High-strength metal material gas-phase antirust film
By designing a multi-layer structure high-strength metal material gas-phase anti-rust film, the problem of winding several circles of anti-rust film increases volume is solved, and the goal of reducing the amount, reducing temporary space and providing multiple protection effects is achieved.
Patent Information
- Application Number
- CN202421320976.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-11
- Publication Date
- 2025-03-21
- Estimated Expiration
- 2034-06-11
AI Technical Summary
Wrapting several circles of anti-rust film will increase the volume and affect storage and space utilization.
A high-strength metal material gas-phase anti-rust film is designed, including a fixed cylinder and a membrane body installed on the circular outer wall of the fixed cylinder. The membrane body is equipped with a multi-layer structure such as an anti-rust film body, a base layer, an wear-resistant layer, an anti-static layer, a flame retardant layer, a heat-resistant layer and a waterproof layer.
Through the multi-layer structure design, the hardness and wear resistance of the anti-rust film are increased, the amount of anti-rust film is reduced, the temporary space for high-strength metal materials after wrapping is reduced, and the protection effects of anti-static, fire, waterproof and high temperature resistance are provided.
Smart Images

Figure CN222645545U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field related to anti-rust films, and specifically relates to a high-strength metal material vapor phase anti-rust film. Background Art
[0002] Vapor phase anti-rust film is a new generation of innovative high-tech products based on the combination of polymer materials and VCI vapor phase anti-rust technology. After the anti-rust items are packaged and sealed using the film, the VCI contained in the film body begins to sublimate and volatilize anti-rust gas factors, which diffuse and penetrate into the surface of the anti-rust items and adsorb on them, forming a dense protective film layer with a thickness of a single molecule, isolating various factors that induce rust from contact with the surface of the anti-rust items, thereby effectively preventing the occurrence of rust. However, when wrapping high-strength metal materials, it is usually necessary to wrap the anti-rust film around the high-strength metal surface for several times to reduce the thickness during transportation or storage to avoid puncture or abrasion. Wrapping the anti-rust film several times will increase the volume, which will affect storage and space utilization. Utility Model Content
[0003] The utility model aims to provide a high-strength metal material vapor phase anti-rust film to solve the problem that winding the anti-rust film several times in the above background technology will increase the volume and affect the storage and space utilization.
[0004] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a high-strength metal material vapor phase anti-rust film, comprising a fixed cylinder and a film body installed on the circular outer wall of the fixed cylinder;
[0005] The film body comprises an anti-rust film body a, a base layer, and an anti-rust film body b;
[0006] The base layer is located at the center of the membrane body;
[0007] The upper outer wall of the base layer is provided with an anti-rust film body a, and the lower outer wall of the base layer is provided with an anti-rust film body b;
[0008] A wear-resistant layer is disposed on the upper side of the anti-rust film body a, and an antistatic layer is disposed on the lower side of the wear-resistant layer.
[0009] Preferably, the lower outer wall of the antistatic layer is provided with a thickening layer a, and the lower outer wall of the thickening layer a is provided with a connecting layer.
[0010] Preferably, the outer wall of the lower end of the connecting layer is provided with a thickening layer b, and the wear-resistant layer, the antistatic layer, the thickening layer a, the connecting layer and the thickening layer b are each provided with two.
[0011] Preferably, the two wear-resistant layers, the antistatic layer, the thickening layer a, the connecting layer and the thickening layer b are respectively arranged on the upper and lower sides of the base layer with the base layer as the central axis of symmetry, and the surface of the antistatic layer is coated with antistatic coating.
[0012] Preferably, a flame retardant layer is provided on the upper side of the anti-rust film body a, and the flame retardant layer includes a heat insulation layer, a heat-resistant layer, a fireproof layer and a waterproof layer.
[0013] Preferably, a heat insulation layer is provided on the lower side of the flame retardant layer, and a heat-resistant layer is provided on the outer wall of the lower end of the heat insulation layer.
[0014] Preferably, the lower outer wall of the heat-resistant layer is provided with a fireproof layer, and the lower outer wall of the fireproof layer is provided with a waterproof layer.
[0015] Preferably, two thermal insulation layers, heat-resistant layers, fireproof layers and waterproof layers are each provided, and the two thermal insulation layers, heat-resistant layers, fireproof layers and waterproof layers are respectively provided on the upper and lower sides of the base layer with the base layer as the central axis of symmetry.
[0016] Compared with the prior art, the utility model provides a high-strength metal material vapor phase anti-rust film, which has the following beneficial effects:
[0017] 1. By installing the wear-resistant layer and the antistatic layer, the wear-resistant layer can increase the hardness and wear resistance of the anti-rust film, extend the service life, and reduce the amount of anti-rust film when wrapping high-strength metal materials. Just wrap with a small amount of anti-rust film to achieve the protective effect of the traditional thick anti-rust film, and reduce the temporary space of the high-strength metal material after wrapping the anti-rust film. The antistatic layer can effectively play an anti-static role, preventing the dust and impurities in the environment attached to the surface of the anti-rust film, as well as the influence of water vapor and static electricity on the anti-rust film and causing damage.
[0018] 2. By installing a flame retardant layer, a heat-resistant layer and a waterproof layer, the flame retardant layer can effectively prevent the occurrence and spread of fire, improve the flame retardant properties of the material, protect the safety of equipment and personnel, and reduce the losses caused by fire. The heat-resistant layer can ensure the normal use of the anti-rust film in a high temperature environment to avoid the occurrence of self-combustion due to excessive temperature. The waterproof layer can prevent liquids from penetrating the anti-rust film and contacting the high-light metal materials wrapped by it. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 The utility model is a schematic diagram of the structure of a high-strength metal material vapor phase anti-rust film.
[0020] Figure 2 It is a schematic diagram of the partial structure of the membrane area section of the utility model.
[0021] Figure 3It is a schematic diagram of the partial structure of the cross section of the wear-resistant layer area of the utility model.
[0022] Figure 4 It is a schematic diagram of the cross-sectional structure of the flame retardant layer area of the present utility model.
[0023] In the figure: 1. fixing tube; 2. membrane body; 3. wear-resistant layer; 4. flame-retardant layer; 5. anti-rust membrane body a; 6. base layer; 7. anti-rust membrane body b; 8. antistatic layer; 9. thickening layer a; 10. connecting layer; 11. thickening layer b; 12. heat-insulating layer; 13. heat-resistant layer; 14. fire-proof layer; 15. waterproof layer. DETAILED DESCRIPTION
[0024] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0025] The utility model provides Figure 1-3 A high-strength metal material vapor phase anti-rust film shown includes a fixed tube 1 and a film body 2 installed on the circular outer wall of the fixed tube 1;
[0026] The film body 2 includes an anti-rust film body a5, a base layer 6, and an anti-rust film body b7;
[0027] The base layer 6 is located at the center of the membrane body 2;
[0028] The upper outer wall of the base layer 6 is provided with an anti-rust film body a5, and the lower outer wall of the base layer 6 is provided with an anti-rust film body b7. When the high-strength metal material is subjected to anti-rust treatment, one side of the film body 2 can be pulled out from the fixed cylinder 1, and the high-strength metal material is wrapped. After the wrapping is complete, the film body 2 can be cut by a cutter. The anti-rust film body a5 and the anti-rust film body b7 inside the film body 2 can emit anti-rust gas factors through the VCI material inside them, diffuse and penetrate to the surface of the anti-rusted object and adsorb thereon, forming a dense protective film layer with a thickness of a single molecule, isolating various factors inducing rust from contacting the surface of the anti-rusted object, thereby effectively preventing the occurrence of rust;
[0029] A wear-resistant layer 3 is provided on the upper side of the anti-rust film body a5, and an antistatic layer 8 is provided on the lower side of the wear-resistant layer 3. When wrapping high-strength metal materials, the wear-resistant layer 3 can increase the surface friction and reduce the speed at which the film body 2 ruptures due to friction under the influence of external force. The antistatic layer 8 can increase the antistatic coefficient of the surface of the film body 2 and avoid the accumulation of dust on the surface of the film body 2.
[0030] like Figure 3 As shown, the lower outer wall of the antistatic layer 8 is provided with a thickening layer a9, the lower outer wall of the thickening layer a9 is provided with a connecting layer 10, the lower outer wall of the connecting layer 10 is provided with a thickening layer b11, and two wear-resistant layers 3, antistatic layers 8, thickening layers a9, connecting layers 10 and thickening layers b11 are each provided. The two wear-resistant layers 3, antistatic layers 8, thickening layers a9, connecting layers 10 and thickening layers b11 are respectively arranged on the upper and lower sides of the base layer 6 with the base layer 6 as the central axis of symmetry, and the surface of the antistatic layer 8 is coated with antistatic coating.
[0031] The thickening layer a9, the connecting layer 10 and the thickening layer b11 can increase the tensile strength of the membrane 2 itself, and when punctured by a sharp object, the effect of the puncture on the membrane 2 can be reduced, and the speed of damage to the membrane 2 itself can be reduced.
[0032] like Figure 4 As shown, a flame retardant layer 4 is arranged on the upper side of the anti-rust film body a5, and the flame retardant layer 4 includes a heat insulation layer 12, a heat resistant layer 13, a fireproof layer 14 and a waterproof layer 15. A heat insulation layer 12 is arranged on the lower side of the flame retardant layer 4, and a heat resistant layer 13 is arranged on the outer wall of the lower end of the heat insulation layer 12.
[0033] The presence of the heat insulation layer 12 can reduce the conduction of heat energy to the anti-rust film body a5, reduce the impact of external heat sources on the body, and protect the anti-rust film body a5 from damage due to overheating. The heat-resistant layer 13 has high temperature resistance and can withstand heat radiation and heat conduction in a high temperature environment, protecting the anti-rust film body a5 from being damaged by high temperature heat sources.
[0034] like Figure 4 As shown, the lower outer wall of the heat-resistant layer 13 is provided with a fireproof layer 14, and the lower outer wall of the fireproof layer 14 is provided with a waterproof layer 15. There are two thermal insulation layers 12, heat-resistant layers 13, fireproof layers 14 and waterproof layers 15. The two thermal insulation layers 12, heat-resistant layers 13, fireproof layers 14 and waterproof layers 15 are respectively arranged on the upper and lower sides of the base layer 6 with the base layer 6 as the central axis of symmetry.
[0035] The function of the fireproof layer 14 is to reduce the impact of fire on the main body, prevent the spread of fire, and protect the anti-rust film main body a5 to have a longer fire resistance time in the fire. The waterproof layer 15 can effectively prevent water or moisture from penetrating into the anti-rust film main body a5, avoid corrosion and damage, and improve the durability and stability of the anti-rust film main body a5.
[0036] The implementation principle of this embodiment is as follows: when the high-strength metal material is subjected to rust-proof treatment, one side of the film body 2 can be pulled out from the fixed cylinder 1 and wrapped around the high-strength metal material. After the wrapping is complete, the film body 2 can be cut by a tool. The anti-rust film body a5 and the anti-rust film body b7 inside the film body 2 can emit anti-rust gas factors through the VCI material inside them, diffuse and penetrate to the surface of the anti-rusted object and adsorb thereon, forming a dense protective film layer with a thickness of a single molecule, isolating various factors inducing rust from contact with the surface of the anti-rusted object, thereby effectively preventing the occurrence of rust. When wrapping the high-strength metal material, the surface friction can be increased by the wear-resistant layer 3 to reduce the speed at which the film body 2 ruptures due to friction under the influence of external force. The anti-static coefficient of the surface of the film body 2 can be increased by the anti-static layer 8 to avoid the accumulation of dust on the surface of the film body 2.
[0037] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A high-strength metal material vapor phase anti-rust film, comprising a fixed tube (1) and a film body (2) mounted on the circular outer wall of the fixed tube (1); The film body (2) comprises an anti-rust film body a (5), a base layer (6), and an anti-rust film body b (7); The base layer (6) is located at the center of the membrane body (2); The upper outer wall of the base layer (6) is provided with an anti-rust film body a (5), and the lower outer wall of the base layer (6) is provided with an anti-rust film body b (7); Features: A wear-resistant layer (3) is arranged on the upper side of the anti-rust film body a (5), and an antistatic layer (8) is arranged on the lower side of the wear-resistant layer (3).
2. The high-strength metal material vapor phase anti-rust film according to claim 1, characterized in that: The lower outer wall of the antistatic layer (8) is provided with a thickening layer a (9), and the lower outer wall of the thickening layer a (9) is provided with a connecting layer (10).
3. A high-strength metal material vapor phase anti-rust film according to claim 2, characterized in that: The outer wall of the lower end of the connecting layer (10) is provided with a thickening layer b (11), and the wear-resistant layer (3), the antistatic layer (8), the thickening layer a (9), the connecting layer (10) and the thickening layer b (11) are each provided with two.
4. The high-strength metal material vapor phase anti-rust film according to claim 1, characterized in that: The two wear-resistant layers (3), the antistatic layer (8), the thickening layer a (9), the connecting layer (10) and the thickening layer b (11) are respectively arranged on the upper and lower sides of the base layer (6) with the base layer (6) as the central axis of symmetry, and the surface of the antistatic layer (8) is coated with an antistatic coating.
5. The high-strength metal material vapor phase anti-rust film according to claim 1, characterized in that: A flame retardant layer (4) is arranged on the upper side of the anti-rust film body a (5), and the flame retardant layer (4) includes a heat insulation layer (12), a heat-resistant layer (13), a fireproof layer (14) and a waterproof layer (15).
6. The high-strength metal material vapor phase anti-rust film according to claim 5, characterized in that: A heat insulation layer (12) is provided on the lower side of the flame retardant layer (4), and a heat-resistant layer (13) is provided on the outer wall of the lower end of the heat insulation layer (12).
7. The high-strength metal material vapor phase anti-rust film according to claim 6, characterized in that: The lower outer wall of the heat-resistant layer (13) is provided with a fireproof layer (14), and the lower outer wall of the fireproof layer (14) is provided with a waterproof layer (15).
8. The high-strength metal material vapor phase anti-rust film according to claim 5, characterized in that: The heat insulating layer (12), the heat resistant layer (13), the fireproof layer (14) and the waterproof layer (15) are each provided with two, and the two heat insulating layers (12), the heat resistant layer (13), the fireproof layer (14) and the waterproof layer (15) are respectively provided on the upper and lower sides of the base layer (6) with the base layer (6) as the central axis of symmetry.