Formwork-free ring beam module
The formwork-free ring beam module addresses the inefficiencies of traditional construction by enhancing bonding strength and structural integrity through direct concrete contact and reduced gaps, thereby speeding up construction and saving costs.
Patent Information
- Application Number
- CN202420693502.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-07
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-04-07
AI Technical Summary
Traditional ring beam construction in building projects requires formwork support and removal, leading to long construction periods, high labor input, and potential quality and appearance issues, affecting overall construction progress and economy.
A formwork-free ring beam module comprising a module bottom plate and side plates with external and internal connection parts, grooves, and friction lines, allowing for direct concrete contact and improved bonding strength, reducing gaps and leakage during concrete pouring.
The module ensures structural integrity, reduces construction time and costs, and enhances the bonding strength between steel bars and concrete, while eliminating the need for formwork, thus improving construction efficiency and safety.
Smart Images

Figure CN222120729U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of construction, in particular to a formwork-free ring beam module. Background Art
[0002] In the wall masonry construction of building projects, the ring beam, as a load-bearing component, can effectively improve the structural stability of the building and enhance the overall anti-overturning capacity of the building. In earthquake zones, the ring beam can bear part of the earthquake force and reduce the damage caused to the building by the earthquake through the synergy of steel bars and concrete. The ring beam can evenly transfer the load of the upper structure such as floor slabs and roof panels to the columns and walls to ensure the reasonable distribution of the load. The reasonable application of the ring beam construction technology helps to ensure safety during the construction process and prevent accidents. In general, the ring beam construction technology plays multiple important roles in the building, such as connecting the upper and lower parts, stabilizing the structure, enhancing earthquake resistance, and distributing loads. It is an indispensable part of modern construction projects.
[0003] The traditional ring beam construction process is generally to support the wooden formwork after the wall is built, which requires processes such as formwork matching, formwork support, fixing, and formwork removal. This process has the problems of long construction period, many construction processes, and the overall quality and construction appearance of the ring beam cannot be guaranteed, which affects the overall construction progress of the wall. The formwork and labor input are large, the economy is not high, and the consumption is high. Therefore, it is necessary to design a ring beam model that does not require formwork support and formwork removal, has a strong bond with concrete, and has high ring beam quality. Utility Model Content
[0004] The utility model provides a formwork-free ring beam module, and a ring beam model is obtained by splicing a plurality of ring beam modules, aiming to solve one or more of the above-mentioned problems and other potential problems.
[0005] The utility model provides a formwork-free ring beam module, characterized in that it comprises: a module bottom plate and side plates installed on both sides of the module bottom plate, adjacent ring beam modules are connected by the side plates, the side plates comprise a side plate body, an external connection portion arranged on the side of the side plate body and an internal connection portion spliced with the external connection portion of the adjacent side plate body, the side plate body has an external decorative surface and an internal decorative surface for direct contact with concrete, and a plurality of grooves are provided on the internal decorative surface of the side plate body.
[0006] The formwork-free ring beam module provided by the utility model is an open model, which is convenient for binding of ring beam reinforcement bars in subsequent projects, and the binding of reinforcement bars does not affect the use of the ring beam module.
[0007] Furthermore, the side panels of the utility model are provided with external connection parts and internal connection parts. When adjacent ring beam modules are connected, the external connection parts of the side panels are connected with the internal connection parts of the adjacent side panels, thereby increasing the connection area of the adjacent side panels and reducing the gap between the adjacent side panels. This makes the splicing of the ring beam modules more firm and better prevents leakage of concrete when pouring the ring beam, thereby better ensuring the integrity of the ring beam.
[0008] Furthermore, the interior surface of the side panel body is provided with a plurality of grooves, the purpose of which is to increase the contact area between the ring beam module and the concrete, improve the bonding strength between the ring beam module and the cast-in-place concrete, and improve the structural integrity of the ring beam module after the concrete solidifies.
[0009] Furthermore, the steel bars tied during the ring beam can be placed in the grooves of the inner surface of the side panels, and the positions of the steel bars can be fixed with the help of the grooves, thereby strengthening the bonding between the steel bars, concrete and the ring beam module.
[0010] In some embodiments, the width of the groove gradually decreases from the interior surface toward the exterior surface.
[0011] In the embodiment, by changing the width of the groove, the width of the groove is gradually reduced from the interior surface toward the exterior surface, thereby further increasing the contact area between the groove and the concrete during use and improving the bonding degree between the ring beam module and the concrete.
[0012] In some embodiments, the minimum width of the groove is 0.5 to 1 times the maximum width of the groove.
[0013] In some embodiments, the depth of the groove is 0.3 to 0.5 times the thickness of the side plate.
[0014] In some embodiments, the side plate is provided with 5 to 10 grooves, the thickness of the side plate is 10 to 20 mm, the maximum width of the grooves is 50 to 100 mm, and the spacing between adjacent grooves is 50 to 100 mm.
[0015] In the embodiment, the maximum width and minimum width and depth of the groove are controlled to facilitate the placement and fixing of the steel bars. Furthermore, the thickness of the side plate and the depth, number, spacing and width of the grooves are controlled to prevent the side plate from being reduced in rigidity due to the provision of the grooves, and to control the rigidity of the side plate so that it is not easy to bend, so as to ensure that the side plate can withstand the pressure of the expansion of the concrete when it solidifies.
[0016] In some embodiments, friction lines are provided in the groove; friction lines are provided on the joint surface between the outer connecting portion and the inner connecting portion of the side panel; and friction lines are provided on the joint surface between the inner connecting portion and the outer connecting portion of the side panel.
[0017] In some embodiments, the friction pattern is a dot pattern or a wave pattern.
[0018] In the embodiment, the groove, the joint surface of the outer connection part and the inner connection part of the side plate, and the joint surface of the inner connection part and the outer connection part of the side plate are all provided with friction lines. The friction lines on the groove are used to increase the roughness of the contact surface between the groove and the concrete, so as to increase the bonding force between the groove and the concrete. The friction lines on the outer connection part and the inner connection part are used to increase the friction force when the adjacent side plates are connected, and reduce the connection gap, so that the connection between the adjacent ring beam modules is more stable, and the concrete is not easy to leak from the connection gap of the side plate during use, reducing the possibility of leakage.
[0019] In some embodiments, the side panel further includes a fixing portion disposed on a connecting surface between the side panel and the module bottom plate, and the module bottom plate is provided with a fixing groove for engaging with the fixing portion.
[0020] In the embodiment, the side panels are connected by snapping the fixing portions with the fixing grooves of the module bottom panel, and the installation method is simple, and the device is easy to carry and install.
[0021] By implementing the above technical solution, the utility model has the following advantages:
[0022] 1. The formwork-free ring beam module provided by the utility model is an open model, which is convenient for binding of ring beam reinforcement in subsequent projects, and the binding of reinforcement does not affect the use of the ring beam module.
[0023] 2. The side panels of the utility model are provided with external connection parts and internal connection parts. When adjacent ring beam modules are connected, the external connection parts of the side panels are connected with the internal connection parts of the adjacent side panels to increase the connection area of the adjacent side panels and reduce the gap between the adjacent side panels, so that the splicing of the ring beam modules is more firm and better prevents leakage of concrete when pouring the ring beam, thereby better ensuring the integrity of the ring beam.
[0024] 3. The interior surface of the side panel body is provided with a number of grooves, the purpose of which is to increase the contact area between the ring beam module and the concrete, improve the bonding strength between the ring beam module and the cast-in-place concrete, and improve the structural integrity of the concrete and the ring beam module after solidification. Furthermore, the steel bars tied during the ring beam can be placed in the grooves of the interior surface of the side panel, and the position of the steel bars can be fixed by means of the grooves, thereby strengthening the bonding between the steel bars, the concrete, and the ring beam module. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0026] Figure 1 It is a structural schematic diagram of the utility model;
[0027] Figure 2 is a cross-sectional view of a side panel of the utility model;
[0028] Figure 3 It is a side view of the side panel of the utility model;
[0029] Figure 4 It is a structural schematic diagram of the module base plate of the utility model;
[0030] Figure 5 It is the installation diagram of the utility model;
[0031] Figure 6 It is an installation cross-sectional view of the utility model.
[0032] The symbols in the figure represent:
[0033] 1. Ring beam module, 11. Module bottom plate, 111. Fixing groove, 12. Side panel, 121. Side panel body, 1211. External finishing surface, 1212. Internal finishing surface, 1222. Groove, 122. External connecting part, 123. Internal connecting part, 124. Fixing part, a. Steel bar, b. Concrete. DETAILED DESCRIPTION
[0034] The utility model is further described in detail below based on the accompanying drawings and specific embodiments.
[0035] It should be noted that the following implementation cases are only used to illustrate the technical solutions of the utility model, rather than to limit it. Those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solutions deviate from the scope of the technical solutions of the implementation cases of the utility model.
[0036] In the following description, terms such as "inside", "outside", "up", "down", "left", "right", etc. that indicate directions or positional relationships are only used to facilitate the description of the embodiments and simplify the description, and do not indicate or imply that the referred device or element must have a specific direction, be constructed and operated in a specific direction. Therefore, it should not be understood as a limitation on the present invention.
[0037] This embodiment provides a formwork-free ring beam module 1, such as Figure 1As shown, it is characterized in that it includes: a module base plate 11 and side plates 12 installed on both sides of the module base plate 11, the adjacent ring beam modules 1 are connected by the side plates 12, the side plates 12 include a side plate body 121, an external connection part 122 arranged on the side of the side plate body 121 and an internal connection part 123 spliced with the external connection part 122 of the adjacent side plate body 121, the side plate body 121 has an external finishing surface 1211 and an internal finishing surface 1212 for direct contact with concrete b, and a plurality of grooves 1222 are provided on the internal finishing surface 1212 of the side plate body 121.
[0038] The formwork-free ring beam module 1 provided in this embodiment is an open model, which is convenient for the binding of the ring beam reinforcement a in the subsequent project, and the binding of the reinforcement a does not affect the use of the ring beam module 1. The side plate 12 is provided with an external connection part 122 and an internal connection part 123. When adjacent ring beam modules 1 are connected, the external connection part 122 of the side plate 12 is connected with the internal connection part 123 of the adjacent side plate 12 to increase the connection area of the adjacent side plates 12 and reduce the gap between the adjacent side plates 12, so that the splicing of the ring beam module 1 is more firm and the leakage of concrete b when pouring the ring beam is better prevented, thereby better ensuring the integrity of the ring beam.
[0039] Furthermore, the interior surface 1212 of the side panel body 121 is provided with a plurality of grooves 1222, the purpose of which is to increase the contact area between the ring beam module 1 and the concrete b, improve the bonding strength between the ring beam module 1 and the cast-in-place concrete b, and improve the structural integrity of the concrete b with the ring beam module 1 after solidification.
[0040] Furthermore, the steel bars a tied during the ring beam formation can be placed in the groove 1222 of the inner surface 1212 of the side panel 12, and the position of the steel bars a can be fixed with the help of the groove 1222 to strengthen the bonding between the steel bars a, the concrete b and the ring beam module 1.
[0041] In some embodiments, Figure 2 As shown, the width of the groove 1222 gradually decreases from the interior surface 1212 toward the exterior surface 1211 .
[0042] In the embodiment, by changing the width of the groove 1222, the width of the groove 1222 is gradually reduced from the interior surface 1212 toward the exterior surface 1211, thereby further increasing the contact area between the groove 1222 and the concrete b during use, thereby improving the bonding degree between the ring beam module 1 and the concrete b.
[0043] In some embodiments, the minimum width of the groove 1222 is 0.5 to 1 times the maximum width of the groove 1222 .
[0044] In some embodiments, the depth of the groove 1222 is 0.3 to 0.5 times the thickness of the side plate 12 .
[0045] In some embodiments, 5 to 10 grooves 1222 are provided on the side plate 12, the thickness of the side plate 12 is 10 to 20 mm, the maximum width of the grooves 1222 is 50 to 100 mm, and the spacing between adjacent grooves 1222 is 50 to 100 mm.
[0046] like Figure 2 As shown, in the embodiment, the interior surface 1212 of the side panel body 121 is provided with 6 grooves 1222, and the maximum width, minimum width and depth of the grooves 1222 are controlled to facilitate the placement and fixing of the steel bars a.
[0047] Furthermore, the thickness of the side panel 12 and the depth, number, spacing and width of the grooves 1222 are controlled to prevent the rigidity of the side panel 12 from being reduced due to the provision of the grooves 1222, and the rigidity of the side panel 12 is controlled to prevent it from being easily bent, thereby ensuring that the side panel 12 can withstand the pressure on the side panel 12 caused by the expansion of the concrete b when it solidifies.
[0048] In some embodiments, Figure 3 As shown, the groove 1222 is provided with friction lines; the joint surface of the outer connecting part 122 and the inner connecting part 123 of the side plate 12 is provided with friction lines, and the joint surface of the inner connecting part 123 and the outer connecting part 122 of the side plate 12 is provided with friction lines.
[0049] In some embodiments, the friction pattern is a dot pattern or a wave pattern.
[0050] like Figure 3 As shown, in the embodiment, the groove 1222, the joint surface between the outer connecting portion 122 and the inner connecting portion 123 of the side plate 12, and the joint surface between the inner connecting portion 123 and the outer connecting portion 122 of the side plate 12 are all provided with friction lines. Figure 3 The friction pattern in the middle is a wave pattern. The friction pattern on the groove 1222 is used to increase the roughness of the contact surface between the groove 1222 and the concrete b, so as to increase the bonding force between the groove 1222 and the concrete b. The friction pattern on the outer connecting part 122 and the inner connecting part 123 is used to increase the friction force when the adjacent side panels 12 are connected, and reduce the connection gap, so that the connection between the adjacent ring beam modules 1 is more stable, and the concrete b is not easy to leak from the connection gap of the side panels 12 during use, reducing the possibility of leakage.
[0051] In some embodiments, Figure 4 As shown, the side plate 12 further includes a fixing portion 124 disposed on the connecting surface of the side plate 12 and the module bottom plate 11 , and the module bottom plate 11 is provided with a fixing groove 111 for engaging with the fixing portion 124 .
[0052] In the embodiment, the side plate 12 is connected to the fixing groove 111 of the module bottom plate 11 by snapping the fixing portion 124 , and the installation method is simple, and it is easy to carry and install.
[0053] like Figure 5 , Figure 6 As shown, when the wall is built to the bottom elevation of the ring beam, the ring beam module 1 is used for masonry, the module bottom plate 11 is fixedly connected to the wall, and the side plate 12 is installed on the module bottom plate 11, the side plate 12 is connected to the fixing groove 111 of the module bottom plate 11 through the fixing part 124, and the adjacent side plates 12 are connected through the outer connecting part 122 and the inner connecting part 123, so as to connect several ring beam modules 1 to form an open-type ring beam model, and both sides of the open-type ring beam model are fixed to the wall to ensure that the subsequent concrete b will not leak out of the open-type ring beam model. After the construction of the open-type ring beam model is completed, the ring beam steel bar a is tied inside the groove 1222 of the ring beam module 1, and after the steel bar a cage is obtained, concrete b is poured into the open-type ring beam model and vibrated. After the concrete b solidifies, a formwork-free ring beam is obtained, and there is no need to remove the formwork, which saves labor, reduces the investment in formwork system materials, reduces construction costs, speeds up construction progress, and reduces the safety risks of high-level operations such as ring beam template support.
[0054] The utility model is convenient to construct, saves time, labor and materials, has excellent performance in one go, and has good aesthetics. It effectively reduces the tedious construction procedures of the ring beam during formwork construction, and while ensuring the firmness of the structure, it greatly improves the construction efficiency, achieving the effect of cost saving and green construction.
[0055] The applicant declares that the above is only a specific implementation method of the utility model, but the protection scope of the utility model is not limited to this. Technical personnel in the relevant technical field should understand that any changes or substitutions that can be easily thought of by technical personnel in the relevant technical field within the technical scope disclosed in the utility model fall within the protection scope and disclosure scope of the utility model.
Claims
1. A formwork-free ring beam module, characterized in that: include: A module bottom plate (11) and side plates (12) mounted on both sides of the module bottom plate (11), adjacent ring beam modules (1) being connected via the side plates (12), the side plates (12) comprising a side plate body (121), an external connection portion (122) arranged on the side of the side plate body (121), and an internal connection portion (123) spliced with the external connection portion (122) of an adjacent side plate body (121), the side plate body (121) having an external finishing surface (1211) and an internal finishing surface (1212) for direct contact with concrete (b), and a plurality of grooves (1222) being provided on the internal finishing surface (1212) of the side plate body (121).
2. The ring beam module according to claim 1, characterized in that: The width of the groove (1222) gradually decreases in a direction from the interior surface (1212) toward the exterior surface (1211).
3. The ring beam module according to claim 2, characterized in that: The minimum width of the groove (1222) is 0.5 to 1 times the maximum width of the groove (1222).
4. The ring beam module according to claim 3, characterized in that: The depth of the groove (1222) is 0.3 to 0.5 times the thickness of the side plate (12).
5. The ring beam module according to claim 4, characterized in that: The side plate (12) is provided with 5 to 10 grooves (1222), the thickness of the side plate (12) is 10 to 20 mm, the maximum width of the grooves (1222) is 50 to 100 mm, and the spacing between adjacent grooves (1222) is 50 to 100 mm.
6. The ring beam module according to claim 5, characterized in that: The groove (1222) is provided with friction lines; the joint surface between the outer connecting portion (122) and the inner connecting portion (123) of the side plate (12) is provided with friction lines, and the joint surface between the inner connecting portion (123) and the outer connecting portion (122) of the side plate (12) is provided with friction lines.
7. The ring beam module according to claim 6, characterized in that: The friction pattern is a dot pattern or a wave pattern.
8. The ring beam module according to claim 7, characterized in that: The side plate (12) further comprises a fixing portion (124) arranged on a connection surface between the side plate (12) and the module bottom plate (11), and a fixing groove (111) for clamping with the fixing portion (124) is provided on the module bottom plate (11).