Polishing pad, method for producing a polishing pad and polishing method

The dual-groove design on polishing pads for CMP devices ensures consistent suspension flow and extended life by alternating groove exposure, addressing inefficiencies in conventional pads and reducing maintenance needs.

DE102016114798B4Active Publication Date: 2024-10-24TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
DE102016114798
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2016-05-18
Filing Date
2016-08-10
Publication Date
2024-10-24
Estimated Expiration
2036-08-10

AI Technical Summary

Technical Problem

Conventional polishing pads for chemical-mechanical planarization (CMP) face inefficiencies in suspension flow rate and pad life due to deep grooves requiring high suspension flow rates and frequent maintenance, leading to reduced polishing effectiveness and increased downtime.

Method used

The introduction of first and second grooves in different horizontal planes on the polishing layer, with the second groove being buried or partially buried, ensures continuous suspension flow and reduced wear, maintaining polishing efficiency and extending pad life by alternating groove exposure.

Benefits of technology

This configuration maintains polishing rate with reduced suspension usage, extends pad life, and decreases maintenance frequency, enhancing the operational efficiency of CMP devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000009_0000
    Figure 00000009_0000
  • Figure 00000010_0000
    Figure 00000010_0000
  • Figure 00000011_0000
    Figure 00000011_0000
Patent Text Reader

Abstract

Polishing pad (120, 120a, 120b, 120c, 120d) for a device (100) for chemical-mechanical polishing, wherein the polishing pad (120, 120a, 120b, 120c, 120d) comprises: a first support layer (128, 128a), wherein the first support layer (128, 128a) has at least one recess (1281), and a polishing layer (122) which is present on the first support layer (128, 128a) and has an upper surface (123) facing away from the first support layer (128, 128a) and at least one first cavity (126, 126a, 126b, 126c) which is arranged above the at least one recess (1281) and which extends at least below the upper surface (123) of the The polishing layer (122) is buried, wherein the at least one first cavity (126, 126a, 126b, 126c) and the at least one recess (1281) are aligned with each other.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND

[0001] Chemical-mechanical polishing / planarization (CMP) is a process for smoothing surfaces using the Combination of chemical and mechanical forces. The process uses an abrasive and corrosive chemical Suspension (slurry) in conjunction with a polishing pad. The CMP process can remove material from a wafer and aims to compensate for an uneven topography of the wafer, making the wafer flat or planar becomes.

[0002] US 2015 / 0 174 826 A1, JP 2005- 294 410 A, US 2006 / 0 286 350 A1 and DE 10 2012 018 200 A1 describe conventional polishing pads. JP 2008- 98 356 A describes a double-sided adhesive tape for attaching a polishing pad to a polishing device. BRIEF DESCRIPTION OF THE DRAWINGS

[0003] Aspects of the present disclosure are best understood from the following detailed description understood when read together with the accompanying drawings. It should be noted that according to the Standard industry procedures mean that various features are not drawn to scale. Dimensions of the various features may be enlarged or reduced as desired for clarity of discussion. Fig. 1 is a perspective view of a chemical mechanical polishing device according to some Embodiments of the present disclosure; Fig. 2 is an enlarged partial view of a polishing pad of the device for chemical polishing shown in Fig. 1. mechanical polishing; Fig. 3 (Prior Art) is a cross-sectional view of the polishing pad taken along line 3-3 shown in Fig. 2 is drawn; Fig. 4 (Prior Art) is a cross-sectional view of the polishing pad shown in Fig. 3 after a first groove of the polishing pad was exposed; Fig. 5 is an enlarged partial view of a polishing layer shown in Fig. 3; Fig. 6 is a cross-sectional view of a polishing pad according to some embodiments of the present Revelation; Fig. 7 is a cross-sectional view of a polishing pad according to some embodiments of the present Revelation; Fig. 8 (Prior Art) is a cross-sectional view of a polishing pad according to some embodiments of the this disclosure; Fig. 9 (Prior Art) is a cross-sectional view of a polishing pad according to some embodiments of the this disclosure; Fig. 10 is a flow chart of a method for manufacturing a polishing pad according to some Embodiments of the present disclosure, and Fig. 11 is a flow diagram of a polishing method according to some embodiments of the present Revelation. DETAILED DESCRIPTION

[0004] The following disclosure provides many different embodiments, or examples, for implementing various features of the subject matter at hand. Specific examples of components and arrangements are described below to simplify the present disclosure. For example, forming a first feature above or on a second feature in the description below include embodiments in which in which the first and second features are formed in direct contact, and may also include embodiments include features in which additional features can be formed between the first and second features, so that the first and second features may not be in direct contact. Furthermore, the present Disclosure may repeat reference numbers and / or letters in the various examples. This repetition is done for the purpose of simplicity and clarity and it does not prescribe any relationship between the different discussed embodiments and / or configurations.

[0005] In addition, terms relating to spatial relativity, such as ´´below´´, ´´under´´, ´´lower´´, ´´above´´, ´´upper´´ and the like, to facilitate the discussion, to Relationship of one element or characteristic to another element or characteristic (to other elements or characteristics), as shown in the figures. The terms relating to spatial relativity should different orientations of the device used or operated in addition to that shown in the figures The device can be oriented in a different way (rotated 90 degrees or otherwise aligned) and the terms used here that concern spatial relativity can equally be interpreted accordingly.

[0006] The present disclosure is described with reference to embodiments in a specific context, a polishing layer of a polishing pad, which has first and second grooves in different horizontal planes. The The first and second grooves can be used to hold a suspension for polishing a wafer. If the second groove is present in the upper surface of the polishing layer, the suspension can flow into the second groove and can through the second groove for polishing the wafer. After the second groove has been worn and disappears, the first groove buried in the polishing layer is exposed through the upper surface of the polishing layer. Consequently, the suspension can flow into the first groove and can be passed through the first groove for continuous polishing of the wafers. However, the embodiments of the disclosure may also be applied to a variety of polishing pads Various embodiments are described with reference to the accompanying drawings explained in detail.

[0007] Fig. 1 is a perspective view of a chemical mechanical polishing apparatus 100 according to some Embodiments of the present disclosure. As shown in Fig. 1, the device for chemical mechanical polishing 100 a clamping plate 110, a polishing pad 120, a suspension supply 130 and a Support device 140. The polishing pad 120 is present on the clamping plate 110 and has a polishing layer 122. The suspension supply 130 and the support device 140 are present above the polishing layer 122. When the When the chemical-mechanical polishing device 100 is in operation, the suspension supply 130 can Suspension 132 onto the polishing layer 122, and the polishing pad 120 can be moved in a direction D1 through the Clamping plate 110 is rotated. After the suspension 132 is distributed over the polishing layer 122 of the polishing pad 120 the carrier device 140 can press a wafer 210 in a direction D2 against the polishing layer 122, so that a the side of the wafer 210 in contact with the polishing layer 122 is polished by the suspension 132. For a further Planarization of the wafer 210, the carrier device 140 can rotate (e.g. also in the direction D1) and simultaneously on the polishing layer 122 of the polishing pad 120, but various embodiments of the present Disclosure is not limited in this regard.

[0008] Fig. 2 is an enlarged partial view of the polishing pad 120 of the apparatus shown in Fig. 1 for chemically mechanical polishing 100. Fig. 3 is a cross-sectional view of the polishing pad 120 in the prior art construction, which is drawn along the line 3-3 shown in Fig. 2. As shown in Fig. 2 and Fig. 3, the polishing pad comprises 120 the polishing layer 122 and a first support layer 128. The polishing layer 122 is present on the first support layer 128. The first support layer 128 is arranged between the clamping plate 110 (see Fig. 1) and the polishing layer 122. The first support layer 128 is harder than the polishing layer 122, so that the first support layer 128 has a load-bearing force to the polishing layer 122 can be provided.

[0009] The polishing layer 122 is arranged on the first support layer 128 and has an upper surface 123 and a lower Surface 125. The lower surface 125 faces away from the upper surface 122 and faces the first support layer 128. The Polishing layer 122 has at least one first groove 124 and at least one second groove 126. In some Embodiments, the second groove 126 may be a cavity formed at least beneath the upper surface 123 of the Polishing layer 122 is buried. The first groove 124 is present on the upper surface 123 of the polishing layer 122. In some embodiments, the second groove 126 is a groove having an opening 1262 on the lower surface 125 of the polishing layer 122, and the opening 1262 of the second groove 126 is covered with the first support layer 128, so that the second Groove 126 can be considered as a buried groove. On the other hand, the first groove 124 is an open groove in the upper surface 123 of the polishing layer 122.

[0010] In other words, the upper surface 123 of the polishing layer 122 has the first groove 124 therein, and the lower Surface 125 of the polishing layer 122 has the second groove 126 therein. The first and second grooves 124, 126 are each on opposite sides of the polishing layer 122 and the opening direction D3 of the first groove 124 is the Opening direction D4 of the second groove 126. It should be noted that the number of first and the second grooves 124, 126 of the polishing layer 122 serves for illustration and various embodiments of the present disclosure are not limited in this regard.

[0011] In some embodiments, the first and second grooves 124, 126 of the polishing layer 122 may be in a concentric arrangement, but various embodiments of the present disclosure are not limited in this regard.

[0012] When the suspension 132 is dispensed onto the polishing layer 122 of the polishing pad 120 and the clamping plate 110 rotates, as shown in Fig. 1 and Fig. 3, the suspension 132 can be applied to the upper surface 123 of the polishing layer 122 flow and can flow into the first groove 124. Consequently, the suspension 132 in the first groove 124 of the polishing layer 122 and the suspension 132 and the polishing layer 122 are used to polish the wafer 210 which is in contact with the polishing layer 122. After the upper surface 123 of the polishing layer 122 is number of wafers 210 has been ground for a period of time, the first groove 124 may be formed due to the fact that it is Suspension 132 and the wafer 210 is ground, are worn and either reduced in size or disappear.

[0013] As shown in Fig. 3, the first groove 124 and the second groove 126 are formed from the upper surface 123 of the Polishing layer 122 separated by various vertical distances. Fig. 4 is a cross-sectional view of the polishing layer 122 shown in Fig. 3 shown polishing pad 120 in the prior art construction, after the second groove 126 of the polishing pad 120 was exposed. When the upper surface 123 of the polishing layer 122 is exposed through the suspension 132 and the wafer 210 (see Fig. 1) is ground, the thickness of the polishing layer 122 is removed, as shown in Fig. 4, so that the first groove 124 can be worn and the second groove 126 can be exposed over the upper surface 123 of the polishing layer 122. Therefore, even if the first groove 124 is worn, the second groove 126 is opened to release the suspension 132 This means that the suspension 132 applied to the upper surface 123 of the polishing layer 122 can also flow into the second groove 126 after the first groove 124 has been filled due to the fact that the upper surface 123 of the Polishing layer 122 is ground by the suspension 132 and the wafer 210 (see Fig. 1) has been worn away.

[0014] Since the second groove 126 can be exposed to receive the suspension 132 when the first groove 124 has been worn, as shown in Fig. 1 and Fig. 4, the suspension 132 can be in both of the first residual groove 124 and the opened second groove 126. As a result of such a design, the first groove 124 and the second groove 126 of the polishing layer 122 can be designed with reduced depths. Because a polishing pad that has a deep groove generally requires a larger flow rate of polishing suspension than a polishing pad that has a shallow groove to produce a similar polishing rate. When the first groove 124 and the second groove 126 of the polishing layer 122 are reduced, the flow rate of the suspension 132 can therefore also be reduced, but the Polishing rate can be maintained. In other words, the amount of suspension 132 used can be reduced become.

[0015] Since the polishing layer 122 has the first and second grooves 124, 126 for receiving the suspension 132, the Furthermore, the number of wafers polished by the polishing layer 122, which receives the suspension 132, is increased. Therefore, the service life of the polishing pad 120 can be extended. Accordingly, if the polishing layer 122 of the Polishing pads 120 having the first and second grooves 124, 126 in the device for chemical-mechanical Polishing 100 is used, the number of preventive maintenance (VI) for the polishing pad 120 during a time can be reduced, so that the operating time of the chemical-mechanical polishing device 100 is extended can be.

[0016] When the wafer 210 is typically polished on an edge portion of the polishing layer 122, such as that shown in Fig. 1 illustrated position of the wafer 210, furthermore, the second groove 126 in the edge portion of the polishing layer 122, corresponding to the position of the wafer 210. Since the portion of the polishing layer 122 on which the Wafer 210 is ground faster than the other portion of the polishing layer 122, the position of the second Groove 126 in the polishing layer 122 depending on the relative position of the wafer 210 and the polishing layer 122 be determined.

[0017] In some embodiments, the first and second grooves 124, 126 are alternately formed in the polishing layer 122 arranged as shown in Fig. 3, and the orthogonal projection of the first groove 124 onto the first base layer 128 does not overlap the orthogonal projection of the second groove 126 onto the first base layer 128. In other words, the Center line L1 of the first groove 124 and the center line L2 of the second groove 126 are parallel and spaced apart by a distance d1. Such a configuration can ensure that the second groove 126 extends over the upper surface 123 of the polishing layer 122 exposed after the first groove 124 has been substantially worn away.

[0018] In some embodiments, the upper surface 123 of the polishing layer 122 has a plurality of first grooves 124 therein, and the lower surface 125 of the polishing layer 122 has a plurality of second grooves 126 therein. The orthogonal projection of each from the second grooves 126 to the upper surface 123 lies between two adjacent first grooves 124.

[0019] The polishing pad 120 may further comprise a second support layer 129 and the first support layer 128 is between the second support layer 129 and the polishing layer 122. In some embodiments, the hardness of the second Base layer 129 is greater than the hardness of the first base layer 128, and the hardness of the first base layer 128 is greater than the Hardness of the polishing layer 122, but various embodiments of the present disclosure are not limited. As a result of such a configuration, the second support layer 129 is used to support the first support layer 128 and the to support polishing layer 122.

[0020] Fig. 5 is an enlarged partial view of the polishing layer 122 shown in Fig. 3. As in Fig. 3 and Fig. 5 As shown, the first groove 124 of the polishing layer 122 has a lower portion 1241 and the second groove 126 of the Polishing layer 122 has a lower portion 1261. In some embodiments, the lower portion 1241 of the first groove 124 and the lower portion 1261 of the second groove 126 in the same horizontal plane. After the first groove 124 has been worn and may have disappeared, as a result of such a design the second groove 126 is continuously exposed over the upper surface 123.

[0021] In some embodiments, a vertical distance d2 between the lower portion 1261 of the second Groove 126 and the upper surface 123 less than or equal to a vertical distance d3 between the lower section 1241 the first groove 124 and the upper surface 123. If the vertical distance d2 between the lower section 1261 and the upper surface 123 is smaller than the vertical distance d3 between the lower section 1241 and the upper surface 123, the polishing layer 122 having such first and second grooves 124, 126 can ensure that the second groove 126 is exposed over the upper surface 123 before the first groove 124 is worn. When the vertical distance d2 between the lower section 1261 and the upper surface 123 equal to the vertical distance d3 between the lower portion 1241 and the upper surface 123, such a polishing layer 122 can ensure that the first groove 124 is worn and at the same time the second groove 126 is exposed over the upper surface 123.

[0022] In some embodiments, the polishing layer 122 has at least a first protruding portion 121a and at least one second protruding portion 121b. The first protruding portion 121a may be a solid section separating at least two of the first grooves 124, and the second groove 126 is buried at least under the first protruding portion 121a of the polishing layer 121a. The first protruding Section 121a is adjacent to the first groove 124, and the second protruding section 121b is adjacent to the second groove 126 adjacent. Furthermore, the first groove 124 may be aligned with the second protruding portion 121b, and the second groove 126 may be aligned with the first protruding portion 121a. Consequently, the first and the second grooves 124, 126 are arranged alternately in the polishing layer 122. After the first protruding portion 121a through the suspension 132 (see Fig. 1) and a number of wafers 210 (see Fig. 1) for a period of time has been ground, the second groove 126 can be exposed and opened to apply the suspension 132 on the polishing layer 122, even if the first groove 124 is gradually worn and less and less of the suspension 132 so that the polishing layer 122 of the polishing pad 120 continues to contain a sufficient amount of the suspension 132 for Polishing of the wafer 210.

[0023] Fig. 6 is a cross-sectional view of a polishing pad 120a according to some embodiments of the present Disclosure. As shown in Fig. 6, the first support layer 128a may further include a recess 1281 therein. The Recess 1281 of the first support layer 128a is connected to the second groove 126 and is essentially directed to the second groove 126 aligned.

[0024] The polishing pad 120a may further comprise an adhesive 1282. The adhesive 1282 is at least between the first support layer 128a and the polishing layer 122 and at least a part of the adhesive 1282 is in the Recess 1281 is present. During the joining of the polishing layer 122 and the first support layer 128a, the adhesive 1282 is coated onto a surface of the first support layer 128a having the recess 1281. Thereafter, the polishing layer 122 can be adhered to the surface of the first support layer 128a. Since the first support layer 128a has the recess 1281 therein, the excess adhesive 1282 can flow into the recess 1281. As As a result of such a design, the recess 1281 in the first support layer 128a can prevent the excess adhesive 1282 flows into the second groove 126 of the polishing layer 122, so that space in the second groove 126 is not occupied by the adhesive 1282. In other words, the recess 1281 of the first support layer 128a ensure that the space of the second groove 126 is used to receive the suspension.

[0025] Fig. 7 is a cross-sectional view of a polishing pad 120b according to some embodiments of the present Disclosure. As shown in Fig. 7, the polishing pad 120b may further comprise another polishing layer 122a. The Structure of the polishing layer 122a may be substantially the same as the structure of the polishing layer 122, and the polishing layer 122a is stacked on the polishing layer 122 so that the lower surface 125 of the polishing layer 122a is in contact with the upper surface 123 the polishing layer 122. In addition, the polishing layers 122, 122a can be made of a material become that Polyurethane, but various embodiments of the present disclosure are not limited in this regard limited.

[0026] In some embodiments, the first groove 124a of the polishing layer 122a may be aligned with the first groove 124 of the Polishing layer 122, and the second groove 126a of the polishing layer 122a may be aligned with the second groove 126 of the Polishing layer 122 must be aligned.

[0027] When the polishing pad 120b is used in a chemical-mechanical polishing device, a Such a configuration due to the fact that the polishing pad 120b has four layers of grooves, each of which has the first groove 124a, the second groove 126a, the third groove 124 and the fourth groove 126, respectively, in different horizontal planes extend the life of the polishing pad 120b and can reduce the number of preventive maintenance (VI) for the Reduce polishing pad 120b.

[0028] Fig. 8 is a cross-sectional view of a polishing pad 120c in the prior art construction. The second groove 126b is not only buried under the upper surface 123 of the polishing layer 122b, but it is also buried under the lower Surface 125 of the polishing layer 122b. When the first groove 124 is worn, the second groove 126b can be upper surface 123 is exposed to continuously receive the suspension 132 (see Fig. 1). Furthermore, some embodiments, the adhesive 1282 between the polishing layer 122b and the first support layer 128 Since the second groove 126b is an enclosed cavity before the first groove 124 wears out, the Adhesive 1282 under the lower surface 125 of the polishing layer 122b does not enter the second groove 126b when the polishing layer 122b is adhered to the first support layer 128. Such a configuration can ensure that the space of the second groove 126b is not occupied by the adhesive 1282.

[0029] Fig. 9 is a cross-sectional view of a polishing pad 120e constructed according to the prior art. As shown in Fig. 9 As shown, the polishing layer 122c further comprises at least one third groove 126c formed at least below the upper surface 123 of the polishing layer 122c. The second groove 126b is separated from the upper surface 123 of the polishing layer 122c by a first vertical distance d4, and the third groove 126c is separated from the upper surface 123 of the polishing layer 122c separated by a second vertical distance d5, and the first vertical distance d4 and the second vertical distance d5 are different. In some embodiments, the first vertical distance d4 is smaller than the second vertical Distance d5. When the polishing pad 120d is used in a chemical-mechanical polishing device, due to the fact that the polishing pad 120d has three layers of grooves, each comprising the first groove 124, the second groove 126b or the third groove 126c, in different horizontal planes, the service life of the polishing pad 120d extended and the number of preventive maintenance (VI) for the polishing pad 120d is reduced.

[0030] Fig. 10 is a flow diagram of a method for manufacturing a polishing pad according to some embodiments of the present disclosure. The method begins with block 310, in which a polishing layer is formed having a upper surface, at least one first groove and at least one second groove. The first groove and the second groove are separated from the upper surface of the polishing layer by various vertical distances. The process continues with block 320 by bonding the polishing layer to at least one support layer. The upper surface of the polishing layer has bonding away from the base layer.

[0031] In some embodiments, the polishing layer of the polishing pad can be produced by three-dimensional (3D) printing For example, the polishing layer can be formed by selective laser sintering (SLS) of a D3 printing In some embodiments, a 3D printer can print polyurethane to produce the polishing pad that The selective laser sintering process can be used to form the first or second groove in the upper surface or the lower surface of the polishing layer. In addition, the accuracy of the polishing pad can be a range of approximately 0.2 mm to 1.2 mm, and the accuracy of selective laser sintering can be less than approximately 0.07 mm, so that the selective laser sintering process corresponds to the accuracy of the polishing pad.

[0032] Alternatively, the first groove may be formed by machining the upper surface of the polishing layer, and the The second groove can be formed by machining the lower surface of the polishing layer. 'Machining', as shown here used to mean any of various processes in which a piece of raw material is turned into a desired final shape and size using a controlled material removal process.

[0033] In some embodiments, the polishing pad may be formed by tires. Forming the polishing layer may comprise the following steps: A first layer of the polishing layer is formed. Thereafter, a first mask placed on the first layer of the polishing layer. After the first mask is placed The first layer of the polishing layer is then matured. Next, the first mask is removed from the first Layer of the polishing layer is removed to create at least one groove space in the first layer of the polishing pad. Subsequently, a second layer of the polishing layer is formed on the first layer of the polishing layer, and the Groove space is buried under the second layer of the polishing layer to be the first groove. The first and second Layer can be made of a material that includes polyurethane, but different embodiments of the present disclosure are not limited in this respect, other materials (e.g. rubber) may also used to form the polishing pad through tires.

[0034] Furthermore, the formation of the polishing layer may further comprise the following steps. A second mask is placed on the second layer of the polishing layer. After the second mask has been placed, the second layer of the polishing layer is matured. The second mask is then removed from the second layer of the polishing layer to to create the second groove in the second layer of the polishing layer. In the following description, a Polishing process described.

[0035] Fig. 11 is a flow diagram of a polishing method according to some embodiments of the present Disclosure. The method begins with block 410, in which a suspension is dispensed onto a polishing pad. The Polishing pad has at least one open groove and at least one buried groove, and the dispensing of the suspension releases at least a portion of the suspension into the open groove. The method continues with block 420, in which at least a workpiece (e.g., a silicon wafer) is held on the polishing pad. The method continues with block 430, in which the The workpiece is rotated relative to the polishing pad. The polishing pad is worn and the buried groove is of turning exposed.

[0036] In some embodiments, dispensing the suspension further comprises dispensing at least one further part of the suspension into the exposed buried groove.

[0037] In order to maintain a certain amount of suspension on a polishing pad and to extend the life of the polishing pad To extend the lifetime of the product, a polishing pad for a chemical-mechanical polishing device, a method for Manufacturing the polishing pad and a polishing process designed to remove the suspension in the first groove and / or the second Groove, which are located on two opposite sides of the polishing layer. When the suspension is released onto the polishing layer of the polishing pad, the first groove in the upper surface of the polishing layer can After the upper surface of the polishing layer has been cleaned by a number of wafers for a period of time has been sanded, the first groove may be worn away and disappear. At this moment, however, the second groove in the lower surface of the polishing layer over the upper surface to expose the suspension continuously Consequently, the planarization and yield rate of the wafer can be improved, and the used The amount of suspension can be reduced, and the life of the polishing pad can be extended. the number of preventive maintenance (VI) for the polishing pad can be reduced over a period of time, so that the operating time of the chemical-mechanical polishing device can be extended.

[0038] According to some embodiments of the present disclosure, a polishing pad for an apparatus for chemical-mechanical polishing a first base layer and a polishing layer. The polishing layer is applied to the first The polishing layer has an upper surface facing away from the first base layer and at least a first cavity buried at least beneath the upper surface of the polishing layer.

[0039] According to some embodiments of the present disclosure, a method for manufacturing a Polishing pads forming a polishing layer having an upper surface, at least one first groove and at least one second groove, wherein the first groove and the second groove are separated from the upper surface of the polishing layer by different vertical The polishing layer is bonded to at least one support layer, with the upper surface of the Polishing layer points away from the base layer after bonding.

[0040] According to some embodiments of the present disclosure, a polishing method comprises dispensing a Suspension onto a polishing pad, wherein the polishing pad has at least one open groove and at least one buried groove and the dispensing of the suspension releases at least a portion of the suspension into the open groove. At least one The workpiece is held on the polishing pad. The workpiece is rotated relative to the polishing pad, whereby the polishing pad is worn and the buried groove is exposed during turning.

[0041] Although the present disclosure has been described in considerable detail with reference to certain embodiments Other embodiments are possible, and therefore the spirit and scope of the invention should be attached Claims are not limited to the description of the embodiments included herein.

[0042] It will be obvious to a person skilled in the art that various modifications and variations of the structure of the present disclosure without departing from the scope and spirit of the invention Disclosure. In view of the foregoing, it is intended that this disclosure Modifications and variations of this disclosure provided they come within the scope of the following claims.

Claims

1. Polishing pad (120, 120a, 120b, 120c, 120d) for a device (100) for chemical-mechanical polishing, wherein the Polishing pad (120, 120a, 120b, 120c, 120d) includes: a first support layer (128, 128a), wherein the first support layer (128, 128a) has at least one recess (1281), and a polishing layer (122) provided on the first support layer (128, 128a) and having a surface separated from the first support layer (128, 128a) facing away upper surface (123) and at least one first cavity (126, 126a, 126b, 126c) which has which is arranged at least one recess (1281) and which is at least below the upper surface (123) of the polishing layer (122), wherein the at least one first cavity (126, 126a, 126b, 126c) and the at least one Recess (1281) are aligned with each other.

2. Polishing pad (120, 120a, 120b, 120c, 120d) according to claim 1, wherein the first cavity (126, 126a, 126b, 126c) has a buried groove (126, 126a, 126b, 126c).

3. Polishing pad (120, 120a, 120b, 120c, 120d) according to claim 1 or 2, wherein the polishing layer (122) has at least one open, first groove (124, 124a) on the upper surface (123) of the polishing layer (122).

4. Polishing pad (120, 120a, 120b, 120c, 120d) according to claim 3, wherein the polishing layer (122) comprises at least one solid portion (121a) separating at least two of the open first grooves (124, 124a), and the first cavity (126, 126a, 126b, 126c) is buried at least beneath the solid portion (121a) of the polishing layer (122).

5. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, wherein the polishing layer (122) has a lower surface (125) facing the first support layer (128, 128a), and the first cavity (126, 126a, 126b, 126c) is buried under the lower surface (125) of the polishing layer (122).

6. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, wherein the polishing layer (122) has a lower surface (125) facing the first support layer (128, 128a), and the first cavity (126, 126a, 126b, 126c) has at least one opening on the lower surface (125) of the polishing layer (122).

7. Polishing pad (120, 120a, 120b, 120c, 120d) according to claim 6, wherein the opening of the first cavity (126, 126a, 126b, 126c) is covered with the first base layer (128, 128a).

8. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, wherein the at least one Recess (1281) is connected to the first cavity (126, 126a, 126b, 126c).

9. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, further comprising: an adhesive (1282) present at least between the first support layer (128, 128a) and the polishing layer (122), wherein at least a portion of the adhesive (1282) is present in the recess (1281).

10. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, wherein the polishing layer (122) further comprising at least one second cavity (126a, 126c) disposed at least beneath the upper surface (123) of the polishing layer (122) is buried, and the first cavity (126, 126a, 126b, 126c) is formed from the upper surface (123) of the Polishing layer (122) is separated by a first vertical distance, the second cavity (126a, 126c) from the upper Surface (123) of the polishing layer (122) is separated by a second vertical distance, and the first vertical distance and the second vertical distance are different.

11. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, wherein the first support layer (128, 128a) is harder than the polishing layer (122).

12. Polishing pad (120, 120a, 120b, 120c, 120d) according to one of the preceding claims, further comprising: a second support layer (129), wherein the first support layer (128, 128a) is arranged between the second support layer (129) and the Polishing layer (122) is arranged.

13. A method for producing a polishing pad (120, 120a, 120b, 120c, 120d), comprising: Forming (310) a polishing layer (122) having an upper surface (123), at least one first groove (124, 124a) and at least one second groove (126, 126a, 126b, 126c), wherein the first groove (124, 124a) and the second groove (126, 126a, 126b, 126c) separated from the upper surface (123) of the polishing layer (122) by different vertical distances are, and Bonding (320) the polishing layer (122) to at least one support layer (128, 128a), wherein the support layer (128, 128a) has a recess (1281), wherein after bonding, the upper surface (123) of the polishing layer (122) faces away from the support layer (128, 128a), the at least one second groove (126, 126a, 126b, 126c) is arranged above the recess (1281), and the at least one second groove (126, 126a, 126b, 126c) and the recess (1281) are aligned with each other.

14. The method according to claim 13, wherein the polishing layer (122) is formed by three-dimensional printing.

15. The method according to claim 13 or 14, wherein forming the polishing layer (122) comprises: Forming a first layer of the polishing layer (122), Arranging a first mask on the first layer of the polishing layer (122), Allowing the first layer of the polishing layer (122) to mature after arranging the first mask, Removing the first mask from the first layer of the polishing layer (122) to form at least one groove space in the first layer of the polishing layer (122), and forming a second layer of the polishing layer (122) on the first Layer of the polishing layer (122) and burying the groove space under the second layer of the polishing layer (122) so that it to the second groove (126, 126a, 126b, 126c).

16. The method of claim 15, wherein forming the polishing layer (122) further comprises: Arranging a second mask on the second layer of the polishing layer (122), allowing the second layer of the polishing layer (122) to mature after arranging the second mask, and Removing the second mask from the second layer of the polishing layer (122) to form the first groove (124, 124a) in the second layer of the polishing layer (122).

17. The method according to any one of claims 13 to 16, wherein the first groove (124, 124a) is formed by machining the upper surface (123) of the polishing layer (122) is formed.

18. The method according to any one of claims 13 to 17, wherein the second groove (126, 126a, 126b, 126c) is formed by machining the lower surface of the polishing layer (122).

19. A polishing process comprising: Dispensing (410) a suspension onto a polishing pad (120, 120a, 120b, 120c, 120d), wherein the polishing pad (120, 120a, 120b, 120c, 120d): a first support layer (128, 128a), wherein the first support layer (128, 128a) has a recess (1281), and a polishing layer (122) provided on the first support layer (128, 128a), wherein the first support layer (128, 128a) at least one open groove (124, 124a) and at least one buried groove (126, 126a, 126b, 126c); wherein the at least one buried groove (126, 126a, 126b, 126c) is arranged above the recess (1281) and the at least one buried groove (126, 126a, 126b, 126c) and the recess (1281) are aligned with each other; and wherein dispensing the suspension dispenses at least a portion of the suspension into the open groove (124, 124a), Holding (420) at least one workpiece on the polishing pad (120, 120a, 120b, 120c, 120d), and rotating (430) the workpiece with respect to the polishing pad (120, 120a, 120b, 120c, 120d), wherein the polishing pad (120, 120a, 120b, 120c, 120d) is worn and the buried groove (126, 126a, 126b, 126c) is exposed during rotation.

20. A polishing method according to claim 19, wherein dispensing the suspension further comprises at least another portion of the Suspension into the exposed buried groove (126, 126a, 126b, 126c).

Citation Information

Patent Citations

  • Method for forming polishing pads with a structured open network

    DE102012018200A1

  • Polishing pad

    JP2005294410A

  • Double-faced adhesive tape and its manufacturing method

    JP2008098356A

  • Chemical mechanical polishing pad having secondary polishing medium capacity control grooves

    US20060286350A1