Method for producing a silicon wafer
Patent Information
- Application Number
- DE112017003457
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-07-08
- Filing Date
- 2017-04-12
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2037-04-12
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
TECHNICAL FIELDThe present invention relates to a silicon wafer production method.BACKGROUND ARTA silicon wafer (hereinafter, sometimes referred to as a "wafer") that can be used as a substrate of a semiconductor device is produced by, for example, polishing a wafer cut from a silicon single crystal that has typically been grown by the Czochralski process (sometimes referred to as a "CZ process"). Some crystals grown by the CZ process have a lattice defect called an grown-in defect.FIG. 1 is a vertical cross section of a silicon single crystal that has been pulled to schematically show an exemplary relationship between the defect distribution and V / G. V represents a pulling speed of the silicon single crystal, and G represents a temperature gradient of the silicon single crystal in a growth direction obtained immediately after the silicon single crystal is pulled.The temperature gradient G is intended to be approximately constant in view of the thermal properties of a hot zone structure of a CZ furnace. Accordingly, V / G can be controlled by adjusting the drawing speed V. Note that FIG. 1 schematically shows the result of observing a cross section of the silicon single crystal taken along its longitudinal axis by X-ray topography, where the silicon single crystal has been grown with a gradual decrease in V / G and heated with Cu applied to its cross section.Referring to FIG. 1, a crystal oriented particle (COP) is a collection of voids resulting from disappearance of atoms to form a crystal lattice during growth of a silicon single crystal. A displacement cluster is a collection of interstitial silicon that is excessively present in a crystal lattice.A COP present in an oxide film during thermal oxidation of a surface of a wafer deteriorates the GOI (Gate Oxide Integrity) property of the resultant semiconductor wafer. A displacement cluster also reduces device characteristics.Accordingly, in order to overcome the above problems, for example, a pulling speed V may be adjusted to grow a silicon single crystal free from COP and displacement clusters.The silicon single crystal thus obtained is intended to have at least one of the regions shown in FIG. 1, i.e., an OSF (Oxidation Induced Stacking Fault) region, a P V- region, and a P I- region. The P V- region is a defect-free region where a point defect based on a gap is dominant, which is located near the COP (collection of gaps). The P I- region is a defect-free region where a point defect based on inter-lattice silicon is dominant, which is adjacent to the displacement cluster.Unfortunately, even such a wafer having defect free regions free of COP and displacement clusters cannot be considered a completely defect free wafer.The P I- region contains almost no oxygen precipitation nucleus in a state as grown, so that oxygen precipitation is unlikely to be generated even after heat treatment.In contrast, the OSF region, which is the defect-free region adjacent to the region where a COP is generated, contains a plate-shaped oxygen precipitation (OSF core) in the as-grown state. Thus, as a result of a thermal oxidation process at a high temperature (usually 1000° C. to 1200° C.), the OSF core is caused to be an OSF. Meanwhile, the P V- region contains an oxygen precipitation nucleus in the as-grown state, so that oxygen precipitation is likely to be generated as a result of a two-stage heat treatment at low temperature and high temperature (e.g., 800° C. and 1000° C.).Such defects inherent in the OSF region and the P V- region can be detected by performing RIE (Reactive Ion Etching) on a wafer in the state as grown, so that the OSF core and the oxygen precipitation core existing in the P V- region are caused as protrusions on the etched surface. The fault / faults to be detected by RIE are referred to as RIE faults below.Such RIE errors inherent in a wafer caused as a result of heat treatment performed under specific conditions have been increasingly less negligible due to their influence on device yield. For example, OSF generated on a surface of a wafer causes a leakage current that reduces device characteristics. It is also likely that a residue of oxygen precipitation in an active layer of a device component causes a leak current in the device, the oxygen precipitation being generated from the oxygen precipitation nucleus in the P V- region during a heat treatment in the device production process.Accordingly, a production method of a wafer that achieves a reduction in an influence on a device yield has been studied (see, for example, Patent Literature 1).According to the production method of Patent Literature 1, a silicon single crystal having only at least a P V- region and a P I- region is grown, and a wafer cut from the silicon single crystal is rapidly heated to a temperature higher than 1300° C. but at most 1400° C., and thus the RIE defects are eliminated in a range from the surface of the wafer to at least 1 μm depth.US 2010 / 00 0 105 191 A1 discloses a method for evaluating OSF, which comprises an RTO process.US 2012 / 0 001 301 A1 discloses an RTP process in a temperature range from 1300° C. to 1400° C., inter alia, for removing OSF.KEEP LISTPATENT LITERATUREPatent Literature 1 JP 5 578 172 B2SUMMARY OF THE INVENTIONOBJECT(S) TO BE ACHIEVED BY THE INVENTION(S)Unfortunately, the production method according to Patent Literature 1 requires that all kinds of wafers must be heated to a temperature higher than 1300° C. regardless of the wafer quality. Thus, for example, a wafer that requires to be heated to Ta °C to sufficiently reduce RIE defects would be heated to Tb °C lower than Ta °C or to Tc °C much higher than Ta °C. The heat treatment at Tb ° C. cannot sufficiently reduce the RIE defects. The heat treatment at Tc °C, which enables sufficient reduction of the RIE defects, causes additional stress to the heat treatment equipment as a result of unnecessary heating. Thus, the heat treatment cannot always be carried out at an appropriate temperature depending on the wafer quality.It is an object of the invention to provide a silicon wafer production method which enables production of a silicon wafer having sufficiently reduced RIE defects by an appropriate heat treatment depending on the quality of the silicon wafer before the heat treatment.MEANS FOR ACHIEVING TASK(S)The inventor found through dedicated studies that silicon wafers free from COP and displacement clusters require different heat treatment conditions for sufficiently reducing RIE defects depending on the generation of OSF before heat treatment, and made this invention based on these findings.According to an aspect of the invention, a silicon wafer production method includes: growing a silicon single crystal free of COP and displacement clusters by a Czochralski process; evaluating the presence of OSF in a first evaluation wafer cut from the silicon single crystal; Subjecting a silicon wafer cut from the silicon single crystal for the first evaluation wafer to a heat treatment, wherein the heat treatment includes an RTO process, wherein the RTO process is performed at a temperature of 1350°C or higher when the first evaluation wafer includes the OSF, and wherein the RTO process is performed at a temperature lower than 1350°C when the first evaluation wafer is free of OSF.Here, the RTO (Rapid Thermal Oxidation) process is a heat treatment by rapid heating / rapid cooling under an oxidizing atmosphere.In the above aspect, the RTO process is executed under different conditions depending on whether OSF is present, so that the RIE errors can be sufficiently reduced in any case. Thus, a silicon wafer with sufficiently reduced RIE defects can be produced by an appropriate heat treatment depending on the quality of the silicon wafer before the heat treatment.In the above aspect, it is preferable that the method further includes evaluating, when the first evaluation wafer is free from OSF, an RIE defect density of a second evaluation wafer cut from the silicon single crystal for the first evaluation wafer, and that the heat treatment includes performing the RTO process on the silicon wafer cut from the silicon single crystal for the second evaluation wafer at a temperature of 1270 ° C. or higher, when the RIE defect density is 5×10 6 / cm 3 or higher, or on the silicon wafer cut from the silicon single crystal for the second evaluation wafer at a temperature of 1250° C. or higher, when the RIE defect density is made smaller than 5×10 6 / cm 3.In the above aspect, the RTO process is performed on a silicon wafer free from OSF under different conditions depending on its RIE defect density, so that the RIE defects can be sufficiently reduced regardless of the RIE defect density.BRIEF DESCRIPTION OF THE DRAWING(S)FIG. 1 schematically shows an exemplary relationship between defect distribution and V / G of a silicon single crystal. FIG. 2 schematically shows an arrangement of a drawing device according to an exemplary embodiment of the invention. FIG. 3 schematically illustrates heat treatment equipment according to the exemplary embodiment. FIG. 4 shows a temperature profile of an RTO process according to the example embodiment. FIG. 5 shows a relationship between an RTO process temperature and an in-plane maximum RIE defect density before / after the RTO process in connection with Experiment 1 for Example(s) of the invention. FIG. 6 shows a relationship between an RTO process temperature and an in-plane maximum RIE defect density before / after the RTO process in connection with Experiment 2 for Example(s) described above.DESCRIPTION OF EMBODIMENT(S)An exemplary embodiment of the invention will be described with reference to the accompanying drawings.A wafer production method according to the exemplary embodiment includes: growing a silicon single crystal free of COP and displacement clusters by a CZ process (growing step); evaluating a first evaluation wafer cut from the silicon single crystal for the presence of OSF (OSF evaluating step); evaluating a second evaluation wafer cut from the same silicon single crystal for the first evaluation wafer free of OSF for the RIE defect density (RIE defect density evaluating step); and executing an RTO process on a silicon wafer cut from the same silicon single crystal for the first and second evaluation wafers based on respective evaluation results of the OSF evaluation cut and the RIE defect density evaluation step (heat treatment step).The drawing means for the growth step and the heat treatment equipment for the heat treatment step will be described below, and then the wafer production method will be described in detail.Device Assembly AssemblyArrangement of the Drawing DeviceAs shown in FIG. 2, a puller 1, which is a device that can be used for the CZ process, includes a puller body 2 and a control unit 3.The puller body 2 includes a chamber 21, a crucible 22 located at a center of the chamber 21, a heating element 23 (heating unit) configured to radiate heat to heat the crucible 22, a heat insulating cylinder 24, a cable 25, and a heat shield 26.A gas inlet 21A through which an inert gas (e.g., Ar gas) is introduced into the chamber 21 is provided at an upper part of the chamber 21. A gas outlet 21B through which the gas in the chamber 21 is discharged when a vacuum pump (not shown) is operated is provided at a lower part of the chamber 21.The inert gas is introduced into the chamber 21 at a predetermined gas flow rate via the gas inlet 21A at the upper part of the chamber 21 under the control of the control unit 3. The introduced gas is then discharged through the gas outlet 21B at the lower part of the chamber 21 after flowing from the upper side to the lower side inside the chamber 21.The crucible 22 is configured to melt silicon (i.e., a material of a wafer) to provide a silicon melt M. The crucible 22 is supported by a support shaft 27 which is rotatable and vertically movable at a predetermined speed. The crucible 22 includes a closed-bottom cylindrical quartz crucible 221 and a graphite crucible 222 accommodating the quartz crucible 221.The heating element 23 is located outside the crucible 22 to heat the crucible 22 so that the silicon inside the crucible 22 melts.The heat insulating cylinder 24 surrounds the crucible 22 and the heating element 23.The cable 25 has a first end connected to a pulling drive (not shown) located above the crucible and a second end attached to a seed crystal SC. The cable 25 is vertically movable at a predetermined speed and rotatable about the axis of the cable 25 when the pulling drive is controlled by the control unit 3.The heat shield 26 is configured to block heat radiation radiated upward from the heating element 23.Based on a control program stored in a memory (not shown) and a setting input by an operator, the control unit 3 controls, for example, a gas flow rate and / or an internal furnace pressure in the chamber 21, a temperature in the chamber 21 heated by the heating element 23, a rotation speed of the crucible 22 and the silicon single crystal SM, and a time for pulling up / lowering the seed crystal SC to produce the silicon single crystal SM.Arrangement of Heat Treatment EquipmentAs shown in FIG. 3, the heat treatment equipment 5 includes a chamber 51.The chamber 51 accommodates a wafer tray 52, a base plate 53 mounted on the wafer tray 52, and three vertical support pins 54 disposed on the base plate 53. The three support pins 54 are arranged at intervals of 120 degrees in a plan view to support a round (silicon) wafer W.An upper heating unit 55, a lower heating unit 56 and a pyrometer 57 are located outside the chamber 51.The upper heating unit 55 includes a plurality of upper heat lamps 551 located above the chamber 51. The lower heating unit 56 includes a plurality of lower heat lamps 561 located below the chamber 51. The upper heat lamps 551 and the lower heat lamps 561 are halogen lamps whose respective light emission states are separately controllable. The above arrangement enables temperature distribution of the in-plane wafer W to be controlled by separately controlling the upper heat lamps 551 and the lower heat lamps 561.The pyrometer 57 is located below the lower heating unit 56 to measure a temperature of the wafer W.The chamber 51 is provided with a gas inlet 51A for introducing, for example, an inert gas or a reactive gas into the chamber 51, a gas outlet 51B for discharging the gas in the chamber 51, and an opening 51C for taking out the wafer W from the chamber 51. The opening 51C is closed by an automatic shutter (not shown) after the wafer W is set in the chamber 51.Wafer Production MethodTo produce a wafer, the step of growing is first performed using the puller 1 shown in FIG. 2.In the growth step, silicon is filled in the crucible 22 and heated for melting under an Ar gas atmosphere. Next, the seed crystal SC attached to the cable 25 is immersed in the silicon melt M and gradually pulled up with rotation of both the seed crystal SC and the crucible 22, and thus the silicon single crystal SM is produced.For the above process, the production conditions are preferably controlled so that an oxygen concentration of the silicon single crystal SM becomes 9.5×10 17 atoms / cm 3 or higher.Further, the production conditions for drawing are preferably controlled such that a ratio V / G of the drawing speed V to the temperature gradient G of the silicon single crystal SM in the growth direction immediately after the silicon single crystal SM is drawn falls within a range between a value corresponding to A and a value corresponding to C in FIG. 1. This enables the silicon single crystal SM to be produced free of COP and displacement clusters. Further, the production conditions are more preferably controlled such that the ratio V / G falls within a range between the value corresponding to A and a value corresponding to B in FIG. 1. This enables the silicon single crystal SM to be produced free of OSF, COP and displacement clusters. It is noted that the above(s) silicon single crystal(s) SM may be produced using the puller 1 having a hot zone structure in which the graphite crucible 222, the heating element 23, the heat insulating cylinder 24, and the heat shield 26 are located, the hot zone structure being modified to adjust a radial distribution in the growth direction of the temperature gradient G of the silicon single crystal SM that has just been pulled.Next, the wafer W is to be obtained.To obtain the wafer W, the silicon single crystal SM is cut into a plurality of blocks, which are then subjected to cutting, lapping, chemical etching, mirror polishing, and other processes to obtain the wafers W.Subsequently, the first evaluation wafer is selected from the cut wafers W and evaluated for the presence of OSF (OSF evaluation step).An exemplary method for evaluating the presence of OSF includes: heating the first evaluation wafer to a temperature of 1000° C.± 30° C. under an oxygen atmosphere for 2 to 5 hours and subsequently to a temperature of 111° C.± 30° C. for 1 to 16 hours; performing secco etching on the first evaluation wafer after the heating; and viewing the first evaluation wafer with a microscope.Next, the second evaluation wafer is cut from the same silicon single crystal SM for the first evaluation wafer free from OSF and evaluated for the RIE defect density (RIE defect density evaluation step). The RIE defect density can be evaluated by the following exemplary method.First, the second evaluation wafer is placed in a reactive ion etching apparatus and etched with a selectivity between Si / SiO 2, which is set to 100 or higher, by about 5 μm under a mixed gas atmosphere of HBr / Cl 2 / He+O 2. Next, after the second evaluation wafer subjected to the reactive ion etching is washed with hydrofluoric acid to remove an adhering reaction product resulting from the reactive ion etching, the respective RIE defect densities of the etched surface are measured at a plurality of positions. The obtained maximum value is evaluated as the RIE defect density of the second evaluation wafer.Next, the wafer W cut from the same silicon single crystal SM for the first and second evaluation wafers is heated based on the evaluation result of the OSF evaluation step and the RIE defect density evaluation step.For heating, an RTO process is performed on the wafer W using the heat treatment equipment 5 shown in FIG. 3 under the conditions shown in FIG. 4. The RTO process basically includes the following steps.First, the wafer W is mounted on the support pins 54 in the chamber 51 which is maintained at a temperature T2by controlling the upper heating unit 55 and the lower heating unit 56.A gas is introduced through the gas inlet 51A while the gas is discharged through the gas outlet 51B, and thereby an oxidizing atmosphere is reached in the chamber 51. The upper heating unit 55 and the lower heating unit 56 are then controlled to quickly heat the wafer W to a process temperature T 3 at a temperature increase rate ΔTu. It is noted that the oxidizing atmosphere is preferably, but not limited to, oxygen (100%), but a mixed gas atmosphere may be, for example, oxygen and an inert gas.Next, the temperature T 3 is maintained for a holding time K.Subsequently, by controlling the upper heating unit 55 and the lower heating unit 56, the wafer W is rapidly cooled to a temperature T 1 and then to the room temperature at a temperature drop rate of Δ Td, and thereby the wafer W with sufficiently reduced RIE defects is obtained.For the above RTO process, the process temperature T3is different as shown in Table 1 below, depending on:▪ OSF is present;▪ OSF is absent and the RIE defect density before the RTO process is 5×10 6 / cm 3 or higher; or6 / OSF is absent and the RIE defect density before the RTO process is lower than 5×10 cm 3.Note that the holding time K is preferably in the range of 10 seconds to 60 seconds, more preferably 30 seconds or less, from the viewpoint of productivity. Table 1 Table 1T31310 °C to 1350°C, excluded. 1350° C1270 °C to 6150°C. 1310 °C1250 °C to 1270 °C, excluded. 1270 °CWhen OSF is present, the process temperature T 3 may be set to any value of 1350° C. or higher, preferably to a value of less than 1350° C., in terms of the lifetime of the heat treatment equipment.Here, for the RTO process, a periphery of the silicon wafer is typically supported with a plurality of pins. In this case, for example, stress due to the dead weight of the silicon wafer acting on the contact points with the support pins and / or thermal stress due to the temperature distribution sometimes causes displacement due to slipping at the contact portions with the support pins.In order to reduce the occurrence of such displacement by slipping, the process temperature T 3 is more preferably set to a lower temperature in each of the above ranges, regardless of the presence / absence of OSF and / or the RIE defect density.By executing the RTO process under conditions that are different depending on the presence / absence of OSF in the first evaluation wafer and / or the RIE defect density before the RTO process, the RIE defects in each of the above cases can be sufficiently reduced.Here, an additional explanation will be given below for the reasons why the above RTO process can provide the wafer W with sufficiently reduced RIE defects.The silicon single crystal SM grown by the CZ method normally contains oxygen of about 10 18 atoms / cm 3 as an impurity. This oxygen, which is in the form of a solid solution in a crystal lattice at a temperature near a melting point of silicon, partially precipitates as silicon oxide (SiO 2), to form a crystal defect, such as an oxygen precipitation nucleus in the P V- region in the wafer W cut from the silicon single crystal SM.When such a wafer W is subjected to the RTO process under an oxidizing atmosphere, the silicon oxide in the crystal defect disappears inside the wafer W as a result of the oxygen atoms constituting the silicon oxide moving into the crystal lattice. After the silicon oxide disappears, gaps remain. Since the RTO process is performed under an oxidizing atmosphere, interstitial silicon is injected from the surface of the wafer W to fill the gaps. This eliminates or reduces OSF caused by an OSF core and / or RIE errors caused by an oxygen precipitation core in the P V- region. Example(s)Next, the invention will be described below in more detail with reference to Examples. It is to be understood, however, that the scope of the invention is in no way limited by these examples.Experiment 1: Relationship between RTO process temperature and the presence of RIE defects before / after RTO process in a wafer having OSF but neither COP nor displacement clustersFirst, using the above puller 1, a silicon single crystal having OSF but neither COP nor displacement clusters was produced by controlling V / G. The presence of OSF was determined by the exemplary method described in the above exemplary embodiment. Next, a wafer was cut from this silicon single crystal, RIE defect densities were measured at multiple positions in the wafer by the exemplary method described in the above exemplary embodiment, and the maximum value thereof was determined as a maximum in-plane RIE defect density.Table 2 shows the measurement results of the maximum in-plane RIE defect density. Table 2 Table 2Experiment. Ex. 111300 °C4,80 × 10 61,60 × 10 5Experiment. Ex. 21310 °C4,80 × 10 6Detection Limit or LessExperiment. Ex. 31315 °C4,80 × 10 6Detection Limit or LessExperiment. Ex. 41325 °C4,80 × 10 6Detection Limit or LessExperiment. Ex. 51335 °C4,80 × 10 6Detection Limit or LessExperiment. Ex. 621290 °C7,92 × 10 77,20 × 10 5Experiment. Ex. 71300 °C7,92 × 10 71,60 × 10 5Experiment. Ex. 81310 °C7,92 × 10 7Detection Limit or LessExperiment. Ex. 91315 °C7,92 × 10 7Detection Limit or LessExperiment. Ex. 101325 °C7,92 × 10 7Detection Limit or LessExperiment. Ex. 111335 °C7,92 × 10 7Detection Limit or LessExperiment. Ex. 1231315 °C1,60 × 10 8Detection Limit or LessExperiment. Ex. 131325 °C1,60 × 10 8Detection Limit or LessExperiment. Ex. 141335 °C1,60 × 10 8Detection Limit or LessExperiment. Ex. 1511315 °C1,15 × 10 8Detection Limit or LessExperiment. Ex. 161325 °C1,15 × 10 8Detection Limit or LessExperiment. Ex. 1751315 °C1,18 × 10 8Detection Limit or LessExperiment. Ex. 181325 °C1,18 × 10 8Detection Limit or LessAs shown in Table 2, the maximum in-plane RIE defect density of each of Experimental Examples 1 to 18 having OSF but neither COP nor displacement clusters exceeded the detection limit (8×10 4 / cm 3).Note that corresponding samples (wafers) of each group of Experimental Examples 1 to 5, Experimental Examples 6 to 11, Experimental Examples 12 to 14, Experimental Examples 15 to 16, and Experimental Examples 17 to 18 were all cut from the same silicon single crystal, so that values of the maximum in-plane RIE defect density of Experimental Example 1, Experimental Example 6, Experimental Example 12, Experimental Example 15, and Experimental Example 17 obtained before the RTO process were used as values of Experimental Examples 2 to 5, Experimental Examples 7 to 11, Experimental Examples 13 to 14, Experimental Example 16, and Experimental Example 18, respectively.Next, the RTO process was carried out on respective samples of Experimental Examples 1 to 18 under the following conditions using the above heat treatment equipment 5, and the maximum in-plane RIE defect density of each of the samples subjected to the RTO process was measured by the above method.Temperature T1: 600° CTemperature T2: 800°CProcess temperature T3: see Table 2Holding time K: 10 secondsTemperature rise rate ΔTu: 50° C. / secTemperature drop rate ΔTd: 33° C. / secNote that the RTO process was not performed on the wafer with which the RIE defect density was measured, but on a wafer cut from the same silicon single crystal for the above wafer with which the RIE defect density was not measured. The results are shown in Table 2. FIG. 5 shows a relationship between the RTO process temperature and the maximum in-plane RIE defect density before / after the RTO process. Note that the number of data elements shown in FIG. 5 is much smaller than that shown in Table 1, because some samples before / after the RTO process had the same maximum in-plane RIE defect density.As shown in Table 2 and FIG. 5, Experimental Examples 2 to 5 and 8 to 18 in which the process temperature T3was 1350° C. or higher each provided a wafer having a maximum RIE defect density in the plane of the detection limit or less, i.e., a wafer having sufficiently reduced RIE defects regardless of the RIE defect density before the RTO process. In contrast, Experimental Examples 1, 6, and 7 in which the process temperature T 3 was lower than 1350° C. (1290° C., 1300° C.) each provided a wafer having a maximum RIE defect density in the plane exceeding the detection limit, i.e., a wafer having insufficiently reduced RIE defects.In view of the above, it was found with reference to Experimental Examples 2 to 5 and 8 to 18 as Examples of the invention and Experimental Examples 1, 6, and 7 as Comparative Examples that a wafer having sufficiently reduced RIE defects can be produced by performing the RTO process on a wafer at the process temperature T 3 of 1350° C. or higher when the wafer has OSF but neither COP nor displacement clusters.Experiment 2: Relationship between RTO process temperature and the presence of RIE defects before / after RTO process in a wafer free of OSF, COP and displacement clustersFirst, a silicon single crystal free of OSF, COP and displacement clusters was produced by controlling V / G for the above puller 1. Respective samples (wafers) of Experimental Examples 19 to 61 were then cut in the same manner as in Experiment 1, and the maximum in-plane RIE defect density of each sample before the RTO process was measured. The results are shown in Tables 3 to 5.Note that Experimental Examples 19 to 53 contain those having the same maximum RIE defect density before the RTO process, and a value of such an example was generally used as those of the other samples in the same manner as in Experiment 1. Table 3 Table 3Experiment. Ex. 1961240 °C3,76 × 10 72,32 × 10 6≥5 × 10 6Experiment. Ex. 201250 °C3,76 × 10 71,20 × 10 6≥5 × 10 6Experiment. Ex. 211260 °C3,76 × 10 71,60 × 10 5≥5 × 10 6Experiment. Ex. 221270 °C3,76 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 231280 °C3,76 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 2471240 °C2,96 × 10 71,92 × 10 6≥5 × 10 6Experiment. Ex. 251250 °C2,96 × 10 78,80 × 10 5≥5 × 10 6Experiment. Ex. 261260 °C2,96 × 10 73,20 × 10 5≥5 × 10 6Experiment. Ex. 271270 °C2,96 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 281280 °C2,96 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 2981240 °C4,88 × 10 79,60 × 10 6≥5 × 10 6Experiment. Ex. 301250 °C4,88 × 10 73,36 × 10 6≥5 × 10 6Experiment. Ex. 311260 °C4,88 × 10 76,40 × 10 5≥5 × 10 6Experiment. Ex. 321270 °C4,88 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 331280 °C4,88 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 3491240 °C7,36 × 10 62,24 × 10 6≥5 × 10 6Experiment. Ex. 351250 °C7,36 × 10 61,44 × 10 6≥5 × 10 6Experiment. Ex. 361260 °C7,36 × 10 66,40 × 10 5≥5 × 10 6Experiment. Ex. 371270 °C7,36 × 10 6Detection Limit or Less≥5 × 10 6Experiment. Ex. 381280 °C7,36 × 10 6Detection Limit or Less≥5 × 10 6 Table 4Table 4Experiment. Ex. 39101240 °C1,33 × 10 61,69 × 10 7≥5 × 10 6Experiment. Ex. 401250 °C1,33 × 10 86,44 × 10 6≥5 × 10 6Experiment. Ex. 411260 °C1,33 × 10 82,29 × 10 6≥5 × 10 6Experiment. Ex. 42111270 °C1,33 × 10 6Detection Limit or Less≥5 × 10 6Experiment. Ex. 431280 °C1,33 × 10 6Detection Limit or Less≥5 × 10 6Experiment. Ex. 44121240 °C2,28 × 10 72,63 × 10 6≥5 × 10 6Experiment. Ex. 451250 °C2,28 × 10 77,63 × 10 5≥5 × 10 6Experiment. Ex. 461260 °C2,28 × 10 79,32 × 10 5≥5 × 10 6Experiment. Ex. 47131270 °C2,28 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 481280 °C2,28 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 49141240 °C2,68 × 10 73,64 × 10 6≥5 × 10 6Experiment. Ex. 501250 °C2,68 × 10 71,02 × 10 6≥5 × 10 6Experiment. Ex. 511260 °C2,68 × 10 77,63 × 10 5≥5 × 10 6Experiment. Ex. 52151270 °C2,68 × 10 7Detection Limit or Less≥5 × 10 6Experiment. Ex. 531280 °C2,68 × 10 7Detection Limit or Less≥5 × 10 6 Table 5Table 5Experiment. Ex. 54161250 °C1,60 × 10 5Detection Limit or Less<5 × 10 6Experiment. Ex. 55171250 °C2,40 × 10 5Detection Limit or Less<5 × 10 6Experiment. Ex. 56181250 °C1,36 × 10 6Detection Limit or Less<5 × 10 6Experiment. Ex. 57191250 °C2,40 × 10 5Detection Limit or Less<5 × 10 6Experiment. Ex. 58201250 °C1,04 × 10 6Detection Limit or Less<5 × 10 6Experiment. Ex. 59211250 °C3,73 × 10 6Detection Limit or Less<5 × 10 6Experiment. Ex. 60221250 °C8,47 × 10 5Detection Limit or Less<5 × 10 6Experiment. Ex. 61231250 °C2,03 × 10 6Detection Limit or Less<5 × 10 6As shown in Tables 3 and 4, each of Experimental Examples 19 to 53 having none of OSF, COP, and displacement clusters had an RIE defect density of 5×10 6 / cm 3 or higher before the RTO process. In contrast, as shown in Table 5, each of Experimental Examples 54 to 61 that had none of OSF, COP, and displacement clusters had an RIE defect density of less than 5×10 6 / cm 3 before the RTO process.Next, a wafer cut from the same silicon single crystal for the respective samples of Experimental Examples 19 to 61 which was not measured for the RIE defect density was subjected to the RTO process and measured for the maximum in-plane RIE defect density after the RTO process in the same manner as in Experiment 1. The results are shown in Tables 3 to 5. FIG. 6 shows a relationship between the RTO process temperature and the maximum in-plane RIE defect density before / after the RTO process.Note that the RTO process was carried out in the same manner as in Experiment 1 except that the process temperature T3was determined in accordance with the conditions shown in Tables 3 to 5.As shown in Tables 3 and 4 and FIG. 6, among Experimental Examples 19 to 53, Experimental Examples 22, 23, 27, 28, 32, 33, 37, 38, 42, 43, 47, 48, 52, and 53 in which the process temperature T 3was 1270 ° C. or higher had a maximum RIE defect density in the plane of the detection limit or less after the RTO process, while the other Experimental Examples in which the process temperature T 3was lower than 1270 ° C. had a maximum RIE defect density in the plane exceeding the detection limit.In view of the above, with reference to Experimental Examples 22, 23, 27, 28, 32, 33, 37, 38, 42, 43, 47, 48, 52, and 53 as examples of the invention and Experimental Examples 19 to 21, 24 to 26, 29 to 31, 34 to 36, 39 to 41, 44 to 46, and 49 to 51 as comparative examples, it has been found that a wafer having sufficiently reduced RIE defects can be produced by carrying out the RTO process on the wafer at the process temperature T 3 of 1270° C. or higher when the wafer is free from OSF, COP, and displacement clusters and has an RIE defect density of 5×10 6 / cm 3 or higher before the RTO process.Meanwhile, as shown in Table 5 and FIG. 6, each of Experimental Examples 54 to 61 had a maximum in-plane RIE defect density at the detection limit or lower after the RTO process. In connection with the above, it is presumed from the results of Experimental Examples 19 to 53 that the maximum in-plane RIE defect density is reduced with an increase in the process temperature T 3.Therefore, it is assumed that when the RIE defect density before the RTO process is less than 5×10 6 / cm 3 the RIE defects at the process temperature T 3 exceeding 1250° C. are sufficiently reduced because the RIE defects at a process temperature T 3 of 1250° C. can be sufficiently reduced.In view of the above, it has been found with reference to Experimental Examples 54 to 61 as examples of the invention that a wafer having sufficiently reduced RIE defects can be produced by performing the RTO process on a wafer at the process temperature T 3 of 1250° C. or higher when the wafer is free from OSF, COP, and displacement clusters and has an RIE defect density of less than 5×10 6 / cm 3 before the RTO process.EXPLANATION OF CODE(S)SM... Silicon single crystal, W... Wafer Wafer
Claims
A silicon wafer production method, comprising: growing a silicon single crystal (SM) free of COP and displacement clusters by a Czochralski process; evaluating the presence of OSF in a first evaluation wafer cut from the silicon single crystal; Subjecting a silicon wafer (W) cut from the silicon single crystal (SM) for the first evaluation wafer to a heat treatment, wherein the heat treatment comprises an RTO process, wherein the RTO process is performed at a temperature of 1350°C or higher when the first evaluation wafer has the OSF, and wherein the RTO process is performed at a temperature of less than 1350°C when the first evaluation wafer is free of OSF.The silicon wafer production method according to claim 1, further comprising evaluating an RIE defect density of a second evaluation wafer cut from the silicon single crystal (SM) for the first evaluation wafer when the first evaluation wafer is free from OSF, wherein the heat treatment comprises performing the RTO process on the silicon wafer (W) cut from the silicon single crystal for the second evaluation wafer at a temperature of 1270 °C or higher when the RIE defect density is 5 × 10 6 / cm 3 or higher, or on the silicon wafer (W) cut from the silicon single crystal for the second evaluation wafer, The RIE defect density is made to be lower than 5×10 6 / cm 3 at a temperature of 1250° C. or higher.
Citation Information
Patent Citations
Method for manufacturing annealed wafers and method for manufacturing devices
JP5578172B2
Method for manufacturing silicon single crystal wafer
US20100105191A1
Annealed wafer, method for producing annealed wafer and method for fabricating device
US20120001301A1