Sand finish paint coating structure
By sprinkling points on the surface of the sand paint layer, and adding a transparent matte paint layer, the problems of consumer aesthetic fatigue and high manufacturer development costs are solved, and visual effects are updated and production costs are reduced.
Patent Information
- Application Number
- CN202421328778.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-11
- Publication Date
- 2025-02-25
- Estimated Expiration
- 2034-06-11
AI Technical Summary
The existing sand topcoat coating structure causes aesthetic fatigue for consumers, and the cost of manufacturers to develop new products is high.
Sprinkle points on the surface of the sand paint layer, and add a transparent matte paint layer to form a new visual effect.
Eliminates consumers' aesthetic fatigue with existing sand topcoat coating structures, reduces the development and time costs of manufacturers, and does not require replacement or redesign of production lines.
Smart Images

Figure CN222524426U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of coating structure technology, in particular to a sand surface paint coating structure. Background Art
[0002] Medium density fiberboard, generally refers to medium density fiberboard, is a kind of man-made board. In China, medium density fiberboard is made of agricultural waste or small firewood as the main raw materials, and its main components are wood fiber, resin glue, etc. It is an environmentally friendly furniture building material substitute for logs after hot grinding, drying, gluing, paving, hot pressing, post-treatment, and sanding.
[0003] Although MDF has the advantages of being relatively cheap compared to logs, easy to process, uniform in material, good in physical properties, good in thermal insulation, no aging, and strong in adhesion, as people's material level improves, their aesthetics of building materials also gradually improves, so building materials companies begin to set up coating structures on MDF to increase the aesthetics of MDF. At present, there are coating structures on the market that coat MDF with sand paint. The coating structure has excellent texture and better visual effects, but over time, consumers will experience aesthetic fatigue, leading to a decline in sales. For this reason, manufacturers generally develop a new product, but developing a new product requires manpower and material resources and a long development time, resulting in increased costs. Therefore, it is necessary to propose a new solution to solve the above problems. Utility Model Content
[0004] In view of this, the present invention aims to solve the deficiencies in the prior art, and its main purpose is to provide a sand-finish paint coating structure, which can effectively solve the problem of consumers' aesthetic fatigue of sand-finish paint coating structures, as well as the problem of high development costs for manufacturers to develop new products.
[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0006] A sand surface paint coating structure comprises a substrate, a first primer layer, a first white primer layer, a second white primer layer, a sand surface paint layer and a transparent matte paint layer; the substrate is a medium-density fiberboard, and the surface of the substrate has a first polishing layer; the first primer layer is coated on the first polishing layer, and the first primer layer has a second polishing layer; the first white primer layer is coated on the second polishing layer, and the surface of the first white primer layer has a third polishing layer; the second white primer layer is coated on the third polishing layer, and the surface of the second white primer layer has a fourth polishing layer; the sand surface paint layer is coated on the fourth polishing layer, and the surface of the sand surface paint layer is formed with a sprinkled surface by a sprinkled method; the transparent matte paint layer is coated on the sand surface paint layer.
[0007] As a preferred embodiment, the model of the first primer layer is TB31007A.
[0008] As a preferred solution, the first white primer layer and the second white primer layer are both water-based two-component white primers, and the model number is TB66005.
[0009] As a preferred solution, the sand topcoat layer is a water-based two-component sand topcoat, and its model is TB86011-10.
[0010] As a preferred solution, the transparent matte paint layer is a water-based two-component transparent matte paint, and its model is TB82009-10.
[0011] Compared with the prior art, the utility model has obvious advantages and beneficial effects. Specifically, it can be seen from the above technical solution that:
[0012] A sprinkled surface is formed by sprinkling dots on the surface of the sand paint layer. The design of the sprinkled surface brings a new visual effect to the existing sand paint coating structure, which can eliminate consumers' aesthetic fatigue of the existing sand paint coating structure. At the same time, manufacturers do not need to redevelop new products or new decorative paints. The production line only needs to add a process step without replacing or redesigning the production line, which greatly reduces the manufacturer's development cost, labor cost and time cost.
[0013] In order to more clearly illustrate the structural features and functions of the present invention, the present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments: BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a cross-sectional view of a preferred embodiment of the utility model.
[0015] Description of the accompanying drawings:
[0016] 10. Base material 11. First polishing layer
[0017] 20. First primer layer 21. Second polishing layer
[0018] 30. First white primer layer 31. Third polishing layer
[0019] 40. Second white primer layer 41. Fourth polishing layer
[0020] 50. Sand the surface with paint 51. Sprinkle some paint on the surface
[0021] 60. Transparent matte paint layer. DETAILED DESCRIPTION
[0022] Please refer to Figure 1 As shown, it shows the specific structure of a preferred embodiment of the utility model, including a substrate 10, a first primer layer 20, a first white primer layer 30, a second white primer layer 40, a sand surface paint layer 50 and a transparent matte paint layer 60.
[0023] The substrate 10 is a medium fiberboard, and a first polishing layer 11 is provided on the surface of the substrate 10 .
[0024] The first primer layer 20 is coated on the first polishing layer 11 , and the first primer layer 20 has a second polishing layer 21 . In the present embodiment, the model of the first primer layer 20 is TB31007A.
[0025] The first white primer layer 30 is coated on the second polishing layer 21 , and the surface of the first white primer layer 30 has a third polishing layer 31 . In the present embodiment, the first white primer layer 30 is a water-based two-component white primer, and its model is TB66005.
[0026] The second white primer layer 40 is coated on the third polishing layer 31 , and the surface of the second white primer layer 40 has a fourth polishing layer 41 . In this embodiment, the second white primer layer 40 is a water-based two-component white primer, and its model is TB66005.
[0027] The sand paint layer 50 is coated on the fourth polishing layer 41, and a sprinkled surface 51 is formed on the surface of the sand paint layer 50 by a sprinkled method; in this embodiment, the sand paint layer 50 is a water-based two-component sand paint, and its model is TB86011-10.
[0028] The transparent matte paint layer 60 is coated on the sand surface paint layer 50; in this embodiment, the transparent matte paint layer 60 is a water-based two-component transparent matte paint, and its model is TB82009-10.
[0029] The production process of this embodiment is described in detail as follows:
[0030] First, take a substrate 10 that has been fully dried and cured, with its wood moisture content controlled below 11%, and use 240# sandpaper to sand the entire white body once, without defects or horizontal sand marks. Then, spray the first sanding layer 11 evenly once, dry for more than 60 minutes to form a first primer layer 20, and sand it smooth with 400# sandpaper to form a second sanding layer 21; then pre-mix the curing agent and water according to the specified ratio, pour it into the topcoat, stir evenly, filter through 120 mesh, spray 2 crosses evenly, and the panel is sprayed without sagging as a whole. Dry at a temperature of 30-40℃ for not less than 4 hours, and control the humidity at 40%-60% to form the first white primer layer 30, and use 400# zinc powder sandpaper to polish it flat, without leaking sand, and all parts and edges and corners cannot be sanded through, so as to form the third polishing layer 31; then continue to pre-mix the curing agent and water according to the specified ratio, and then pour it into the topcoat and stir evenly, filter it with 120 mesh, and evenly spray 2 crosses. The panel is sprayed without sagging as a whole, and dried at a temperature of 30-40℃ for not less than 4 hours, and control the humidity at 40%-60 %, forming a second white primer layer 40, which is polished with 400# zinc powder sandpaper to make it smooth, without leaking sand, and without sanding through all parts, edges and corners, so as to form a fourth polishing layer 41; then, the curing agent and water are pre-mixed evenly according to the prescribed ratio, and then poured into the topcoat and stirred evenly, filtered through 120 mesh, and all are evenly sprayed with 2 crosses, and the panel is sprayed without sagging as a whole, and dried at a temperature of 30-40°C for not less than 4 hours, and the humidity is controlled at 40%-60%, to form a sand topcoat layer 50, and then sprinkle points evenly on the surface of the sand topcoat layer 50 with reference to the color plate , forming a dotted surface 51, the color of the dot can be a single color, or it can be a variety of different colors of dotted; finally, pre-mix the curing agent and water according to the prescribed ratio, pour it into the topcoat, stir it evenly, filter it through 200 mesh, spray 2 crosses evenly, spray the whole panel without sagging, level it at room temperature for 8-10 minutes, and dry it in a drying room with good air flow for at least 4 hours, and the temperature is guaranteed to be 30-40℃, the humidity is controlled at 40%-60%, and the paint film is cured for at least 8 hours to form a transparent matte paint layer 60, which is packaged and shipped.
[0031] The design focus of the utility model is: a sprinkled surface is formed by sprinkling dots on the surface of the sand surface paint layer. The design of the sprinkled surface brings a new visual effect to the existing sand surface paint coating structure, which can eliminate consumers' aesthetic fatigue of the existing sand surface paint coating structure. At the same time, manufacturers do not need to redevelop new products or new decorative paints. The production line only needs to add one process step, and there is no need to replace or redesign the production line, which greatly reduces the manufacturer's development cost, labor cost and time cost.
[0032] The above description is only a preferred embodiment of the present invention and does not limit the technical scope of the present invention. Therefore, any slight modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A sand topcoat coating structure, characterized in that: It includes a substrate, a first primer layer, a first white primer layer, a second white primer layer, a sand surface paint layer and a transparent matte paint layer; the substrate is a medium-density fiberboard, and the surface of the substrate has a first polished layer; the first primer layer is coated on the first polished layer, and the first primer layer has a second polished layer; the first white primer layer is coated on the second polished layer, and the surface of the first white primer layer has a third polished layer; the second white primer layer is coated on the third polished layer, and the surface of the second white primer layer has a fourth polished layer; the sand surface paint layer is coated on the fourth polished layer, and the surface of the sand surface paint layer is formed with a sprinkled surface by sprinkling; the transparent matte paint layer is coated on the sand surface paint layer.
2. The sand topcoat coating structure according to claim 1, characterized in that: The model of the first primer layer is TB31007A.
3. The sand topcoat coating structure according to claim 1, characterized in that: The first white primer layer and the second white primer layer are both water-based two-component white primers, and the model number is TB66005.
4. The sand topcoat coating structure according to claim 1, characterized in that: The sand topcoat layer is a water-based two-component sand topcoat, and its model is TB86011-10.
5. The sand topcoat coating structure according to claim 1, characterized in that: The transparent matte paint layer is a water-based two-component transparent matte paint, and its model is TB82009-10.