Continuous annealing device for aluminum magnesium alloy wire production
By setting two sets of electric heating plates on the annealing table and adjusting the distance using a hydraulic telescopic rod, the problem of uneven heating of the inner and outer layers during the annealing process of aluminum-magnesium alloy wire was solved, achieving uniform heating and efficient production of aluminum-magnesium alloy wire.
Patent Information
- Application Number
- CN202422967824.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-12-03
- Publication Date
- 2025-11-18
- Estimated Expiration
- 2034-12-03
AI Technical Summary
The existing annealing process for aluminum-magnesium alloy wires suffers from uneven heating between the inner and outer layers, resulting in uneven hardness of the aluminum-magnesium alloy wires.
A continuous annealing device was designed. By setting two sets of electric heating plates on the annealing table and using a hydraulic telescopic rod to adjust the up and down position of the electric heating plates, the distance between the aluminum-magnesium alloy wire and the electric heating plates can be controlled to achieve uniform heating.
This technology enables uniform heating of aluminum-magnesium alloy wires of different specifications, improving processing efficiency and product quality consistency.
Smart Images

Figure CN223561639U_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The utility model relates to annealing technical field especially relates to a continuous annealing device for aluminium magnesium alloy wire production. BACKGROUND
[0002] Aluminium magnesium alloy aluminium wire main element is aluminium, again incorporate a small amount of magnesium or other metal materials to strengthen its hardness, in order to enhance the stress of aluminium magnesium alloy wire, the annealing process is particularly important in production and processing, the current aluminium magnesium alloy wire annealing is usually placed in annealing box and carries out annealing treatment, but for aluminium magnesium alloy wire, since it is winding packing, therefore can cause this kind of process when processing aluminium magnesium alloy wire inner and outer layer aluminium magnesium alloy wire uneven heating, in view of the above problem, the present scheme proposes a kind of continuous annealing device for aluminium magnesium alloy wire production. SUMMARY
[0003] The utility model discloses a kind of continuous annealing devices for aluminium magnesium alloy wire production, the two groups of electric heating plate one and electric heating plate two of being set on the annealing table are set, so as to realize for aluminium magnesium alloy wire heating in annealing treatment, the first hydraulic telescopic link and second hydraulic telescopic link are respectively set, and electric heating plate one and electric heating plate two are realized up and down adjustment, the approach distance between the outer surface of the aluminium magnesium alloy wire that passes and electric heating plate one and electric heating plate two is adjusted respectively by adjusting, so as to facilitate the passage of various specifications of aluminium magnesium alloy wire, and the effective control and adjustment of distance when heating.
[0004] The utility model also provides a kind of continuous annealing device for aluminium magnesium alloy wire production with the above, it include: annealing table, the lower surface of the annealing table is fixedly connected with telescopic rod seat through support on both sides, the upper surface of both sides telescopic rod seat is fixedly connected with first hydraulic telescopic link, the upper surface of both sides upper telescopic rod seat is fixedly connected with second hydraulic telescopic link, the upper surface left and right sides of the annealing table is movably connected with electric heating plate two, the upper surface of electric heating plate two is movably connected with electric heating plate one;The front and back sides of electric heating plate two, electric heating plate one are fixedly connected with support frame, the lower surface of front and back sides support frame is fixedly connected with heat insulation pad, the output end of front and back sides first hydraulic telescopic link is fixedly connected with the support frame of electric heating plate one front and back sides through heat insulation pad, the output end of front and back sides second hydraulic telescopic link is fixedly connected with the support frame of electric heating plate two front and back sides through heat insulation pad.
[0005] According to the continuous annealing device for aluminium magnesium alloy wire production, the third guide base is arranged between the electric heating plates two on the left and right sides, the third guide base is fixedly connected with the annealing table, the second guide base is fixedly connected with the upper surface of the left side of the annealing table, and the fourth guide base is fixedly connected with the upper surface of the right side of the annealing table. The third guide base provides support for the aluminium magnesium alloy wire that passes.
[0006] The utility model relates to a continuous annealing device for aluminium magnesium alloy wire production, the left side end surface of annealing platform is fixedly connected with the inclined board no.
[0007] The utility model relates to a continuous annealing device for aluminium magnesium alloy wire production, the lower end surface of inclined board no.
[0008] The utility model relates to a continuous annealing device for aluminium magnesium alloy wire production, the right side end surface of annealing platform is fixedly connected with the inclined board no.
[0009] The utility model relates to a continuous annealing device for aluminium magnesium alloy wire production, the lower end surface of inclined board no.
[0010] The utility model relates to a continuous annealing device for aluminium magnesium alloy wire production, the wire reel support, the wire reel support are equipped with three groups, the lead seat no.
[0011] Beneficial effects
[0012] 1、Compared with the prior art, the continuous annealing device for aluminum magnesium alloy wire production, through the setting of the two groups of electric heating plates one and electric heating plates two on the annealing table, realizes the heating and annealing treatment of the aluminum magnesium alloy wire, through the setting of the first hydraulic telescopic rod and the second hydraulic telescopic rod, the electric heating plate one and the electric heating plate two are adjusted up and down respectively, and the distance between the outer surface of the passing aluminum magnesium alloy wire and the electric heating plate one and the electric heating plate two is adjusted respectively through adjustment, so that the aluminum magnesium alloy wire of various specifications passes through, and the effective control and adjustment of the distance during heating are facilitated. BRIEF DESCRIPTION OF DRAWINGS
[0013] The utility model is further explained below in combination with the drawings and examples;
[0014] Fig. 1 It is the overall structural drawing of the utility model of a kind of aluminum magnesium alloy wire production continuous annealing device;
[0015] Fig. 2 It is the plan view of the utility model of a kind of aluminum magnesium alloy wire production continuous annealing device;
[0016] Fig. 3 It is the bottom view of the utility model of a kind of aluminum magnesium alloy wire production continuous annealing device.
[0017] Legend:
[0018] 1, feed rack;2, inclined plate one;3, pay-off reel support;4, pay-off reel;5, lead seat one;6, first guide seat;7, cleaning bin;8, second guide seat;9, electric heating plate one;10, first hydraulic telescopic rod;11, telescopic rod seat;12, support frame;13, electric heating plate two;14, second hydraulic telescopic rod;15, heat insulation pad;16, third guide seat;17, annealing table;18, fourth guide seat;19, heat removal bin;20, fifth guide seat;21, lead seat two;22, take-up reel support;23, take-up reel;24, take-up rack;25, inclined plate two. DETAILED DESCRIPTION
[0019] This part will describe the specific embodiments of the utility model in detail, the preferred embodiments of the utility model are shown in the drawings, the role of the drawings is to supplement the description of the text part with graphics, so that people can intuitively and visually understand each technical feature and overall technical scheme of the utility model, but it cannot be understood as the limitation of the protection scope of the utility model.
[0020] REFERENCE Figs. 1-3The utility model discloses an aluminium -magnesium alloy wire production is with continuous annealing device, it includes: annealing platform 17, the lower surface of annealing platform 17 both sides are fixedly connected with telescopic link seat 11 through the support, the upper surface of both sides telescopic link seat 11 is fixedly connected with first hydraulic telescopic link 10, the upper surface of both sides upper telescopic link seat 11 is fixedly connected with second hydraulic telescopic link 14, the upper surface of annealing platform 17 both sides is movably connected with electric hot plate two 13, is equipped with electric heating wire inside, generates heat after power on, the upper surface of electric hot plate two 13 is movably connected with electric hot plate one 9, is equipped with electric heating wire inside, generates heat after power on, the front and rear sides of electric hot plate two 13, electric hot plate one 9 are fixedly connected with support frame 12, the lower surface of both sides support frame 12 is fixedly connected with heat insulation pad 15, and the output of both sides first hydraulic telescopic link 10 is fixedly connected with the support frame 12 of electric hot plate one 9 front and rear sides through heat insulation pad 15, and the output of both sides second hydraulic telescopic link 14 is fixedly connected with the support frame 12 of electric hot plate two 13 front and rear sides through heat insulation pad 15.
[0021] The third guide base 16 is arranged between the electric hot plate two 13 on the left and right sides, and the third guide base 16 is fixedly connected with the annealing platform 17. The left upper surface of the annealing platform 17 is fixedly connected with the second guide base 8, and the right upper surface of the annealing platform 17 is fixedly connected with the fourth guide base 18. The left end surface of the annealing platform 17 is fixedly connected with the inclined plate one 2. The upper surface of the inclined plate one 2 is fixedly connected with the first guide base 6. The upper surface of the inclined plate one 2 is fixedly connected with the cleaning bin 7. The cleaning bin 7 is internally provided with cleaning cloth. The aluminium-magnesium alloy wire running on the surface of the cleaning cloth can be cleaned.
[0022] The right side end surface of the annealing table 17 is fixedly connected with an inclined plate two 25, the upper surface of the inclined plate two 25 is fixedly connected with a heat-reducing bin 19, and the inside is provided with a forced air cooling device, so that the temperature of the aluminum-magnesium alloy wire is reduced through the cold air. The upper surface of the inclined plate two 25 is fixedly connected with a fifth guide seat 20. The lower end surface of the inclined plate two 25 is fixedly connected with a material collecting rack 24, the upper surface of the material collecting rack 24 is fixedly connected with a wire collecting reel support 22, the inside of the wire collecting reel support 22 is detachably connected with a material collecting wire reel 23, the upper surface of the material collecting rack 24 is fixedly connected with a lead seat two 21, the upper wire rod seat is moved back and forth through a motor driving reciprocating wire rod, the wire rod seat is installed through a wire ring, the aluminum-magnesium alloy wire is threaded in the wire ring, and the wire is guided. The wire reel support 3 and the wire collecting reel support 22 are each provided with three groups, the lead seat one 5 and the lead seat two 21 are each provided with three groups, and the first guide seat 6, the second guide seat 8, the third guide seat 16, the fourth guide seat 18 and the fifth guide seat 20 are each provided with three groups.
[0023] Working principle: when in use, the material wire reel 4 wound with the aluminum-magnesium alloy wire is installed on the wire reel support 3, enters the first guide seat 6 through the lead seat one 5, enters the cleaning bin 7 through the first guide seat 6, the cleaned aluminum-magnesium alloy wire is introduced into the annealing table 17 through the second guide seat 8, sequentially passes between the two groups of electric heating plates one 9 and electric heating plates two 13, the distance between the electric heating plates one 9 and the electric heating plates two 13 is adjusted through the first hydraulic telescopic rod 10 and the second hydraulic telescopic rod 14, the aluminum-magnesium alloy wire is guided out through the fourth guide seat 18 and enters the heat-reducing bin 19, and then is introduced into the lead seat two 21 through the fifth guide seat 20, so that the aluminum-magnesium alloy wire is orderly wound on the material collecting wire reel 23 through the lead seat two 21.
[0024] The above embodiment of the utility model is described in detail in combination with the drawings, but the utility model is not limited to the above embodiment, and various changes can be made within the knowledge range possessed by those skilled in the art without departing from the purpose of the utility model.
Claims
1. A continuous annealing apparatus for producing aluminum-magnesium alloy wire, characterized in that, Include: Annealing table (17), the lower surface of the annealing table (17) is fixedly connected with the telescopic rod seat (11) on both sides, the upper surface of both sides of the telescopic rod seat (11) is fixedly connected with the first hydraulic telescopic rod (10), the upper surface of both sides of the telescopic rod seat (11) is fixedly connected with the second hydraulic telescopic rod (14), the upper surface of both sides of the annealing table (17) is movably connected with the electric heating plate two (13), the upper surface of the electric heating plate two (13) is movably connected with the electric heating plate one (9); The front and back of the electric heating plate two (13), the electric heating plate one (9) is fixedly connected with the support frame (12), the lower surface of the front and back of the support frame (12) is fixedly connected with the heat insulation pad (15), the output end of the front and back of the first hydraulic telescopic rod (10) is fixedly connected with the support frame (12) of the electric heating plate one (9) through the heat insulation pad (15), the output end of the front and back of the second hydraulic telescopic rod (14) is fixedly connected with the support frame (12) of the electric heating plate two (13) through the heat insulation pad (15).
2. The continuous annealing apparatus for an aluminum magnesium alloy wire according to claim 1, characterized by The third guide seat (16) is arranged between the electric heating plate two (13) on both sides, the third guide seat (16) is fixedly connected with the annealing table (17), the left upper surface of the annealing table (17) is fixedly connected with the second guide seat (8), the right upper surface of the annealing table (17) is fixedly connected with the fourth guide seat (18).
3. The continuous annealing apparatus for an aluminum magnesium alloy wire according to claim 1, characterized by The left end surface of the annealing table (17) is fixedly connected with the inclined plate one (2), the upper surface of the inclined plate one (2) is fixedly connected with the first guide seat (6), the upper surface of the inclined plate one (2) is fixedly connected with the cleaning bin (7).
4. The continuous annealing apparatus for an aluminum magnesium alloy wire according to claim 3, characterized by The lower end surface of the inclined plate one (2) is fixedly connected with the feeding frame (1), the upper surface of the feeding frame (1) is fixedly connected with the pay-off reel support (3), the inside of the pay-off reel support (3) is detachably connected with the pay-off reel (4), the upper surface of the feeding frame (1) is fixedly connected with the lead seat one (5).
5. The continuous annealing apparatus for an aluminum magnesium alloy wire according to claim 1, characterized by The right end surface of the annealing table (17) is fixedly connected with the inclined plate two (25), the upper surface of the inclined plate two (25) is fixedly connected with the heat removal bin (19), the upper surface of the inclined plate two (25) is fixedly connected with the fifth guide seat (20).
6. The continuous annealing apparatus for an aluminum magnesium alloy wire according to claim 5, characterized by The lower end surface of the inclined plate two (25) is fixedly connected with the receiving frame (24), the upper surface of the receiving frame (24) is fixedly connected with the take-up reel support (22), the inside of the take-up reel support (22) is detachably connected with the take-up reel (23), the upper surface of the receiving frame (24) is fixedly connected with the lead seat two (21).
7. The continuous annealing apparatus for an aluminum magnesium alloy wire according to claim 4, characterized by The pay-off reel support (3), the take-up reel support (22) are provided with three groups, the lead seat one (5), the lead seat two (21) are provided with three groups, the first guide seat (6), the second guide seat (8), the third guide seat (16), the fourth guide seat (18), the fifth guide seat (20) are provided with three groups.