Preparation system of spherical lithium adsorbent

Through the spherical lithium adsorbent preparation system, small droplets are formed by spraying raw materials to cure in the air, solving the problems of large particle size and poor morphology of the existing lithium adsorbent, and achieving efficient and wear-resistant spherical lithium adsorbent preparation. Improved adsorption rate and production adaptability.

CN222111860UActive Publication Date: 2024-12-06XUNYANG ADVSORBENT NEW MATERIALS TECHNOLOGY CO LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420167058.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-23
Publication Date
2024-12-06
Estimated Expiration
2034-01-23

AI Technical Summary

Technical Problem

The existing lithium adsorbent has poor form and large particle size, which leads to slow adsorption rate and easy wear, cumbersome process control, high cost, and mass fluctuations and environmental protection pressure.

Method used

The preparation system of spherical lithium adsorbent is adopted, including raw material mixing device, spraying device and curing device, and small droplets are formed by spraying raw materials and curing in air. The spherical lithium adsorbent is prepared by using the principle of jet molding, with a particle size of less than 1.2mm. Improves adsorption rate and wear resistance.

Benefits of technology

It realizes efficient preparation of spherical lithium adsorbents, with small particle size, fast adsorption and desorption rate, small column pressure, and wear resistance, suitable for large-scale production, reducing environmental protection pressure and production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222111860U_ABST
    Figure CN222111860U_ABST
Patent Text Reader

Abstract

The utility model provides a preparation system of a spherical lithium adsorbent. The preparation system comprises a raw material mixing device, a spraying device and a curing device, the spraying device comprises a liquid storage tank, a perforated plate, a vibration exciter and an air pump. According to the equipment disclosed by the utility model, the jet flow forming principle is adopted, the forming liquid of the lithium adsorbent is jetted into air through the air pump, the liquid is crushed into small liquid drops through the vibration exciter, the liquid drops are changed into spheres under the action of surface tension, and finally, the spheres are cured and formed in the curing column. The device is simple in structure, easy to control the technological process, high in preparation speed and suitable for large-scale production; the prepared spherical adsorbent is small in column pressure, resistant to abrasion and long in service life during application, the particle size of the prepared spherical adsorbent particles is smaller than 1.2 mm, the adsorption and desorption rate is high, and the use efficiency of the lithium adsorbent is greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of lithium adsorption, and in particular to a preparation system of a spherical lithium adsorbent. Background Art

[0002] Among the adsorbents, aluminum-based adsorbents (lithium aluminum hydrotalcite) and ion sieve type adsorbents (manganese lithium ion sieve adsorbents, titanium ion sieve adsorbents) have the most obvious advantages and are well developed, but they all have disadvantages such as being in powder form, poor fluidity and permeability, and high dissolution rate. Therefore, they are bonded together to prepare granular materials to meet the requirements of chemical adsorption column operation.

[0003] At present, the main preparation methods of lithium adsorbents are: 1. Dissolve the binding material with a solvent and mix it with the adsorbent powder, or melt the binding material and mix it with the adsorbent powder, and then prepare it into columnar or granular adsorbent particles through the high pressure of an extruder or a tablet press. The prepared lithium adsorbents are mostly irregular particles or columnar particles. When used in an adsorption column, the particle size is large, the adsorption rate is slow, the pressure drop is large, and it is easy to wear; 2. Use suspension polymerization or reverse suspension polymerization. These two methods are to add lithium adsorbent powder to an oil phase or water phase composed of polymer monomers, adjust the size of the suspension droplets by controlling stirring and dispersants, and initiate polymerization after rising to a certain temperature to obtain lithium adsorbent beads. The main problem of this method is that the process control is cumbersome, the cost is high, and the quality fluctuation is very likely to occur. In addition, the lithium adsorbent is easily transferred to another phase, causing losses, and the organic waste liquid generated will also increase environmental pressure. The lithium adsorbents obtained by the powder granulation method currently used are mostly 1-2mm columnar, broken or spherical particles. When used, due to the large particle size, the adsorption rate is slow. Utility Model Content

[0004] Therefore, the technical problem to be solved by the utility model is that the existing lithium adsorbents have poor morphology and large particle size, thereby providing a preparation system for spherical lithium adsorbents.

[0005] To this end, the utility model adopts the following technical solutions:

[0006] The utility model provides a preparation system for a spherical lithium adsorbent, comprising a raw material mixing device, a spraying device and a curing device;

[0007] The injection device comprises a liquid storage tank, a porous plate, a vibrator and an air pump.

[0008] Furthermore, the porous plate is arranged at the bottom of the liquid storage tank; the diameter of the holes in the porous plate is 0.3-0.8 mm, and the diameter of the holes in the more preferred porous plate is 0.5-0.8 mm; the thickness of the porous plate is 3 mm;

[0009] The air pump is connected to the upper part of the liquid storage tank through an air pipe;

[0010] The exciter is connected to the upper part of the liquid storage tank; the vibration frequency of the exciter is 150Hz-550Hz, and the preferred vibration frequency is 220Hz-400Hz.

[0011] The raw material mixing device comprises a mixing tank, a filter and a peristaltic pump.

[0012] The mixing tank is connected to the filter through a pipeline;

[0013] The filter is connected to a liquid storage tank in the injection device through a peristaltic pump.

[0014] The solidification device comprises a solidification column, a circulating water tank, a water pump and a filter screen.

[0015] Furthermore, the solidification column is arranged directly below the liquid storage tank;

[0016] The solidification column is connected to the circulating water tank through a pipeline, and a water pump is arranged on the pipeline;

[0017] The filter screen is arranged just above the circulating water tank.

[0018] Preferably, the diameter of the holes in the porous plate is 0.3-0.8 mm, more preferably the diameter of the holes in the porous plate is 0.5-0.8 mm, and the thickness of the porous plate is 3 mm;

[0019] The filtering accuracy of the filter is 50-200 μm; the filtering accuracy of the filter net is 0.1-0.5 mm.

[0020] The liquid storage tank is provided with a first heating device and a pressure gauge; the mixing tank is provided with a second heating device and a stirrer; and the filter is provided with a heat preservation device.

[0021] The utility model also provides a method for preparing a spherical lithium adsorbent using the above system, including heating and stirring the material used to prepare the lithium adsorbent in a mixing tank, allowing the material to enter a filter for filtration, and sending the filtered liquid into a liquid storage tank through a peristaltic pump, while turning on the air pump and the vibrator, giving the liquid storage tank a certain pressure and vibration frequency, allowing the liquid to be ejected through a porous plate, forming a liquid column of a certain height in the air, and dispersing into small droplets, which drip into the solidification liquid of the solidification column. The spherical lithium adsorbent particles solidified in the solidification liquid flow out from the bottom of the solidification column, are collected by a filter, and are transferred to a water bath, and are further solidified for 12h-48h to obtain spherical lithium adsorbent particles.

[0022] Furthermore, the materials for preparing the lithium adsorbent include lithium adsorbent powder, a binder, a porogen and a solvent;

[0023] Wherein, the solvent includes one or more of N,N-dimethylformamide, tetrahydrofuran or dichloromethane;

[0024] The lithium adsorbent powder is a material that selectively adsorbs lithium ions, including aluminum, titanium, manganese, crown ethers, etc. The particle size of the lithium adsorbent powder is less than 75 μm; the mass of the lithium adsorbent powder is 30-90% of the mass of the solvent, preferably 40-60%;

[0025] The binder is a mixture of polyvinyl chloride, polyacrylonitrile and polyacrylamide. The mass of the binder is 20%-60% of the mass of the lithium adsorbent powder, preferably 40-50%; the mass ratio of polyvinyl chloride, polyacrylonitrile and polyacrylamide is 50-75:10-30:5-15, preferably 60-70:15-25:10-15;

[0026] The porogen includes one or more inorganic salts such as sodium chloride, potassium chloride, sodium sulfate, potassium sulfate, etc. The particle size of the porogen powder is 20-75μm, preferably 20-38μm; the mass of the porogen is 5-20% of the mass of the lithium adsorbent powder, preferably 10-15%.

[0027] The heating temperature in the mixing tank is 50-80°C, preferably 55-70°C;

[0028] The solidifying liquid is one or more of pure water, ethanol, methanol and acetone; the temperature of the solidifying liquid is less than 30°C.

[0029] The technical solution of the utility model has the following advantages:

[0030] The utility model adopts the jet forming principle, sprays the forming liquid of the lithium adsorbent into the air through an air pump, and breaks the liquid into small droplets through an exciter. The droplets become spherical under the action of surface tension, and finally solidify and form in a solidification column. The utility model has a simple structure, easy to control the process, fast preparation speed, and is suitable for large-scale production; the prepared spherical adsorbent has a small column pressure during application, is wear-resistant, and has a long service life. The prepared spherical adsorbent particles have a particle size of <1.2mm and a high adsorption and desorption rate, which greatly improves the use efficiency of the lithium adsorbent. BRIEF DESCRIPTION OF THE DRAWINGS

[0031] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0032] Figure 1 This is a schematic structural diagram of a system for preparing a spherical lithium adsorbent in Example 1 of the present utility model;

[0033] Figure 2 This is a schematic diagram of the structure of a porous plate in the preparation system of a spherical lithium adsorbent in Example 1 of the utility model.

[0034] Reference numerals:

[0035] 1-filter; 2-first valve; 3-mixing tank; 4-agitator; 5-liquid storage tank; 6-signal generator; 7-power amplifier; 8-exciter; 9-second valve; 10-air pump; 11-porous plate; 12-filter; 13-circulating water tank; 14-water pump; 15-curing column; 16-third valve; 17-peristaltic pump. DETAILED DESCRIPTION

[0036] The following embodiments are provided for a better understanding of the present invention, but are not limited to the best implementation mode described herein, and do not constitute limitations on the content and protection scope of the present invention. Any product identical or similar to the present invention obtained by anyone under the inspiration of the present invention or by combining the features of the present invention with other prior arts shall fall within the protection scope of the present invention.

[0037] If no specific experimental steps or conditions are specified in the examples, the experiments can be carried out according to the conventional experimental steps or conditions described in the literature in the art, and the reagents are all commercially available standard reagents.

[0038] The following specific embodiments are further explanations of the present invention. The examples cited cannot list all implementation methods of the present invention. Only some implementation methods are used as examples for explanation. The specific embodiments are as follows:

[0039] Example 1

[0040] This embodiment provides a system for preparing a spherical lithium adsorbent, such as Figure 1 As shown, it includes a raw material mixing device, a spraying device and a curing device.

[0041] The spraying device comprises a liquid storage tank 5, a porous plate 11, an exciter 8 and an air pump 10; the porous plate 11 is arranged at the bottom of the liquid storage tank 5; the porous plate 11 is as Figure 2 As shown, the diameter of the hole is 0.3-0.8 mm, and the thickness of the porous plate 11 is 3 mm. The liquid storage tank 5 is provided with a first heating device and a pressure gauge.

[0042] The air pump 10 is connected to the upper part of the liquid storage tank 5 through an air pipe, and a second valve 9 is provided on the air pipe;

[0043] The exciter 8 is connected to the upper part of the liquid storage tank 5. The exciter 8 is connected to a power amplifier 7 and a signal generator 6.

[0044] The raw material mixing device includes a mixing tank 3 , a filter 1 and a peristaltic pump 17 .

[0045] The mixing tank 3 is connected to the filter 1 through a pipeline, and a first valve 2 is provided on the pipeline;

[0046] The filter 1 is connected to the liquid storage tank 5 in the injection system through a peristaltic pump 17, and a third valve 16 is provided on the pipeline. The mixing tank 3 is provided with a second heating device and an agitator 4; the filter 1 is provided with a heat preservation device and a filter element is provided inside, and the filtering accuracy of the filter 1 is 50-200 μm.

[0047] The curing device includes a curing column 15 , a circulating water tank 13 , a water pump 14 and a filter screen 12 .

[0048] The solidification column 15 is arranged directly below the liquid storage tank 5;

[0049] The solidification column 15 is connected to the circulating water tank 13 through a pipeline, and a water pump 14 is arranged on the pipeline;

[0050] The filter screen 12 is arranged directly above the circulating water tank 13. The filtering accuracy of the filter screen 12 is 0.1-0.5 mm.

[0051] Example 2

[0052] This embodiment provides a method for preparing a spherical lithium adsorbent, using the preparation system in Example 1, and the specific steps are as follows:

[0053] (1) Grind aluminum lithium adsorbent powder and sodium chloride, pass through a 400-mesh sieve, and set aside; take 10 kg of N,N-dimethylformamide and add it to a mixing tank 3, start stirring and heat it to 60° C., add 1.8 kg of polyvinyl chloride, 0.36 kg of polyacrylonitrile, and 0.18 kg of polyacrylamide respectively, stir for 20 minutes, then add 4 kg of aluminum lithium adsorbent powder and 0.5 kg of sodium chloride, and keep stirring for 30 minutes;

[0054] (2) After the feed liquid is mixed in the mixing tank 3, the first valve 2 and the third valve 16 are opened to allow the feed liquid to pass through the filter 1, and then the feed liquid is sent to the liquid storage tank 5 through the peristaltic pump 17. At the same time, the air pump 10 and the second valve 9 are opened, and the air pressure is adjusted to 0.005-0.01Mpa. The exciter 8 is opened, and the vibration frequency is adjusted to 300Hz. The feed liquid is ejected from the porous plate 11 (the hole diameter of the porous plate 11 is 0.5mm). The water pump 14 is opened to send the solidified liquid in the circulating water tank 13 into the solidification column 15. The liquid column formed by the feed liquid is broken into small droplets in the air and falls into the solidification column 15 to form a crude spherical lithium adsorbent. The solidified liquid is a mixture of water and methanol, and its mass ratio of water: methanol = 50:50.

[0055] (3) The crude spherical lithium adsorbent is collected by the filter screen 12 through the pipeline below the curing column 15, and then transferred to a water bath. After deep curing for 18 hours, the spherical lithium adsorbent particles are obtained by washing.

[0056] The particle size of the spherical aluminum-based lithium adsorbent is 0.6-1.2 mm, and the uniformity coefficient is less than 1.25. Under static adsorption conditions, the lithium adsorbent is saturated in 2 hours, and the adsorption capacity is 3.2 g / L. The desorption rate of the lithium adsorbent reaches 100% in 30 minutes.

[0057] Example 3

[0058] This embodiment provides a method for preparing a spherical lithium adsorbent, using the preparation system in Example 1, and the specific steps are as follows:

[0059] (1) Grind titanium lithium adsorbent powder and potassium chloride, pass through a 325-mesh sieve, and set aside; add 18 kg of N,N-dimethylformamide to mixing tank 3, start stirring and heat to 60° C., add 3.5 kg of polyvinyl chloride, 0.65 kg of polyacrylonitrile, and 0.36 kg of polyacrylamide, respectively, stir for 20 minutes, then add 7.5 kg of titanium lithium adsorbent powder and 1.2 kg of potassium chloride, and stir for 1 hour;

[0060] (2) After the feed liquid is mixed, open the first valve 2 and the third valve 16, so that the feed liquid passes through the filter 1, and then is sent to the liquid storage tank 5 through the peristaltic pump 17. At the same time, open the air pump 10 and the second valve 9, adjust the air pressure to 0.008-0.011Mpa, turn on the vibrator 8, adjust the vibration frequency to 250Hz, and the feed liquid is ejected from the porous plate 11 (the hole diameter of the porous plate 11 is 0.5mm). Turn on the water pump 14, and send the solidified liquid in the circulating water tank 13 into the solidification column 15. The liquid column formed by the feed liquid is broken into small droplets in the air and falls into the solidification column 15 to form a crude spherical lithium adsorbent. The solidified liquid is a mixture of water and methanol, and its mass ratio of water: methanol = 70:30.

[0061] (3) The crude spherical lithium adsorbent is collected by the filter screen 12 through the pipeline below the curing column 15, and then transferred to a water bath. After deep curing for 18 hours, the spherical lithium adsorbent particles are obtained by washing.

[0062] The particle size of the spherical aluminum-based lithium adsorbent is between 0.8 and 1.2 mm. The lithium adsorbent is saturated with adsorption within 2.5 hours, and the adsorption capacity is 4.15 g / L. The desorption rate of the lithium adsorbent reaches 100% within 60 minutes.

[0063] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention of the utility model.

Claims

1. A system for preparing a spherical lithium adsorbent, characterized in that: It includes a raw material mixing device, a spraying device and a curing device; The injection device comprises a liquid storage tank, a porous plate, a vibrator and an air pump; The porous plate is arranged at the bottom of the liquid storage tank; The air pump is connected to the upper part of the liquid storage tank through an air pipe; The vibrator is connected to the upper part of the liquid storage tank; The raw material mixing device includes a mixing tank, a filter and a peristaltic pump; The mixing tank is connected to the filter through a pipeline; The filter is connected to the liquid storage tank in the injection device through a peristaltic pump; The curing device comprises a curing column, a circulating water tank, a water pump and a filter screen; The solidification column is arranged directly below the liquid storage tank; The solidification column is connected to the circulating water tank through a pipeline, and a water pump is arranged on the pipeline; The filter screen is arranged just above the circulating water tank.

2. The preparation system according to claim 1, characterized in that: The diameter of the holes in the porous plate is 0.3-0.8 mm, and the thickness of the porous plate is 3 mm.

3. The preparation system according to claim 2, characterized in that: The filtering accuracy of the filter is 50-200 μm; the filtering accuracy of the filter net is 0.1-0.5 mm.

4. The preparation system according to claim 3, characterized in that: The liquid storage tank is provided with a first heating device and a pressure gauge; the mixing tank is provided with a second heating device and a stirrer; and the filter is provided with a heat preservation device.