Environment-friendly platinum crystal plate

By setting up splicing components and waterproof and moisture-proof structures on the platinum crystal panel, the problem of platinum crystal panels being difficult and water-seepage is solved, and rapid disassembly and seamless splicing is achieved, improving waterproof and moisture-proof properties and extending service life.

CN223104025UActive Publication Date: 2025-07-15FUJINGTE DECORATION CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202422400198.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-09-30
Publication Date
2025-07-15
Estimated Expiration
2034-09-30

AI Technical Summary

Technical Problem

Platinum crystal panels on the market are not easy to splice quickly, and they are prone to cracks during installation to cause water seepage, which shortens the use time.

Method used

Splicing components are adopted, including connecting seats, splicing grooves, magnetic reinforcement grooves, clamping strips, connecting grooves, splicing plates, magnetic reinforcement plates and clamping grooves. These components are used to quickly disassemble and seamlessly splice, and improve waterproof and moisture resistance through vacuum cavity, noise reduction cotton, polyethylene moisture-proof film and other structures.

Benefits of technology

It realizes rapid disassembly and seamless splicing of platinum crystal panels, enhances waterproof and moisture resistance, and extends usage time.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN223104025U_ABST
    Figure CN223104025U_ABST
Patent Text Reader

Abstract

The utility model discloses an environment-friendly platinum crystal plate, which relates to the technical field of platinum crystal plates and comprises a polymer base material layer and a splicing component, a PUR ecological glue layer is mounted on the upper surface of the polymer base material layer, and the splicing component is arranged on the surface of the polymer base material layer. Each splicing assembly comprises a connecting base, a splicing groove, a magnetic attraction reinforcing groove, a clamping strip, a connecting groove, a splicing plate, a magnetic attraction reinforcing plate and a clamping groove, the connecting base is arranged at the lower end of the left surface of the macromolecule base material layer, the connecting base and the macromolecule base material layer are of an integrated structure, and the splicing groove is formed in the upper surface of the connecting base. According to the environment-friendly platinum crystal plate, the platinum crystal plates can be rapidly disassembled and assembled through the splicing assemblies, every two adjacent platinum crystal plates are seamlessly spliced, the noise reduction performance and the moisture resistance of the platinum crystal plates can be enhanced through the vacuum cavities, noise reduction cotton, a polyethylene moisture-proof film and a polyethylene moisture-proof film, and then the overall quality is improved; and the service time is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of platinum crystal plates, and specifically relates to an environment-friendly platinum crystal plate. Background Art

[0002] A platinum crystal plate is a high-end environment-friendly plate material, which is made by using a new composite material technology. It is a decorative material mainly used for the decoration of home and commercial spaces. It has the characteristics of beauty and practicality. The platinum crystal plate not only has a beautiful appearance, but also has very excellent practicality. It can effectively protect the wall and reduce damage during daily use, achieving a balance between beauty and practicality in the space. Currently, in order to improve the beauty and practicality of home decoration, platinum crystal plates are usually required.

[0003] The platinum crystal plates on the market are usually not easy to be quickly spliced and installed, and gaps will be generated during installation, causing internal water seepage, making them prone to moisture damage and shortening the service life. For this reason, we propose an environment-friendly platinum crystal plate. Content of the Utility Model

[0004] The purpose of the utility model is to provide an environment-friendly platinum crystal plate to solve the problems raised in the above background art.

[0005] To achieve the above purpose, the utility model provides the following technical solution: An environment-friendly platinum crystal plate, including a polymer base material layer and a splicing component. A PUR ecological glue layer is installed on the upper surface of the polymer base material layer. The splicing component is arranged on the surface of the polymer base material layer, and the splicing component includes a connecting seat, a splicing groove, a magnetic absorption reinforcement groove, a clamping strip, a connecting groove, a splicing plate, a magnetic absorption reinforcement plate and a clamping groove. The connecting seat is arranged at the lower end of the left surface of the polymer base material layer, and the connecting seat and the polymer base material layer are of an integrated structure. A splicing groove is opened on the upper surface of the connecting seat, and a magnetic absorption reinforcement groove is opened on the rear surface inside the splicing groove. A clamping strip is installed at the upper end of the left surface of the polymer base material layer, and the clamping strip and the polymer base material layer are of an integrated structure.

[0006] Further, a connecting groove is opened at the right end of the lower surface of the polymer base material layer, and a splicing plate is installed on the upper surface inside the connecting groove.

[0007] Further, the splicing plate is snap-fitted with the inside of the splicing groove, and a magnetic absorption reinforcement plate is installed on the rear surface of the splicing plate. The magnetic absorption reinforcement plate is snap-fitted with the inside of the magnetic absorption reinforcement groove.

[0008] Further, a clamping groove is opened on the right surface of the polymer base material layer, and the inside of the clamping groove is snap-fitted with the clamping strip.

[0009] Further, a PVC decorative layer is arranged on the upper surface of the PUR ecological glue layer, and a nano-violet light layer protection film is connected to the upper surface of the PVC decorative layer.

[0010] Further, a vacuum chamber is provided inside the polymer substrate layer, and noise reduction cotton is filled inside the vacuum chamber.

[0011] Further, a polyurethane waterproof coating is provided on the upper surface of the polymer substrate layer, and a polyethylene moisture-proof film is connected to the lower surface of the polyurethane waterproof coating.

[0012] Further, the inner side of the connection groove is snap-connected to the connection seat, and the connection seat is a rigid structure.

[0013] The present utility model provides an environment-friendly platinum crystal plate, which has the following beneficial effects:

[0014] 1. By providing a splicing component, the splicing component includes a connection seat, a splicing groove, a magnetic attraction reinforcement groove, a clamping strip, a connection groove, a splicing plate, a magnetic attraction reinforcement plate and a clamping groove. During use, the two platinum crystal plates are spliced together through the snap connection between the connection seat and the connection groove. When the connection groove and the connection seat are spliced, the splicing plate is inserted into the inner side of the splicing groove, and at the same time, the clamping strip is snap-connected to the inner side of the clamping groove to reinforce the splicing of the two platinum crystal plates. During the splicing process, the two platinum crystal plates are further fixed through the snap connection between the magnetic attraction reinforcement plate and the inner side of the magnetic attraction reinforcement groove, so that the device can realize the rapid disassembly and assembly of the platinum crystal plates, and there is a seamless splicing between two adjacent platinum crystal plates.

[0015] 2. By providing a vacuum chamber, noise reduction cotton, a polyurethane waterproof coating and a polyethylene moisture-proof film. During use, the vacuum chamber can make the inside of the polymer substrate layer have a good sound insulation effect, and the noise reduction cotton filled inside the vacuum chamber can further improve the noise reduction performance of the platinum crystal plate. The polyurethane waterproof coating has a good waterproof effect, and the polyethylene moisture-proof film can improve the moisture-proof performance at the bottom of the platinum crystal plate. The double-layer waterproof structure prevents water from seeping into the inside from the bottom, so that the device can enhance the noise reduction and moisture-proof performance of the platinum crystal plate, and further improve the overall quality to extend its service life. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 is a three-dimensional structural schematic diagram of an environment-friendly platinum crystal plate of the present utility model;

[0017] Figure 2 is a bottom three-dimensional structural schematic diagram of an environment-friendly platinum crystal plate of the present utility model;

[0018] Figure 3 is a three-dimensional structural schematic diagram of a splicing component of an environment-friendly platinum crystal plate of the present utility model;

[0019] Figure 4 is a three-dimensional sectional structural schematic diagram of a polymer substrate layer of an environment-friendly platinum crystal plate of the present utility model.

[0020] In the figure: 1, polymer base material layer; 2, PUR ecological glue layer; 3, splicing component; 301, connecting seat; 302, splicing groove; 303, magnetic attraction reinforcement groove; 304, clamping strip; 305, connecting groove; 306, splicing plate; 307, magnetic attraction reinforcement plate; 308, clamping groove; 4, PVC decoration layer; 5, nano-violet light layer protection film; 6, vacuum cavity; 7, noise reduction cotton; 8, polyurethane waterproof coating; 9, polyethylene moisture-proof film. Specific embodiments

[0021] The following further describes in detail the embodiments of the present utility model in conjunction with the accompanying drawings and examples. The following examples are used to illustrate the present utility model, but cannot be used to limit the scope of the present utility model.

[0022] As Figures 1 to 4 shown, an environment-friendly platinum crystal plate includes a polymer base material layer 1 and a splicing component 3. The upper surface of the polymer base material layer 1 is provided with a PUR ecological glue layer 2. The splicing component 3 is arranged on the surface of the polymer base material layer 1, and the splicing component 3 includes a connecting seat 301, a splicing groove 302, a magnetic attraction reinforcement groove 303, a clamping strip 304, a connecting groove 305, a splicing plate 306, a magnetic attraction reinforcement plate 307 and a clamping groove 308. The connecting seat 301 is arranged at the lower end of the left surface of the polymer base material layer 1, and the connecting seat 301 and the polymer base material layer 1 are of an integrated structure. The upper surface of the connecting seat 301 is provided with a splicing groove 302, and the inner rear surface of the splicing groove 302 is provided with a magnetic attraction reinforcement groove 303. The upper end of the left surface of the polymer base material layer 1 is provided with a clamping strip 304, and the clamping strip 304 and the polymer base material layer 1 are of an integrated structure.

[0023] The specific operation is as follows. When in use, the polymer base material layer 1 is made of polymer, aerogel and white carbon, which improves the oxidation resistance and has higher hardness. The PUR ecological glue layer 2 makes the platinum crystal plate more environmentally friendly and safe, and has strong durability. Through the snap connection of the connecting seat 301 and the connecting groove 305, two groups of platinum crystal plates are spliced together. When the connecting groove 305 is spliced with the connecting seat 301, the splicing plate 306 is snapped into the inner side of the splicing groove 302. At the same time, the clamping strip 304 is snap-connected with the inner side of the clamping groove 308 to reinforce the splicing of the two groups of platinum crystal plates. During the splicing process, through the snap connection of the magnetic attraction reinforcement plate 307 and the inner side of the magnetic attraction reinforcement groove 303, the two groups of platinum crystal plates are further fixed.

[0024] Please refer to Figures 3 to 4, a connection groove 305 is provided at the right end of the lower surface of the polymer base material layer 1, and a splicing plate 306 is installed on the upper surface inside the connection groove 305. The splicing plate 306 is snap-connected to the inside of the splicing groove 302, and a magnetic attraction reinforcement plate 307 is installed on the rear surface of the splicing plate 306. The magnetic attraction reinforcement plate 307 is snap-connected to the inside of the magnetic attraction reinforcement groove 303. A clamping groove 308 is provided on the right surface of the polymer base material layer 1, and the inside of the clamping groove 308 is snap-connected to the clamping strip 304. A PVC decorative layer 4 is provided on the upper surface of the PUR ecological glue layer 2, and a nano-violet light layer protection film 5 is connected to the upper surface of the PVC decorative layer 4. A vacuum cavity 6 is provided inside the polymer base material layer 1, and noise reduction cotton 7 is filled inside the vacuum cavity 6. A polyurethane waterproof coating 8 is provided on the upper surface of the polymer base material layer 1, and a polyethylene moisture-proof film 9 is connected to the lower surface of the polyurethane waterproof coating 8. The inside of the connection groove 305 is snap-connected to the connection seat 301, and the connection seat 301 is a rigid structure;

[0025] The specific operation is as follows. When in use, the nano-violet light layer protection film 5 has an anti-ultraviolet effect. Through the vacuum cavity 6, the inside of the polymer base material layer 1 can have a good sound insulation effect. The noise reduction cotton 7 filled inside the vacuum cavity 6 can further improve the noise reduction performance of the platinum crystal plate. The polyurethane waterproof coating 8 has a good waterproof effect. The polyethylene moisture-proof film 9 can improve the moisture-proof performance at the bottom of the platinum crystal plate. The double-layer waterproof structure prevents water from seeping into the interior from the bottom.

[0026] In summary, as Figures 1 to 4 shown, for this environmentally friendly platinum crystal plate, when in use, first of all, the polymer base material layer 1 is made of polymer, aerogel and white carbon, which improves the antioxidant property and has a higher hardness. The PUR ecological glue layer 2 makes the platinum crystal plate more environmentally friendly and safe, and has strong durability. When installing the platinum crystal plate, through the snap connection between the connection seat 301 and the connection groove 305, two groups of platinum crystal plates are spliced together. When the connection groove 305 is spliced with the connection seat 301, the splicing plate 306 is snapped into the inside of the splicing groove 302. At the same time, the clamping strip 304 is snap-connected to the inside of the clamping groove 308 to reinforce the splicing of the two groups of platinum crystal plates. During the splicing process, through the snap connection between the magnetic attraction reinforcement plate 307 and the inside of the magnetic attraction reinforcement groove 303, the two groups of platinum crystal plates are further fixed. During the use of this device, through the vacuum cavity 6, the inside of the polymer base material layer 1 can have a good sound insulation effect. The noise reduction cotton 7 filled inside the vacuum cavity 6 can further improve the noise reduction performance of the platinum crystal plate. The polyurethane waterproof coating 8 has a good waterproof effect. The polyethylene moisture-proof film 9 can improve the moisture-proof performance at the bottom of the platinum crystal plate. The double-layer waterproof structure prevents water from seeping into the interior from the bottom. The nano-violet light layer protection film 5 has an anti-ultraviolet effect.

[0027] The embodiments of the present utility model are given for purposes of illustration and description, and are not exhaustive or limit the present utility model to the disclosed forms. Many modifications and variations are obvious to those of ordinary skill in the art. The embodiments are chosen and described in order to better explain the principles of the present utility model and its practical applications, and to enable those of ordinary skill in the art to understand the present utility model so as to design various embodiments with various modifications suitable for specific purposes.

Claims

1. An environmentally friendly platinum crystal plate, comprising a polymer substrate layer (1) and a splicing component (3), characterized in that: The upper surface of the polymer substrate layer (1) is provided with a PUR ecological glue layer (2). The splicing assembly (3) is arranged on the surface of the polymer substrate layer (1), and the splicing assembly (3) includes a connecting seat (301), a splicing groove (302), a magnetic attraction reinforcement groove (303), a clamping strip (304), a connecting groove (305), a splicing plate (306), a magnetic attraction reinforcement plate (307) and a clamping groove (308). The connecting seat (301) is arranged at the lower end of the left surface of the polymer substrate layer (1), and the connecting seat (301) and the polymer substrate layer (1) are of an integrated structure. The upper surface of the connecting seat (301) is provided with a splicing groove (302), and the rear surface inside the splicing groove (302) is provided with a magnetic attraction reinforcement groove (303). The upper end of the left surface of the polymer substrate layer (1) is provided with a clamping strip (304), and the clamping strip (304) and the polymer substrate layer (1) are of an integrated structure.

2. The environmentally friendly platinum crystal plate according to claim 1, characterized in that, A connecting groove (305) is opened at the right end of the lower surface of the polymer substrate layer (1), and a splicing plate (306) is installed on the upper surface inside the connecting groove (305).

3. The environmentally friendly platinum crystal plate according to claim 2, characterized in that, The splicing plate (306) is snap-connected to the inside of the splicing groove (302), and a magnetic attraction reinforcement plate (307) is installed on the rear surface of the splicing plate (306). The magnetic attraction reinforcement plate (307) is snap-connected to the inside of the magnetic attraction reinforcement groove (303).

4. An environment-friendly platinum crystal plate according to claim 1, characterized in that, A clamping groove (308) is opened on the right surface of the polymer substrate layer (1), and the inside of the clamping groove (308) is snap-connected to the clamping strip (304).

5. An environmentally friendly platinum crystal plate according to claim 1, wherein, A PVC decorative layer (4) is arranged on the upper surface of the PUR ecological glue layer (2), and a nano-violet light layer protective film (5) is connected to the upper surface of the PVC decorative layer (4).

6. An environmentally friendly platinum crystal plate according to claim 1, characterized in that, A vacuum cavity (6) is opened inside the polymer substrate layer (1), and noise reduction cotton (7) is filled inside the vacuum cavity (6).

7. An environmentally friendly platinum crystal plate according to claim 1, characterized in that A polyurethane waterproof coating (8) is arranged on the upper surface of the polymer substrate layer (1), and a polyethylene moisture-proof film (9) is connected to the lower surface of the polyurethane waterproof coating (8).