Display panel
The display panel design with a thin film encapsulation and barrier layer addresses pad contamination issues, enhancing yield and reliability by preventing OCR glue flow and ensuring consistent bonding, thus simplifying operations and reducing scrap rates.
Patent Information
- Application Number
- CN202420876908.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-25
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-04-25
AI Technical Summary
Existing display panel manufacturing processes face issues with pad contamination and product failure due to centrifugally flowing OCR glue, leading to reduced yield and increased operational complexity, especially when using solid glue, which affects bonding strength and parallelism.
A display panel design featuring a thin film encapsulation layer and a barrier layer with specific dimensions to prevent OCR glue from contaminating the pad, integrating the thin film encapsulation and barrier layer to enhance product reliability and yield.
The integrated thin film encapsulation and barrier layer structure effectively prevents pad contamination, improving product yield and reliability by maintaining bonding strength and alignment, simplifying the process while reducing scrap rates.
Smart Images

Figure CN222126578U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of micro-displays, and specifically relates to a display panel. Background Art
[0002] In the existing display panel manufacturing process, a dispensing device is used to combine the light-emitting silicon substrate and CG (English: CoverGlass; Chinese: Cover glass; abbreviated: CG) with an OCR glue (English: Optical Clear Resin; abbreviated; OCR; Chinese: Optical Clear Glue). Since the OCR glue is in liquid form, the subsequent chipping operation requires centrifugal drying of the water, which will cause part of the OCR glue to flow and be thrown onto the pad, easily causing pad contamination. In severe cases, it affects the cleanliness of the pad, causing product failure and scrapping, and affecting product yield.
[0003] Therefore, it is necessary to fill glue into the dispensing syringe through the tooling accessories, and use air pressure to squeeze the OCR glue filled in the syringe through the dispensing needle onto the TFE (English: Thin Film Encapsulation; abbreviated as: TFE; Chinese: Thin Film Encapsulation), and then place the CG on the TFE for assembly and bonding, and then place the bonded product under ultraviolet light for curing and then cracking.
[0004] However, in the production process of splitting, pure water is needed when cutting the splits. In order to keep the chip clean and pollution-free after splitting, high-speed centrifugal spinning is required to dry the pure water to avoid pure water residue on the chip during the entire production process that affects subsequent operations; because the splitting centrifugation will cause the OCR glue to separate and contaminate the pad, such as Figure 2 As shown by the arrow in the middle, the residual OCR glue on the pad will cause pollution. In subsequent welding operations, the product will be scrapped due to the residual OCR glue on the pad.
[0005] In the prior art, there is a way to improve this type of anomaly:
[0006] Solid glue is used to bond CG and TFE. However, the above method will cause a difference in parallelism between CG and TFE due to the poor fluidity of solid glue. In addition, this method does not have enough bonding strength when using solid glue to bond TFE. Compared with OCR glue, solid glue is too expensive and causes chip function failure. Therefore, this method will increase the difficulty of operation and product performance.
[0007] For example, the patent document with publication number CN111048686A discloses a display device and a packaging method using the display device, wherein the display device reserves space between the cover plate and the end surface of the adhesive material, and then fills the high water-resistance polymer material between the cover plate and the substrate and solidifies it, so that water vapor and oxygen first pass through the high water-resistance polymer material, and then enter the moisture-absorbing adhesive layer containing a desiccant, thereby slowing down the packaging failure process of the display device and increasing the life of the display device. The technical solution disclosed in the patent document also cannot solve the technical problems described above. Utility Model Content
[0008] The utility model aims to solve at least one of the technical problems existing in the prior art. To this end, the utility model provides a display panel, the purpose of which is to improve the product yield.
[0009] In order to achieve the above-mentioned purpose, the technical solution adopted by the utility model is: a display panel includes a solder pad, a thin film encapsulation layer, an OCR glue layer and a barrier layer arranged between the solder pad and the OCR glue layer.
[0010] The thin film encapsulation layer and the barrier layer are integrally formed.
[0011] The distance between the pad and the barrier layer is 300-350 um.
[0012] The height of the barrier layer is 3-5 um.
[0013] The width of the barrier layer is 1-3 um.
[0014] The thin film encapsulation layer is located between the OCR glue layer and the silicon substrate, and the OCR glue layer is located between the cover glass and the thin film encapsulation layer.
[0015] The display panel of the utility model can effectively improve the reliability and yield of the product by arranging a barrier layer to prevent the OCR glue from centrifugally flowing toward the pad and causing contamination of the pad. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] This specification includes the following drawings, which show the following contents:
[0017] Figure 1 It is a structural schematic diagram of the display panel of the utility model;
[0018] Figure 2 It is a schematic diagram of the structure of a display panel in the prior art;
[0019] The markings in the figure are: 1. Silicon substrate; 2. Anode; 3. Thin film encapsulation layer; 4. OCR glue layer; 5. Cover glass; 6. Solder pad; 7. Barrier layer; 8. Display device. DETAILED DESCRIPTION
[0020] The specific implementation methods of the utility model are further explained in detail below with reference to the accompanying drawings through the description of embodiments, with the aim of helping technicians in the field to have a more complete, accurate and in-depth understanding of the concept and technical solution of the utility model and facilitating its implementation.
[0021] like Figure 1 As shown, the utility model provides a display panel, including a silicon substrate 1, a display device 8, an anode 2, a cover glass 5, a solder pad 6, a thin film encapsulation layer 3, an OCR glue layer 4 and a barrier layer 7 arranged between the solder pad 6 and the OCR glue layer 4.
[0022] Specifically, if Figure 1 As shown, the anode 2, the display device 8, the thin film encapsulation layer 3 and the pad 6 are arranged on the silicon substrate 1, the thin film encapsulation layer 3 covers the display device 8, the display device 8 is located between the anode 2 and the thin film encapsulation layer 3, the thin film encapsulation layer 3 is located between the OCR glue layer 4 and the silicon substrate 1, and the OCR glue layer 4 is located between the cover glass 5 and the thin film encapsulation layer 3. The thin film encapsulation layer 3 and the barrier layer 7 are integrally formed, and the thin film encapsulation layer 3 is connected to one end of the barrier layer 7, and the two are made of the same material.
[0023] The silicon substrate 1 is mainly used to provide a supporting foundation for the chip, the anode 2 is used to provide current transmission to the display device 8, the thin film encapsulation layer 3 is used to protect the display device 8 and the anode 2 from damage, the OCR glue layer 4 is used to bond the cover glass 5 and the thin film encapsulation layer 3, the cover glass 5 is used to protect the thin film encapsulation layer 3 from damage, and the pad 6 is used to conduct the anode 2.
[0024] Preferably, the height of the barrier layer 7 is 3-5um, the height of the barrier layer 7 refers to the distance between the top surface and the bottom surface of the barrier layer 7, the bottom surface of the barrier layer 7 is connected to the silicon substrate 1, the width of the barrier layer 7 is 1-3um, and the width direction of the barrier layer 7 is perpendicular to its height direction.
[0025] Preferably, the distance between the pad 6 and the barrier layer 7 is 300-350 um to prevent the pad 6 from colliding with the barrier layer 7 during welding.
[0026] The display panel with the above structure can effectively improve the failure resistance of the product by changing the structure of the thin film package, and has the characteristics of simple process and significantly improved yield.
[0027] The above is an exemplary description of the utility model in conjunction with the accompanying drawings. Obviously, the specific implementation of the utility model is not limited to the above-mentioned method. As long as various non-substantial improvements are made using the method concept and technical solution of the utility model; or the above concept and technical solution of the utility model are directly applied to other occasions without improvement, they are all within the protection scope of the utility model.
Claims
1. A display panel, comprising a pad, a thin film encapsulation layer and an OCR glue layer, characterized in that: It also includes a barrier layer arranged between the soldering pad and the OCR glue layer.
2. The display panel according to claim 1, characterized in that: The thin film encapsulation layer and the barrier layer are integrally formed.
3. The display panel according to claim 1, wherein: The distance between the pad and the barrier layer is 300-350 um.
4. The display panel according to any one of claims 1 to 3, characterized in that: The height of the barrier layer is 3-5 um.
5. The display panel according to any one of claims 1 to 3, characterized in that: The width of the barrier layer is 1-3 um.
6. The display panel according to any one of claims 1 to 3, characterized in that: The thin film encapsulation layer is located between the OCR glue layer and the silicon substrate, and the OCR glue layer is located between the cover glass and the thin film encapsulation layer.
Citation Information
Patent Citations
Display device and packaging method adopting display device
CN111048686A