Scarband and method for producing it

DE502020009261D1Active Publication Date: 2024-10-02BENECKE KALIKO AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502020009261
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-01-31
Filing Date
2020-11-25
Publication Date
2024-10-02
Estimated Expiration
2040-11-25

AI Technical Summary

Technical Problem

Existing grain tapes lose structure and adhesion at high temperatures, limiting the production of films with deep structures and causing residue issues, and current methods for high-temperature film production are either costly or result in odor emissions or low tensile strength.

Method used

A thermoplastic olefin grain tape with an electron beam-crosslinked layer and a lacquer coating that can withstand up to 210°C, allowing for three-dimensional structuring and improved adhesion, using polymers like ethylene-propylene copolymers and crosslinking aids, and a carrier substrate for stability.

Benefits of technology

The solution provides a durable, high-temperature-resistant grain tape that maintains structure and adhesion, reducing residue issues and odor emissions, enabling efficient production of films with deep structures and improved tensile strength.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a scar band comprising at least one layer of a thermoplastic olefin with a three-dimensionally structured upper surface, which is intended for the production of a film by applying liquid or pasty plastic to form the film in a reverse process and subsequently removing the film from the surface.

[0002] Such textured tapes are known and are used in a so-called reverse process to produce a film or foil. This involves applying a layer of liquid or paste-like plastic to the structured textured tape, allowing the plastic to harden, and then peeling off the layer as a film. The negative structure of the textured tape is thus transferred as a positive impression to the surface of the film. This production process is usually continuous, with the textured tape either being an endless belt circulated by a suitable drive unit, or a serial belt that is supplied to the production plant according to the desired texture and structure of the film.

[0003] From the generic DE 44 22 871 A1, it is known to produce such a polyolefin-based graining strip which, due to the raw material properties, can be coated with a suitable plastic and baked at temperatures up to 155 °C. However, at temperatures above 150 °C, the known graining strip loses its structure, and in particular, fine structures on the surface melt away, the mattifying or gloss level changes, and, for example, polyurethane coatings produced on such a graining strip lose their desired structure.

[0004] To address this problem, polyurethane coatings, for example, are applied to such polyolefin-based graining strips only up to a temperature of approximately 155 °C, then peeled off the graining strip and subsequently completely baked out in a further costly process, whereas PVC coatings can only be produced in this way to a very limited extent. Furthermore, silicone-based systems cannot yet be directly structured in this way; rather, only superficially smooth films can be produced, which then have to be structured in a subsequent step. DE 10 2016 225469 A1 discloses a method for producing a painted grained film or a film laminate with a painted grained top film and with at least one bottom film.

[0005] Alternative silicone-based constructions allow for structuring of the silicone-based coating, but only within a specific process time window. Outside this time window, structural integration is currently only possible to a limited extent or insufficiently.

[0006] Furthermore, the surface of the known grain bands is unmodified, meaning that the adhesion between the grain band and the coating medium is determined solely by the applied coating medium itself. If the surface area-to-area ratio is too high, for example with a very deep grain structure, this leads to extremely high adhesion to the grain band, resulting in residues repeatedly remaining on the grain band that require time-consuming cleaning.

[0007] While coating systems based on peroxide-curing silicone offer the possibility of producing an unstructured grain band on a calender at temperatures between room temperature and up to 120 °C, followed by structuring and baking above 150 °C, this process results in an undesirable odor on the final grain band due to the peroxide curing agent. Alternative options include the use of polymethylpentene (PMP), such as TPX, a semi-crystalline thermoplastic belonging to the group of (modified) polyolefins, which can be used at higher temperatures. This also applies to elastomer-based systems, such as rubber.

[0008] The only established method in the prior art for producing films or foils using the reverse process at temperatures above 155 °C is the use of paper strips as a graining strip. These strips have a relief-like pattern embossed onto them, extending to the reverse side of the paper, resulting in a corrugated fine structure in cross-section corresponding to the embossing. While such a paper strip is simple and inexpensive to produce, it has low tensile strength, leading to relatively short wear and limited use. Furthermore, it is difficult, if not impossible, to introduce a deep structuring pattern into such a paper strip.

[0009] DE 10 2016 225 469 A1 and EP 1 688 460 A1 disclose methods for producing a lacquered textured film that is textured in an embossing step and subsequently treated with electron beams. However, the production of textured strips with a surface that allows coating with liquid or pasty plastic to form a film in a reverse process and subsequent removal of the film is not addressed in these documents.

[0010] Furthermore, DE 10 2005 051 392 A1 and EP 1 538 175 each disclose the production of textured plastic molded parts treated with electron beams. However, these documents do not address the production of textured strips with a surface that allows coating with liquid or pasty plastic to form a film in a reverse process and subsequent removal of the film.

[0011] The object of the invention is therefore to propose a graining tape of the type mentioned above and a method for producing it, which can be used with a wide variety of polymer systems and processing temperatures, can replace the paper graining tapes used to date, is resistant to high temperatures and can be produced while avoiding odor emissions.

[0012] To solve the problem posed, the invention proposes the design of a scar band according to the features of claim 1.

[0013] A method for producing such a scar band is the subject of claim 12.

[0014] Advantageous embodiments and further developments of the invention are the subject of the dependent claims.

[0015] The inventive proposal provides that the at least one layer is electron beam cross-linked and the upper surface is formed by a lacquer layer onto which the liquid or pasty plastic can be applied following the production of the scar tape.

[0016] The crosslinking of the at least one layer with electron beams, as provided for in the invention, achieves a previously unattainable temperature resistance of the thermoplastic olefin used to produce the at least one layer, which can reach up to 210 °C in long-term applications. Before crosslinking, the desired three-dimensional structure, for example a leather grain, can be introduced, with the lacquer coating forming the final surface being applied both before and after the introduction of the three-dimensional structuring, but before crosslinking.

[0017] According to one proposal of the invention, polymers based on ethylene, propylene, ethylene-propylene copolymers, graft copolymers and / or terpolymers are used as thermoplastic olefins to form the at least one layer.

[0018] Alternatively, at least one layer can also be formed from a coating containing a dispersion of the thermoplastic olefin and up to 50% by weight of a polyurethane dispersion, which is applied to a smooth substrate, such as paper, to create a suitable film. This method allows for thinner layers.

[0019] According to a further proposal of the invention, the at least one layer contains suitable crosslinking aids for improving the crosslinking properties by means of electron beams.

[0020] According to a further proposal of the invention, crosslinking agents can include polybutadiene, unmodified and / or modified acrylate compounds, allyl compounds, and / or silanes. Examples of crosslinking agents include mono-, di-, and trifunctional acrylates, polybutadiene, triallyl cyanurate (TAC), and triallyl isocyanurate (TAIC).

[0021] According to a further aspect of the invention, the raw material mixture for producing the at least one layer can include fillers such as chalks or aluminas, flame retardants, thermal conductivity additives such as silicon carbides, diamond powder, boron nitride, silver as an element or in compounds, aluminum oxides or copper particles, lubricants, external and internal stabilizers against heat influence, fluxes, pigments and / or dyes, blowing agents, and impact modifiers. Thermochromic pigments can also be used, thus enabling the temperature profiles to be identified within the corresponding temperature ranges.

[0022] To adjust the surface energy or adhesion behavior of the surface of the post-belt according to the invention, it is provided with a lacquer coating, which then forms the surface onto which the liquid or pasty plastic is subsequently applied to form the film when the post-belt is used and then removed. This lacquer coating is preferably made of a thermally stable and ideally thermoset lacquer, wherein, in addition to water- and solvent-based lacquer systems with corresponding isocyanates, carbodiimides, melamines, and azeridines, UV-crosslinking and, in particular, fully crosslinking systems, as well as optionally water-based systems, are preferably used. These lacquer systems exhibit higher temperature stability and, due to their radical crosslinking, allow covalent bonding to unmodified polyolefin surfaces.

[0023] The coating is either crosslinked together with the at least one layer during the action of the electron beams or separately immediately after the coating is applied.

[0024] Furthermore, according to another proposal of the invention, this coating system can be mixed with appropriate matting agents, silicone oils, acrylates, polyurethanes and fluoride-based components to form the coating, and may optionally contain heat stabilizers.

[0025] The at least one layer of the scar band according to the invention can, for example, be produced in a known manner in a calender or extruder, wherein, according to the invention, several, in particular two to four, layers of thermoplastic and electron-beam crosslinked olefin can also be provided one above the other to form the scar band according to the invention. Preferably, one or two layers are used which, on the one hand, offer good embossability and scar reproduction accuracy, and on the other hand, also have good heat absorption and thermal conductivity with simultaneously low heat capacity.

[0026] For example, a calender application is carried out at temperatures of 120 °C to 220 °C, preferably at 150 °C to 200 °C, resulting in a stable film.

[0027] According to another proposal, the underside of the grain band facing away from the paint coating is bonded to a carrier substrate, which gives the grain band, for example, low stretchability or elongation, high temperature resistance and a homogeneous thickness distribution, as well as enabling stability across the width.

[0028] Suitable substrates include textile fabrics, such as nonwovens (which may also be hydroentangled), knitted fabrics, and crocheted fabrics. The substrate, made from a textile fabric, can be based on glass fibers, carbon fibers, mineral fibers, cotton, viscose, polyamide, polyester, or aramid fibers, or blends thereof. In addition to textiles, metal foils, paper, or metal strips can also be used.

[0029] According to a further proposal of the invention, the carrier substrate is bonded to the underside surface by means of a suitable adhesive, for which, for example, two-component adhesives based on polyurethanes, epoxy resins, acrylates or modified silicones are considered suitable.

[0030] To improve adhesion, the underside surface of at least one layer, which is to be bonded firmly to the substrate, can also be modified by plasma or corona treatment using oxygen and possibly under the influence of moisture, in such a way that reactive groups are formed on the surface which can be reacted with appropriate adhesives or crosslinkers.

[0031] A procedure for producing a scar band of the type described above includes the following steps: a) Production of a film with at least one layer of a thermoplastic olefin, optionally containing crosslinking agent; b) Application of a lacquer coating to the produced film; c) Three-dimensional structuring of at least the lacquer coating applied to the film; d) Crosslinking of the at least one layer of the film and optionally the lacquer coating by action of electron beams.

[0032] The embossing or structuring of the polyolefin film, which may be laminated with a carrier substrate and coated with lacquer on the opposite side, is achieved in a temperature range between 120 and 290 °C, preferably between 180 and 260 °C, by using embossing tools such as vacuum embossing rollers, silicone embossing rollers, or steel embossing rollers. Following the embossing step, crosslinking is carried out using electron beams.

[0033] Crosslinking occurs at approximately 1 to 400 kilogray [kGy], depending on the raw material, preferably at approximately 10 to 100 kGy. The electron velocity at which the at least one layer is penetrated can be controlled by adjusting the applied voltage; typically, approximately 650 to 950 kV is applied, depending on the layer thickness, to ensure complete penetration.

[0034] The lamination of the at least one layer of the scar band according to the invention with a carrier substrate can take place at different times. In general, the following process sequences are available, particularly when producing the at least one layer in a calender or extruder: Version A: 1. Create a film with at least one layer; 2. Apply the lacquer coating and, if necessary, crosslink it; 3. Emboss the film; 4. Crosslink the film; 5. Laminate the film with a suitable substrate. Version B: 1. Create a film with at least one layer; 2. Laminate the film with a suitable substrate; 3. Apply the lacquer coating and, if necessary, crosslink it; 4. Emboss the film; 5. Crosslink the film. Version C: 1. Create a film with at least one layer; 2. Apply the lacquer coating and, if necessary, crosslink it; 3. Laminate the film with a suitable substrate; 4. Emboss the film; 5. Crosslink the film.

[0035] The invention is explained in further detail below with reference to exemplary embodiments shown in the drawing. The drawing shows: Figure 1 shows a schematic cross-section through a first embodiment of a scar band according to the invention; Figure 2 shows a schematic cross-section through a second embodiment of a scar band according to the invention.

[0036] From the Figures 1 and 2 Cross-sections of scar bands are visible, such as those used for the reverse process in the production of polyurethane coatings.

[0037] The scar band globally marked with reference symbol 1 according to Figure 1 comprises a layer 10 made of a thermoplastic olefin, for example a polyolefin, containing suitable crosslinking aids, such as polybutadiene.

[0038] If layer 10 has been produced by coating a polyolefin dispersion mixed with a polyurethane dispersion of up to 50% by weight onto a paper substrate, the thickness can be approximately 50 to 500 µm.

[0039] Alternatively, layer 10 can also be produced by calendering or extrusion, whereby layer thicknesses of approximately 150 to 2000 µm can be produced by calendering and of approximately 75 to 3000 µm by extrusion.

[0040] A lacquer coating 11 is applied to the top surface of layer 10 using a single or multiple roller application with an exemplary dry basis weight of 2 to 30 g / m², which simultaneously forms the later surface 110 of the grain band 1, on which the film is applied and removed in a reverse process.

[0041] The surface 110 is three-dimensionally structured, for example in the manner of a leather grain, which has been introduced into at least the lacquer coating 11 and optionally also the underlying layer 10 by the action of appropriate embossing rollers. The embossing depth can be between 0 and 1500 µm, preferably between 0 and 800 µm.

[0042] On the underside 100 facing away from the paint coating 11, the layer 10 is bonded to a carrier substrate 12, for example a water jet bonded nonwoven fabric with a basis weight of 25 to 800 g / m 2<, by means of a laminating adhesive applied, for example with a dry basis weight of 20 to 250 g / m 2<.

[0043] The alternative design according to Figure 2 differs from the design according to Figure 1 by using 10 layers of thermoplastic polyolefin instead of just one. Figure 1 in the representation according to Figure 2 A film is provided comprising two discrete layers 10.1, 10.2 of the thermoplastic polyolefin. The further structure corresponds to that of the Figure 1 , so that corresponding explanations can be omitted to avoid repetition.

[0044] Both in the exemplary embodiment according Figure 1as well as in the exemplary embodiment according Figure 2 The surface 110 is structured three-dimensionally, at least in the area of ​​the paint coating 11, and then exposed to the action of electron beams generated by applying a potential between 650 and 950 kV, so that preferably about 10 to 100 kGy are absorbed.

[0045] As a result of the crosslinking aid introduced into the at least one layer 10, 10.1, 10.2 of thermoplastic olefin, electron beam crosslinking of these layers 10, 10.1, 10.2 and optionally also of the lacquer coating 11 is effected, which leads to the curing of the irradiated layers and gives them outstanding temperature resistance up to 210 °C under long-term stress.

[0046] The result is a thermoplastic olefin-based grain tape with high wear resistance, which, for example, can easily withstand up to 400 oven cycles in polyurethane coatings, depending on the applied temperature and tensile force.

[0047] The scar tape according to the invention can be produced simply and efficiently and can be structured directly with any available embossing rollers, whereby desired haptic properties can be specifically adjusted and harmful emissions are largely avoided.

[0048] The grain band according to the invention can be used in particular in the production of coatings based on polyolefins, silicones, PVC and polyurethanes, as well as in the production of embossable silicone artificial leathers, which are made of silicone alone or in mixture with standard polymers such as PVC, polyolefins, celluloses, polyurethanes, polyamides or comparable systems. Reference symbol list:

[0049] 1. Grain band 10, 10.1, 10.2 Layer 11. Lacquer coating 12. Carrier substrate 100 Underside 110 Surface

Claims

1. Grain tape (1) comprising at least one layer (10, 10.1, 10.2) formed from a thermoplastic olefin having a three-dimensionally structured top surface (110), intended for production of a film by application of plastic in liquid or paste form for formation of the film by the inversion method and subsequent detachment of the film from the surface, characterized in that the at least one layer (10, 10.1, 10.2) has been electron beam-crosslinked and the top surface (110) is formed by a varnish coating (11) to which the plastic in liquid or paste form is applicable.

2. Grain tape (1) according to Claim 1, characterized in that the thermoplastic olefin used to form the at least one layer (10, 10.1, 10.2) is polymers based on ethylene, propylene, ethylene-propylene copolymers, graft copolymers and / or terpolymers.

3. Grain tape (1) according to Claim 1 or 2, characterized in that the at least one layer (10, 10.1, 10.2) has been formed from a spreadable coating comprising a dispersion of the thermoplastic olefin and up to 50% by weight of a polyurethane dispersion.

4. Grain tape (1) according to any of Claims 1 to 3, characterized in that the at least one layer (10, 10.1, 10.2) contains crosslinking aids.

5. Grain tape (1) according to Claim 4, characterized in that the crosslinking aids present are polybutadienes, unmodified and / or modified acrylate compounds, allyl compounds and / or silanes.

6. Grain tape (1) according to any of Claims 1 to 5, characterized in that the thermoplastic olefin contains fillers, flame retardants, thermal conductivity additives, lubricants, stabilizers, flow agents, pigments, dyes, blowing agents and / or impact modifiers.

7. Grain tape (1) according to any of Claims 1 to 6, characterized in that the varnish coating (11) is based on a thermally stable water- or solvent-based and / or UV-crosslinking varnish system.

8. Grain tape (1) according to any of Claims 1 to 7, characterized in that the varnish coating (11) contains flatting agents, silicones, acrylates, polyurethanes and / or fluoride-based components, and thermal stabilizers.

9. Grain tape (1) according to any of Claims 1 to 8, characterized in that it comprises two to four layers (10, 10.1, 10.2) of thermoplastic and electron beam-crosslinked olefin.

10. Grain tape (1) according to any of Claims 1 to 9, characterized in that the bottom side (100) remote from the varnish coating (11) is firmly bonded to a carrier substrate (12).

11. Grain tape (1) according to Claim 10, characterized in that the carrier substrate (12) is formed by a textile fabric, a metal foil or a paper or metal strip.

12. Grain tape (1) according to either of Claims 10 and 11, characterized in that the carrier substrate (12) is firmly bonded to the bottom surface (100) by means of an adhesive.

13. Method of producing a grain tape (1) according to any of the preceding claims, comprising the steps of: a) producing a film having at least one layer (10, 10.1, 10.2) of a thermoplastic olefin; b) applying a varnish coating (11) to the film produced; c) three-dimensionally structuring at least the varnish coating (11) applied to the film; d) crosslinking the at least one layer (10, 10.1, 10.2) of the film by the action of electron beams.

14. Method according to Claim 13, characterized in that the at least one-layer film is produced by calendering or extrusion or by spreading an olefin dispersion containing up to 50% by weight of a polyurethane dispersion onto a smooth substrate.

15. Method according to Claim 13 or 14, characterized in that the film produced, prior to the crosslinking in step d), is firmly bonded to a carrier substrate (12) on the bottom side (100) opposite the varnish coating (11).

16. Method according to any of Claims 13 to 15, characterized in that the three-dimensional structuring in step c) is brought about by roll embossing at a temperature of 120 to 290°C.