Soft package battery packaging effect testing device

By designing a test device for soft-pack lithium-ion batteries, using the gas source components and air channel system, the problem of the inability to evaluate the overall heat sealing effect of aluminum-plastic film in the prior art is solved, and the battery packaging effect is achieved quickly Numerical evaluation and weak area identification improve the safety and reliability of the battery.

CN222124651UActive Publication Date: 2024-12-06JIANGSU ZENIO NEW ENERGY BATTERY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420776771.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-15
Publication Date
2024-12-06
Estimated Expiration
2034-04-15

AI Technical Summary

Technical Problem

The prior art cannot effectively evaluate the overall heat sealing effect of aluminum-plastic film of soft-pack lithium-ion batteries, resulting in the inability to determine the internal pressure and weak areas of the heat sealing area it bears in actual use, affecting the safety and reliability of the battery. .

Method used

A soft-pack battery packaging effect testing device is designed, including a bracket, a first block, a second block, a battery cell mold and a gas source assembly. The flexible packaging film is punctured when clamping the battery cell mold and inserted tightly with the insertion part. , the first gas channel and the second gas channel are connected, and gas is passed through to test the overall packaging effect and pressure resistance of the aluminum-plastic film.

Benefits of technology

It can quickly understand the overall packaging effect and voltage resistance of the flexible packaging film, identify the weak areas of the packaging, improve the packaging effect, and improve the safety and reliability of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222124651U_ABST
    Figure CN222124651U_ABST
Patent Text Reader

Abstract

The utility model provides a soft package battery packaging effect testing device which comprises a support, a first pressing block, a second pressing block, a battery cell mold and an air source assembly.According to the testing device, through the structural design of the battery cell mold, the first pressing block and the second pressing block, the outer surface of the battery cell mold is packaged with a soft package film; when the first pressing block and the second pressing block clamp and press the battery cell mold, the puncturing part of the second pressing block punctures a flexible packaging film of the battery cell mold and is in tight insertion fit with the insertion part, so that the first air guide channel is communicated with the second air guide channel, and the air source assembly is connected with an air inlet of the first air guide channel; the first air guiding channel and the second air guiding channel are communicated through the air source assembly, so that air enters the space between the battery cell mold and the flexible packaging film from the air outlet of the second air guiding channel, and the overall packaging effect of the flexible packaging film on the battery cell mold is tested by using the pressure of the air introduced by the air source assembly. And the numeralization result of the pressure-resistant effect of the flexible package film packaging can be quickly obtained.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of battery detection, in particular to a soft-pack battery packaging effect testing device. Background Art

[0002] Soft-pack lithium-ion batteries are usually packaged in aluminum-plastic film. The aluminum-plastic film heat sealing process of soft-pack lithium-ion batteries is to use a heating block to apply pressure and temperature to the heat-sealing area of ​​the aluminum-plastic film for heat sealing. The reliability of the heat-sealing effect of the aluminum-plastic film directly affects the reliability of the battery cell. Therefore, it is usually necessary to test and evaluate the heat-sealing effect of the aluminum-plastic film.

[0003] In the related art, the test method for the heat-sealing effect of the aluminum-plastic film is usually to indirectly evaluate the local heat-sealing area, and it is impossible to test and evaluate the overall heat-sealing effect of the battery cell. Therefore, it is impossible to know the internal pressure that the aluminum-plastic film can withstand during the actual use of the battery cell, and it is impossible to know the weak areas of the heat-sealing area. Once the battery cell is bloated during use, it is easy to cause excessive internal pressure in the battery cell and explode, affecting the safety and reliability of the battery. Utility Model Content

[0004] The purpose of the utility model is to provide a soft-pack battery packaging effect test device to solve the technical problem that the overall heat sealing effect of the aluminum-plastic film of the battery core cannot be evaluated in the prior art. The preferred technical solution among the many technical solutions provided by the utility model can produce many technical effects as described below.

[0005] The present application provides a soft-pack battery packaging effect testing device, comprising: a bracket, a first pressing block, a second pressing block, a battery cell mold and an air source assembly, wherein the first pressing block is arranged on the bracket; the second pressing block is arranged opposite to the first pressing block, and the second pressing block can move in a direction away from or close to the first pressing block, a puncture portion is provided on the surface of the second pressing block facing the first pressing block, a first air guide channel is provided inside the second pressing block, and an air outlet of the first air guide channel is located at the puncture portion; the battery cell mold is arranged between the first pressing block and the second pressing block, a soft packaging film is encapsulated on the outer surface of the battery cell mold, and a first air guide channel is provided inside the battery cell mold. There is a second air guiding channel, and an insertion part matching the puncturing part is provided on the surface of the battery cell mold facing the second pressing block, and the air inlet of the second air guiding channel is located at the insertion part. When the first pressing block and the second pressing block clamp and press the battery cell mold, the puncturing part punctures the soft packaging film and fits tightly with the insertion part, so that the first air guiding channel and the second air guiding channel are connected, and the air outlet of the second air guiding channel is located at the contact surface between the battery cell mold and the soft packaging film; the air source component is connected to the air inlet of the first air guiding channel, and is used to introduce gas into the space between the battery cell mold and the soft packaging film through the first air guiding channel and the second air guiding channel.

[0006] In one or more embodiments of the present application, a lifting device is provided on the bracket, and the second pressing block is fixed to the movable end of the lifting device.

[0007] In one or more embodiments of the present application, the lifting device is a cylinder.

[0008] In one or more embodiments of the present application, the puncturing portion is in a cone structure, and the air outlet of the first air guide channel is located in the middle of the cone structure.

[0009] In one or more embodiments of the present application, the insertion portion is a through-hole structure that penetrates through two surfaces of the battery cell mold in a thickness direction.

[0010] In one or more embodiments of the present application, a first sealing groove is provided on the surface of the second pressing block and around the puncture portion, a second sealing groove corresponding to the first sealing groove is provided on the surface of the battery cell mold facing the second pressing block, and a seal is sealed between the first sealing groove and the second sealing groove.

[0011] In one or more embodiments of the present application, the air inlet of the first air guide channel is located on the side of the second pressing block, and the first air guide channel extends from the side of the second pressing block to a side of the puncture portion facing the battery cell mold.

[0012] In one or more embodiments of the present application, the air outlet of the second air guide channel is located on the side of the battery core mold and / or on the surface along the thickness direction of the battery core mold.

[0013] When the air outlet of the second air guiding channel is located on the surface along the thickness direction of the battery core mold and facing the second pressing block, the air outlet of the second air guiding channel is located outside the second sealing groove.

[0014] In one or more embodiments of the present application, the gas source assembly includes:

[0015] Compressed air source;

[0016] An air pipeline, one end of which is connected to a compressed air source, and the other end of which is connected to an air inlet of a first air guide channel of a second pressing block;

[0017] The pressure regulating device and the pressure measuring device are respectively arranged on the gas transmission pipeline.

[0018] In one or more embodiments of the present application, a protection pad is provided on the surface of the first pressing block facing the battery core mold.

[0019] Based on the above technical solution, the beneficial technical effects of the soft-pack battery packaging effect testing device provided by the present application are:

[0020] The soft-pack battery packaging effect testing device provided in the embodiment of the present application is designed through the structure of the battery cell mold, the first pressing block and the second pressing block, and the soft packaging film is packaged on the outer surface of the battery cell mold, so that when the first pressing block and the second pressing block clamp and press the battery cell mold, the piercing part of the second pressing block pierces the soft packaging film of the battery cell mold and is tightly plugged with the insertion part, so that the first air guide channel and the second air guide channel are connected, and the air source component is connected to the air inlet of the first air guide channel so that air can be ventilated into the first air guide channel and the second air guide channel through the air source component, so that the gas passes through the first air guide channel. An air guide channel and a second air guide channel enter between the battery cell mold and the flexible packaging film from the air outlet of the second air guide channel, and then the gas pressure introduced by the air source component can be used to test the overall packaging effect of the flexible packaging film on the battery cell mold, such as the heat sealing effect of the aluminum-plastic film on the battery cell. The numerical result of the pressure resistance effect of the flexible packaging film can also be quickly obtained. At the same time, the packaging weak area of ​​the flexible packaging film can also be known, so as to improve the packaging effect of the flexible packaging film, or evaluate the pressure resistance effect of the weak area, so as to quickly obtain the overall packaging effect of the flexible packaging film. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0022] Figure 1 A schematic diagram of the overall structure of a soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0023] Figure 2 A three-dimensional structural schematic diagram of a partial structure of a soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0024] Figure 3 A schematic diagram of a partial front view of a soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0025] Figure 4 for Figure 3 AA section diagram in;

[0026] Figure 5 A schematic diagram of a right view of a partial structure of a soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0027] Figure 6 for Figure 5 BB cross-section diagram in;

[0028] Figure 7A schematic diagram of the structure of a battery cell mold in a soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0029] Figure 8 A schematic structural diagram of the bottom view of the battery cell mold in the soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0030] Fig. 9 A schematic diagram of the top view of the structure of a battery cell mold in the soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0031] Fig.10 for Fig. 9 AA section diagram in;

[0032] Fig.11 for Fig. 9 BB cross-section diagram in;

[0033] Fig.12 A schematic diagram of the structure of the second pressing block in the soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0034] Fig.13 A front view of a second pressing block in the soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0035] Fig.14 A schematic diagram of the top view of the second pressing block in the soft-pack battery packaging effect testing device provided in an embodiment of the present application;

[0036] Fig.15 for Fig.14 Schematic diagram of the AA section in.

[0037] In the figure: 1- bracket; 2- first pressing block; 3- second pressing block; 4- battery cell mold; 5- flexible packaging film; 6- lifting device; 7- compressed air source; 8- pressure regulating device; 9- pressure measuring device; 10- gas pipeline; 11- sealing member; 12- top frame; 13- side frame; 14- bottom frame; 21- protection pad; 31- first air guide channel; 32- first sealing groove; 33- puncturing part; 34- mounting hole; 40- inserting part; 41- second air guide channel; 42- second sealing groove; 43- chamfering structure; 51- cavity. DETAILED DESCRIPTION

[0038] In order to make the technical problems, technical solutions and beneficial effects to be solved by the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0039] It should be noted that when an element is referred to as being "fixed to" or "disposed on" another element, it can be directly on the other element or indirectly on the other element. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or indirectly connected to the other element.

[0040] It should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0041] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0042] Existing lithium batteries include soft-pack lithium batteries, square-shell lithium batteries and cylindrical lithium batteries. Among them, soft-pack lithium batteries are widely used in the 3C and power industries due to their high volume utilization and flexible shapes. The biggest difference between soft-pack lithium batteries and other forms of lithium batteries is that they use aluminum-plastic film as the outer packaging. Therefore, the reliability of the aluminum-plastic film packaging directly affects the reliability of the battery cell. For example, insufficient heat sealing will lead to low packaging strength, resulting in cracking and leakage in the heat-sealed area after inflation. At the same time, insufficient heat sealing will also cause the heat-sealed thickness to be too large. Long-term use will easily allow moisture to penetrate into the battery cell, causing inflation. In the related art, the test of heat sealing effect is generally to measure the packaging thickness of the heat sealing area or to measure the peeling force of the aluminum-plastic film on both sides after cutting off the heat sealing area separately. However, the above two methods only indirectly evaluate the local heat sealing area and cannot evaluate the overall heat sealing effect. For example, when the battery cell is bloated during actual use, the internal pressure gradually accumulates. It is impossible to know whether the aluminum-plastic film can withstand a certain internal pressure to avoid leakage. At the same time, it is also impossible to know whether the heat sealing area can crack and release pressure after the internal pressure reaches a certain value to avoid explosion due to excessive internal pressure.

[0043] Based on the above considerations, in order to solve the technical problem that the overall thermal packaging effect of the aluminum-plastic film of the battery cell cannot be evaluated in the related art, the present application provides a soft-pack battery packaging effect testing device, including a bracket, a first pressing block, a second pressing block, a battery cell mold and an air source assembly, the first pressing block is arranged on the bracket; the second pressing block is arranged opposite to the first pressing block, and the second pressing block can move in a direction away from or close to the first pressing block, a puncture portion is provided on the surface of the second pressing block facing the first pressing block, a first air guide channel is provided inside the second pressing block, and the air outlet of the first air guide channel is located at the puncture portion; the battery cell mold is arranged between the first pressing block and the second pressing block, and the battery cell mold is provided with a gas source assembly. The outer surface of the tool is encapsulated with a soft packaging film, a second air guide channel is provided inside the battery cell mold, an insertion part matching the puncture part is provided on the surface of the battery cell mold facing the second pressing block, and the air inlet of the second air guide channel is located at the insertion part, when the first pressing block and the second pressing block clamp and press the battery cell mold, the puncture part punctures the soft packaging film and is tightly fitted with the insertion part, so that the first air guide channel and the second air guide channel are connected, and the air outlet of the second air guide channel is located at the contact surface between the battery cell mold and the soft packaging film; the air source component is connected to the air inlet of the first air guide channel, and is used to introduce gas into the space between the battery cell mold and the soft packaging film through the first air guide channel and the second air guide channel.

[0044] Through the structural design of the battery cell mold, the first pressing block and the second pressing block, and encapsulating the soft packaging film on the outer surface of the battery cell mold, when the first pressing block and the second pressing block clamp and press the battery cell mold, the puncture part of the second pressing block punctures the soft packaging film of the battery cell mold and is tightly matched with the insertion part, so that the first air guide channel and the second air guide channel are connected, and the air source component is connected to the air inlet of the first air guide channel so that air can be ventilated into the first air guide channel and the second air guide channel through the air source component, so that the gas passes through the first air guide channel and the second air guide channel from the air outlet of the second air guide channel to enter between the battery cell mold and the soft packaging film, and then the gas pressure introduced by the air source component can be used to test the overall packaging effect of the soft packaging film on the battery cell mold, such as the heat sealing effect of the aluminum-plastic film on the battery cell, and the numerical result of the pressure resistance effect of the soft packaging film can also be quickly obtained. At the same time, the packaging weak area of ​​the soft packaging film can also be known, so as to improve the packaging effect of the soft packaging film, or the pressure resistance effect of the weak area can be evaluated, so as to quickly obtain the overall packaging effect of the soft packaging film.

[0045] The soft-pack battery packaging effect testing device of the present application can be applicable to the field of overall packaging effect detection or evaluation of soft-pack lithium-ion batteries, and is suitable for daily inspection of heat sealing effects during mass production.

[0046] The technical solution of the present application is described in detail below in conjunction with the accompanying drawings.

[0047] Please also read Figure 1 , Figure 2 , Figure 3and Figure 6 The embodiment of the present application provides a soft-pack battery packaging effect testing device, including: a bracket 1, a first pressing block 2, a second pressing block 3, a battery core mold 4 and an air source component, the first pressing block 2 is arranged on the bracket 1, the second pressing block 3 is arranged opposite to the first pressing block 2, and the second pressing block 3 can move in a direction away from or close to the first pressing block 2, the second pressing block 3 is provided with a puncture portion 33 on the surface facing the first pressing block 2, the second pressing block 3 is provided with a first air guide channel 31 inside, the air outlet of the first air guide channel 31 is located at the puncture portion 33, the battery core mold 4 is arranged between the first pressing block 2 and the second pressing block 3, a soft packaging film 5 is encapsulated on the outer surface of the battery core mold 4, and a second An air guide channel 41, an insertion portion 40 matching the puncture portion 33 is provided on the surface of the battery cell mold 4 facing the second pressing block 3, and the air inlet of the second air guide channel 41 is located at the insertion portion 40. When the first pressing block 2 and the second pressing block 3 clamp and press the battery cell mold 4, the puncture portion 33 punctures the soft packaging film 5 and is tightly plugged with the insertion portion 40, so that the first air guide channel 31 and the second air guide channel 41 are connected. The air outlet of the second air guide channel 41 is located at the contact surface between the battery cell mold 4 and the soft packaging film 5. The air source component is connected to the air inlet of the first air guide channel 31, and is used to introduce gas between the battery cell mold 4 and the soft packaging film 5 through the first air guide channel 31 and the second air guide channel 41.

[0048] The support 1 may be a component capable of supporting and installing the first pressing block 2, the second pressing block 3, the battery mold 4 and the gas source assembly. In some embodiments, the support 1 may be composed of a top frame 12, a side frame 13 and a bottom frame 14, wherein the side frame 13 is connected between the top frame 12 and the bottom frame 14 and is located on one side of the top frame 12 and the bottom frame 14 so that a space for accommodating and installing at least the first pressing block 2, the second pressing block 3 and the battery mold 4 is formed between the top frame 12, the side frame 13 and the bottom frame 14.

[0049] The first pressing block 2 is fixed to the side of the top frame 12 of the bracket 1 facing the bottom frame 14. In some embodiments, the first pressing block 2 is fixed to the top frame 12 by fixing parts such as bolts. In some embodiments, the first pressing block 2 is a cylindrical structure. In some embodiments, the first pressing block 2 can be made of metal materials, such as aluminum alloy. In some embodiments, the second pressing block 3 is a cylindrical structure. In some embodiments, the second pressing block 3 is made of metal materials such as aluminum alloy. It can be understood that the first pressing block 2 and the second pressing block 3 are arranged relative to each other, and the second pressing block 3 can be moved in a direction away from or close to the first pressing block 2. It can be understood that: the pressing surfaces of the first pressing block 2 and the second pressing block 3 are arranged relative to each other, and when the first pressing block 2 is fixed to the top frame 12, the pressing surface of the second pressing block 3 can be moved in a direction close to or away from the pressing surface of the first pressing block 2, so that the first pressing block 2 and the second pressing block 3 can press the object to be tested or take out the object to be tested.

[0050] The battery mold 4 can be a dummy battery. During testing, the outer surface of the battery mold 4 is covered with a soft packaging film 5, such as an aluminum-plastic film, for heat sealing to serve as a dummy battery. The size of the battery mold 4 can be made according to the length, width, and thickness of the roll core in the actual battery. The contact surface between the battery mold 4 and the soft packaging film 5 can refer to the outer surface of the battery mold 4, including: the upper surface, the lower surface, and the surrounding side surfaces.

[0051] In the technical solution of the embodiment of the present application, through the structural design of the battery mold 4, the first pressing block 2 and the second pressing block 3, and the soft packaging film 5 is encapsulated on the outer surface of the battery mold 4, when the first pressing block 2 and the second pressing block 3 clamp and press the battery mold 4, the piercing portion 33 of the second pressing block 3 pierces the soft packaging film 5 of the battery mold 4 and is tightly plugged with the insertion portion 40, so that the first air guide channel 31 of the second pressing block 3 is connected to the second air guide channel 41 of the battery mold 4, and the air source component is connected to the air inlet of the first air guide channel 31, so that the air source component can be used to supply air to the first air guide channel 31 and the second air guide channel 41. Internal ventilation allows the gas to pass through the first air guide channel 31 and the second air guide channel 41 and enter between the battery cell mold 4 and the flexible packaging film 5 from the air outlet of the second air guide channel 41. The pressure of the gas introduced by the air source component can then be used to detect the overall packaging effect of the flexible packaging film 5 on the battery cell mold 4, such as the heat sealing effect of the aluminum-plastic film. The numerical result of the packaging pressure resistance effect of the flexible packaging film 5 can be quickly obtained, and the packaging weak area of ​​the flexible packaging film 5 can also be known, so as to improve the packaging effect of the flexible packaging film 5, or evaluate the pressure resistance effect of the weak area, so as to quickly obtain the overall packaging effect of the flexible packaging film.

[0052] In some embodiments, please refer to Figures 1 to 6 A lifting device 6 is provided on the bracket 1 , and the second pressing block 3 is fixed to the movable end of the lifting device 6 .

[0053] The bottom of the lifting device 6 is fixed to the surface of the bottom frame 14 facing the top frame 12 .

[0054] In the technical solution of the embodiment of the present application, a lifting device 6 is arranged on the bracket 1, and the second pressure block 3 is fixed to the movable end of the lifting device 6, so that the lifting device 6 can be used to drive the second pressure block 3 to move toward the direction close to the first pressure block 2, and then the first pressure block 2 and the second pressure block 3 can be pressed and clamped to the battery cell mold 4, or the lifting device 6 can be used to drive the second pressure block 3 to move away from the first pressure block 2, so as to separate the first pressure block 2 and the second pressure block 3, and then take out the battery cell mold 4.

[0055] In some embodiments, the lifting device 6 is a cylinder.

[0056] In some embodiments, please refer to Figure 6 and Fig.15The piston rod of the cylinder can be inserted into and fixed inside the second pressing block 3, so that the piston rod of the cylinder is fixed inside the second pressing block 3. At the same time, a mounting hole 34 is provided on the surface of the second pressing block 3 facing the lifting device 6, so that the end of the piston rod of the cylinder is fixed in the mounting hole 34.

[0057] In the technical solution of the embodiment of the present application, the lifting device 6 is set as a cylinder so that the piston rod of the cylinder can be inserted into and fixed in the mounting hole 34 of the second pressure block 3, so that the piston rod of the cylinder and the second pressure block 3 are firmly connected, and it is not easy for the piston rod of the cylinder to shake during the movement. Driven by the cylinder, the second pressure block 3 can be moved in the direction close to the first pressure block 2, and the battery cell mold 4 can be clamped more stably.

[0058] In some embodiments, please refer to Fig.12 and Fig.13 The puncturing portion 33 is in a cone structure, and the air outlet of the first air guide channel 31 is located in the middle of the cone structure.

[0059] The puncture portion 33 may be a conical protrusion structure that is narrow at the top and wide at the bottom and is disposed on the surface of the second pressing block 3. The air outlet of the first air guide channel 31 is located in the middle of the cone structure, which can be understood as the air outlet of the first air guide channel 31 is located at the center of the surface of the cone structure away from the second pressing block 3.

[0060] In the technical solution of the embodiment of the present application, the puncture portion 33 is set to a cone structure, and the air outlet of the first air guide channel 31 is located in the middle of the cone structure, so that when the first pressing block 2 and the second pressing block 3 press the battery cell mold 4, the soft packaging film 5 of the battery cell mold 4 is punctured by the puncture portion 33 of the cone structure, so that the gas enters the second air guide channel 41 of the battery cell mold 4 from the first air guide channel 31, and then enters between the battery cell mold and the soft packaging film, thereby achieving the purpose of detecting the overall heat sealing effect of the soft packaging film.

[0061] In some embodiments, please refer to Figures 8 to 11 The insertion portion 40 is a through-hole structure that penetrates through both surfaces of the battery core mold 4 in the thickness direction.

[0062] In the technical solution of the embodiment of the present application, the insertion portion 40 is set to a through-hole structure that passes through the two surfaces of the battery cell mold 4 in the thickness direction, so that when the first pressing block 2 and the second pressing block 3 clamp the battery cell mold 4, the insertion portion 40 of the through-hole structure provides space for the puncture portion 33 of the second pressing block 3, so that under the action of pressure, the puncture portion 33 can puncture the soft packaging film 5, so that the first air guide channel 31 and the second air guide channel 41 are connected. At the same time, the cooperation of the puncture portion 33 and the insertion portion 40 can facilitate the positioning of the battery cell mold 4 by the second pressing block 3. In other embodiments, the through-hole structure that passes through the two surfaces of the battery cell mold 4 in the thickness direction can also serve as the air outlet of the second air guide channel 41.

[0063] In some embodiments, please refer to Figure 7 The edge of the battery core mold 4 is set as a chamfer structure 43 to make it free of burrs.

[0064] In some embodiments, please refer to Fig.10 , Fig.11 and Fig.12 A first sealing groove 32 is provided on the surface of the second pressing block 3 and around the puncture portion 33, and a second sealing groove 42 corresponding to the first sealing groove 32 is provided on the surface of the battery core mold 4 facing the second pressing block 3, and a sealing member 11 is sealed and installed between the first sealing groove 32 and the second sealing groove 42.

[0065] In the technical solution of the embodiment of the present application, a first sealing groove 32 is provided on the surface of the second pressing block 3 and around the puncture portion 33, and a second sealing groove 42 corresponding to the first sealing groove 32 is provided on the surface of the battery mold 4 facing the second pressing block 3, so that a sealing member 11 is sealed and installed between the first sealing groove 32 and the second sealing groove 42. The sealing member 11 is then used to effectively seal the connection between the puncture portion 33 and the insertion portion 40, so that it is not easy for the gas to escape outside the soft packaging film 5, so that the gas introduced from the first air guide channel 31 can all enter the cavity of the soft packaging mold 5 and the battery mold 4.

[0066] In some embodiments, the seal 11 may be an O-ring. The first sealing groove 32 is an annular groove surrounding the puncture portion 33, and the longitudinal section of the first sealing groove 32 is a trapezoidal structure that is narrow at the top and wide at the bottom. The groove depth of the first sealing groove 32 is less than the diameter of the seal 11, and the width of the narrow mouth of the first sealing groove 32 is less than the diameter of the seal 11, so it is not easy for the seal 11 to fall off. The second sealing groove 42 may be an annular groove formed on the surface of the battery mold 4. The position of the second sealing groove 42 corresponds to the position of the first sealing groove 32. When the first pressing block 2 and the second pressing block 3 are in an unpressed state, the top of the seal 11 protrudes from the top of the first sealing groove 32. When the first pressing block 2 and the second pressing block 3 clamp and press the battery mold 4, the seal 11 is installed in the first sealing groove 32, and its protruding part approaches the second sealing groove 42 and gradually fits and compresses the seal in the process of the two pressing blocks approaching. The seal 11 forms an interference fit with the first sealing groove 32 and the second sealing groove 42. Furthermore, the seal 11 is utilized to effectively seal, and it is not easy for the gas to escape to the outside of the flexible packaging film 5 , so that the gas introduced from the first air guide channel 31 can all enter the cavity of the flexible packaging mold 5 and the battery core mold 4 .

[0067] In some embodiments, the edge of the second sealing groove 42 is a chamfered structure. In some embodiments, the edge of the second sealing groove 42 is a 45° chamfered structure.

[0068] In some embodiments, please refer to Fig.12 and Fig.15 The air inlet of the first air guide channel 31 is located on the side of the second pressing block 3 , and the first air guide channel 31 extends from the side of the second pressing block 3 to the side of the puncture portion 33 facing the battery core mold 4 .

[0069] In the technical solution of the embodiment of the present application, the air inlet of the first air guide channel 31 is connected to the air source component so that the gas provided by the air source component enters the first air guide channel 31 and enters the cavity 51 of the battery core mold 4 and the soft packaging film 5 from the first air guide channel 31.

[0070] In some embodiments, please refer to Figure 7 and Figure 8 The air outlet of the second air guide channel 41 is located on the side of the battery core mold 4 and / or on the surface along the thickness direction of the battery core mold 4.

[0071] When the air outlet of the second air guiding channel 41 is located on the surface along the thickness direction of the battery core mold 4 and facing the second pressing block 3 , the air outlet of the second air guiding channel 41 is located outside the second sealing groove 42 .

[0072] In some embodiments, the insertion portion 40 is a through-hole structure that penetrates through both surfaces of the battery core mold 4 in the thickness direction. Then, when the piercing portion 33 is inserted into the insertion portion 40, the through-hole of the insertion portion 40 away from the second pressing block 3 can serve as one of the air outlets of the second air guide channel 41. In some embodiments, the second air guide channel 41 can be provided with multiple air outlets, such as Figure 7 shown.

[0073] In the technical solution of the embodiment of the present application, the outlet of the second air guide channel 41 is arranged on the side of the battery mold 4 and / or on the surface along the thickness direction of the battery mold 4, and when the outlet of the second air guide channel 41 is located on the surface along the thickness direction of the battery mold 4 and facing the second pressing block 3, the outlet of the second air guide channel 41 is located outside the second sealing groove 42. In this way, the gas entering through the insertion portion 40 can be quickly diffused in all directions along the outlets and enter the cavity 51 between the battery mold 4 and the flexible packaging film 5, so that the air pressure in the cavity 51 quickly reaches the withstand pressure value of the flexible packaging film 5.

[0074] In some embodiments, please refer to Figure 1 The gas source assembly includes: a compressed air source 7, a gas pipeline 10, a pressure regulating device 8 and a pressure measuring device 9. One end of the gas pipeline 10 is connected to the compressed air source 7, and the other end of the gas pipeline 10 is connected to the air inlet of the first air guide channel 31 of the second pressing block 3; the pressure regulating device 8 and the pressure measuring device 9 are respectively arranged on the gas pipeline 10.

[0075] The compressed air source 7 may be a component capable of providing compressed air. The pressure regulating device 8 may be a device capable of adjusting the maximum value of the input air pressure, for example, the pressure regulating device 8 may be a pressure regulating valve. The pressure measuring device 9 may be a device capable of displaying the real-time air pressure and recording it, for example, the pressure measuring device 9 may be a barometer.

[0076] In some embodiments, a compressed air source 7, a pressure regulating device 8 and a pressure measuring device 9 can be arranged on the top frame 12 of the bracket 1, one end of the gas pipeline 10 is connected to the compressed air source 7, and the other end of the gas pipeline 10 passes through the pressure regulating device 8 and the pressure measuring device 9 in sequence and then is connected to the air inlet of the first air guide channel 31.

[0077] In the technical solution of the embodiment of the present application, compressed air is introduced into the cavity 51 between the flexible packaging film 5 and the battery core mold 4 through the compressed air source 7, and the maximum value of the input air pressure is adjusted by the pressure regulating device 8. At the same time, the air pressure value is recorded in real time by the pressure measuring device 9. When the pressure inside the cavity is so large that the flexible packaging film 5 ruptures and releases pressure, the maximum pressure recorded by the pressure measuring device 9 is the pressure resistance value of the flexible packaging film 5 after packaging.

[0078] In some embodiments, a protection pad 21 is disposed on the surface of the first pressing block 2 facing the battery core mold 4 .

[0079] The protection pad 21 may be a silicone pad.

[0080] In the technical solution of the embodiment of the present application, by arranging a protective pad 21 on the surface of the first pressing block 2 facing the battery cell mold 4, it is less likely to cause air leakage in the cavity 51 of the soft packaging film 5 due to abnormal damage caused by squeezing the soft packaging film 5 by the first pressing block 2, thereby causing abnormal air pressure data.

[0081] In some embodiments, the lifting device 6 and the compressed air source 7 can be connected to and controlled by a PLC control system, so that the lifting device 6 and the compressed air source 7 can be automatically turned on or off by the PLC control system.

[0082] The method of using the soft pack battery packaging effect test device of the embodiment of the present application is as follows:

[0083] Step 1: Cover the outer surface of the battery mold 4 with a soft packaging film 5 (such as an aluminum-plastic film) and then heat seal it to make a dummy battery (test battery). It should be noted that, like the normal battery heat sealing, the tabs need to be placed at the corresponding positions of the battery mold 4.

[0084] Step 2: Place the fake battery (cell mold 4) between the first pressing block 2 and the second pressing block 3. The side of the cell mold 4 with the insertion portion 40 needs to face downward, and align with the puncture portion 33 of the second pressing block 3 with a conical structure. Start the lifting device 6 (which can be automatically controlled by the PLC control system). Under the extrusion of the first pressing block 2 and the second pressing block 3, the puncture portion 33 of the second pressing block 3 will puncture the soft packaging film (aluminum-plastic film) at the corresponding insertion portion 40 on the cell mold 4. Turn on the compressed air source 7, and the compressed air enters the second air guide channel 41 inside the cell mold 4 and diffuses into the soft packaging film cavity. At the same time, under the action of the O-ring, the compressed air will not leak. The air pressure in the soft packaging film cavity continues to rise, and finally the soft packaging film cavity cracks in the weak area of ​​the heat-sealed area, and the pressure no longer rises.

[0085] Step 3: At this time, the maximum pressure recorded by the pressure measuring device 9 (barometer) is the withstand pressure value of the flexible packaging film. Turn off the switch of the compressed air source 7 and reset the lifting device 6, remove the battery mold 4, and prepare for the next test. Remove the coated flexible packaging mold 5, and the battery mold 4 can be reused.

[0086] Table 1 below shows the aluminum-plastic film rupture pressure value of a certain 800mAh soft-pack battery cell tested by the soft-pack battery packaging effect testing device of the embodiment of the present application under different heat sealing conditions.

[0087] Table 1 The rupture pressure of aluminum-plastic film of 800mAh soft-pack battery under different heat sealing conditions

[0088] Heat sealing conditions Aluminum plastic film rupture pressure / Mpa 1(Normal condition) 0.150 2 (Temperature increase) 0.170 3 (Pressure Increased) 0.166 4 (temperature + pressure increase) 0.195

[0089] As can be seen from Table 1, the soft-pack battery packaging effect testing device of the embodiment of the present application can quickly obtain the numerical results of the pressure resistance effect of the aluminum-plastic film heat sealing under different heat sealing conditions. The pressure resistance value of the battery cell after the overall heat sealing is quickly evaluated, and the internal pressure value of the heat seal failure is obtained, so that the overall heat sealing effect of the aluminum-plastic film can be quickly obtained.

[0090] In summary, the soft-pack battery packaging effect testing device of the present application is designed through the structure of the battery mold, the first pressing block and the second pressing block. During the test, it is only necessary to position the battery mold and the second pressing block. The rupture of the aluminum-plastic film and the sealing of the rupture can be automatically completed in the process of the lifting device pushing the second pressing block onto the first pressing block and pressing the battery mold. No manual operation is required, which saves operation time and can maintain the repeatability and consistency of the entire operation. At the same time, the pressure can be automatically recorded by the pressure measuring device. It only needs to provide a compressed air source with a sufficiently large pressure source to obtain the rupture pressure of the aluminum-plastic film in one test. Compared with manually adjusting the input air pressure of different gradients and placing the fake battery cell in water to confirm whether bubbles emerge to judge whether the aluminum-plastic film is leaking, it saves a lot of operation time, and does not require water or a sink, simplifying the device.

[0091] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A soft pack battery packaging effect testing device, characterized in that: include: Bracket (1); A first pressing block (2) is arranged on the support (1); A second pressing block (3) is arranged opposite to the first pressing block (2), and the second pressing block (3) can move in a direction away from or close to the first pressing block (2), a puncture portion (33) is provided on the surface of the second pressing block (3) facing the first pressing block (2), a first air guide channel (31) is provided inside the second pressing block (3), and an air outlet of the first air guide channel (31) is located at the puncture portion (33); A cell mold (4) is arranged between the first pressing block (2) and the second pressing block (3); a soft packaging film (5) is encapsulated on the outer surface of the cell mold (4); a second air guide channel (41) is arranged inside the cell mold (4); an insertion portion (40) matching the puncturing portion (33) is arranged on the surface of the cell mold (4) facing the second pressing block (3); and an air inlet of the second air guide channel (41) is located on the insertion portion (40); when the first pressing block (2) and the second pressing block (3) clamp and press the cell mold (4), the puncturing portion (33) punctures the soft packaging film (5) and is tightly fitted with the insertion portion (40), so that the first air guide channel (31) and the second air guide channel (41) are connected; and an air outlet of the second air guide channel (41) is located on the contact surface between the cell mold (4) and the soft packaging film (5); An air source component is connected to the air inlet of the first air guide channel (31) and is used to introduce gas between the battery core mold (4) and the soft packaging film (5) through the first air guide channel (31) and the second air guide channel (41).

2. The soft pack battery packaging effect testing device according to claim 1, characterized in that: A lifting device (6) is provided on the bracket (1), and the second pressing block (3) is fixed to a movable end of the lifting device (6).

3. The soft pack battery packaging effect testing device according to claim 2, characterized in that: The lifting device (6) is a cylinder.

4. The soft pack battery packaging effect testing device according to claim 1, characterized in that: The puncturing portion (33) is in the form of a cone structure, and the air outlet of the first air guiding channel (31) is located in the middle of the cone structure.

5. The soft pack battery packaging effect testing device according to claim 1, characterized in that: The insertion portion (40) is a through-hole structure that penetrates through two surfaces of the battery core mold (4) in the thickness direction.

6. The soft pack battery packaging effect testing device according to any one of claims 1 to 5, characterized in that: A first sealing groove (32) is provided on the surface of the second pressing block (3) and around the puncturing portion (33); a second sealing groove (42) corresponding to the first sealing groove (32) is provided on the surface of the battery core mold (4) facing the second pressing block (3); and a sealing member (11) is sealedly installed between the first sealing groove (32) and the second sealing groove (42).

7. The soft pack battery packaging effect testing device according to claim 1, characterized in that: The air inlet of the first air guide channel (31) is located on the side of the second pressing block (3), and the first air guide channel (31) extends from the side of the second pressing block (3) to a side of the puncturing portion (33) facing the battery core mold (4).

8. The soft pack battery packaging effect testing device according to claim 6, characterized in that: The air outlet of the second air guide channel (41) is located on the side of the battery core mold (4) and / or on the surface along the thickness direction of the battery core mold (4). When the air outlet of the second air guide channel (41) is located on the surface along the thickness direction of the battery core mold (4) and in the direction toward the second pressing block (3), the air outlet of the second air guide channel (41) is located outside the second sealing groove (42).

9. The soft pack battery packaging effect testing device according to claim 1, characterized in that: The gas source assembly comprises: A compressed air source (7); An air delivery pipeline (10), one end of the air delivery pipeline (10) being connected to the compressed air source (7), and the other end of the air delivery pipeline (10) being connected to the air inlet of the first air guide channel (31) of the second pressing block (3); The pressure regulating device (8) and the pressure measuring device (9) are respectively arranged on the gas transmission pipeline (10).