Transfer construction

The transfer structure with a release layer and adhesion-promoting film layer simplifies manufacturing and enhances security by direct layer application and permanent bonding, addressing inefficiencies in existing transfer structures.

DE102023119166B3Active Publication Date: 2024-10-17GIESECKE & DEVRIENT CURRENCY TECHNOLOGY GMBH
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
DE102023119166
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-07-20
Publication Date
2024-10-17
Estimated Expiration
2043-07-20

AI Technical Summary

Technical Problem

Existing transfer structures for valuable documents and identification items lack efficiency in manufacturing complexity and require additional adhesive layers, which increase costs and complexity, while providing inadequate protection against manipulation.

Method used

A transfer structure comprising a carrier substrate and a transfer element with a release layer, a film layer having an adhesion-promoting surface, and a functional multi-layer structure, which allows direct application of subsequent layers without additional adhesives, and a connecting adhesive layer for permanent bonding to a target substrate, enhancing chemical and mechanical resistance.

Benefits of technology

The solution reduces manufacturing complexity, lowers costs, and provides enhanced protection against manipulation by ensuring a permanent and secure attachment to the target substrate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A transfer system comprising a temporary carrier and a multi-layered transfer material is provided. The transfer material includes a transfer element characterized by the fact that the film layer of the transfer element has an adhesion-promoting surface on one side, allowing subsequent layers of lacquer to be directly and securely bonded to the film layer of the transfer element by printing.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The present invention relates to an improved transfer structure comprising a carrier substrate and a Transfer element for value documents and a method for producing a transfer structure.

[0002] Data carriers, such as valuables or identity documents, but also other valuables, such as branded goods, are often provided with security elements for security purposes, which allow verification of the authenticity of the data carrier and which also serve as protection against unauthorized reproduction. Security elements can, for example, be be integrated into the substrate of the data carrier (security thread ...) or as a transfer element on the substrate of the A permanent bond between the transfer element and the target substrate is usually achieved by means of an adhesive that can be activated, for example thermally.

[0003] In the prior art, it is known for the application of security elements to the data carrier Transfer structures comprising a multilayer transfer material and a temporary carrier material. Transfer structures are used, as described for example in WO 2010 / 031543 A1, to transfer elements of the transfer material to a target substrate (banknote substrate in sheet or web form). Typically, the temporary carrier material is removed from the transfer elements after their transfer. In WO 2010 / 031543 A1, a A carrier material with two laminated film layers is proposed for such transfer structures.

[0004] Inverted transfer structures are also known, as described, for example, in DE 10 2019 001 422 A1. As ´´inverted´´ refers to those transfer structures in which the film in the transfer structure is under (or in the transmitted state above) the functional layers that contain the security features of the Provide transfer elements.

[0005] DE 10 2017 113 787 A1 relates to a method for producing a transfer film for transferring one or more Film elements onto a target substrate, wherein the method comprises the following steps: Providing a Laminating film, which has a plastic film, laminating the laminating film onto a carrier layer, introducing a or several patterns of recesses in the laminating film, which at least partially cut through in such a way that in one or more first partial areas of the laminating film at least one of the patterns It is intended to at least partially cut the laminating film along the boundary line between the respective first Partial area and a surrounding second part of the laminating film and peeling off the second part of the Laminating film from the carrier layer, whereby the one or more first Parts of the laminating film that are provided to one or more film elements

[0006] DE 10 2020 001 666 A1 relates to a method for producing a value document, comprising sticking a security element onto the value document substrate, wherein the security element has the form of a foil strip or of a patch. For bonding, both the security element and the value document substrate are a heat-sealing adhesive layer, wherein at least the heat-sealing adhesive layer of the security element Contains anti-blocking agents and is tack-free. The security element is heat-sealed to the value document substrate connected, and the connecting adhesive layer is then cured.

[0007] DE 10 2022 109 850 A1 relates to a laminate comprising a security element which is sandwiched between a recording layer and a cover layer, with an adhesive layer adhering to the recording layer and a release layer adheres to the cover layer or the adhesive layer adheres to the cover layer and the release layer adheres to the recording layer and the laminate is designed such that the adhesive layer of the security element by a tensile force exerted by the recording layer and the cover layer on the security element can be split

[0008] Against this background, the invention is based on the object of providing an improved transfer structure or a to provide appropriate manufacturing processes.

[0009] This object is achieved by the method for producing a transfer structure according to the independent Claim 1. Advantageous embodiments of the manufacturing process are defined in the dependent claims.

[0010] A transfer structure which is not part of the invention but purely for the comprehensive explanation of the invention comprises a carrier substrate and a transfer element for a value document. The transfer element comprises a release layer in a firmly adhesive, detachable anchorage on the carrier substrate, a film layer in a firmly adhesive connection with the release layer by a first adhesive layer, a functional multi-layer structure comprising an optical Security feature firmly anchored on the film layer, and a bonding adhesive layer in strong bond with the functional multi-layer structure. Bonding adhesive layer is suitable to form a permanent bond with a target substrate.

[0011] The transfer structure comprises that the film layer has an adhesion-promoting surface on one side.

[0012] An advantage of the film layer with a one-sided adhesion-promoting surface is that for applying the no adhesive is required for the subsequent layer, but the subsequent layer is applied directly to the film layer can be applied or printed and can thus be firmly anchored to the film layer.

[0013] The adhesion-promoting surface acts as an adhesion promoter and improves the adhesion of a coating to the Foil layer.

[0014] A strong bond can be achieved by means of a material bond, for example when gluing, in particular by laminating, Two layers in a strong bond form a body in which the two layers are are immovable, i.e. they can no longer slide or be moved against each other.

[0015] A strong anchoring can be achieved by printing, whereby the printed material on a lower layer Layer is immovable relative to the lower layer, but depending on the acceptance pressure it can be detached from the lower layer can.

[0016] The transfer structure also has advantages regarding chemical and mechanical resistance of the functional Multi-layer structure with the security feature, as this is protected by the film layer.

[0017] Preferably, the adhesion-promoting surface is formed by a pressure-accepting layer. The film layer therefore includes a pressure acceptance layer on one side.

[0018] Particularly preferably, the pressure-accepting layer is an acrylate layer. The acrylate layer can be a very thin layer already arranged on the film layer. In other words, the film layer can be coated with a very thin Acrylate layer must be pre-coated on one side.

[0019] Preferably, the side of the film layer having the adhesion-promoting surface is exposed to the functional In this case, the layer following the film layer is a layer made of the functional multi-layer structure, for example a thin lacquer layer by means of which an embossed lacquer layer is applied on the The embossing lacquer layer can be UV-cured, made of solvent-based raw materials and / or contain a thermoplastic.

[0020] Preferably, the film layer has a thickness between 4 µm and 12 µm, particularly preferably 6 µm. Reducing the thickness of the film layer to a maximum of 6 µm has the additional advantage that the transfer structure as a whole is considerably thinner and has improved stacking and flatness.

[0021] Advantageously, the carrier substrate comprises a carrier film layer and a support film layer, wherein the The carrier film layer and the support film layer are firmly bonded together by an adhesive layer. The release layer of the transfer element is firmly and removably anchored to the carrier film layer of the carrier substrate. In other words, the release layer is anchored to the carrier film layer in such a way that it adheres firmly with respect to subsequent application of further layers is, however, when applying the transfer element to the target substrate from the carrier film layer. Such anchoring of the release layer can be achieved by a special The thickness of the release layer can be controlled. Preferably, the release layer has a thickness that corresponds to 2 2 2 Weight per area between 0.5 g / m and 5 g / m , preferably 2.5 g / m .

[0022] Weight specifications such as these refer to the dried material. In this case, the following applies roughly 2 Approximation the conversion according to which a weight per area of ​​1 g / m corresponds to a thickness of 1 µm.

[0023] The carrier film layer may have a thickness between 12 µm and 23 µm, preferably a thickness of 19 µm.

[0024] The support film layer may have a thickness between 6 µm and 23 µm, preferably a thickness of 12 µm.

[0025] The release layer lies on top of the target substrate after the application of the transfer element and thus forms at least partially the surface of the applied transfer element or patch. It is advantageous if the Release layer is suitable as a pressure acceptance layer.

[0026] Preferably, the functional multi-layer structure comprises a structured embossing lacquer layer and / or a Metallization and / or a dielectric layer and / or a printing ink layer and / or a color-shifting Multi-layer structure.

[0027] The structured embossing lacquer layer can be structured with micromirrors, holograms and / or nanostructures. Transfer element can be equipped with or without clear text. The metallization can consist of simple layers as well as can also be constructed from complex layer sequences of different elements.

[0028] Preferably, the bonding adhesive layer comprises a heat-sealing lacquer or a UV heat-sealing lacquer. This has the Advantage that the transfer element can be permanently connected to the target substrate, so that the structure of the Transfer element is destroyed in any attempt to tamper with the patch. This means that the patch cannot be removed from the The UV heat seal lacquer is then additionally crosslinked using UV radiation after application.

[0029] The target substrate can be a paper or a polymer substrate. The transfer element or patch can be Hole and / or window (in the target substrate) as well as not applied to the hole or window.

[0030] According to the invention, a method for producing a transfer structure comprising a Carrier substrate and a transfer element for a value document. The method comprises the following steps, preferably in in the following order: a) printing a release layer of the transfer element onto a carrier film layer of the carrier substrate, b) Laminating a film layer onto the release layer, c) Applying a functional multi-layer structure comprising an optical security feature to the film layer, d) Laminating a support film layer onto the carrier film layer of the carrier substrate, e) Applying a bonding adhesive layer to the functional multi-layer structure.

[0031] Accordingly, in contrast to the conventional manufacturing process of transfer structures, the Carrier film layer and the film layer of the transfer element are bonded together before the support film layer is bonded to the This has the advantage that the functional multi-layer structure is applied to a total smaller stacks. This can at least partially reduce the manufacturing complexity or improved stacking and flatness can be achieved.

[0032] Advantageously, step c) comprises directly applying a thin layer of lacquer to the Foil layer, wherein the foil layer comprises an adhesion-promoting surface formed by a pressure-accepting layer, preferably an acrylate layer, and an embossing lacquer layer of the functional multi-layer structure by means of the thin layer of varnish can be firmly anchored.

[0033] This has the additional advantage that the functional multi-layer structure can be used without an additional laminating adhesive layer can be applied to the adhesion-promoting surface of the film layer. Thus, a laminating adhesive layer can be saved, which translates into a more efficient transfer structure, especially with regard to lower manufacturing complexity and thus lower costs.

[0034] Further details and features of the invention will become apparent from the following description in conjunction with the drawing. Shown are: Fig. 1 is a cross-sectional view of a transfer assembly according to an embodiment not forming part of the invention; and Fig. 2 is a flow diagram of an embodiment of the manufacturing method according to one aspect of the invention; Detailed description of the invention

[0035] Fig. 1 shows a cross-section of a transfer structure.

[0036] The transfer element 10 is a multi-layer element. The outer shape of the transfer element 10 can be a motif or a simple geometric shape. For example, the transfer element can be a local patch on the valuable document or as a strip extending over the valuable document (e.g. banknote).

[0037] In section A of Fig. 1, the transfer structure 1 is shown before transfer of the transfer element 10 to the target substrate 30 shown. In this state, the transfer element 10 is firmly anchored to the carrier substrate 20. The transfer element 10 can be arranged flush with the carrier substrate 20. In other embodiments, the surface of the carrier substrate 20 must be larger than the underside of the transfer element 10.

[0038] The strong anchoring between transfer element 10 and carrier substrate 20 is achieved by the arrangement of the Release layer 11 is realized on the carrier film layer 21. The carrier film layer 21 can be a polyethylene terephthalate (PET) film and have a thickness between 12 µm and 23 µm, preferably 19 µm. The release layer 11 can a layer of paint with a thickness 2 2 2 which corresponds to a weight per unit area of ​​between 0.5 g / m and 5 g / m , preferably 2.5 g / m , to which carrier film layer 21. The lacquer layer can be printed from solvent-based raw materials, with be cured with ultraviolet (UV) light or be a thermoplastic lacquer layer. Thus, the release layer 11 printed on the carrier film layer 21 in such a way that the release layer 11 is available for further production steps of the Transfer element 10 is anchored firmly enough, but when applying the transfer element 10 to the target substrate 30 can be efficiently mechanically detached from the carrier film layer 21.

[0039] A film layer 13 is laminated onto the release layer 11, ie by means of a first adhesive layer 12, in particular the first laminating adhesive layer, is brought into a strong bond with the release layer 11. The film layer 13 can have a thickness between 4 µm and 12 µm, ie 4 µm, 5 µm, 6 µm, 7 µm, 8 µm, 9 µm, 10 µm, 11 µm or 12 µm, preferably 6 µm. The film layer 13 comprises on one side an adhesion-promoting surface 18, which in the embodiment of Fig. 1 is formed by a very thin acrylate layer and in Fig. 1 as a thick The very thin acrylate layer can advantageously be applied before the production of the transfer element 10 onto the film from which the film layer 13 is formed. In other words, the Film layer 13 is pre-coated on one side with an adhesion-promoting surface 18. The surface 18 acts as Adhesion promoter, since a further layer, for example a lacquer layer, is applied directly to this, ie without a laminating adhesive layer, The side with the adhesion-promoting surface 18, i.e. the thin acrylate layer in Fig. 1, is the upper side of the film layer 13, i.e. the side facing the functional multi-layer structure 14; 15; 16.

[0040] For an application of the transfer element 10 on a hole in the target substrate 30, it is advantageous if the Film layer 13 has a thickness of 12 µm. For application of the transfer element 10 to the target substrate 30 without Hole, the thickness of the film layer 13 is preferably 6 µm.

[0041] The functional multi-layer structure 14; 15; 16 is firmly adhered to the adhesion-promoting surface 18 of the film layer 13 The functional multilayer structure 14; 15; 16 generally comprises at least one optical Security feature intended to protect the data carrier or valuable document. Particularly preferred the optical security feature is structured differently in certain areas and / or has an optically variable design (changed impression for the viewer when tilting or turning).

[0042] In the transfer structure of Fig. 1, the first layer of the functional multilayer structure 14; 15; 16 is a thin A lacquer layer is printed on the surface, by means of which a subsequent embossing lacquer layer 14 can be firmly anchored. Embossing lacquer layer 14 cannot be removed from the foil layer 13 without causing damage. The thin lacquer layer has a thickness 2 2 2 which corresponds to a weight per unit area of ​​between 0.2 g / m and 1.5 g / m , preferably of approximately 0.75 g / m . Embossing lacquer layer 14 can be structured with micromirrors, holograms and / or nanostructures. Nanostructures can be a dielectric layer or a metallic layer, for example a metallization, which increases reflection. Optionally, a wash ink layer 15 is applied to the embossing lacquer layer 14. printed, from which cleartext areas can subsequently be washed out. By washing out the Wash ink creates non-metallized areas where clear text can be provided. As an additional functional A color-shifting multi-layer structure 16 can optionally be applied. In one embodiment, the color-shifting multilayer structure 16 a chromium layer as absorber, a layer comprising a dielectric, such as preferably SiO2, optionally a thin adhesion-promoting layer, such as Cr or Ti, and a reflector layer, preferably consisting of Al. The dielectric can also be made of MgF or ZnS. The reflector layer can also be made of Ti or Ag. Paints with metallic pigments can also be used as a color coating. be used.

[0043] A support film layer 22 is laminated onto the carrier film layer 21 of the carrier substrate 20, ie by means of a second adhesive layer 23, in particular second laminating adhesive layer, in adhesive connection with the carrier film layer 21 The support film layer 22 can have a thickness between 6 µm and 23 µm, preferably 12 µm. Both the support film layer 22 and the carrier film layer 21 are preferably made of PET. The thickness of the 2 second laminating adhesive layer 23 can correspond to a weight per area of ​​between 0.7 and 3.5 g / m. the second laminating adhesive layer 23, the carrier film layer 21 and the support film layer 22 are firmly bonded to each other tied together.

[0044] On the functional multi-layer structure 14; 15; 16, a Bonding adhesive layer 17 is applied. The bonding adhesive layer 17 can contain a primer and a heat sealing lacquer or UV heat seal lacquer. After the application of the transfer structure 10 on the target substrate 30, the The bonding adhesives in contact with the target substrate 30 are thermally activated by the application of heat, so that a permanent connection between between the transfer element 10 and the target substrate 30. Due to the permanent connection, the transfer element 10 can no longer be detached from the target substrate 30 without destruction.

[0045] In section B of Fig. 1, the transfer element 10 is shown after its transfer to the target substrate 30. The In this state, transfer element 10 is permanently connected to the target substrate 30. The carrier substrate 20 is connected to the Application of the transfer element 10 to the target substrate 30 from the transfer element 10 or from its release layer 11 been replaced.

[0046] The bonding adhesive layer 17 is permanently bonded to the target substrate 30 in the embodiment. the bonding adhesive layer 17, the layers are arranged as shown in section A in the reverse order as described above. Thus, the release layer 11 in the applied state forms the upper end of the Transfer element 10 or patch. The release layer 11 is advantageously suitable as a print-receiving layer.

[0047] By arranging the pre-coated film layer 13 above the functional multi-layer structure 14; 15; 16, the latter can be protected from chemical and mechanical attacks. The film layer 13 thus serves as Barrier for the functional multilayer structure 14; 15; 16, which comprises at least one optical security feature.

[0048] Fig. 2 shows a flow diagram of an embodiment of the manufacturing method according to one aspect of the Invention.

[0049] The production of a transfer structure 1 according to one aspect of the invention starts in step a) from the Carrier film layer 21, onto which a release layer 11 is printed and thus firmly and yet releasably anchored becomes.

[0050] In step b), a film layer 13 is laminated onto the release layer 11, ie by means of a first Laminating adhesive layer 12 is firmly bonded to the release layer 11. The film layer can have a adhesion-promoting surface 18, which can be designed as a pressure-accepting layer. The pressure-accepting layer points upwards after production step b), i.e. in the opposite direction to the carrier film layer 21, and lies open. The film layer 13 can also be untreated, i.e. without pre-coating with an adhesion-promoting surface 18 can be laminated.

[0051] In step c), a functional multilayer structure 14; 15; 16 is applied to the film layer 13. For this purpose, If the film has an adhesion-promoting surface 18, first apply a layer of lacquer to the side of the film layer 13 with the adhesion-promoting surface 18. A thin application of the lacquer layer corresponds to a weight per 2 2 2 Area between 0.2 g / m and 1.5 g / m , preferably approximately 0.75 g / m . On the thin, cured layer of lacquer, subsequently an embossing lacquer layer 14 is applied, preferably with a thickness corresponding to a weight per area of ​​between 2 2 2 2 g / m and 10 g / m , preferably approximately 4 g / m . The printed embossing lacquer layer can then be embossed for example by incorporating optically effective microstructures and / or holograms and / or nanostructures. The embossing lacquer layer 14 can be cured with UV light or can be a lacquer layer consisting of solvent-based raw materials, or a thermoplastic lacquer layer. In this step, optionally a Wash ink layer 15 is printed, which subsequently forms the cleartext areas. If in step b) a Foil layer 13 was laminated without an adhesion-promoting surface 18, the embossing lacquer layer 14 is applied by means of a additional adhesive layer or primer layer, e.g. laminating adhesive layer, anchored to the film layer 13.

[0052] Further in step c), a color-shifting multi-layer structure 16 can be applied to the embossing lacquer layer 14. Afterwards, the printed wash ink can be washed off on transfer elements with Cleartext, which metallized areas with clear text are created.

[0053] In step d), a support film layer 22 is laminated onto the carrier film layer 21, ie by means of a second Adhesive layer 23 is firmly bonded to the carrier film layer 21. Accordingly, the support film layer 22 is only a complete application of the optical security feature.

[0054] In step e), a bonding adhesive layer 17 is applied to the functional multi-layer structure 14; 15; 16. The bonding adhesive layer 17 may comprise a primer and layers of heat seal lacquer or UV heat seal lacquer.

[0055] After carrying out steps a) to e) in the order shown, the transfer structure 1 is completely manufactured and can be provided for application of the transfer element 10 on the target substrate 30. List of reference symbols 1 Transfer setup Transfer element 10 11 Release layer 12 first layer of adhesive 13 film layers 14 embossing lacquer layer 15 wash paint layers 16 color-shifting multi-layer structure 17 Bonding adhesive layer 18 adhesion-promoting surface of the film layer 13 20 Carrier substrate 21 Carrier film layer 22 Support film layer 23 second adhesive layer

Claims

1. Method for producing a transfer structure (1) comprising a carrier substrate (20) and a transfer element (10) for a valuable document, the procedure comprising the following steps, preferably in the following order: a) printing a release layer (11) of the transfer element (10) onto a carrier film layer (21) of the carrier substrate (20), b) laminating a film layer (13) onto the release layer (11), c) applying a functional multi-layer structure (16) comprising an optical security feature to the film layer (13), d) laminating a support film layer (22) onto the carrier film layer (21) of the carrier substrate (20), e) applying a bonding adhesive layer (17) to the functional multi-layer structure (16).

2. The method according to claim 1, wherein step c) further comprises directly applying a thin layer of lacquer to the film layer (13), wherein the film layer has an adhesion-promoting surface (18) which is formed by a pressure-accepting layer, preferably an acrylate layer, and an embossing lacquer layer (14) of the functional Multi-layer structure (14; 15; 16) can be firmly anchored by means of the thin lacquer layer.

3. Method according to one of the preceding claims, wherein the film layer (13) has a thickness between 4 µm and 12 µm, preferably 6 µm.

4. Method according to one of the preceding claims, wherein the functional multi-layer structure (14; 15; 16) has a structured embossing lacquer layer (14) and / or a metallization (15) and / or a dielectric layer and / or a color-shifting multi-layer structure (16).

5. Method according to one of the preceding claims, wherein the bonding adhesive layer (17) comprises a heat-sealing lacquer or a UV heat seal varnish.

Citation Information

Patent Citations

  • Method for producing a transfer film, method for producing a film element, and transfer film, laminating film, and film element

    DE102017113787A1

  • Transfer device and method in a transfer device

    DE102019001422A1

  • Foil security element and method for producing a security document using the foil security element

    DE102020001666A1

  • Laminate and methods for manufacturing a laminate

    DE102022109850A1

  • Security element transfer material with multi-layered carrier

    WO2010031543A1