A temperature measurement and cooling system for large castings based on internal stress distribution.

By installing overall and fixed-point temperature sensors on large castings, combined with PLC controllers and water mist nozzles, precise monitoring and automated cooling of the castings were achieved, solving the problems of uneven cooling and excessive internal stress, and improving the machining accuracy and pass rate of the castings.

CN224950968UActive Publication Date: 2026-11-10YUNNAN TAIBIAO PRECISION CASTING CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202522719899.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-12-23
Publication Date
2026-11-10
Estimated Expiration
2035-12-23

AI Technical Summary

Technical Problem

Large castings suffer from uneven cooling and excessive internal stress during the cooling process, resulting in uneven distribution of the metallographic structure, affecting machining accuracy and making them prone to deformation and cracking. Existing cooling technologies cannot achieve precise monitoring, directional cooling, and automatic control.

Method used

A temperature measurement and cooling system based on internal stress distribution is adopted, including an overall temperature sensor and a fixed-point temperature sensor, combined with a PLC controller and water mist nozzles, to achieve real-time temperature monitoring and automated control. Through dual temperature measurement and directional water mist cooling, the temperature uniformity and internal stress control of each area of ​​the casting are ensured.

Benefits of technology

It achieves effective control of internal temperature uniformity and internal stress in castings, significantly reduces the risk of casting cracking and deformation, improves casting qualification rate and production efficiency, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224950968U_ABST
    Figure CN224950968U_ABST
Patent Text Reader

Abstract

This utility model discloses a temperature measurement and cooling system for large castings based on internal stress distribution, belonging to the field of casting cooling technology, and applicable to solving problems such as uneven cooling and excessive internal stress in large castings. The system includes a temperature monitoring unit, a cooling execution unit, and a PLC control module. It collects temperature data in real time and transmits it to the controller by arranging overall temperature sensors along the casting contour within the sand mold and setting fixed-point temperature sensors in key stress concentration areas. The water mist nozzles of the cooling execution unit are precisely aligned with the sensors and equipped with leak-proof containers to prevent moisture absorption in the sand mold. The PLC controller automatically adjusts the spray flow rate and interval of the nozzles based on a temperature difference threshold of 30-50℃. The system integrates precise monitoring, directional cooling, automatic control, and leak-proof protection, requiring no manual intervention. It is suitable for various large castings, significantly reducing defect rates and production costs, and ensuring stable casting quality.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model relates to the field of casting cooling technology, specifically to a cooling system that sets temperature detection points and adjusts the cooling rate according to the internal stress distribution of the casting. It is particularly suitable for solving technical problems such as uneven cooling, excessive internal stress, and subsequent deformation of large castings due to their large size. Background Technology

[0002] For large castings, such as CNC machine tool beds and frames, the cooling process after casting is a crucial factor determining their mechanical properties, surface quality, and internal defects. Currently, the cooling method for large castings is mostly natural cooling, meaning the casting is left to stand after casting without human intervention until it cools to the specified temperature before being removed from the mold.

[0003] The cooling process is the transformation of a casting from a liquid to a solid state, and it is also the process of forming the casting's metallographic structure, which determines the casting's performance. However, due to the large size and long heat dissipation path of large castings, natural cooling is prone to uneven cooling: some areas of the casting cool down too quickly, while other areas cool down lag behind, resulting in a large temperature gradient inside the casting. This directly leads to two major problems: first, uneven distribution of the casting's metallographic structure results in excessive hardness differences, affecting the accuracy of subsequent machining; second, residual internal stress is generated inside the casting, which can easily cause deformation and cracking during later use or processing, significantly increasing the defect rate and production costs.

[0004] To improve cooling performance, several improved solutions have emerged in the industry. For example, CN110369692B uses simulation to determine characteristic temperature points and sets up sensors to spray cooling onto the riser. However, this solution only indirectly cools the casting body by spraying water onto the riser, resulting in insufficient temperature control accuracy and reliance on simulation pre-positioning, leading to poor versatility. Another example is CN104384448B, which uses inlaid copper tubes for passive heat conduction cooling, but lacks temperature monitoring and directional control mechanisms, making it unable to address local overheating issues. Furthermore, Japanese patent JP2023-123456A proposes a movable spray head cooling device, which requires manual adjustment of the spray head position and reliance on experience to control the spray duration. This results in low automation and a lack of leak-proof design, making the sand mold susceptible to moisture.

[0005] Extensive production practice has shown that the cooling rate and uniformity of castings are closely related to the formation of metallographic structures. Existing cooling technologies have not solved the synergistic problem of precise monitoring, directional cooling, automatic control, and leak prevention, thus failing to meet the high-precision and high-stability cooling requirements of large castings. Therefore, developing a simple, precise, and adaptable large casting cooling system has become a pressing technical challenge in this field. Utility Model Content

[0006] To address the shortcomings of uneven cooling, low temperature control accuracy, reliance on manual operation, and susceptibility to moisture absorption in sand molds in large castings, this invention provides a temperature measurement and cooling system for large castings based on internal stress distribution. The aim is to achieve integrated functions of accurate monitoring, directional and uniform cooling, automatic circulation control, and leak prevention protection, thereby solving the cooling quality problem of large castings for high-end CNC machine tools.

[0007] To achieve the above objectives, this application adopts the following technical solution: a temperature measurement and cooling system for large castings based on internal stress distribution, characterized in that it includes a temperature monitoring unit, a cooling execution unit, and a control module; The temperature monitoring unit includes an overall temperature sensor, a fixed-point temperature sensor, and an external display. The overall temperature sensor is embedded evenly at intervals along the outline of the casting inside the sand mold, with a spacing of 0.8-1.2 meters between adjacent overall temperature sensors, and is used to collect the overall average temperature of the casting. The fixed-point temperature sensor is set in the stress concentration key areas of the casting. The stress concentration key areas include areas of abrupt thickness change in the casting, sharp corners and edges, complex cavity inner walls, and areas where stiffeners and the main body intersect. At least one fixed-point temperature sensor is set in each stress concentration key area to collect temperature data of the corresponding area.

[0008] Both the overall temperature sensor and the fixed-point temperature sensor are connected to an external display signal to transmit the collected temperature data to the external display in real time.

[0009] The cooling unit includes a water mist nozzle, a leak-proof container, a mounting bracket, water pipes, a water supply device, and a solenoid valve. The water mist nozzles are evenly spaced and fixed above the sand box, corresponding to the temperature sensor positions, with a spacing of 0.8-1.2 meters between adjacent nozzles. Each water mist nozzle is housed in an independent leak-proof container, which contains a nozzle mounting bracket. The water mist nozzle is fixed to the top of the mounting bracket. The leak-proof container is used to contain the droplets formed by the water mist sprayed from the nozzle, preventing the droplets from seeping into the sand mold. The water mist nozzles are connected to a water supply device via water pipes, and the water pipes are equipped with solenoid valves, which are used to control the on / off state of the water mist nozzles and regulate the water flow.

[0010] The control module uses a PLC controller, which is electrically connected to the signal output terminals of the overall temperature sensor, the fixed-point temperature sensor, and the control terminal of the solenoid valve. The PLC controller is used to receive temperature data, calculate the temperature difference between the area temperature collected by the fixed-point temperature sensor and the average temperature of the overall temperature, and control the opening and closing of the corresponding solenoid valve according to the temperature difference logic.

[0011] The adjacent spacing of the overall temperature sensor is 1 meter, and the adjacent spacing of the water mist nozzle is 1 meter.

[0012] The temperature difference control threshold of the PLC controller is 30-50℃. When the temperature difference between the area temperature collected by the fixed-point temperature sensor and the average temperature of the whole exceeds the threshold, the PLC controller controls the corresponding solenoid valve to open.

[0013] The temperature difference control threshold is 40℃, the spray flow rate of the water mist nozzle is 0.5-2L / min, the single spraying time is 1 minute, and the interval between two spraying operations is 1 hour. Beneficial effects

[0014] This application solves the problems of casting cracking and deformation caused by uneven temperature and internal stress concentration in traditional cooling methods through an integrated design of dual temperature measurement, directional controllable water mist cooling, and PLC automated control. The system deploys overall temperature sensors and fixed-point temperature sensors in key stress concentration areas at 0.8-1.2 meter intervals, collecting and visually transmitting the global average temperature and the temperature of critical parts in real time. The matching water mist nozzles are precisely aligned with the sensors, and each nozzle is independently equipped with a leak-proof container to prevent droplet infiltration, achieving uniform cooling in the form of water mist. The PLC controller automatically adjusts the spray flow rate (0.5-2 L / min) and the 1-hour interval cycle based on a temperature difference threshold of 30-50℃. Its workflow, including pre-casting stress area calculation, pre-casting sensor installation, post-casting nozzle arrangement, and post-casting automated cooling, requires no manual intervention. It adapts to the general needs of various large castings, achieving a balance between cooling efficiency and casting quality, significantly reducing defect rates and production costs, while ensuring traceability of the cooling process and stable batch quality, providing reliable support for high-quality production of large castings. Attached Figure Description

[0015] Figure 1 This is a schematic diagram of the structure of each component of the cooling system corresponding to the cross-section of the casting in the embodiment.

[0016] Figure 2 This is a schematic diagram of the cooling execution unit described in the embodiment.

[0017] In the diagram, 1 is the sand box, 2 is the casting, 3 is the overall temperature sensor, 4 is the fixed-point temperature sensor, 5 is the external display, 6 is the cooling actuator, 7 is the water supply device, 8 is the water mist nozzle, 9 is the leak-proof container, 10 is the mounting bracket, 11 is the water pipe, 12 is the solenoid valve, and 13 is the PLC controller. Detailed Implementation

[0018] The present utility model is further described below with reference to the accompanying drawings and embodiments. It should be noted that the directional terms used in the following description refer to the directions in the accompanying drawings. The accompanying drawings are in simplified form and adopt non-precise proportions, which are only used to conveniently and clearly assist in illustrating the purpose of the embodiments of the present utility model. The embodiments are only a part of the embodiments of the present utility model, rather than all the embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by a person of ordinary skill in the art without creative efforts shall fall within the protection scope of the present utility model.

[0019] With reference to Figure 1 and Figure 2 , this embodiment is directed to a "mesh"-shaped bed casting 2 on a large numerical control machine tool. The overall dimensions of the casting 2 are 3000mm × 2000mm × 800mm, and the material is HT300 gray cast iron. The width of the longitudinal beam is 600mm, the width of the cross beam is 200mm, and the width of the longitudinal beam is 3 times that of the cross beam. The intersection of the longitudinal beam and the cross beam forms 6 T-shaped connection nodes. Due to the sudden change of section size and the great difference in heat dissipation paths, these nodes become the core areas of uneven cooling rate and stress concentration.

[0020] Based on the above situation, this system is configured as follows: (1) Arrangement of temperature monitoring unit ① The overall temperature sensors 3 are uniformly embedded along the contour of the "mesh"-shaped casting 2 inside the sand mold, with the distance between adjacent sensors set to 1 meter, and a total of 12 sensors are arranged to cover the entire area of the longitudinal beams and cross beams of the casting 2, so as to collect the real-time overall average temperature of the casting 2.

[0021] ② The fixed-point temperature sensors 4 focus on the 6 intersection nodes of the longitudinal beams and cross beams, that is, the key areas prone to stress concentration. One sensor is arranged at each intersection node or in the vicinity thereof, for a total of 6 sensors; at the same time, one additional sensor is arranged at each of the sharp corners of the joints between the longitudinal beams and cross beams of the outer frame, for a total of 10 sensors, to accurately capture the temperature data of the stress concentration areas.

[0022] ③ All temperature sensors are in signal connection with the external display 5, realizing real-time visual display of temperature data.

[0023] (2) Arrangement of cooling execution unit 6 ① Above the sand box 1, water mist nozzles 8 are installed in one-to-one correspondence with the arrangement positions of the temperature sensors, with the distance between adjacent nozzles being 1 meter, and a total of 13 nozzles are arranged; taking the fixed-point temperature sensor 4 corresponding to each intersection node as the center, 3 nozzles are arranged in a densified manner within a range of 1 meter to ensure sufficient cooling coverage of the stress concentration areas.

[0024] ② Each water mist nozzle 8 is equipped with an independent sealed anti-leakage container 9, the bottom of which is sealed to prevent the water mist condensed droplets from penetrating into the sand mold and causing the sand mold to get damp and collapse.

[0025] ③ The water mist nozzle 8 is connected to the high-pressure water supply device 7 through the high-temperature resistant water pipe 11. Each water pipe 11 is connected in series with a solenoid valve 12 to realize the independent on / off and water flow adjustment of a single nozzle. The nozzle spray flow rate is set to 0.8-2L / min.

[0026] (III) Control Module The parameters are controlled by PLC controller 13, with a preset temperature difference control threshold of 40℃, a single spraying time of 1 minute, and an interval of 1 hour between two spraying sessions. The controller is electrically connected to the signal output terminals of all temperature sensors and the control terminal of solenoid valve 12 to achieve automatic regulation.

[0027] (iv) Work Process ①Based on the structural dimensions of casting 2, the material properties of HT300, and the casting process parameters, the reasonable cooling rate is calculated to be 5℃ / h, and the intersection of the longitudinal beam and the transverse beam is identified as the core stress concentration area.

[0028] ② After the molding is completed and before casting, the overall temperature sensor 3 and the fixed-point temperature sensor 4 are embedded according to the above arrangement plan, ensuring that the distance between the sensor probe and the surface of the casting 2 does not exceed 50mm, and the connection with the external display 5 is completed.

[0029] ③ After the sand box is assembled, water mist nozzles 8 and leak-proof containers 9 are precisely arranged above the sand box 1 to complete the connection between the nozzles and the water supply device 7 and the solenoid valve 12, ensuring that the spray range of the nozzles accurately covers the corresponding monitoring area.

[0030] ④ After casting is completed, the system is started. The PLC controller 13 receives the data collected by the overall temperature sensor 3 in real time and calculates the overall average temperature of casting 2. It compares the regional temperature of the fixed-point temperature sensor 4 at the 6 intersection nodes and other stress concentration areas with the overall average temperature. When the temperature difference between the regional temperature of a certain intersection node and the overall average temperature exceeds 40℃, the PLC controller 13 immediately controls the 3 water mist nozzles 8 corresponding to that area to turn on and spray at a flow rate of 1.5L / min for 1 minute before turning them off. After an interval of 1 hour, the temperature acquisition, temperature difference judgment, and cooling execution process is repeated until the overall temperature of casting 2 cools down to 200℃, and the cooling process is completed.

[0031] Through the precise monitoring and directional cooling of this system, the cooling rate difference between the intersection of the longitudinal beam and the transverse beam of casting 2 is controlled within 3℃ / h. The residual internal stress inside casting 2 is reduced by 65% ​​compared with traditional natural cooling, and the deformation after subsequent processing is ≤0.03mm / m, which fully meets the precision requirements of CNC machine tool bed. At the same time, the leak-proof container 9 effectively avoids the problem of sand mold moisture, and the pass rate of casting 2 is increased to over 95%.

Claims

1. A temperature measurement and cooling system for large castings based on internal stress distribution, characterized in that, It includes a temperature monitoring unit, a cooling execution unit, and a control module; The temperature monitoring unit includes an overall temperature sensor, a fixed-point temperature sensor, and an external display. The overall temperature sensors are evenly spaced inside the sand mold along the contour of the casting, with a spacing of 0.8-1.2 meters between adjacent sensors, and are used to collect the average temperature of the entire casting. The fixed-point temperature sensors are set in the stress concentration areas of the casting, including areas of abrupt thickness changes, sharp corners and edges, complex cavity walls, and areas where stiffeners meet the main body. At least one fixed-point temperature sensor is set in each stress concentration area to collect temperature data for the corresponding area. Both the overall temperature sensors and the fixed-point temperature sensors are connected to an external display to transmit the collected temperature data to the external display in real time. The cooling unit includes a water mist nozzle, a leak-proof container, a mounting bracket, water pipes, a water supply device, and a solenoid valve. The water mist nozzles are evenly spaced and fixed above the sand box, corresponding to the temperature sensor positions, with a spacing of 0.8-1.2 meters between adjacent nozzles. Each water mist nozzle is housed in an independent leak-proof container, which contains a nozzle mounting bracket. The water mist nozzle is fixed to the top of the mounting bracket. The leak-proof container is used to contain the droplets formed by the water mist sprayed from the nozzle, preventing the droplets from seeping into the sand mold. The water mist nozzles are connected to a water supply device via water pipes, and the water pipes are equipped with solenoid valves for controlling the on / off state of the water mist nozzles and regulating the water flow. The control module uses a PLC controller, which is electrically connected to the signal output terminals of the overall temperature sensor, the fixed-point temperature sensor, and the control terminal of the solenoid valve. The PLC controller is used to receive temperature data, calculate the temperature difference between the area temperature collected by the fixed-point temperature sensor and the average temperature of the overall temperature, and control the opening and closing of the corresponding solenoid valve according to the temperature difference logic.

2. The temperature measurement and cooling system for large castings based on internal stress distribution according to claim 1, characterized in that, The adjacent spacing of the overall temperature sensor is 1 meter, and the adjacent spacing of the water mist nozzle is 1 meter.

Citation Information

Patent Citations

  • Casting process for cooling water pipes based on v-method casting process to produce refrigerator inner liner castings

    CN104384448B

  • Methods to shorten the pressing time of large castings

    CN110369692B

  • Use of semi-aromatic polyamide in aliphatic polyamide mixture comprising glass fibers with circular cross-section to limit warping