MANUFACTURING METHOD FOR SURFACE-TREATED COMPONENT AND DEVICE FOR THEREWARDS

DE102015203483B4Active Publication Date: 2024-10-17ASTEMO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
DE102015203483
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2014-02-28
Filing Date
2015-02-26
Publication Date
2024-10-17
Estimated Expiration
2035-02-26

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Manufacturing method for a surface-treated component (4) by locally treating corresponding surfaces of several steel bars (11) which are aligned without a gap in an axial direction of the steel bars (11) while the steel bars (11) are moved in the axial direction, wherein the method comprises: a movement step of moving the steel bars (11) in the axial direction with a movement device (22, 31) moving the steel bars (11);a detection step of using a pushing device (24) which is either downstream of the moving device (22, 31) or arranged in a center of the moving device (22, 31) to push one of the several steel rods (11) in a radial direction of the one steel rod (11) when the one steel rod (11) arrives at the pushing device (24) while moving in the axial direction, such that one end of the one steel rod (11) is displaced in the radial direction relative to one end of another steel rod (11) adjacent to the one steel rod (11), and of detecting the end of the one steel rod (11) or the end of the other steel rod (11) with a detection device (26);and a surface treatment step of locally forming a surface-treated area on each of the steel bars (11) with a surface treatment device (27) according to a time specification for the surface treatment which is determined based on a detection result by the detection device (26).
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTIONThe present invention relates to a manufacturing method for a surface-treated component and an apparatus for locally treating steel rods (including hollow and solid steel rods), for example, rods of cylinder devices such as hydraulic cylinders and hydraulic shock absorbers.A hydraulic shock absorber as a cylinder device mounted on a moving device such as an automobile basically comprises a cylinder having a piston and a rod connected at one end thereof to the piston in the cylinder and retractably projecting at the other end from the cylinder through a rod guide.The rod has an annular stop element (impact stop) which is attached to the outer periphery of an axially intermediate position of the rod. When the rod is extended, the stop abuts against the rod guide, thereby defining the most extended position of the rod. The stopper is fixed to the rod by the so-called metal flow bonding. That is, a groove extending over the entire circumference is formed on an outer circumferential surface of the rod, and a part of the stopper is pressed into the groove extending over the entire circumference by plastic deformation.In manufacturing such a rod, a steel rod (steel base material) as a blank (material) for a rod is locally quenched to form quenched portions other than portions subjected to plastic working or cutting, for example, at the ends of the steel rod and in a portion where a full-circumference groove is to be formed (see, for example, Japanese Patent Application Publication No. 2013 209 709 A). Chinese Utility Model CN 2 01 610 436 U discloses a roll high frequency quenching machine equipped with a means for detecting the quenching length using a rotary encoder. Korean patent KR 10 0 771 451 B1 discloses an apparatus for connecting pipes connected to a sensor for detecting the ends of the pipes. Korean patent KR 10 1 169 709 B1 discloses an apparatus for heat treatment of steel pipes with a lifting unit.SUMMARY OF THE INVENTIONWhen a steel rod is to be locally subjected to surface treatment such as quenching, it is necessary to detect the position of the steel rod in order to distinguish regions of the steel rod to be subjected to surface treatment from those not to be subjected to surface treatment. In particular, when the surface treatment is to be locally performed on a plurality of steel bars aligned in the axial direction in an end-to-end arrangement while the steel bars are moved in the axial direction for productivity enhancement, for example, it is desirable that an end (an end portion or an end surface) of a steel bar defining the boundary between a pair of steel bars adjacent to each other in the axial direction can be securely detected.The present invention has been devised in view of the above-described problem in the prior art. Accordingly, it is an object of the present invention to provide a surface-treated component manufacturing method and an apparatus with which an end (an end portion or an end surface) of a steel bar can be securely gripped and thus productivity can be improved.In order to solve the above-described problem, the invention provides a surface-treated component manufacturing method in which respective surfaces of a plurality of steel bars aligned in an axial direction of the steel bars in an end-to-end orientation are subjected to local treatment while the steel bars are moved in the axial direction. The method includes a moving step of moving the steel rods in the axial direction with a moving device moving the steel rods, a detecting step of using a urging device for urging one of the plurality of steel rods in a radial direction of the one steel rod such that an end of the one steel rod is displaced in the radial direction relative to an end of another steel rod adjacent to the one steel rod, the urging device being either downstream of or disposed in the moving device, and detecting the end of the one steel rod or the end of the other steel rod with a detecting device, and a surface treatment step of locally forming a surface treated region on each of the steel rods with a surface treatment device within a surface treatment timing, which is set based on the detection result by the detecting means.In addition, the present invention provides a surface-treated component manufacturing apparatus that locally undergoes surface treatment of a plurality of steel bars aligned in an axial direction of the steel bars in an end-to-end arrangement while the steel bars are moved in the axial direction. The apparatus includes moving means that moves the steel rod in the axial direction, urging means that is either downstream of the moving means or disposed in the moving means for urging one of the steel rods in a radial direction of the one steel rod such that an end of the one steel rod in the radial direction is offset relative to an end of another steel rod adjacent to the one steel rod, detecting means that detects the end of the one steel rod offset in the radial direction by the urging means or the end of the other steel rod, and surface treatment means that forms a surface treated region on each of the steel rods according to a surface treatment timing set based on the detection result by the detecting means.According to the present invention, when a plurality of steel bars aligned in an end-to-end arrangement in the axial direction are to be locally subjected to surface treatment while the steel bars move in the axial direction, it is possible to securely grasp an end (an end portion or an end surface) of each steel bar and thus improve productivity.BRIEF DESCRIPTION OF THE DRAWINGSFIG. 1 is a vertical cross-sectional view of a hydraulic shock absorber having a rod according to an embodiment of the present invention. FIG. 2 is a partial sectional side view illustrating a surface treatment apparatus (quenching apparatus) according to the embodiment. FIG. 3 is a partial sectional side view illustrating a surface treatment apparatus (quenching apparatus) as viewed from the same direction as in FIG. 2 when a steel bar is radially displaced by the feeding of a pressure roller means. FIG. 4 is an enlarged sectional view taken from the direction of the arrow IV-IV in FIG. 2. FIG. 5 is an enlarged sectional view taken from the direction of arrow V-V in FIG. 2. FIG. 6 is an enlarged partial sectional side view illustrating the part (VI) in FIG. 3. FIG. 7 is a diagram illustrating the manufacturing steps for a rod according to the embodiment in the order from step (A) to step (D). FIG. 8 is a partial sectional side view illustrating a surface treatment apparatus (quenching apparatus) according to a modification of the present invention.DETAILED DESCRIPTION OF PREFERRED EMBODIMENTS OF THE INVENTIONA manufacturing method of a surface-treated component and an apparatus according to an embodiment of the present invention will be described below in detail by way of example with reference to FIGS. 1 to 7, wherein as the surface treatment, quenching is performed on a rod of a cylinder apparatus.FIG. 1 shows a hydraulic shock absorber 1 having a rod 4 locally subjected to quenching as a surface treatment process by a surface treatment component (quenched component) manufacturing method and a corresponding apparatus according to an embodiment of the present invention. The hydraulic shock absorber 1 as a cylinder device basically includes a cylinder 2, a piston 3, a rod (piston rod) 4, and a rod guide 5.The cylinder 2 has therein a hydraulic fluid sealed therein and is open at one end thereof (upper end in FIG. 1 ). Specifically, the cylinder 2 has a double tube structure including an inner tube 2A and an outer tube 2B. The bottom of the cylinder 2 is closed with a bottom cap 2C. The piston 3 is axially slidably fitted in the inner tube 2A of the cylinder 2 so as to divide the interior of the inner tube 2A into two chambers.The rod (piston rod) 4 as a quenched component (surface-treated component) has an axial end (the upper end in FIG. 1 ) that extends through the opening of the cylinder 2 toward the outside of the cylinder 2. The other axial end (lower end in FIG. 1 ) of the rod 4 is connected to the piston 3. The rod guide 5, which serves as a support member for the rod 4, is disposed in the opening of the cylinder 2 so as to be in sliding contact with the rod 4 via a collar 5A and a seal ring 5B (with relative displacement).The rod 4 is formed as an elongated circular column member (circular column rod or circular cylindrical tube) extending in an axial direction (the vertical direction in FIG. 1 ). The rod 4 is formed by the following manufacturing method. Specifically, the rod 4 is formed as a quenched component (surface-treated component) obtained by performing local quenching on a steel rod 11 (as a steel raw material) formed of a steel material (see FIGS. 2 to 7 ), the steel rod formed of a steel material being solid or hollow and having a circular (annular) cross section. Specifically, the rod 4 is formed by subjecting the steel rod 11 to quenching (high-frequency induction quenching), machining (plastic working, cutting working, machining, polishing working, etc.), coating (hard chromium coating), annealing, etc.The rod 4 has a sliding portion 4A and an intermediate portion 4B corresponding to quenched regions 12 and 13 described later, respectively (see FIGS. 2, 3, 6, and 7 ). The rod 4 further includes each of a mounting portion 4C at one end, a mounting portion 4D at the other end, and a machined portion 4E corresponding to the non-quenched regions 14, 15, and 16 described later (see FIGS. 2, 3, 6, and 7 ), respectively. The sliding portion 4A of the rod 4 is a region between the one-end attachment portion 4C and the machined portion 4E. When the hydraulic shock absorber 1 springs in and out, the sliding portion 4A (or the outer circumferential surface thereof) is in sliding contact with (i.e., moves in sliding contact with) the collar 5A and the seal ring 5B of the rod guide 5.The intermediate portion 4B of the rod 4 is a region between the other end attachment portion 4D and the machined portion 4E. The intermediate portion 4B is interposed between the piston 3 and a stopper 7 in the completed hydraulic shock absorber 1. In the embodiment, quenching (local quenching) is performed in regions of the rod 4 that are located on the axially opposite sides of the processed portion 4E, which corresponds to the sliding portion 4A and the intermediate portion 4B.One end (the upper end in FIG. 1 ) of the rod 4 forms a mounting portion 4C at the one end and has an outer diameter smaller than that of the sliding portion 4A and the intermediate portion 4B. The attachment portion 4C at the one end is fixed to a member not illustrated, for example, on the vehicle body side of a vehicle. The attachment portion 4C at the one end is a region cut to a reduced diameter and externally threaded by cutting or the like. Therefore, the attachment portion 4C at the one end was not quenched.The other end (the lower end in FIG. 1 ) of the rod 4 forms a fitting portion 4D at the other end and has a diameter smaller than that of the sliding portion 4A and the intermediate portion 4B. The attachment portion 4D at the other end has the piston 3 fixed thereto. By a nut 6 threadedly engaged with the distal end of the attachment portion 4D at the other end, the piston 3 is prevented from coming off the rod 4. The attachment portion 4D at the other end is a region cut to a reduced diameter and externally threaded by cutting or the like, and therefore the attachment portion 4D at the other end has not been quenched.The processed portion 4E of the rod 4 is a region interposed between the quenched regions 12 and 13, i.e., between the sliding portion 4A and the intermediate portion 4B. The machined portion 4E is provided with a full-circumference groove 4E 1 by plastic working or cutting working, and therefore the machined portion 4E has not been quenched. The full-circumference groove 4E1 is provided with a stopper (impact stopper) 7 abutting against the rod guide 5 to restrict further extension of the rod 4 when the rod 4 is already extended by a considerable amount. The stop 7 is fastened to the groove 4E 1 running over the entire circumference by a joining method, for example by metal flow joining.Next, referring to FIG. 7, a manufacturing method of the rod 4 for the hydraulic shock absorber 1 will be described.The rod 4 shown in FIG. 1 is formed by performing a quenching operation, a machining operation, a coating operation, a hardening operation, etc. on a solid or hollow steel rod 11 cut to a predetermined length as shown in part (A) of FIG. 7. Specifically, the steel bar 11 shown in part (A) of FIG. 7 is formed into the bar 4 shown in FIG. 1 by being sequentially subjected to a "quenching step" shown in part (B) of FIG. 7, a "machining step" shown in part (C) of FIG. 7, and a "machining step" shown in part (D) of FIG. 7, which are followed by a "coating step", a "hardening step", a "measurement step" (control step), etc., which are not shown in the figure, however.In the "quenching step" shown in FIG. 7(B), the steel bar 11 shown in FIG. 7(A) is "quenched" at two axially spaced portions by high-frequency induction quenching, thereby forming locally quenched regions 12 and 13. Of the two quenched portions 12 and 13, the quenched portion 12 located closer to the one end (the left end in FIG. 7 ) is formed in a portion which will become the sliding portion 4A when the rod 4 is completed. The other quenched portion 13, which is separated from the quenched portion 12 in the axial direction, i.e., located closer to the other end (the right end in FIG. 7 ), is formed in a region that will become an intermediate portion 4B when the rod 4 is completed. Regions on the opposite sides of the quenched regions 12 and 13 (which are the surface-treated regions) are non-quenched regions 14, 15, and 16 (i.e., regions that are not surface-treated). The non-quenched regions 14, 15, and 16 will form a mounting portion 4C at one end, a mounting portion 4D at the other end, and a machined portion 4E, respectively, in the finished rod 4. Note that the "quenching step" will be described in more detail later.After the quenched portions 12 and 13 are formed at two locations on the steel bar 11 as shown in part (B) of FIG. 7, the "machining step" shown in part (C) of FIG. 7 is performed. In the "machining step", a portion of the steel rod 11 located between the two quenched portions 12 and 13 is subjected to plastic working or cutting working to form a full-circumference groove 4E 1. The "machining step" can be formed by, for example, performing a cutting process in which the full-circumference groove 4E 1 is formed by a cutting tool 17 using a lathe or the like, or performing a plastic machining process in which the full-circumference groove 4E 1 is formed by pressing a non-illustrated roller against the steel bar 11. In this case, the region between the two quenched portions 12 and 13, i.e., the region which will become the processed portion 4E in the finished rod 4, is not quenched (non-quenched portion 15). Therefore, it is possible to easily and stably perform the plastic working or the cutting working for forming the full-circumference groove 4E 1.Further, in the "machining step" shown in FIG. 7(C), for example, the opposite ends of the steel rod 11 are also subjected to cutting machining to reduce the diameter of the end portions, thereby forming a mounting portion 4C at one end and a mounting portion 4D at the other end. In this case, like the portion where the full-circumference groove 4E 1 is formed, the ends of the steel rod 11 are not quenched (and form non-quenched portions 14 and 16). Therefore, here as well, it is possible to easily and stably perform the processing for forming the attachment portion 4C at the one end and the attachment portion 4D at the other end.After the full-circumference groove 4E 1, the attachment portion 4C at the one end, and the attachment portion 4D at the other end are formed as shown in part (C) of FIG. 7, the "machining step" shown in part (D) of FIG. 7 is performed. The "machining step" is performed before the "coating step". That is, before the "coating step", a machining operation or a polishing operation is performed at least on a part of a region to be coated in the "coating step", that is, a region of the steel rod 11 between the full-circumference groove 4E 1 and the attachment portion 4D at the other end. The "machining step" can be performed, for example, by performing a machining operation in which the surface of the steel bar 11 is ground with a grinding stone 18 using a grinding machine, or by performing a polishing operation in which the surface of the steel bar 11 is polished using a grinding cloth, paper, or grain, or another grinding material.Consequently, the surface roughness of the area to be coated can be smoothed before the "coating step". Consequently, it is possible to improve the surface condition of a coating layer formed in the subsequent "coating step" and the adhesion properties (the strength of the coating) of the coating layer. Note that the "coating step", the "hardening step", the "measurement step (control step)", etc. following the "machining step" are described in, for example, the above-described Japanese Patent Application Publication No. 2013-209 709, and therefore, further explanations thereof are omitted.Next, referring to FIGS. 2 to 6, the "quenching step" in which the steel rod 11 is locally quenched will be described.FIGS. 2 to 6 show a quenched component manufacturing apparatus 21 (surface-treated component), which will hereinafter be simply referred to as "the manufacturing apparatus 21", which locally quenches (surface-treated) a plurality of steel bars 11 aligned in the axial direction in an end-to-end arrangement while the steel bars 11 are moved in the axial direction. The manufacturing apparatus 21 includes a feed roller device 22, a pressure roller device 24, a guide member 25, a detection sensor 26, and a quenching device 27.The feed roller device (steel bar feeding device) 22 functioning as the moving device moves the steel bars 11 in the axial direction of the steel bars 11. that is, the feed roller device 22 feeds (feeds) the steel bars 11 in the running direction of the steel bars 11, whereby a plurality of steel bars 11 arranged in the axial direction without a clearance are moved in the axial direction. The feed roller device 22 includes a plurality of rotating rollers (feed rollers) 22A that feed the steel rods 11, a base 22B in which the rotating rollers 22A are rotatably supported, and a motor, not shown, that rotationally drives the rotating rollers 22A. The term "without clearance" will be described below. A steel bar disposed downstream of the feed roller device 22 in the running direction of the steel bars is moved by a force in the axial direction exerted by another steel bar just passing through the feed roller device 22. Consequently, the "clearance" is a state in which one steel rod can be advanced by power transmission via another steel rod adjacent to the one steel rod, and in which the one steel rod can be displaced radially relative to the other steel rod with the urging force from the pressure roller device 24.The base 22B of the feed roller device 22 is provided with, for example, ten rotary rollers 22A divided into two groups (upper and lower) of five rotary rollers 22A vertically opposing each other. In other words, the base 22B of the feed roller device 22 is provided with five sets of a pair of (upper and lower) rotary rollers 22A, i.e., a total of ten rotary rollers 22A. Consequently, the feed roller device 22 feeds (or "pushes" out) steel bars 11 by clamping the steel bars 11 from above and below with a plurality of rotary rollers 22A, and rotationally driving the rotary rollers 22A with a motor. As shown in Fig. 4, each rotary roller 22A in this case is formed substantially into an hourglass shape having a smaller diameter in an intermediate portion in the axial direction of the rollers than at the opposite ends thereof.The base 22B of the feed roller device 22 includes an upper roller supporting portion 22B 1 disposed on the upper side of the steel rods 11 moving in the axial direction such that the upper rotary rollers 22A are supported, and a lower roller supporting portion 22B 2 disposed on the lower side of the steel rods 11 such that the lower rotary rollers 22A are supported. In this case, the lower roller support portion 22B 2 extends forward in the running direction (the moving direction) of the steel bars 11 more than the upper roller support portion 22B 1, and the front end of the lower roller support portion 22B 2 is connected to the base 24C of the later-described press roller device 24.A portion of the lower roller supporting portion 22B 2 downstream of the rotating rollers 22A (i.e., located more forward in the running direction of the steel bars 11) is provided with a plurality of (two) idle rollers (support rollers) 23 located below the axially moving steel bars 11. The idle rollers 23 guide the steel bars 11 discharged from the region between the vertically opposed rotary rollers 22A toward the axially more forward side, i.e., the running direction of the steel bars 11, and the idle rollers 23 are vertically opposed to a guide member 25 described later. That is, unlike the rotary rollers 22A, the idle rollers 23 are not opposed to corresponding roller counterparts. It should be noted that the idle rollers 23, as well as the rotary rollers 22A, are also substantially in the form of an hourglass.The pressure roller device 24 functions as a urging device and is disposed downstream of the feed roller device 22. Specifically, the pressure roller device 24 of the front-most rotating rollers 22A in the running direction is disposed downstream of the feed roller device 22 (specifically, the front-most idler roller 23) in the running direction in such a manner as to be disposed vertically opposite to the guide member 25. As shown in Fig. 6, the press roller means 24 advances a steel rod 11 passing thereover (directed toward the press roller means 24) such that an end portion 11A of a steel rod 11 (a steel rod disposed opposite to the press roller means) crossing the press roller means 24 is radially displaced relative to an end portion 11B of another steel rod 11 adjacent to the one steel rod 11. In the embodiment, the press roller device 24 presses the rear side (the rear side in the running direction of the steel bars 11; the rear side and the counter running direction side, respectively) of the one steel bar 11 to be raised (displaced upward) from the running direction of the steel bars 11.Consequently, the pressurizing roller device 24 basically includes an elastic member 24A formed of, for example, a coil spring, a pressurizing roller 24B that presses the steel bar 11 in a radial direction of the steel bar 11 in the radial direction with the elastic force of the elastic member 24A while guiding the steel bar 11 in the running direction, and a base 24C that supports the pressurizing roller 24B via the elastic member 24A.The base 24C of the pressure roller device 24 is connected to the base 22B of the feed roller device 22, i.e., to the front end of the lower roller supporting portion 22B2. Consequently, the base 22B of the feed roller device 22 and the base 24C of the pressure roller device 24 are integrally formed with each other. It should be noted that the pressure roller 24B may be formed substantially in the shape of an hourglass roller as in the case of the idle rollers 23 and the rotary rollers 22A.The guide member 25 is disposed as a guide means across the steel bar 11 at a position opposite to the platen roller 24B, i.e., on a side toward which the steel bar 11 is pressed by the platen roller means 24, so as to be opposite to the platen roller means 24 (or the platen roller 24B thereof). The guide member 25 guides the steel rod 11 when the latter has been displaced in its radial direction.That is, when the steel bar 11 has been released from the pinch by the feed roller means 22 from the pinch by the feed roller means 22, that is, when the rear end portion 11A of the steel bar 11 has advanced over the most upstream rotary rollers 22A, thereby releasing it from the clamping action of the rotary rollers 22A, and further passes over the most upstream idler roller 23, the rear end (end portion 11A) of the steel bar 11 is raised (displaced upward) by the urging force of the pressure roller means 24. When the steel bar is displaced upward by the urging force of the press roller device 24 (i.e., by the pressure of the press roller 24B), the guide member 25 limits the amount of displacement of the steel bar 11 within a predetermined range (i.e., prevents the steel bar 11 from being radially displaced more than a predetermined amount).Consequently, the guide member 25 is formed as a substantially plate-shaped horizontally extending member and has a recess 25A disposed at a position facing the platen device 24 so as to abut against (or receive) the radially offset steel rod 11. In this case, the position of the bottom of the recess 25A corresponding to the displacement amount of the steel bar 11 is set such that the steel bar 11 can be displaced toward a position at which a detection sensor 26 described later can detect the presence or absence of an end (an end portion 11A or 11B or an end surface) of a steel bar 11. Specifically, the position of the bottom of the recess 25A may be set so that the steel rod 11 can be displaced until the end portion 11A of the steel rod 11 is brought out of alignment with the detection position of the detection sensor 26 (or a position opposite to a detection portion 26A) by the urging force of the press roller device 24.When the steel rods 11 to be quenched are changed to use rods whose diameters and / or lengths are different from the rods quenched so far, the position of the guide member 25 is adjusted according to the dimensions of the steel rods 11 to be quenched from now on. Consequently, it is possible to simplify a change in setup (the adjustment of the manufacturing apparatus 21) when quenching of steel bars 11 different in size from the steel bars thus far quenched is started.The detection sensor (detector) 26 functioning as detection means is disposed between the platen means 24 and the guide member 25. The detection sensor 26 detects the presence or absence of an end (an end portion 11A or an end surface) of the one steel rod 11 that has been radially displaced by the platen device 24, or the end (the end portion 11B or the end surface) of the other steel rod 11.The detection portion 26A is disposed, for example, at a position where the detection portion 26A is not directed to (or faces) an end portion 11A of the one steel bar 11 when the end portion 11A is radially offset by the urging force (the pressing force) of the press roller device 24, and where the detection portion 26A is directed to (or faces) the one steel bar 11 when the end portion 11A is not radially offset. In this case, the detection sensor can detect that the end (the end portion 11A or the end surface) of the one steel bar 11 has passed the detection portion 26A when a state in which the detection portion 26A faces the steel bar 11 has changed to a state in which the detection portion 26A is not opposed to the steel bar 11. Further, the detection sensor 26 can detect the fact that the end (the end portion 11B or the end surface) of another steel rod 11 has passed the detection portion 26A by changing (changing) a state in which the detection portion 26A is not opposed to the steel rod 11 to a state in which the steel rod 11 is opposed to the detection portion 26A. In any case, it is possible to surely detect the passing of the end (the end portion 11A or 11B or the end surface) of one or the other steel rod 11.Note that the detection sensor 26 may be attached to the guide member 25. In this case, various combinations of the detection sensor 26 and the guide member 25 are conceivable for various groups of steel bars 11 to be quenched, which differ from each other in diameter of the length, etc. That is, various combinations of the detection sensor 26 and the guide member 25 can be provided, each having positional and dimensional relationships corresponding to various dimensions of the steel bars 11 to be quenched. When the steel bars 11 to be quenched are changed to have different dimensions as compared with the steel bars quenched so far, the guide member 25 is changed, together with the detection sensor 26 attached thereto, to another combination of the guide member 25 and the detection sensor 26 suitable for detecting the steel bars 11 to be quenched from now on. Consequently, when quenching of steel bars 11 different in dimension from the steel bars quenched to date is started, it is possible to simplify a change in setup, i.e., adjustment of the manufacturing apparatus 21.The detection sensor 26 may be, for example, a non-contact sensor or switch, e.g., a load sensor, which detects the fact that the end portion 11A of the one steel rod 11 abuts against the recess 25A of the guide member 25. That is, the detection sensor 26 may be selected from any sensors and switches capable of detecting the presence or absence of an end (the end portion 11A or the end surface) of the one steel rod 11 or the end (the end portion 11B or the end surface) of the other steel rod 11 (i.e., capable of detecting the passage of the end).Further, in the embodiment, the detection sensor 26 (or the detection portion 26A thereof) is disposed at a position corresponding to that end of the steel bar 11 which is displaced by the urging force of the press roller device 24 and is located on the rear side (the side opposite to the running direction; the side located on the rear side or the downstream side in the running direction) at which the one steel bar 11 is raised (or displaced upward). As shown by the two-dot chain line 26A' in FIG. 3, the detection sensor 26' (or the detection portion 26A' thereof) may be disposed at a position corresponding to the end of the one steel bar 11 that has been radially displaced by the urging force and is located on the front side (the side disposed in the running direction; the front or upstream side in the running direction) at which the one steel bar 11 is lowered (or displaced downward). Further, it is also possible to arrange the detection sensors 26 (or the detection portions 26A thereof) at positions corresponding to the rear and front ends of the one steel bar 11, respectively.The quenching device 27 as a surface treatment device is disposed downstream of the detection sensor 26 in the running direction of the steel bars 11. The quenching means 27 is, for example, a high frequency induction quenching means having an induction heating coil 27A surrounding the entire periphery of a steel rod 11. The quenching means 27 sets a quenching time, i.e., a timing for energizing (i.e., turning on) and de-energizing (i.e., turning off) the induction heating coil 27A based on the detection result by the detection sensor 26, and forms the quenched portions 12 and 23 on the steel bar 11 at the set timings.That is, the quenching device 27 energizes (i.e., turns on) the induction heating coil 27A when the portions of a steel bar 11 where quenched portions 12 and 13 are to be formed pass through the induction heating coil 27A, and de-energizes (i.e., turns off) the induction heating coil 27A when the portions of a steel bar 11 pass through the induction heating coil 27A that are to form non-quenched portions 14, 15, and 16. In this regard, the timing of energizing and deenergizing the induction heating coil 27A may be set based on, for example, the time elapsed from the detection of the end portion (the end portion 11A or 11B or the end surface) of the one or other steel bar 11 by the detection sensor 26 (i.e., from the time when the detection sensor 26 detects the passing of the aforementioned end). The minimum range within which the induction heating coil 27A can perform quenching when a steel rod passes through the induction heating coil 27A is sufficiently short relative to a width of the non-quenched portions 15, 16 and the quenched portion 13.In this case, the timing of quenching performed by the quenching device 27 (i.e., the timing of energizing and deenergizing the induction heating coil 27A) may be determined based on the detection result of the detection sensor 26 capable of reliably detecting the end (the end portion 11A or 11B or the end surface) of one or the other steel rod 11. Therefore, the quenching device 27 can accurately form the quenched portions 12 and 13 on each of the axially moving steel bars 11 at the desired positions.In addition, a combination of revolving rolls 28 and a holding plate 29 is disposed in front of and behind the quenching device 27, i.e., both on the side downstream of the quenching device 27 in the running direction of the steel bars 11 and on the upstream side. The revolving rollers 28 rotate the steel rods 11 moving in the axial direction in the circumferential direction. The holding plate 29 prevents the steel bars 11 rotating in the circumferential direction by the revolving rollers 28 from coming off the revolving rollers 28 upward, i.e., guides the steel bars 11 rotating in the circumferential direction in the running direction thereof.In addition, a sprinkler 30 is disposed downstream of the quenching device 27 for cooling the steel bars 11 which have passed through the induction heating coil 27A of the quenching device 27. The revolving rollers 28 can rotate a steel rod 11 passing through the induction heating coil 27A in the circumferential direction. Thus, the quenched portions 12 and 13 can be formed uniformly over the circumferential direction of the steel rod 11.Note that the embodiment is configured such that the urging force of the press roller device 24 causes the back side of the one steel bar 11 to be raised (displaced upward) and the front side of the one steel bar 11 to be lowered (displaced downward). Consequently, the corresponding revolving roller 28 is arranged to be displaced from its position corresponding to the front side (the front end) of the one steel bar 11 when the rear side of the one steel bar 11 is raised (radially displaced) by the urging force of the press roller means 24. Alternatively, by arranging the associated revolving roller 28 at a position corresponding to the front side (the front end of the one steel bar 11) when only the rear side of the one steel bar 11 is raised, the arrangement may be configured such that only the rear side of the one steel bar 11 is raised, which means that the front side of the one steel bar 11 continues unchanged in the running direction while only the rear side of the steel bar 11 is raised radially.In an arrangement in which both the front and rear sides of the one steel bar 11 are displaced from the running direction by the urging force of the pressure roller device 24, as in this embodiment, the inclination angle (the displacement angle from the running direction) of the entire one steel bar 11 can be set larger with respect to the displacement amount (the amount of radial displacement) on the rear side of the one steel bar 11 than in an arrangement in which the front side of the steel bar 11 is not displaced (i.e., in which only the rear side thereof is displaced). Consequently, it is possible to improve the reliability of detection by the detection sensor 26 while restraining the increase in the displacement amount (an amount of radial displacement) of the rear side of the one steel rod 11. As a result, it is possible to achieve both stable axial movement of a plurality of steel rods 11 and reliable detection.The following is a manufacturing method using the manufacturing apparatus 21 according to the embodiment having the above-described structure.The manufacturing method according to the embodiment subjects a plurality of steel bars 11 to a local quenching process as a surface treatment, the steel bars being lined up in an end-to-end arrangement in the axial direction while the steel bars 11 are moved in the axial direction. The manufacturing method includes a moving step, a detecting step, and a quenching step.In the moving step, the steel bars 11 are moved in the axial direction by the feed roller device 22 moving the steel bars 11. Further, in the moving step, the steel bars 11 are pinched between the pairs of rotary rollers 22A (upper and lower rotary rollers 22A) of the feed roller device 22, and in this state, moved by a predetermined portion by the rotation of the rotary rollers 22A. Therefore, the steel bars 11 advance toward the detection sensor 26 and the quenching device 27.In the subsequent detection step, the pressurizing roller device 24 applies a urging force to a steel rod 11 arriving at the pressurizing roller device 24 while moving in the axial direction of the steel rods 11 such that an end portion 11A of the one steel rod 11 is displaced in the radial direction of the steel rod 11 relative to an end portion 11B of another steel rod 11 adjacent to the one steel rod 11, and the detection sensor 26 detects the passage of the end (the end portion 11A or 11B or the end surface) of the one or the other steel rod 11. In the detection step, the pressurizing roller device 24 urges the one steel rod 11 to be displaced in the radial direction thereof, and the guide member 25 guides the one steel rod 11 displaced in the radial direction, that is, when the one steel rod 11 is displaced radially, It abuts against the bottom of the recess 25A in the guide member 25, thereby preventing the steel bar from being further displaced in the radial direction (raised further upward).The above-described detecting step is designed such that the rear side of the one steel bar 11 is displaced when the one steel bar 11 is released from the clamping action by the feed roller device 22. More specifically, by the urging force of the pressure roller device 24, both the front side and the rear side of the one steel bar 11 are then radially displaced from the running direction (the front side is lowered; the rear side is raised). Then, in the detecting step, detection of the radially offset end of the one steel rod 11 is performed. Specifically, the detecting step is configured to detect the passage of the rear end (of the end portion 11A or the end surface) of the one steel bar 11 radially offset by the urging force of the pressurizing roller device 24, or the passage of the front end (of the end portion 11B or the end surface) of the other steel bar 11 adjacent to the one steel bar 11. Consequently, the passage of the end portion 11A or 11B or the end surface of one or the other steel rod 11 can be detected securely with the detection sensor 26.In the subsequent quenching step as the surface treatment step, the timing of quenching (surface treatment) of the steel rod 11 is determined based on the detection result of the detection sensor 26, and locally quenched portions 12 and 13 are formed on the steel rod 11 by the quenching device 27. In this case, the timing for quenching is determined based on the detection result by the detection sensor 26 suitable for reliably detecting the passage of the end (the end portion 11A or 11B or the end surface) of the one or the other steel rod 11. Therefore, the quenching device 27 can accurately form the quenched portions 12 and 13 on the axially moving steel rod 11 at the desired positions. Further, as shown in part (C) of FIG. 7, the quenching step is followed by a processing step in which plastic processing or cutting processing is performed on the non-quenched portions 14, 15, and 16 of the steel bar 11. Since the non-quenched portions 14, 15, and 16 are left in a non-quenched state, a machining operation such as plastic working or cutting working can be easily performed.Therefore, according to the embodiment, when a plurality of steel bars aligned in the axial direction in an end-to-end arrangement are locally quenched while the steel bars are axially moved, it is possible to securely grasp an end portion 11A or 11B or an end surface (or passage thereof) of each steel bar 11, and therefore it is possible to improve productivity.That is, the embodiment is designed so that, in a plurality of steel bars 11 moving axially in an end-to-end arrangement, it can detect, by means of the detection sensor 26, the presence or absence of an end portion 11A or an end face of one steel bar 11 radially offset by the pressure roller device 24, or an end face 11B of another steel bar 11 adjoining the one steel bar 11. Consequently, it is possible to securely grasp the passage of the end portion 11A or 11B or the end surface of one or the other steel rod 11. Further, the timing for quenching by the quenching device 27 is set based on the detection result by the detection sensor 26. Therefore, the quenching device 27 can accurately form quenched portions 12 and 13 on each of the axially moving steel bars 11 at the desired positions.As a result, the productivity of the steel bars 4 can be improved. In particular, it is possible to obtain the following improvements in productivity: an increase in productivity (i.e., an increase in production rate) obtained by the end-to-end alignment in the axial direction of the steel bars 11; a reduction in machining enabled by omitting a machining step that would otherwise be necessary to facilitate the detection of the end portion 11A or 11B of the steel bars 11 (i.e., a step of applying a chamfer or other machining operations to the end portion 11A of each steel bar 11); a reduction in scrap (i.e., an increase in yield) obtained by allowing the quenched portions 12 and 13 to be formed accurately; and so forth.According to the embodiment, the moving step is configured such that the steel bars 11 are moved by the feed roller device 22 including pairs of rotary rollers 22A through a predetermined portion by sandwiching the steel bars 11 between the pairs of rotary rollers 22A. In this case, a plurality of steel bars oriented end-to-end in the axial direction can be stably moved in the axial direction by the rotary roller pairs 22A.According to the embodiment, the detecting step is configured such that a steel rod 11 is radially displaced in the radial direction of the steel rod 11 by the urging force of the pressurizing roller device 24, and the steel rod 11 is guided by the guide member 25 when the steel rod 11 is radially displaced. In this case, the steel rod 11 can be stably displaced in the radial direction by the pressure roller means 24. In addition, the radially offset steel rod 11 is guided by the recess 25A of the guide member 25, whereby the detection sensor 26 makes it possible to stably detect the presence or absence of an end (an end portion 11A or 11B or an end surface) of a steel rod 11 or another steel rod 11 adjacent thereto.According to the embodiment, the detecting step is configured such that the back side of the one steel bar 11 is displaced when released from the gripping by the feed roller device 22. That is, the back side of the one steel bar 11 is radially displaced from the axial direction, which is the running direction of the steel bars 11, by the urging force of the pressure roller device 24. Consequently, the steel rod 11 can be stably radially displaced while being moved in the running direction.The embodiment is configured such that the radially offset end (the end portion 11A or the end surface) of the one steel rod 11 is detected. That is, the embodiment is configured such that the rear end (the end portion 11A or the end surface) of the one steel rod 11 radially displaced by the urging force of the pressure roller device 24 is detected. Consequently, it is possible to improve the reliability of detection of the end portion 11A or the end surface of the one steel bar 11 by detecting, with the detection sensor 26, the presence or absence of the rear end (the end portion 11A or the end surface) of the one steel bar 11 (i.e., detecting whether or not the rear end has passed the detection sensor 26).The embodiment is configured such that after the quenching step, the processing step is performed in which the non-quenched portions 14, 15, and 16 of the steel rod 11 are subjected to plastic processing or cutting processing. In this case, since the non-quenched portions 14, 15, and 16 are not quenched, the plastic working and the cutting working can be easily performed, respectively.According to the embodiment, the feed roller device 22 is configured to nip the steel bars 11 from above and below with a plurality of rotation rollers 22A. In this case, a plurality of steel bars 11 can be stably moved in the axial direction by a plurality of rotating rollers 22A clamping the steel bars 11 from above and below.According to the embodiment, the detection sensor 26 is mounted on the guide member 25 which guides a radially offset steel rod 11. Therefore, it is possible to simplify the setting (or a change in setup) of the manufacturing apparatus 21 when starting to quench steel bars 11 which differ in their dimensions from the steel bars quenched so far.Note that the present invention has been described in the foregoing embodiment by way of an example in which the pressure roller device 24 functioning as the urging device is disposed downstream of the feed roller device 22 functioning as the moving device. However, the present invention is not limited to this described structure. For example, as a modification shown in FIG. 8, a feed roller device 31 functioning as a moving device may have two (multiple) separate (separate) regions, i.e., an upstream region 31A and a downstream region 31B, and the pressure roller device 24 may be disposed at the center of the feed roller device 31 (i.e., between the upstream region 31A and the downstream region 31B).In the foregoing embodiment, the invention has been described by way of an example in which the feed roller device 22 functioning as a moving device is configured to nip the steel bars 11 from above and below with a plurality of rotation rollers 22A. However, the present invention is not limited to this described structure. For example, the moving device (the feed roller device) may be configured to clamp the steel bars laterally (for example, from the left and right sides) with a plurality of rotating rollers. The same applies to the modification described above.In the foregoing embodiment, the present invention has been described by way of an example in which quenching as a surface treatment is performed on each steel bar 11 at two positions (i.e., the quenched portions 12 and 13 are formed at two positions), but the present invention is not limited thereto. Quenching may be performed on each steel bar at one position (e.g., a quenched region may be formed between un-quenched regions located at opposite ends of the steel bars). Alternatively, quenching may be performed on each steel bar at three or more positions. The same applies to the modification.In the foregoing embodiment, the present invention has been described by way of example in which the steel bars 11 are circular in cross section, but the invention is not limited thereto. For example, the cross-sectional configuration of the steel bars may be rectangular or polygonal or otherwise may deviate from a circular shape. The same applies to the modification.In the foregoing embodiment, the present invention has been described by way of an example in which, in the pressure roller device 24 functioning as the urging device, an urging force was applied to the steel rod 11 using the elastic force of an elastic member 24A. However, the present invention is not limited to this described structure. For example, a urge force may be applied to the steel rod using gas pressure (in the form of a gas spring), for example, air pressure. That is, it is possible to use any urging means capable of applying urging force to the steel rod in the radial direction thereof. The same applies to the modification.In the foregoing embodiment, the present invention has been described by way of an example in which a urging force is applied (pressed) to the steel bar 11 by the pressing roller 24B. However, the present invention is not limited to this described structure. The steel rod can be directly acted upon by a urging device with a urging force. For example, it is possible to employ a structure in which a urging force is radially applied to the steel rod directly against the steel rod by inflating a gas, e.g., compressed air, functioning as urging means.In the foregoing embodiment, the present invention has been described by way of an example in which the present invention is applied to a rod 4 used as a quenched component in the hydraulic shock absorber 1. However, the application of the present invention is not limited thereto. For example, the present invention can also be applied to a rod used in another cylinder device, e.g., a hydraulic cylinder. Further, the present invention is applicable not only to rods of cylinder equipment but also to quenched components contained in other apparatuses, and in particular, the invention is applicable to quenched components to be locally provided with quenched portions.In the foregoing embodiment, the present invention has been described by way of an example in which quenching is carried out as a surface treatment, but the present invention is not limited thereto. For example, the present invention can be implemented for any operation in which the surface of a component is to be locally subjected to surface treatment, for example, a plating operation such as a chrome plating, a plating operation, a coloring operation, a cutting operation, etc.According to the foregoing embodiment, when performing surface treatment (quenching) on a plurality of steel bars aligned in an end-to-end arrangement in the axial direction, it is possible to securely grasp one end (an end portion or an end surface) of each steel bar while the steel bars are moved axially, enabling an increase in productivity.That is, the embodiment is configured to detect, with a detection means, an end of a steel rod radially displaced by a urging means or an end of another steel rod that adjoins the one steel rod (i.e., detect the presence or absence of the end of the one or the other steel rod) among the plurality of steel rods axially moving in an end-to-end axial alignment relationship. Consequently, it is possible to securely grasp the end of one or the other steel rod (e.g., passing through the end). Further, the timing for the surface treatment (quenching) by a surface treatment device (quenching device) is determined based on the detection result by the detection device. Therefore, a surface-treated portion (a quenched portion) can be accurately formed on each axially moving steel rod at a desired position.As a result, regarding the surface-treated components (quenched components) to be locally subjected to surface treatment (quenching), it is possible to improve productivity. In particular, it is possible to achieve the following productivity improvements: an increase in productivity (i.e., an increase in production rate) due to the end-to-end alignment of the steel bars in the axial direction; a reduction in machining yield obtained by omitting a machining step that would otherwise be necessary to facilitate the detection of an end of each steel bar (e.g., a step of applying a chamfer or other machining features to the end portion of each steel bar); a reduction in scrap (i.e., an increase in yield) obtained by accurately forming the surface-treated regions (quenched regions), etc.According to the embodiment, the moving step is configured such that the steel bars are moved by a predetermined portion using a moving device having a pair of rotary rollers by sandwiching the steel bars between the pair of rotary rollers. In this case, a plurality of steel bars aligned in the axial direction in an end-to-end arrangement can be stably moved in the axial direction by the pair of rotation rollers.According to the embodiment, the detecting step is configured such that a steel rod is radially displaced in the radial direction of the steel rod by applying a urging force to the steel rod with the urging means, and the radially displaced steel rod is guided using a guide means. In this case, the steel bar can be stably displaced in the radial direction by the urging means. In addition, the radially offset steel rod is guided by the guide means, whereby it is possible to stably detect with the detection means an end of one steel rod or another steel rod adjacent thereto (i.e., to detect the presence or absence of an end of one or the other steel rod).According to the foregoing embodiment, the detecting step is configured such that the rear side of the one steel rod is displaced when the one steel rod is released from the clamping action by the moving means. Specifically, the rear side (the rear side in the running direction; the rear or trailing side in the running direction) of the one steel bar is radially displaced from the axial direction, which is the running direction of the steel bars, by the urging force of the urging means. Consequently, the one steel rod can be stably radially displaced while being moved in the running direction.According to the embodiment, the radially offset end of the one steel rod is gripped. That is, the embodiment is configured such that the rear end (the rear end in the running direction; the rear or trailing end in the running direction) or the front end (the front end in the running direction; the front or leading end in the running direction) of the one steel bar radially displaced by the urging force of the urging means is detected. Consequently, it is possible to improve the reliability of detecting the end of the steel bar by detecting the presence or absence of the rear end or the front end of the steel bar by the detecting means (i.e., by detecting whether or not the rear or the front end has passed the detecting means). In this case, the reliability of the detection can be further improved by performing detection of the presence or absence of both the rear and front ends.According to the embodiment, the surface treatment step (quenching step) is followed by a processing step of performing plastic working or cutting working on a non-surface treated region (a non-quenched region) of the steel rod. Since the non-surface treated portion (non-quenched portion) has not undergone surface treatment (quenching), the plastic working or the cutting working can be easily performed.According to the embodiment, the moving means is configured to nip a steel bar from above and below with a plurality of rotating rollers. In this case, by the plurality of rotation rollers clamping the steel bars from above and below, a plurality of steel bars can be stably moved in the axial direction.According to the embodiment, the moving device is designed to laterally clamp a steel bar having a plurality of rotating rollers. In this case, by the plurality of rotation rollers laterally sandwiching the steel bars, a plurality of steel bars can be stably moved in the axial direction.According to the embodiment, the detection means is mounted on a guiding means which guides a steel rod when it is laterally offset. Therefore, it is possible to provide various combinations of detection and guide means for various groups of steel bars which are to be subjected to surface treatment (quenching) and different from each other in diameter, length, etc. That is, it is possible to provide various combinations of a detection sensor and a guide member having positional and dimensional relationships corresponding to various dimensions of the steel bars to be subjected to surface treatment (quenching). When the steel bars to be subjected to surface treatment (quenching) are changed to be different from the steel bars which have been surface-treated (quenched) so far, the guide means is changed, together with the detection means attached thereto, to another combination of a guide means and a detection means which are suitable for the dimensions of the steel bars to be subjected to surface treatment (quenching) from now on. Therefore, it is possible to facilitate a modification of the setup when surface treatment (quenching) of steel bars different in dimension from the previously surface-treated (quenched) steel bars is started.

Claims

A manufacturing method for a surface-treated component (4) by locally treating respective surfaces of a plurality of steel bars (11) aligned without a clearance in an axial direction of the steel bars (11) while the steel bars (11) are moved in the axial direction, the method comprising: a moving step of moving the steel bars (11) in the axial direction with a moving device (22, 31) moving the steel bars (11); a detecting step of using a urging means (24) disposed either downstream of the moving means (22, 31) or at a center of the moving means (22, 31) to urge one of the plurality of steel bars (11), when the one steel bar (11) arrives at the urging means (24) while moving in the axial direction, in a radial direction of the one steel bar (11) such that an end of the one steel bar (11) is displaced relative to an end of another steel bar (11) adjacent to the one steel bar (11) in the radial direction, and detecting the end of the one steel bar (11) or the end of the other steel bar (11) with a detecting means (26); and a surface treatment step of locally forming a surface treated region on each of the steel bars (11) with a surface treatment device (27) according to a timing for the surface treatment set based on a detection result by the detection device (26).The production method for a surface-treated component (4) according to claim 1, wherein the surface treatment is quenching.The manufacturing method for a surface-treated component (4) according to claim 1 or 2, wherein the moving means (22, 31) includes a pair of rotating rollers (22A), and the steel bars (11) are moved through a predetermined portion in the moving step by sandwiching the steel bars (11) between the pair of rotating rollers (22A).The manufacturing method for a surface-treated component (4) according to any one of claims 1 to 3, wherein the one steel bar (11) is displaced in the radial direction by a urging action by the urging means (24) in the detecting step, and the one steel bar (11) is guided by a guide means (25) when displaced in the radial direction.The manufacturing method for a surface-treated component (4) according to any one of claims 1 to 4, wherein in the detecting step, a rear end of the one steel bar (11) is displaced when the one steel bar (11) is released from a clamping action by the moving means (22, 31).The manufacturing method for a surface-treated component (4) according to any one of claims 1 to 5, wherein the end of the one steel rod (11) offset in the radial direction is detected in the detecting step.The manufacturing method for a surface-treated component (4) according to claim 1, wherein the surface treatment step is followed by a processing step of applying plastic working or cutting working to a non-surface-treated region (14, 15, 16) of each steel bar (11).A manufacturing apparatus (21) for a surface-treated component (4) configured to locally surface-treat a plurality of steel bars (11) aligned in an end-to-end arrangement in an axial direction of the steel bars (11) while the steel bars (11) are moved in the axial direction, the apparatus comprising: moving means (22, 31) configured to move the steel bars (11) in the axial direction; a urging means (24) disposed either downstream of the moving means (22, 31) or at a center of the moving means (22, 31) for urging one of the plurality of steel rods (11) in a radial direction of the one steel rod (11) such that an end of the one steel rod (11) in the radial direction is offset relative to an end of another steel rod (11) adjacent to the one steel rod (11); a detecting means (26) configured to detect the end of the one steel rod (11) offset in the radial direction by the urging means (24) or the end of the other steel rod (11); and a surface treatment device (27) configured to locally form a surface treated region (12, 13) on each of the steel bars (11) according to a timing for the surface treatment, the timing being set based on a detection result by the detection device (26).The manufacturing apparatus (21) for a surface-treated component (4) according to claim 8, wherein the moving means (22, 31) is configured to nip the steel bars (11) from above and below with a plurality of rotating rollers (22A).The manufacturing apparatus (21) for a surface-treated component (4) according to claim 8, wherein the moving means (22, 31) is configured to laterally clamp the steel bars (11) with a plurality of rotating rollers (22A).The manufacturing apparatus (21) for a surface-treated component (4) according to any one of claims 8 to 10, wherein the detection means (26) is attached to a guide means (25) configured to guide the steel rod (11) when offset in the radial direction.

Citation Information

Patent Citations

  • Roller Horizontal High Frequency Quenching Machine Tool

    CN201610436U

  • Method for producing plated component and plated component

    JP2013209709A

  • Pipe coupling machine

    KR100771451B1

  • Apparatus for heat treating steel pipe

    KR101169709B1

  • CN000201610436U