transport device (11).

2. The device for pre-lithiation of a silicon-based negative electrode according to claim 1, characterized in that: The upper gas mixing zone (5) is connected to a first air inlet pipe (12), and the lower gas mixing zone (6) is connected to a second air inlet pipe (13). Both the first air inlet pipe (12) and the second air inlet pipe (13) are provided with stop valves (14).

3. The device for pre-lithiation of a silicon-based negative electrode according to claim 2, characterized in that: An upper manifold plate (15) and a lower manifold plate (16) are arranged in sequence from top to bottom in the reaction chamber (1); an upper gas mixing zone (5) and a reaction zone (4) are separated by the upper manifold plate (15); a lower gas mixing zone (6) and a reaction zone (4) are separated by the lower manifold plate (16); and ventilation holes (17) are provided on both the upper manifold plate (15) and the lower manifold plate (16).

4. The device for pre-lithiation of a silicon-based negative electrode according to claim 3, characterized in that: The vent holes (17) are evenly distributed in at least two layers of concentric rings on the upper splitter plate (15) and the lower splitter plate (16), and the inner diameters of the vent holes (17) in different layers gradually increase from the inside to the outside.

5. The device for pre-lithiation of a silicon-based negative electrode according to claim 4, characterized in that: The intersection point of the central axes of the vent holes (17) on the upper splitter plate (15) and the lower splitter plate (16) is located above the upper splitter plate (15), and the intersection point of the central axes of the vent holes (17) on the lower splitter plate (16) is located below the lower splitter plate (16).

6. The device for pre-lithiation of a silicon-based negative electrode according to claim 3, characterized in that: The inclination angles of the vent holes (17) distributed on the upper splitter plate (15) and the lower splitter plate (16) with respect to the vertical direction gradually increase from the inner layer to the outer layer.

7. The device for pre-lithiation of a silicon-based negative electrode according to claim 6, characterized in that: A support ring (18) for supporting the upper splitter plate (15) or the lower splitter plate (16) is provided on the bottom surface of each of the upper splitter plate (15) and the lower splitter plate (16).

8. The device for pre-lithiation of a silicon-based negative electrode according to claim 1, characterized in that: The side wall of the reaction chamber (1) is connected to an air pump (19).

9. The device for pre-lithiation of silicon-based negative electrode according to claim 3, characterized in that: A sealing door (20) is provided on the side wall of the reaction chamber (1).

10. The device for pre-lithiation of silicon-based negative electrode according to claim 1, characterized in that: The mixing funnel (7) is provided with a gate valve (21).