SEMICONDUCTOR DEVICE

A hybrid substrate with polysilicon and oxide semiconductor TFTs, along with ITO and organic insulation layers, addresses unevenness and step separation issues in semiconductor devices, enhancing reliability and performance.

DE112020005248B4Active Publication Date: 2024-12-05MAGNOLIA WHITE CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
DE112020005248
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-12-04
Filing Date
2020-11-06
Publication Date
2024-12-05
Estimated Expiration
2040-11-06

AI Technical Summary

Technical Problem

In semiconductor devices with planar image sensors, unevenness and step separation occur near the photodiode due to irregularities in the formation of switching TFTs and driving circuits, leading to reliability issues.

Method used

The use of a hybrid device substrate combining polysilicon semiconductor TFTs for peripheral circuits and oxide semiconductor TFTs for sensor areas, along with specific layer structures and etching techniques to prevent unevenness and step separation, including the use of ITO layers to protect the cathode and organic insulation layers to flatten the surface.

Benefits of technology

This configuration enhances the reliability of the photosensor by preventing unevenness and step separation, ensuring stable connections and improved performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Semiconductor device containing an optical sensor, wherein the optical sensor comprises: a thin-film transistor formed on a substrate (100) and a photodiode (10) formed over the thin-film transistor, wherein the photodiode (10) contains an anode (131), a thin photoconductive layer (130) and a cathode (126), the cathode (126) is formed from a thin titanium layer, and a first thin transparent conductive layer is formed between the thin titanium layer and the thin photoconductive layer (130), wherein the thin photoconductive layer (130) is made from a thin a-Si layer having an n+ layer, an i-layer (intrinsic layer) and a p+ layer on the cathode side, wherein the semiconductor device is characterized in that the first thin transparent conductive layer has an opening section at a position that overlaps with the thin photoconductive layer (130) and the n+ layer and the cathode (126) are in direct contact with each other at the opening section.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION(1) Field of invention

[0001] The present invention relates to a semiconductor device comprising an optical sensor which uses a photoelectric conversion element. (2) Description of the related area

[0002] Optical sensors that utilize photoelectric conversion have been used in fields such as biometric authentication and image recognition, and their use has become widespread. In the PIN photodiode, an intrinsic layer is positioned between a p+ layer and an n+ layer, resulting in excellent response speed and low dark current, thus enabling a high signal-to-noise ratio.

[0003] The vertical-mode PIN photosensor using a-Si is described in patent document 1. Patent document 2 discloses an example in which a PIN photodiode in a planar structure is used as an image sensor. Furthermore, WO 2017 / 031 109 A1 (see patent document 3) describes a method for manufacturing image sensor devices, particularly on a glass substrate for X-ray imaging. The method combines traditional semiconductor materials and processes with organic materials to reduce manufacturing costs and improve performance. It involves the formation of multiple layers, including metallized thin-film transistors, dielectric intermediates, electron transport layers, and bulk heterojunction layers, to enable efficient and cost-effective fabrication of image sensors. US 2019 / 170 884 A1 (see patent document 4) describes an imaging panel and its manufacturing process for X-ray imaging.The panel comprises a thin-film transistor, a photoconversion layer, and an upper electrode with a protective layer. The protective layer covers the upper electrode and extends between its edge and the edge of the photoconversion layer, thus enabling a reduction treatment to decrease leakage current without metal ions or organic substances adhering to the side surfaces of the photoconversion layer. Finally, US 2008 / 237474 A1 (see patent document 5) describes a semiconductor photodetector and its fabrication method. The photodetector includes a special structure in which the periphery of the metal electrode lies within the periphery of the semiconductor layer. This arrangement prevents metal particles from adhering to the side surface of the semiconductor layer during selective etching.This reduces the leakage current at the side surface, resulting in improved sensitivity and a better signal-to-noise ratio. [Reference to the state of the art][Patent document] [Patent Document 1] JP H02 - 159 772 A [Patent Document 2] JP H06 - 314 779 A [Patent document 3] WO 2017 / 031 109 A1 [Patent document 4] US 2019 / 170 884 A1 [Patent document 5] US 2008 / 237 474 A1 SUMMARY OF THE INVENTION

[0004] When a photodiode is used as a planar image sensor, a switching TFT or a driver TFT is formed by a TFT (thin-film transistor) together with a photodiode. Additionally, a power supply line, a detection line, a sampling line, and similar components are required to supply power to the photodiode or to detect an output from the photodiode.

[0005] A thin film is used for an electrode connected to a photodiode. However, a switching TFT and a driver circuit are positioned adjacent to or beneath the photodiode, such that the area where the photodiode is located is prone to unevenness. Consequently, these irregularities cause step separation in the conductive thin film connected to the photodiode, impairing its reliability as a sensor.

[0006] One object of the present invention is to realize a particularly reliable photosensor by preventing the occurrence of an unevenness in the vicinity of a photodiode and a step separation of an electrode connected to a photodiode.

[0007] The present invention solves the problems described above and its specific main means is as follows.

[0008] The problem is solved by the features of claim 1. Specific embodiments are described in the dependent claims. BRIEF DESCRIPTION OF THE DRAWINGS Fig. 1 is a top view of an optical sensor; Fig. 2 is a top view of an optical sensor element; Fig. Figure 3 is a cross-sectional view of the optical sensor; Fig. Figure 4 is a precise top view of problematic sections of the optical sensor element; Fig. 5 is a cross-sectional view along line AA of Fig. 4; Fig. Figure 6 is a cross-sectional view along line BB of Fig. 4; Fig. 7 is a cross-sectional view of a structure of embodiment 1; Fig. Figure 8A is a cross-sectional view of a first process of a process flow to realize a structure of embodiment 1; Fig. 8B is a cross-sectional view of a process that relates to the process of Fig. 8A follows; Fig. 8C is a cross-sectional view of a process that relates to the process of Fig. 8B follows; Fig. 8D is a cross-sectional view of a process that is based on the process of Fig. 8C follows; Fig. 8E is a cross-sectional view of a process that relates to the process of Fig. 8D follows; Fig. 8F is a cross-sectional view of a process that relates to the process of Fig. 8E follows; Fig. 9 is a cross-sectional view of a structure of embodiment 2; Fig. 10A is a cross-sectional view of a first process of a first process flow to realize a structure of embodiment 2; Fig. 10B is a cross-sectional view of a process that relates to the process of Fig. 10A follows; Fig. 11A is a cross-sectional view of a process that relates to the process of Fig. 10B follows in a first process flow; Fig. 11B is a cross-sectional view of a process that relates to the process of Fig. 11A follows in the first process flow; Fig. 11C is a cross-sectional view of a process that relates to the process of Fig. 11B follows in the first process flow; Fig. 12A is a cross-sectional view of a process that relates to the process of Fig. 10B follows in a second process flow; Fig. 12B is a cross-sectional view of a process that relates to the process of Fig. 12A follows in the second process sequence; Fig. 12C is a cross-sectional view of a process that relates to the process of Fig. 12B follows in the second process flow; Fig. 12D is a cross-sectional view of a process that is based on the process of Fig. 12C follows in the second process flow; Fig. 13 is a cross-sectional view of a structure of embodiment 3; Fig. Figure 14A is a cross-sectional view of a first process of a process flow to realize a structure of embodiment 3; Fig. 14B is a cross-sectional view of a process that relates to the process of Fig. 14A follows; Fig. 14C is a cross-sectional view of a process that relates to the process of Fig. 14B follows; Fig. 14D is a cross-sectional view of a process that is based on the process of Fig. 14C follows; Fig. 14E is a cross-sectional view of a process that relates to the process of Fig. 14D follows; and Fig. 15 is a cross-sectional view of another structure of embodiment 3. DETAILED DESCRIPTION OF THE PREFERRED EXECUTION FORMS

[0009] Fig. Figure 1 is a top view of an optical sensor device to which the present invention is applied. Fig. 1. Sensor elements are formed in a matrix within the sensor area. For example, the sensor area has a lateral diameter of 3 cm and a vertical diameter yy of 3 cm. Within the sensor area, scanning lines 11 run horizontally (in the x-direction) and are arranged vertically (in the y-direction). A detection line 12 and a power supply line 13 also run vertically and are arranged horizontally. A region enclosed by a scanning line 11 and a detection line 12, or a region enclosed by a scanning line 11 and a power supply line 13, forms a sensor element. Each sensor element includes a switching TFT 15, a PIN diode 10 with a thin photoconductive layer, and a storage capacitor 16. One electrode of the storage capacitor 16 is connected to the source of the TFT 15, and the other electrode is connected, for example, to a reference potential.

[0010] A scanning line control circuit 20 is arranged transversely outside the sensor area, a power supply circuit 40 is arranged in the upward direction, and a detection circuit 30 is arranged in the downward direction. The scanning line control circuit 20 and the detection circuit 30 are formed from TFTs. The scanning line 11 is selected sequentially from the upper section by the shift register in the scanning line control circuit 20.

[0011] The power supply line 13 is connected to an anode of each photodiode, runs vertically, and is connected to the same power supply in the power supply circuit 40 above the sensor area. An anode potential is then applied to the power supply line 13. The detection line 12 is connected to the drain of the switching TFT, and the source of the switching TFT is connected to the cathode of photodiode 10. A detection line 12 runs downwards from each sensor element, and a photocurrent is detected in the detection circuit 30. Fig. 1 When light is applied to the sensor element selected by the scanning line 11, a photocurrent is generated by the photodiode 10 and this photocurrent is detected by the detection circuit 20 via the detection line 12.

[0012] Fig. Figure 2 is a top view of each sensor element. To avoid complicating the drawing, the following are shown: Fig. 2. Some electrodes or the like are omitted. The size of each sensor element is, for example, 50 µm in the transverse direction x1 and 50 µm in the vertical direction y1. In Fig. 2. The scanning lines 11 run in the horizontal direction (the x-direction) and are arranged in the vertical direction (the y-direction). Furthermore, the power supply line 13 and the detection line 12 run in the vertical direction and are arranged in the horizontal direction. A cathode 126 of a photodiode, a thin photoconductive layer 130, an anode 131, and the like are formed in a region surrounded by a scanning line 11 and a power supply line 13, or in a region surrounded by a scanning line 11 and a detection line 12.

[0013] The thin semiconductor layer 107 extends in the x-direction from the detection line 12 through the through-hole 140 and passes under the scanning line 11. At this point, a TFT is formed. In this case, the scanning line 11 is the gate electrode of the TFT. The thin semiconductor layer 107 extends in the y-direction and is connected to the cathode 126 of the photodiode, which is made of titanium (Ti), in the through-hole 125. As shown in Fig. As described in Figure 3, the through-hole 125 is formed in a thick, thin organic passivation layer such that its diameter is large. A thin photoconductive layer 130 is formed at the cathode 126, and an anode 131 is formed from ITO (indium tin oxide) on the thin layer. Thus, a photodiode is formed.

[0014] In Fig. Power is supplied to the photodiode via the connecting electrode 133 between the anode 131 and the power supply line 13. The power supply line 13 can run directly to the power supply circuit 40 on the surface of the thin insulating layer, or it can run through a through-hole to the same layer as the drain electrode of the TFT or the same layer as the source electrode.

[0015] Fig. Figure 3 is a cross-sectional view of the optical sensor device of Fig. 1. In the optical sensor, which is in Fig. As shown in Figure 3, light is entered from the side opposite substrate 100, i.e., from the side of anode 131. As shown in Fig. Figure 1 shows a driver circuit formed from a TFT, located outside the sensor area. Since polysilicon semiconductors have high mobility, it is advantageous that the TFT forming the driver circuit is made of a polysilicon semiconductor.

[0016] On the other hand, it is advantageous that the switching TFT formed in the sensor area is made of an oxide semiconductor (sometimes referred to as OS: oxide semiconductor) which has a low leakage current. Therefore, in this embodiment, a hybrid array substrate is used, employing both a polysilicon semiconductor TFT and an oxide semiconductor TFT. Fig. 3 is the left side a polysilicon TFT for a peripheral circuit and the central section is a PIN photodiode and a switching TFT for it.

[0017] Polysilicon is a so-called low-temperature polysilicon, in which α-Si is polysiliconized by an excimer laser. However, since the annealing temperature of a polysilicon semiconductor exceeds the process temperature required to form an oxide semiconductor, a polysilicon semiconductor TFT is formed first, followed by an oxide semiconductor TFT. Thus, a peripheral circuit is formed first.

[0018] In Fig. 3 is a thin base layer 101, which is made from a laminated thin layer of silicon nitride (SiN) and silicon oxide (SiO) formed on a glass substrate 100. This serves to prevent the polysilicon semiconductor 102 and the oxide semiconductor 107 from being contaminated by impurities on the glass substrate 100. The thickness of the thin SiO layer is, for example, 200 nm and the thickness of the thin SiN layer is, for example, 20 nm.

[0019] A thin polysilicon layer 102 is formed on the thin base layer 101. Within the thin polysilicon layer 102, a thin α-Si layer is first formed, and then the α-Si is converted to polysilicon and patterned using an excimer laser. The thickness of the thin polysilicon layer 102 is, for example, 50 nm. It should be noted that the thin SiO layer and the thin SiN layer, which serve as the thin base layer 101, and the thin α-Si layer can be formed continuously by CVD.

[0020] Next, the first thin gate insulating layer 103, made of SiO₂, is formed covering the thin polysilicon semiconductor layer 102. The thickness of the first thin gate insulating layer 103 is, for example, 100 nm. Then, a first gate electrode 104, made of metal or a metal alloy, is formed. The first gate electrode 104 is, for example, made of MoW. The peripheral circuitry and the sensor area are formed simultaneously. Simultaneously with the formation of the first gate electrode 104, a thin light-shielding layer 105, made of the same material as the first gate electrode 104, is formed in a section corresponding to the switching TFT in the sensor area. This thin light-shielding layer 105 can be used as a lower gate electrode of an oxide semiconductor TFT to be formed later.

[0021] A first thin insulating layer 106 is formed from a stacked thin layer of a thin SiO₂ layer and a thin SiN layer, covering the first gate electrode 104 and the thin light-shielding layer 105. For example, the thin SiN layer has a thickness of 300 nm and the thin SiO₂ layer has a thickness of 200 nm. A thin oxide semiconductor layer 107 is formed over the first thin insulating layer 106. IGZO (indium gallium zinc oxide), ITZO (indium tin zinc oxide), ZnON (zinc oxide nitride), and IGO (indium gallium oxide) are used as oxide semiconductors. In this embodiment, IGZO is used as the oxide semiconductor.

[0022] To maintain the properties of an oxide semiconductor, it is important to maintain a certain amount of oxygen. Therefore, the top layer of the first thin insulating intermediate layer 106 must be a thin SiO₂ layer. This is because SiN₂ supplies hydrogen and reduces the oxide semiconductor. When the thin SiO₂ layer is in contact with the thin oxide semiconductor layer 107, oxygen can be supplied from the thin SiO₂ layer to the oxide semiconductor.

[0023] A drain protection electrode 108 is stacked in a drain region of the thin oxide semiconductor layer 107, and a source protection electrode 109 is formed in its source region. The drain protection electrode 108 and the source protection electrode 109 are made of a metal and prevent the thin oxide semiconductor layer 107 from being lost due to hydrofluoric acid (HF) in the through-holes on the oxide semiconductor TFT side when the through-holes on the polysilicon TFT side are cleaned with hydrofluoric acid (HF).

[0024] A second thin gate insulating layer 110 is formed from a thin SiO layer covering the thin oxide semiconductor layer 107. The thickness of the thin SiO layer is approximately 100 nm. A thin aluminum oxide gate layer 111 is formed on the thin SiO layer 110, and a second gate electrode 112 is formed on it, for example, by a MoW alloy. By supplying oxygen to the thin oxide semiconductor layer 107 from the second thin gate insulating layer 110, which is formed from SiO, and to the thin aluminum oxide gate layer 111, the properties of the thin oxide semiconductor layer 107 are stabilized.

[0025] In this embodiment, a storage capacitor is formed by the second thin gate insulating layer 110 and the thin aluminum oxide capacitance layer (thin AlOx capacitance layer) 113 by extending the source protection electrode 109 and forming the capacitor electrode 114, which has the same structure as the gate electrode 112, in the opposite section. The thin aluminum oxide capacitance layer (thin AlOx capacitance layer) 113 and the capacitor electrode 114 are formed simultaneously with the thin aluminum oxide gate layer 111 and the gate electrode 112. Since the thickness of the thin aluminum oxide capacitance layer (thin AlOx capacitance layer) 113 is 10 nm or less, it has little effect on the capacitance value.

[0026] A second thin insulating layer 115 is formed from a laminated thin layer of a thin SiO₂ layer and a thin SiN layer, covering the second gate electrode 112 and the capacitor electrode 114. The thickness of the thin SiO₂ layer is, for example, 300 nm and the thickness of the thin SiN layer is, for example, 100 nm. In many cases, a thin SiO₂ layer is located on the underside, closer to the thin oxide semiconductor layer 107. After the formation of the second thin insulating layer 115, through holes 120 and 121 are formed on the polysilicon TFT side of the peripheral circuit, and simultaneously, through holes 122 and 123 are formed on the oxide semiconductor TFT side of the sensor area.

[0027] The through-holes 120 and 121 on the polysilicon TFT side are subjected to hydrofluoric acid cleaning (HF cleaning) to remove the thin oxide layer. At this stage, hydrofluoric acid (HF) is also introduced into the through-holes 122 and 123 on the oxide semiconductor TFT side, and the drain protection electrode 108 and the thin source protection metal layer 109 are used to prevent the thin oxide semiconductor layer 107 from being lost.

[0028] A first drain electrode 116 and a first source electrode 117 are formed corresponding to the through holes 120 and 121 on the polysilicon TFT side; a second drain electrode 118 and a second source electrode 119 are formed corresponding to the through holes 122 and 123 on the oxide semiconductor TFT side. The second drain electrode 118 is connected to the detection line 12. The first drain electrode 116, the first source electrode 117, the second drain electrode 118, the second source electrode 119, and the like are formed from a stacked thin layer of Ti, Al, and Ti, with each layer having a thickness of, for example, 50 nm, 450 nm, and 50 nm sequentially from the layer below.

[0029] An organic thin passivation layer 124, e.g., made of acrylic resin, is formed covering the second thin insulating intermediate layer 115. Since the organic thin passivation layer 124 also serves as a thin planarization layer, it is formed to have a thickness of approximately 2 µm. A through-hole 125 for a source electrode 119 of the TFT is formed in the organic thin passivation layer 124, corresponding to the connection of the source electrode 119 to the cathode 126 of the photodiode. Because the organic thin passivation layer 124 is thick, the diameter of the through-hole 125 is also large.

[0030] A cathode 126 is formed by Ti on the organic thin passivation layer 124. The cathode 126 has a thickness of approximately 100 nm and extends into the through-hole 125 of the organic thin passivation layer 124. A thin PIN layer 130 is formed on the cathode 126. The thin PIN layer 130 has a structure in which an n+ layer 127 with a thickness of approximately 40 nm is formed on the cathode 126, an i-layer (a-Si layer) 128 with a thickness of 600 nm is formed on the n+ layer 127, and a p+ layer 129 with a thickness of 30 nm is formed on the i-layer (a-Si layer) 128. It should be noted that these values ​​for the thin PIN layer 130 are examples. The n+ layer 127, the i layer 128, and the p+ layer 129 are all formed from α-Si. They can all be continuously formed by CVD. Hereinafter, the thin PIN layer 130 (the thin photoconductive layer 130) can simply be referred to as a thin α-Si layer 130.

[0031] A thin ITO layer 131, acting as an anode, is formed on the p+ layer 129, e.g., with a thickness of 50 nm. To prevent electrical loss, a third thin insulating layer 132, e.g., made of SiN, is then formed. A hole is formed on the surface of the anode 131 in the third thin insulating layer 132, and the anode potential can be supplied from this section via the supply line 13 and the connecting electrode 133.

[0032] In Fig. A connecting electrode 133, formed simultaneously with the power supply line 13, extends across the third thin insulating layer 132, is connected to the anode 131 in the hole of the third thin insulating layer 132, and supplies an anode potential to the photodiode. The connecting electrode 133 is formed from a stacked structure of a thin titanium layer with a thickness of 100 nm, a thin aluminum layer with a thickness of 300 nm, and a thin titanium layer with a thickness of 100 nm.

[0033] An inorganic thin passivation layer 134 is formed from SiN, which covers, for example, the connecting electrode 133, the anode 131, the third thin insulating intermediate layer 132, and the like. Fig. 3. The organic thin passivation layer 124 is covered in sections other than the cathode 126 by the third thin insulating intermediate layer 132 and the inorganic thin passivation layer 134. The organic thin passivation layer 124 absorbs moisture from the atmosphere during the process. If this moisture is released from the organic thin passivation layer 124 during operation, a thin layer detachment or similar occurs. A drain hole 135 is then formed in the third thin insulating intermediate layer 132 and the inorganic thin passivation layer 134, covering the organic thin passivation layer 124 in such a way that any moisture contained within it can be released.

[0034] As described above, the optical sensor device is complete; however, in this state, since the surface is a thin SiN layer 134 with a thickness of approximately 200 nm, the mechanical strength is insufficient. Therefore, to mechanically protect the optical sensor, an organic thin protective layer 136 can be formed on the inorganic thin passivation layer 134. The organic thin protective layer 136 is, for example, made of an acrylic resin and has a thickness of, for example, 2 µm.

[0035] Fig. Figure 4 is a top view of a sensor element. Fig. The TFT is omitted in section 4. Fig. 4 is a sensor element formed in an area surrounded by the detection line 12, the power supply line 13 and the scanning line 11. In Fig. 4 is a cathode 126 made of Ti covering a through-hole 125 formed in an organic thin passivation layer 124. A thin photoconductive layer 130, made of a-Si and having a PlN structure, is formed on the cathode 126, and an anode 131, made of ITO, is formed on the thin photoconductive layer 130. Then, a connecting electrode 133 runs from the power supply line 13 to the anode 131 and provides a potential to the anode 131. In Fig. Section AA and Section BB are sections of the problem that is to be solved by the present invention.

[0036] Fig. 5 is a cross-sectional view taken along line AA from Fig. 4 was taken, which is a first problem that the present invention is intended to solve. In Fig. 5 is omitted except for the layer containing the problematic section. In Fig. 5 A source electrode 119 is formed on the second thin insulating intermediate layer 115 and is connected to a cathode 126, formed from Ti, through a through-hole 125 formed in the organic thin passivation layer 124. A thin a-Si layer 130 is formed as a thin photoconductive layer (thin PIN layer) on a cathode 126 and an anode 131, formed from ITO, is formed thereon.

[0037] In Fig. 5. The thin a-Si layer 130, which is a thin photoconductive layer, is formed by dry etching. However, at this stage, since the etch selectivity between the thin a-Si layer 130 and the thin Ti layer 126 (the cathode 126) is low, the thin Ti layer, which is also the cathode 126, is etched and the cathode 126 is narrowed. In particular, the cathode 126 is damaged in the through-hole 125.

[0038] Fig. 6 is a cross-sectional view taken along line BB from Fig. Figure 4 was taken and shows a second problem and a third problem that the present invention is intended to solve. Fig. 6 is different from the layer of the problematic section. In Fig. 6 A source electrode 119 is formed on the second thin insulating layer 115 and is connected to a cathode 126, formed from Ti, through a through-hole 125 formed in the organic thin passivation layer 124. A thin a-Si layer 130 is formed as a thin photoconductive layer 130 on a cathode 126, and an anode 131, formed from ITO, is formed thereon. A third thin insulating layer 132 is formed such that it covers the perimeter of the anode 131 and the thin photoconductive layer 130; and a connecting electrode 133 is formed thereon.

[0039] In Fig. Figure 6 shows a thin photoconductive layer 130 formed from a-Si, patterned by dry etching. However, the etch selectivity between a thin a-Si layer 130 and an organic thin passivation layer 124 is even lower than the etch selectivity ratio between a thin a-Si layer 130 and a thin Ti layer 126. Accordingly, when the thin a-Si layer 130 is dry etched, the organic thin passivation layer 124 is etched using the thin Ti layer 126, which is a cathode, as a mask (see right side of Figure 6). Fig. 6) If the third thin insulating layer 132 and the connecting electrode 133 are formed to cover the step section of the organic thin passivation layer 124 that has formed so far, the third thin insulating layer 132 cannot cover this step. Additionally, there is a risk of the connecting electrode 133 separating due to this step. This is a second problem.

[0040] In Fig. Figure 6 shows a thin photoconductive layer 130 formed from a p+ layer 129, an a-Si layer (i-layer) 128, and an n+ layer 127, and patterned by dry etching. The etch rate of a p+ layer 129 is lower than the etch rate of an a-Si layer 128 and an n+ layer 127. Therefore, after patterning, an overhang of the p+ layer 129 is formed in the thin photoconductive layer 130. Then, when the third thin insulating layer 132 and the connecting electrode 133 are formed covering this, the connecting electrode 133 is damaged due to the influence of the p+ layer 129 overhang. This is a third problem.

[0041] The following section describes a configuration for solving the first problem according to embodiment 1; a configuration for solving the second problem according to embodiment 2; and a configuration for solving the third problem according to embodiment 3. Design 1

[0042] Fig. Figure 7 is a cross-sectional view showing a configuration of embodiment 1 that solves the first problem. Fig. 7 is from Fig. 5 differs in that a thin ITO layer 201 is formed over the cathode 126. The thin ITO layer 201 has a thickness in the range of 30 to 50 nm. Since the selection ratio of dry etching between ITO and a-Si is high, the thin ITO layer 201 is hardly etched when the thin a-Si layer 130 is dry etched. Accordingly, the thin Ti layer 126, which is a deeper layer of the cathode, is protected, and separation of the cathode 126 is prevented.

[0043] However, to maintain the photodiode properties, it is preferred to arrange the n+ layer 127 and the thin Ti layer 126 in contact with each other. Therefore, the thin ITO layer 201 is removed, except for the section that is in contact with the circumferential section of the n+ layer 127, to form the opening section 2011, and the n+ layer 127 is in contact with the thin Ti layer 126 in the opening section 2011 of the thin ITO layer 201. However, the thin ITO layer 201 can have a structure in which the opening 2011 is not provided and the n+ layer 127 and the thin ITO layer 201, which is stacked on the cathode 126, are in direct contact with each other.

[0044] Fig. 8A to Fig. 8F are cross-sectional views that illustrate a process of realizing the configuration of Fig. 7 illustrate. Fig. Figure 8A is a cross-sectional view showing a state in which a thin ITO layer 201 is formed on a thin Ti layer 126, which is a cathode. Fig. Figure 8B is a cross-sectional view showing a state in which the thin ITO layer 201 and the thin Ti layer 126 have been removed except for the area around the photodiode using the masking agent 500. Fig. 8C is a cross-sectional view showing a state in which the thin ITO layer 201 is separated from a section in which the thin photoconductive layer (the thin a-Si layer) 130 is formed.

[0045] Fig. Figure 8D is a cross-sectional view showing a state in which a thin a-Si layer 130 is formed over the cathode 126 and the thin ITO layer 201, and a thin ITO layer 131, serving as an anode 131, is formed on it. Fig. Figure 8E is a cross-sectional view showing a state in which an anode 131 is formed by patterning on a thin ITO layer 131 on a thin a-Si layer 130.

[0046] Fig. Figure 8F is a cross-sectional view showing a state in which the thin a-Si layer 130 is patterned to form a thin photoconductive layer 130. When the thin a-Si layer 130 is dry-etched, the thin ITO layer 201 is hardly affected because of the high etch selectivity between a-Si and ITO. Thus, a stable cathode 126 can be formed. Design 2

[0047] Fig. Figure 9 is a cross-sectional view showing a configuration of embodiment 2 that solves the second problem. Fig. 9 is from Fig. 6 differs in that a thin ITO layer 202 is formed beneath the cathode 126. The thin ITO layer 202 has a thickness in the range of 30 to 50 nm. The selectivity of dry etching between ITO and α-Si is high. In other words, after patterning of the thin Ti layer 126 as the cathode 126, the thin ITO layer 202 remains as a deeper layer, and in this state, the thin α-Si layer 130 is patterned as the thin photoconductive layer 130. At this point, since the organic thin passivation layer 124 is protected by the thin ITO layer 202, it is not dry-etched. Therefore, the formation of a step of the organic thin passivation layer 124, which is created when the thin α-Si layer 130 is dry-etched, can be avoided. Then, after the thin a-Si layer 130 has been dry-etched, the thin ITO layer 202 is patterned.

[0048] Fig. 10A, Fig. 10B and Fig. 11A to Fig. 11C are cross-sectional views that provide a first example of a process flow for realizing the configuration of Fig. 9 illustrate. In Fig. In 10A, an organic thin passivation layer 124 is formed, covering the second thin insulating intermediate layer 115 and the source electrode 119; and a through-hole 125 is formed in the organic thin passivation layer 124. A thin ITO layer 202 and a cathode 126, which are made from a thin Ti layer, are formed covering the organic thin passivation layer 124 and the through-hole 125. Fig. Figure 10B is a cross-sectional view showing a state in which only the cathode 126 is patterned on the thin ITO layer 202.

[0049] Fig. Figure 11A is a cross-sectional view showing a state in which a thin a-Si layer 130, which is a thin photoconductive layer, is formed over the thin ITO layer 202 and the cathode 126. Fig. Figure 11B is a cross-sectional view showing a state in which a thin a-Si layer 130, which is a thin photoconductive layer, is patterned. When the thin a-Si layer 130 is patterned, it is not dry-etched because the organic thin passivation layer 124 is covered by the thin ITO layer 202, and therefore no step is formed. The thin ITO layer 202 is then patterned. The thin ITO layer 202 is patterned in essentially the same way as the cathode 126.

[0050] Fig. Figure 11C is a cross-sectional view showing a state in which a thin ITO layer 131, serving as an anode, is formed over the thin photoconductive layer 130, and then the anode 131 is patterned using a masking agent. At this stage, the thin ITO layer 202 is also patterned using the thin Ti layer 126 as a cathode, forming a mask. As described above, according to the first process flow, it is possible to prevent a step from being created in the organic thin passivation layer 124 and to prevent damage to the connecting electrode 133.

[0051] Fig. 10A, Fig. 10B and Fig. 12A to Fig. 12D are cross-sectional views, which provide a second example of a process flow for realizing the configuration of Fig. 9 illustrate. Fig. 10A and Fig. 10B are structured as described in the first process flow. Fig. Figure 12A is a cross-sectional view showing a state in which a thin a-Si layer 130, serving as a thin photoconductive layer, is formed over a thin ITO layer 202 and a cathode 126 formed from Ti, and a thin ITO layer 131, serving as an anode, is formed on it.

[0052] Fig. 12B is a cross-sectional view showing a state in which an anode 131 is formed by patterning on a thin ITO layer 131. Fig. Figure 12C is a cross-sectional view showing a state in which the masking agent 500 has been formed and the thin a-Si layer 130 has been patterned. Subsequently, the thin ITO layer 202 is patterned using the thin Ti layer 126, which is a cathode, as the masking agent. Since the thin ITO layer 202 and the organic thin passivation layer 124 have a high selectivity, the organic thin passivation layer 124 is not etched during patterning on the thin ITO layer 202.

[0053] Fig. Figure 12D is a cross-sectional view showing a state in which the masking agent 500 is located away from the anode 131. As shown in Fig. As shown in 12D, it is also possible in the second process flow to use a configuration that is in Fig. 9 is shown, to realize and thereby prevent separation of the connecting electrode and improve the reliability of the photosensor. embodiment 3

[0054] Fig. Figure 13 is a cross-sectional view showing a configuration of embodiment 3 that solves the third problem. Fig. 13 differs from Fig. 6 such that a thin organic insulating layer 300 is formed covering the anode 131 and the third thin insulating intermediate layer 132 and the connecting electrode 133 is connected to the anode 131 through a through hole 145 formed in the thin organic insulating layer 300.

[0055] Since the thickness of the thin organic insulating layer 300 is approximately 2 µm, the surface is flat and the influence of ridges or the like of the p+ layer 129, which are formed on the thin photoconductive layer 130, does not affect the connecting electrode 133. Accordingly, separation of the connecting electrode 133 can be prevented. In the configuration shown in Fig. As shown in Figure 13, the second problem, i.e., the influence of the step caused by the etching of the organic thin passivation layer 124 at the end of the thin Ti layer 126, which is a cathode, can be eliminated. This is because the step formed in the organic thin passivation layer 124 is also covered by the thin organic insulating layer 300. In other words, the configuration shown in Figure 13 can be eliminated. Fig. As shown in 13, the second and third problems can be solved simultaneously.

[0056] Fig. 14A to Fig. 14E is a process flow for implementing the configuration of Fig. 13. Fig. Figure 14A is a sectional view showing a state in which a thin a-Si layer 130, which is a thin photoconductive layer 130, is formed at a cathode 126, which is formed at an organic thin passivation layer 124, and an anode 131 is formed at the thin photoconductive layer 130. Fig. 14B is a cross-sectional view showing a state in which a third thin insulating intermediate layer 132 is formed covering an organic thin passivation layer 124, a cathode 126, a thin a-Si layer 130 and a section of an anode 131.

[0057] Fig. Figure 14C is a cross-sectional view showing a state in which a thin organic insulating layer 300 is formed covering the third thin insulating intermediate layer 132 and the anode 131, and the through-hole 145 in the thin organic insulating layer 300 is formed in a section corresponding to the anode 131. As shown in Fig. As shown in Figure 14C, since an end section of the thin a-Si layer 130 and an end section of the cathode 126 are covered with a thin organic insulating layer 300, even if an irregular shape is produced in this section, there is no influence on the surface of the thin organic insulating layer 300 in which the connecting electrode 133 is formed.

[0058] Fig. Figure 14D is a cross-sectional view showing the state in which the connecting electrode 133 is formed in the through-hole 145 in the thin organic insulating layer 300. Since the surface of the thin organic insulating layer 300 is flattened and smoothed, no separation occurs in the connecting electrode 133. Subsequently, the entire photosensor is protected by an inorganic thin passivation layer 134. Thus, a particularly reliable photosensor can be formed in Fig. As shown in 13, it can be realized.

[0059] Fig. 15 is a change from Fig. 14. Fig. 15 is from Fig. 13 differs in that there is no third thin insulating layer formed from an inorganic thin layer such as SiN covering the thin a-Si layer 130, the anode 131, the organic thin passivation layer 124, and the like. If impurities such as moisture generated by the organic thin passivation layer 124, or the like, do not contaminate the thin a-Si layer or the like, which is the thin photoconductive layer 130, the third thin insulating layer can be omitted.

[0060] The configuration of Fig. 15 can be achieved through a process flow such as that of Fig. 14A and Fig. 14C to Fig. 14E are formed, with the exception that the step from Fig. 14B is not necessary. In the configuration that is in Fig. As shown in Figure 15, the process of forming the third thin insulating intermediate layer is unnecessary and can therefore reduce manufacturing costs compared to the configuration of Fig. 14 will be reduced. [Explanation of reference symbols]

[0061] 10 - Photodiode, 11 - Sampling line, 12 - Detection line, 13 - Power supply line, 16 - Storage capacitor, 20 - Sampling line drive circuit, 30 - Detection circuit, 40 - Power supply circuit, 100 - Substrate, 101 - Thin base layer, 102 - Thin polysilicon semiconductor layer, 103 - First thin gate insulating layer, 104 - First gate electrode, 105 - Thin light shielding layer, 106 - First thin insulating intermediate layer, 107 - Thin oxide semiconductor layer, 108 - Drain protection electrode, 109 - Source protection electrode, 110 - Second thin gate insulating layer, 111 - Thin gate aluminum oxide layer (thin gate AlOx layer), 112 - Second gate electrode, 113 - Thin aluminum oxide capacitance layer (thin AlOx capacitance layer), 114 - Capacitor electrode, 115 - Second thin insulating layer, 116 - First drain electrode, 117 - First source electrode, 118 - Second drain electrode, 119 - Second source electrode, 120 - First through hole,121 - Second through hole, 122 - Third through hole, 123 - Fourth through hole, 124 - Organic thin passivation layer, 125 - Fifth through hole, 126 - Cathode, 127 - n+ layer, 128 - i layer (a-Si layer), 129 - p+ layer, 130 - Thin photoconductive layer (thin a-Si layer), 131 - Anode, 132 - Third thin insulating layer, 133 - Connecting electrode, 134 - Inorganic thin passivation layer, 135 - Drain hole, 136 - Organic thin protective layer, 140 - Through hole, 145 - Through hole, 201 - Thin ITO layer, 202 - Thin ITO layer, 300 - Thin organic insulating layer, 2011 - Opening section

Claims

[1] A semiconductor device including an optical sensor, the optical sensor comprising: a thin-film transistor formed on a substrate (100), and a photodiode (10) formed over the thin-film transistor, wherein the photodiode (10) contains an anode (131), a thin photoconductive layer (130) and a cathode (126), the cathode (126) is formed from a thin titanium layer, and a first thin transparent conductive layer is formed between the thin titanium layer and the thin photoconductive layer (130), wherein the thin photoconductive layer (130) is made from a thin a-Si layer having, from the cathode side, an n+ layer, an i-layer (intrinsic layer) and a p+ layer, wherein the semiconductor device characterized by is that the first thin transparent conductive layer has an opening portion at a position overlapping with the thin photoconductive layer (130), and the n+ layer and the cathode (126) are in direct contact with each other at the opening portion. [2] The semiconductor device according to claim 1, wherein the first thin transparent conductive layer has a first portion overlapping with the thin photoconductive layer (130) and a second portion not overlapping with the thin photoconductive layer (130). [3] A semiconductor device according to claim 1, wherein the anode (131) is formed of a second thin transparent conductive layer.

Citation Information

Patent Citations

  • Pin vertical type photosensor

    JP1990159772A

  • Image sensor

    JP1994314779A

  • Semiconductor photodiode and method for manufacturing same, radiation detection device, and radiation imaging apparatus

    US20080237474A1

  • Imaging panel and method for producing same

    US20190170884A1

  • Method of manufacturing an image sensor device

    WO2017031109A1