METHOD FOR SOLDERING AT LEAST ONE COMPONENT WITH AT LEAST ONE SUPPORT ELEMENT

DE502022002021D1Active Publication Date: 2024-11-14ENDRESS & HAUSER GMBH & CO KG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE502022002021
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-12-17
Filing Date
2022-11-28
Publication Date
2024-11-14
Estimated Expiration
2042-11-28

AI Technical Summary

Technical Problem

Conventional soldering methods often result in voids and unstable joints due to insufficient flux escape, particularly with heavy components like LGA components, leading to stress-induced cracks and reliability issues in field devices.

Method used

A method using two solders with different liquidus temperatures, where the second solder melts earlier than the first, allowing flux to evaporate before the actual soldering process, creating a stable and low-void joint by maintaining a minimum distance between the connection and contact surfaces.

Benefits of technology

This approach significantly reduces voids and enhances the stability of solder joints, preventing air inclusions and stress-induced cracks, thereby improving the reliability of field devices.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method for soldering at least one component to at least one carrier element, wherein the at least one component has at least one connection surface, wherein the at least one carrier element has at least one contact surface, wherein the at least one connection surface and the at least one contact surface are designed to be soldered to one another.

[0002] Field devices in process and automation technology are used to monitor and / or determine at least one process variable, for example, a chemical and / or physical variable, of a medium. For the purposes of this application, field devices essentially refer to all measuring devices that are used close to the process and that provide or process-relevant information. A large number of such field devices are manufactured and distributed by companies in the Endress+Hauser Group.

[0003] The process variable to be determined by the field device can be the fill level, flow, pressure, temperature, pH value, redox potential, or conductivity of the respective medium. The various possible measuring principles underlying the determination of the process variable are known from the state of the art and will not be explained further here. Field devices for measuring fill levels are designed in particular as microwave level gauges, ultrasonic level gauges, time domain reflectometric level gauges (TDR), radiometric level gauges, capacitive level gauges, conductive level gauges, and vibronic level gauges. Field devices for measuring flow, on the other hand, operate according to the Coriolis, ultrasonic, vortex, thermal, and / or magnetic inductive measuring principles.Pressure measuring devices are typically absolute, gauge, or differential pressure devices. In addition to the previously mentioned measuring devices and actuators, field devices also include remote I / Os, wireless adapters, and generally devices located at the field level.

[0004] A field device typically comprises a sensor that comes into contact with the process medium at least partially and / or at least temporarily, and an electronics unit that serves, for example, to acquire, evaluate, and / or supply signals. The electronics unit of the field device is typically arranged in a housing and additionally has at least one connection element for connecting the electronics unit to the sensor and / or an external unit and for transmitting data and / or power. The connection element can be any desired connection; a wireless connection is also possible. The electronics unit and the sensor of the field device can be designed as separate units with separate housings or as a single unit with one housing.

[0005] As a rule, at least the electronics unit has at least one carrier element, such as a printed circuit board, with components arranged thereon, which are electrically and mechanically connected via at least one solder joint between a connection surface of the component and a contact surface of the carrier element. For the reliability of the electronics unit or the field device, high quality solder joints between the connection surfaces of the component and the contact surfaces of the carrier element is of great importance. The quality of the solder joints depends, among other things, on whether the distance between the connection surface and the contact surface (the so-called solder gap height) is sufficiently large. If the solder gap height is too small, stress-induced cracks can occur in the solder joint due to temporal temperature fluctuations, for example.Particularly with a heavy component and the resulting low solder gap height of the solder joint, there is a risk of unwanted air inclusions, so-called voids, forming within the solder joints. This is especially true when the component's connection surfaces are located beneath the component. Such voids are the result of the flux contained in the solder not completely escaping from the solder joint. The applicant's investigations have shown that with such heavy components, voids within the solder joint cannot be completely avoided, even when using vacuum soldering processes.

[0006] A method for producing a soldered connection is known, for example, from US 2011 / 220398 A1.

[0007] The object of the present invention is therefore to provide a method which enables a stable and low-void solder joint between a component and a carrier element.

[0008] According to the invention, the object is achieved by a method according to claim 1 for soldering at least one component to at least one carrier element, wherein the at least one component has at least one connection surface, wherein the at least one carrier element has at least one contact surface, wherein the at least one connection surface and the at least one contact surface are designed to be soldered to one another, wherein the method comprises the following steps: Applying a first solder having a first liquidus temperature to the at least one connection surface, remelting the first solder on the at least one connection surface at a remelting temperature that exceeds the first liquidus temperature of the first solder, wherein the remelted first solder forms a solder deposit, applying a second solder having a second liquidus temperature to the at least one contact surface, wherein the second solder has a different composition than the first solder, wherein the first liquidus temperature is up to 20 K higher than the second liquidus temperature, positioning the at least one component relative to the at least one carrier element such that the at least one connection surface faces the at least one contact surface, heating the at least one component and the at least one carrier element in a soldering furnace to a predetermined soldering temperature,such that a first time period between reaching the second liquidus temperature and reaching the first liquidus temperature is up to 25 s, soldering the at least one connection surface to the at least one contact surface in the soldering furnace for a second time period at the predetermined soldering temperature, which is above the first liquidus temperature and the second liquidus temperature.

[0009] Typically, to solder a component to a support element, the components and the support element are each printed with the same solder, whereby the solder may be remelted on either the component or the support element. The same solder therefore has a common liquidus temperature, so that during the soldering process, the solder on the component and the solder on the support element melt simultaneously.

[0010] According to the invention, two different solders are used, the first solder and the second solder, which differ in their respective liquidus temperatures. Both the first solder and the second solder have a flux contained in the respective solder. If the first solder and / or the second solder has a melting range, the first liquidus temperature and / or second liquidus temperature is to be regarded as the lowest temperature of the melting range. During the soldering process, the temperature in the soldering furnace is continuously increased until a predetermined soldering temperature is reached at which both the first solder and the second solder are melted. Because the second solder has a lower second liquidus temperature than the first solder, the second solder will melt earlier than the first solder during the heating process.Depending on the solders used, there is a time delay between the melting of the second solder and the melting of the first solder, which can be up to 25 s and corresponds to the first time period.

[0011] During the first time period or time offset, the second solder melts while the first solder is still solid in the form of the solder deposit. The flux contained in the second solder will already partially evaporate during the time offset and escape from the solder and the soldering joint. Since the solder deposit from the first solder has not yet melted, the height of the solder deposit sets a minimum distance between the at least one connection surface and the at least one contact surface, which facilitates the escape of the flux from the second solder. The first time period should not be chosen so long that the flux can re-enter the second solder, which is why initial time periods exceeding 25 seconds should be avoided. After the temperature in the soldering oven has been increased to the specified soldering temperature, the first solder melts and is soldered to the second solder.

[0012] By remelting the first solder and forming a solder deposit, the flux contained in the first solder has already largely evaporated and is no longer contained in the solder deposit. By melting the second solder before the first solder, the flux in the second solder has also largely escaped from the second solder before the actual soldering process, which includes melting both the first solder and the second solder, begins. This means that there is hardly any or only a small amount of flux left in the first solder and the second solder, which can potentially remain as an air inclusion in the formed solder joint. This creates a low-void and stable solder joint between the at least one connection surface and the at least one contact surface.

[0013] Preferably, the first solder and the second solder are completely melted in the soldering furnace when soldering the at least one connection surface to the at least one contact surface.

[0014] Preferably, the first liquidus temperature is up to 10 K higher than the second liquidus temperature.

[0015] In particular, the first liquidus temperature is up to 5 K higher than the second liquidus temperature.

[0016] In one embodiment, the first time period between reaching the second liquidus temperature and reaching the first liquidus temperature is up to 15 s.

[0017] In particular, the first time period between reaching the second liquidus temperature and reaching the first liquidus temperature is up to 10 s.

[0018] In a further development, the specified soldering temperature is at least 15 K higher than the first liquidus temperature.

[0019] Preferably, a first printed circuit board is used as the at least one carrier element. In one embodiment, an LGA component is used as the at least one component, wherein the LGA component is a second printed circuit board with an integrated circuit arranged on a first surface of the second printed circuit board, wherein one surface of the at least one component is formed by a second surface of the second printed circuit board opposite the first surface, wherein the at least one connection surface of the at least one component is designed as a land grid array arranged on the surface of the at least one component. Such LGA components are comparatively heavy components due to their integrated circuit, which leads to a large number of voids in the solder joints between the component and the carrier element during conventional soldering processes.The proposed method is particularly advantageous for LGA components, since the staggered melting of the second solder and the first solder during the soldering process creates a minimum distance between the at least one connection surface and the at least one contact surface due to the unmelted first solder. When using two identical solders, the simultaneous melting of the solder on the connection surface and the contact surface causes the LGA component to sink toward the carrier element, reducing the distance between the LGA component and the carrier element and hindering the escape of flux from the solder. LGA components typically have a large number of connection surfaces.

[0020] The remelting of the first solder is preferably carried out in a reflow soldering oven or a curing oven.

[0021] Preferably, the soldering of the at least one connection surface to the at least one contact surface takes place in a reflow soldering oven.

[0022] In one embodiment, a limit value is specified for the duration of thermal stress on the at least one component and / or the at least one support element. If exceeded, the at least one component and / or the at least one support element is damaged. The at least one component and / or the at least one support element are generally susceptible to high temperatures and may therefore only be exposed to high temperatures up to a (temporal) limit value. The sum of the first time period and the second time period should not exceed the limit value for the duration of the thermal stress.

[0023] In the following, the present invention will be explained with reference to the following figures Fig. 1-7 are explained in more detail. They show: Fig. 1 : a schematic representation of the component before printing with solder. Fig. 2 : a schematic representation of the component after printing with solder. Fig. 3 : a schematic representation of the component with the remelted solder deposit. Fig. 4 : a schematic representation of the component and the carrier element in a soldering furnace before soldering. Fig. 5 : a schematic graph of the soldering process. Fig. 6 : a schematic representation of a top view of an LGA device (according to the state of the art). Fig. 7 : a schematic cross-sectional view of an LGA device (according to the state of the art).

[0024] The method according to the invention serves for soldering at least one component 1 to at least one carrier element 2. The present invention can be used in all types of field devices, a non-limiting selection of which was mentioned at the beginning.

[0025] In Fig. 1 The at least one component 1 is shown schematically. The component 1 has at least one connection surface 3, which are separated from each other, for example, by solder stops 17. In addition, an optional stencil 18 is shown, by means of which the first solder 5 with a first liquidus temperature T1 is applied to the at least one connection surface 3. After removing the stencil 18, the solder 5 is located on the connection surfaces 3 of the component 1, as shown in Fig. 2 shown. Subsequently, the first solder 5 is remelted at a remelting temperature that exceeds the first liquidus temperature T1 of the first solder 5. This step of remelting the first solder 5 takes place, for example, in a reflow soldering oven or a curing oven. The remelted first solder 5 forms one or more solder deposits 6, which in Fig. 3 is shown schematically.

[0026] In a next step, a second solder 7, which has a second liquidus temperature T2, is applied to at least one contact surface 4 of the at least one carrier element 2. The carrier element 2 is, for example, a first printed circuit board 9. Analogous to Fig. 1 This can be done, for example, using a stencil. A carrier element 2 printed with the second solder 7 is shown, for example, in Fig. 4 The carrier element 2 is then positioned and aligned relative to the component 1 such that the connection surfaces 3 face the contact surfaces 4. As shown in Fig. 4 As can be seen, the connection surfaces 3 and the contact surfaces 4 are aligned one above the other in the soldering oven 8. To solder the component 1 to the carrier element 2, the component 1 is placed on the carrier element 2 (not shown). In the selected example, only one carrier element 2 and one component 1 are shown, each of which has a plurality of connection surfaces 3 or contact surfaces 4. It is also possible, for example, to solder a plurality of components 1 to one carrier element 2. The at least one contact surface 4 and the at least one connection surface 3 are designed to be soldered to one another. In order to achieve a mechanical and electrical connection between the component 1 and the carrier element 2, the at least one connection surface 3 and the at least one contact surface 4 are designed to be electrically conductive, for example by being provided with metallized surfaces.

[0027] The first solder 5 and the second solder 7 have different compositions. The first liquidus temperature T1 of the first solder 5 is up to 20 K, in particular up to 10 K, in particular up to 5 K, higher than the second liquidus temperature T2 of the second solder 7. The component 1 and the carrier element 2 are heated in the soldering furnace 8 to a predetermined soldering temperature T3, wherein a first time period Δt1 between reaching the (lower) second liquidus temperature T2 and the (higher) first liquidus temperature T1 is up to 25 s, in particular up to 15 s, in particular up to 10 s.

[0028] The temperature profile during soldering of component 1 and carrier element 2 is shown schematically in the Fig. 5 shown. The temperature T rises with time t while the soldering furnace 8 is heated up. At a time t1, the second liquidus temperature T2 of the second solder 7 is initially reached. The first time period Δt1 = t2 - t1 elapses until the first liquidus temperature T1 of the first solder 5 is reached. Within the first time period Δt1, the second solder 7 is melted and the flux can already escape from the second solder 7, while the first solder 5 has not yet begun to melt. The height of the solder deposit 6 of the first solder 5 above the connection surfaces 3 thus specifies a minimum distance below which the distance between connection surfaces 3 and contact surfaces 4 cannot fall. The flux can thus easily escape from the second solder 7 and evaporate. The first solder 5 also originally contains flux, but most of it escapes from the first solder 5 when the first solder 5 is remelted.

[0029] After the first liquidus temperature T1 has been exceeded, the soldering furnace 8 finally reaches a predetermined soldering temperature T3, which lies above the first liquidus temperature T1 and the second liquidus temperature T2 and at which the soldering of the connection pads 3 to the contact pads 4 takes place. In particular, the first solder 5 and the second solder 7 are completely melted when the connection pads 3 are soldered to the contact pads 4. The soldering of the connection pads 3 to the contact pads 4 takes place, for example, in a reflow soldering furnace. The predetermined soldering temperature T3 is maintained for a second time period Δt 2 = t4 - t3 before the soldered component 1 and the carrier element 2 are cooled. For example, the second time period Δt 2 is between 30 s and 90 s, in particular between 30 s and 70 s. The predetermined soldering temperature T3 is optionally at least 15 K higher than the first liquidus temperature T1.The intervals between the different temperatures and times are given in . Fig. 5 shown only schematically, no absolute values ​​or relations can be derived from Fig. 5 be derived.

[0030] For example, the first solder 5 can have a first liquidus temperature T1 of approximately 227°C, and the second solder 7 can have a second liquidus temperature T2 of 217°C. The difference between the two liquidus temperatures T1, T2 is thus approximately 10°C. The first time period Δt 1 is, for example, approximately 9 s. The second time period Δt 2 is, for example, approximately 30 to 70 s.

[0031] Furthermore, a limit value can be specified for the duration of a thermal load on the at least one component and / or the at least one support element 2; if exceeded, the at least one component 1 and / or the at least one support element 2 is damaged. This limit value must be taken into account when designing the first time period Δt 1 and / or the second time period Δt 2.

[0032] In Fig. 6 An exemplary component 1 is shown in plan view. In this example, component 1 is an LGA component 10, which has a plurality of connection pads 3 formed on the surface 14 of the LGA component 10 in the form of a land grid array. Due to the size and weight of the LGA component 10, the flux can only escape from the solder with difficulty and incompletely, particularly from the internal connection pads 3, using conventional soldering methods, resulting in a high number of air inclusions in the formed solder joints.

[0033] Fig. 7 shows a schematic cross-section through an LGA component 10. An integrated circuit 13 is arranged on a first surface 12 of a second circuit board 11, which is optionally arranged in a housing 16. The second surface 15 of the second circuit board 11 lies opposite the first surface 12 and forms the surface 14 of the LGA component 10. The integrated circuit is electrically connected to the connection pads 3 via connections 19. Bezugszeichenliste

[0034] 1Component 2Carrier element 3Connection surface 4Contact surface 5First solder 6Solder deposit of the first solder 7Second solder 8Soldering oven 9First circuit board 10LGA component 11Second circuit board 12First surface of the second circuit board 13Integrated circuit 14Surface of the component 15Second surface of the second circuit board 16Housing 17Solder mask 18Stencil 19Connection T1first liquidus temperature of the first solder T2second liquidus temperature of the second solder T3specified soldering temperature Δt 1 first time period Δt 2 second time period

Claims

1. A method for soldering at least one component (1) with at least one carrier element (2), wherein the at least one component (1) has at least one connecting surface (3), wherein the at least one carrier element (2) has at least one contact surface (4), wherein the at least one connecting surface (3) and the at least one contact surface (4) are designed to be soldered together, wherein the method comprises the following steps: - Applying a first solder (5) containing a first flux with a first liquidus temperature (T1) to the at least one connecting surface (3), - Remelting the first solder (5) on the at least one connecting surface (3) at a remelting temperature, which is higher than the first liquidus temperature (T1) of the first solder (5), wherein the remelted first solder (5) forms a solder deposit (6), characterized by the following steps: - Applying a second solder (7) containing a second flux with a second liquidus temperature (T2) to the at least one contact surface (4), wherein the second solder (7) has a different composition to the first solder (5), wherein the first liquidus temperature (T1) is different from the second liquidus temperature (T2) and is up to 20 K higher than the second liquidus temperature (T2), - Positioning the at least one component (1) relative to the at least one carrier element (2) in such a way that the at least one connecting surface (3) is facing the at least one contact surface (4), - Heating the at least one component (1) and the at least one carrier element (2) in a soldering oven (8) to a specified soldering temperature (13) in such a way that a first time period (Δt1) from when the second liquidus temperature (T2) is reached until when the first liquidus temperature (T1) is reached lasts for up to 25 s, wherein the second solder melts during the first time period (Δt1) while the first solder remains solid, - Soldering the at least one connecting surface (3) to the at least one contact surface (4) in a soldering oven (8) for a second time period (Δt2) at the specified soldering temperature (T3), which is above the first liquidus temperature (T1) and the second liquidus temperature (T2).

2. The method as claimed in claim 1, wherein the first solder (5) and the second solder (7) are completely melted when the at least one connecting surface (3) is soldered to the at least one contact surface (4) in a soldering oven (8).

3. The method as claimed in at least one of claims 1 and 2, wherein the first liquidus temperature (T1) is up to 10 K higher than the second liquidus temperature (T2).

4. The method as claimed in at least one of claims 1 to 3, wherein the first liquidus temperature (T1) is up to 5 K higher than the second liquidus temperature (T2).

5. The method as claimed in at least one of claims 1 to 4, wherein the first time period (Δt1) from when the second liquidus temperature (T2) is reached until when the first liquidus temperature (T1) is reached lasts for up to 15 s.

6. The method as claimed in at least one of claims 1 to 5, wherein the first time period (Δt1) from when the second liquidus temperature (T2) is reached until when the first liquidus temperature (T1) is reached lasts for up to 10 s.

7. The method as claimed in at least one of claims 1 to 6, wherein the specified soldering temperature is at least 15 K higher than the first liquidus temperature (T1).

8. The method as claimed in at least one of claims 1 to 7, wherein a first PCB (9) is used as the at least one carrier element (2).

9. The method as claimed in at least one of claims 1 to 8, wherein an LGA component (10) is used as the at least one component (1), wherein a second PCB (11) with an integrated circuit (13) arranged on a first surface (12) of the second PCB (11) is used as the LGA component (10), wherein one surface (14) of the at least one component (1) is formed by a second surface (15) of the second PCB (11) which is opposite the first surface (12), wherein the at least one connection surface (3) of the at least one component (1) is configured as a land grid array arranged on the surface (14) of the at least one component (1).

10. The method as claimed in at least one of claims 1 to 9, wherein the first solder (5) is remelted in a reflow soldering oven or a curing oven.

11. The method as claimed in at least one of claims 1 to 10, wherein the at least one connecting surface (3) is soldered to the at least one contact surface (4) in a reflow soldering oven.

12. The method as claimed in at least one of claims 1 to 11, wherein a limit value for the duration of thermal loading of the at least one component (1) and / or the at least one carrier element (2) is specified which, if exceeded, will result in damage to the at least one component (1) and / or the at least one carrier element (2).