Extruder for processing polyester type powder coating

By designing a sealing mechanism and a motor-driven conveying system in the extruder for polyester powder coating processing, the problem of coatings being easily contaminated by impurities during the extrusion process is solved, and higher quality paint discharge and more effective material transportation are achieved.

CN222538242UActive Publication Date: 2025-02-28江苏幻豹新材料科技有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420510246.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-16
Publication Date
2025-02-28
Estimated Expiration
2034-03-16

AI Technical Summary

Technical Problem

Existing polyester powder coatings are susceptible to air impurities and dust contamination during the extrusion process, resulting in a decrease in the quality of the coating.

Method used

An extruder for processing polyester powder coating is designed, and a sealing mechanism is used to open the discharge hole through the separation of the rubber plug and the discharge hole to prevent impurities from entering. At the same time, the effective extrusion and transportation of materials are achieved through the motor-driven rotating shaft and the transmission track.

Benefits of technology

It effectively prevents impurities in the air from entering the extrusion box, improves the purity and quality of the paint, and ensures smooth discharge of materials and avoids blockage of the inner wall of the extrusion box.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222538242U_ABST
    Figure CN222538242U_ABST
Patent Text Reader

Abstract

The utility model discloses an extruder for polyester type powder coating processing, which comprises an extrusion box, a discharge hole is arranged on one side of the extrusion box, a placing frame is arranged at the top of the extrusion box, a processing barrel is fixedly arranged on the inner wall of the placing frame, a plugging mechanism is arranged on one side of the extrusion box, and the plugging mechanism comprises a mounting plate, a rubber plug, a connecting rod and a fixing plate. And a fixing plate is slidably connected to one side of the extrusion box, a connecting rod is fixedly mounted on one side of the fixing plate, a mounting plate is fixedly mounted at one end of the connecting rod, and a rubber plug matched with the discharging hole is fixedly mounted on one side of the mounting plate. A fixing plate moves to enable a connecting rod to move, a rubber plug can be driven by a mounting plate to be separated from a discharging hole, and the discharging hole is opened, so that the discharging hole can be opened, better discharging of the extrusion box is facilitated, and impurities in air are prevented from floating into the extrusion box through the discharging hole; and the coating in the extrusion box can be better protected.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of an extruder for processing polyester type powder coatings, in particular to an extruder for processing polyester type powder coatings. Background Art

[0002] Powder polyester coating is a coating made of amorphous resin prepared with isophthalic acid and neopentyl glycol as main monomers. It is brittle, solid and has a high glass transition temperature. The coating film is hard and tough and has a low cross-linking density. After processing, the coating needs to be extruded.

[0003] At present, when the paint is extruded, most of the existing ones are discharged directly from the discharge hole. After the discharge hole discharges the paint, it is not sealed, which makes it easy for impurities and dust in the air to enter the extrusion box through the discharge hole and pollute the paint. Utility Model Content

[0004] In order to solve the above problems, the purpose of the utility model is to provide an extruder for processing polyester powder coatings to solve the problems raised in the above background technology.

[0005] To achieve the above-mentioned purpose, the utility model proposes an extruder for processing polyester powder coatings, comprising an extrusion box, a discharge hole is opened on one side of the extrusion box, a placement rack is provided on the top of the extrusion box, and a processing barrel is fixedly provided on the inner wall of the placement rack;

[0006] A sealing mechanism is provided on one side of the extrusion box, and the sealing mechanism includes a mounting plate, a rubber plug, a connecting rod and a fixed plate. A fixing plate is slidably connected to one side of the extrusion box, a connecting rod is fixedly installed on one side of the fixed plate, a mounting plate is fixedly installed on one end of the connecting rod, and a rubber plug matching the discharge hole is fixedly installed on one side of the mounting plate.

[0007] In one example, a motor is fixedly mounted on one side of the extrusion box, a rotating shaft is fixedly mounted on the output shaft of the motor, and the rotating shaft penetrates and extends into the extrusion box.

[0008] In one example, a transmission shoe is fixedly mounted on the outer ring of the rotating shaft located in the extrusion box.

[0009] In one example, a rotating rod is rotatably connected to one side of the extrusion box, and a crank is fixedly mounted on one end of the rotating rod.

[0010] In one example, an extrusion plate is fixedly mounted on the outer ring of the rotating rod, and the extrusion plate is connected to the fixed plate.

[0011] In one example, a feed pipe penetrating through and extending into the extrusion box is fixedly installed at the bottom end of the processing barrel, and a control valve is fixedly installed on the outer ring of the feed pipe.

[0012] The polyester powder coating processing extruder proposed by the utility model can bring the following beneficial effects:

[0013] 1. This polyester powder coating processing extruder moves a fixing plate to move a connecting rod, and the rubber plug can be driven to separate from the discharge hole through the mounting plate to open the discharge hole, thereby opening the discharge hole, making it easier for the extrusion box to discharge the material, and preventing impurities in the air from floating into the extrusion box through the discharge hole, thereby better protecting the coating in the extrusion box.

[0014] 2. This polyester powder coating processing extruder can drive the rotating shaft to rotate by starting the motor, and drive the transmission shoe to rotate, so that the material transported to the extrusion box by the feeding pipe can be extruded and transported to the discharge hole for discharge, thereby preventing the material from being blocked on the inner wall of the extrusion box and better discharging the material in the extrusion box. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation on the present invention. In the drawings:

[0016] Figure 1 It is a schematic diagram of the structure of the utility model;

[0017] Figure 2 This is a schematic diagram of the cross-sectional structure of the extrusion box of the utility model;

[0018] Figure 3 This is a schematic diagram of the connecting rod connection structure of the utility model.

[0019] In the figure: 1. extrusion box; 2. placement rack; 3. processing barrel; 4. discharge pipe; 5. control valve; 6. motor; 7. rotating shaft; 8. transmission shoe; 9. discharge hole; 10. mounting plate; 11. rubber plug; 12. connecting rod; 13. fixing plate; 14. extrusion plate; 15. rotating rod; 16. crank. DETAILED DESCRIPTION

[0020] In order to more clearly illustrate the overall concept of the present invention, a detailed description is given below in the form of examples in conjunction with the accompanying drawings.

[0021] like Figure 1 to Figure 3As shown, the embodiment of the utility model provides an extruder for processing polyester powder coatings, comprising an extrusion box 1, a discharge hole 9 is opened on one side of the extrusion box 1, a placement rack 2 is provided on the top of the extrusion box 1, and a processing barrel 3 is fixedly provided on the inner wall of the placement rack 2;

[0022] A sealing mechanism is provided on one side of the extrusion box 1, and the sealing mechanism includes a mounting plate 10, a rubber plug 11, a connecting rod 12 and a fixed plate 13. The fixed plate 13 is slidably connected to one side of the extrusion box 1, the connecting rod 12 is fixedly installed on one side of the fixed plate 13, the mounting plate 10 is fixedly installed on one end of the connecting rod 12, and a rubber plug 11 matching the discharge hole 9 is fixedly installed on one side of the mounting plate 10.

[0023] Specifically, a motor 6 is fixedly installed on one side of the extrusion box 1, and a rotating shaft 7 is fixedly installed on the output shaft of the motor 6. The rotating shaft 7 penetrates and extends into the extrusion box 1. The motor 6 drives the rotating shaft 7 to rotate, and the rotating shaft 7 drives the transmission shoe 8 to rotate to extrude the material in the extrusion box 1.

[0024] Specifically, a transmission shoe 8 is fixedly installed on the outer ring of the rotating shaft 7 located in the extrusion box 1 , and the material in the extrusion box 1 is transported and extruded through the transmission shoe 8 .

[0025] Specifically, a rotating rod 15 is rotatably connected to one side of the extrusion box 1 , and a crank 16 is fixedly installed at one end of the rotating rod 15 . The crank 16 is fixed by the rotating rod 15 , and the rotation of the crank 16 drives the extrusion plate 14 to move through the rotating rod 15 .

[0026] Specifically, an extrusion plate 14 is fixedly installed on the outer ring of the rotating rod 15, and the extrusion plate 14 is connected to the fixed plate 13. The fixed plate 13 is squeezed by the extrusion plate 14, and the mounting plate 10 is driven to move by the connecting rod 12, so that the rubber plug 11 can be separated from the discharge hole 9, and the discharge hole 9 can be opened.

[0027] Specifically, a feed pipe 4 penetrating through and extending into the extrusion box 1 is fixedly installed at the bottom end of the processing barrel 3 , and a control valve 5 is fixedly installed on the outer ring of the feed pipe 4 . The material in the processing barrel 3 is processed through the feed pipe 4 , and the control valve 5 controls the feed pipe 4 .

[0028] Working principle: After the processing barrel 3 is processed, the control valve 5 is rotated to open the discharge pipe 4. At this time, the material in the processing barrel 3 is transported to the extrusion box 1. At this time, the crank 16 is rotated to drive the extrusion plate 14 to rotate through the rotating rod 15, and the fixed plate 13 is squeezed, which will move the connecting rod 12, and the rubber plug 11 can be driven to separate from the discharge hole 9 through the mounting plate 10, and the discharge hole 9 is opened. At this time, the motor 6 is started again to drive the rotating shaft 7 to rotate, and the transmission shoe 8 is driven to rotate, so that the material transported to the extrusion box 1 by the discharge pipe 4 can be squeezed and transported to the discharge hole 9 for discharge, so as to prevent the material from being blocked on the inner wall of the extrusion box 1, and the material can be better extruded and discharged.

[0029] Each embodiment in this specification is described in a progressive manner, and the same or similar parts between the embodiments can be referred to each other, and each embodiment focuses on the differences from other embodiments. In particular, for the system embodiment, since it is basically similar to the method embodiment, the description is relatively simple, and the relevant parts can be referred to the partial description of the method embodiment.

[0030] The above description is only an embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent substitution, improvement, etc. made within the spirit and principle of the present invention shall be included in the scope of the claims of the present invention.

Claims

1. An extruder for processing polyester powder coating, comprising an extrusion box (1), a discharge hole (9) being provided on one side of the extrusion box (1), a placement frame (2) being provided on the top of the extrusion box (1), and a processing barrel (3) being fixedly provided on the inner wall of the placement frame (2); Features: A sealing mechanism is provided on one side of the extrusion box (1), and the sealing mechanism comprises a mounting plate (10), a rubber plug (11), a connecting rod (12) and a fixing plate (13); one side of the extrusion box (1) is slidably connected to the fixing plate (13); one side of the fixing plate (13) is fixedly mounted with the connecting rod (12); one end of the connecting rod (12) is fixedly mounted with the mounting plate (10); and one side of the mounting plate (10) is fixedly mounted with a rubber plug (11) matching the discharge hole (9).

2. The extruder for processing polyester powder coating according to claim 1, characterized in that: A motor (6) is fixedly mounted on one side of the extrusion box (1), a rotating shaft (7) is fixedly mounted on the output shaft of the motor (6), and the rotating shaft (7) passes through and extends into the extrusion box (1).

3. The extruder for processing polyester powder coating according to claim 2, characterized in that: The outer ring of the rotating shaft (7) located inside the extrusion box (1) is fixedly mounted with a transmission shoe (8).

4. The extruder for processing polyester powder coating according to claim 2, characterized in that: A rotating rod (15) is rotatably connected to one side of the extrusion box (1), and a crank (16) is fixedly mounted on one end of the rotating rod (15).

5. The extruder for processing polyester powder coating according to claim 4, characterized in that: An extrusion plate (14) is fixedly mounted on the outer ring of the rotating rod (15), and the extrusion plate (14) is connected to the fixed plate (13).

6. The extruder for processing polyester powder coating according to claim 1, characterized in that: A feed pipe (4) is fixedly mounted on the bottom end of the processing barrel (3) and penetrates through and extends into the extrusion box (1), and a control valve (5) is fixedly mounted on the outer ring of the feed pipe (4).