Method for manufacturing an image sensor

The use of chemical plasma etching in the manufacturing of image sensors addresses the issue of polymer fiber formation, ensuring a reliable and consistent manufacturing process by preventing irregularities and enhancing the structural integrity of microlenses.

FR3126170B1Active Publication Date: 2024-10-04STMICROELECTRONICS (CROLLES 2) SAS
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2021008614
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-08-10
Publication Date
2024-10-04
Estimated Expiration
2041-08-10

AI Technical Summary

Technical Problem

Existing methods for manufacturing image sensors with microlenses suffer from issues such as the formation of polymer fibers or filaments during etching, leading to sealing and integrity defects, which affect the reliability and consistency of the manufacturing process.

Method used

Implementing a chemical plasma etching process that is isotropic and uses dioxygen-based plasma to etch the resin layer, replacing the traditional anisotropic physical etching, which reduces the formation of polymer fibers and ensures a smooth surface for the protective layer, thereby enhancing the manufacturing process's reliability.

Benefits of technology

The chemical plasma etching method prevents the formation of polymer fibers, ensuring a smooth and reliable manufacturing process with improved integrity and consistency of the image sensor's microlenses, reducing the need for additional cleaning steps and maintaining the structural integrity of the microlenses.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000011_0000
    Figure 00000011_0000
  • Figure 00000011_0001
    Figure 00000011_0001
  • Figure 00000011_0002
    Figure 00000011_0002
Patent Text Reader

Abstract

Method for manufacturing an image sensor. This description relates to a method for manufacturing an image sensor comprising: a) the formation of a plurality of microlenses (23) in a layer (15) of a first resin; b) after step a), the formation of a mask (25) of a second resin, on and in contact with said layer (15); etc.; and b) after step b), the chemical etching of said layer (15) by plasma through the mask (25). Figure for the abstract: Fig. 11
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Method for manufacturing an image sensor Technical field

[0001] The present description relates generally to the field of image sensors and more particularly relates to a method of manufacturing an image sensor. Prior art

[0002] An image sensor generally comprises a plurality of photodetectors, for example photodiodes, integrated in and on a semiconductor substrate.

[0003] We are particularly interested here in image sensors whose photodetectors are surmounted by a layer of microlenses. This layer of microlenses makes it possible to focus the incident radiation onto the photodetectors.

[0004] It would be desirable to improve at least in part certain aspects of the known methods of manufacturing an image sensor comprising a microlens layer. Summary of the invention

[0005] One embodiment provides a method of manufacturing an image sensor comprising: a) forming a plurality of microlenses in a layer of a first resin; b) after step a), forming a mask of a second resin, on and in contact with said layer; and c) after step b), chemical plasma etching of said layer, through the mask.

[0006] According to one embodiment, said layer covers one face of a semiconductor substrate in which a plurality of photodetectors have been previously formed.

[0007] According to one embodiment, said layer further covers a contact recovery pad previously formed on the substrate.

[0008] According to one embodiment, during step c), the contact recovery pad is exposed.

[0009] According to one embodiment, in step a), the formation of the microlenses comprises a step d) of forming microlens-shaped structures in a layer of a third resin, followed by a step e) of transferring said structures into the layer of the first resin by physical etching.

[0010] According to one embodiment, in step d), the structures are formed by photolithography and finishing.

[0011] According to one embodiment, the method comprises, after step c), a step of depositing a protective and insulating layer on the surface and on the sides of the layer in the first resin.

[0012] According to one embodiment, after step c), the mask is removed using a solvent.

[0013] According to one embodiment, the layer of the first resin is crosslinked.

[0014] According to one embodiment, the layer of the first resin is non-photosensitive.

[0015] According to one embodiment, the plasma comprises dioxygen.

[0016] One embodiment provides an image sensor comprising a semi- conductor in and on which a plurality of photodetectors are integrated, the substrate being coated with a layer of a first resin in which a plurality of microlenses are formed, said layer comprising an opening facing a contact recovery pad arranged on the substrate, said opening having inclined side walls. Brief description of the drawings

[0017] These characteristics and advantages, as well as others, will be explained in detail in the following description of particular embodiments given without limitation in relation to the attached figures among which:

[0018] [Fig.l] is a sectional view illustrating a device obtained at the end of a step of an example of a method for manufacturing an image sensor;

[0019] [Fig.2] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0020] [Fig.3] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0021] [Fig.4] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0022] [Fig.5] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0023] [Fig.6] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0024] [Fig.7] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0025] [Fig.8] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0026] [Fig.9] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0027] [Fig. 10] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor;

[0028] [Fig.l 1] is a sectional view illustrating a device obtained at the end of a step of an example of a method of manufacturing an image sensor according to an implementation mode;

[0029] [Fig. 12] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor according to an embodiment; and

[0030] [Fig. 13] is a sectional view illustrating a device obtained at the end of another step of an example of a method of manufacturing an image sensor according to one embodiment. Description of the embodiments

[0031] The same elements have been designated by the same references in the different figures. In particular, the structural and / or functional elements common to the different embodiments may have the same references and may have identical structural, dimensional and material properties.

[0032] For the sake of clarity, only the steps and elements useful for understanding the embodiments described have been shown and are detailed. In particular, the production of the photodetectors of the image sensors described, as well as their control circuits, has not been detailed, the production of these elements being within the scope of the person skilled in the art from the indications of the present description.

[0033] Unless otherwise specified, when referring to two elements connected to each other, this means directly connected without intermediate elements other than conductors, and when referring to two elements connected (in English "coupled") to each other, this means that these two elements can be connected or be connected by means of one or more other elements.

[0034] In the following description, when reference is made to absolute position qualifiers, such as the terms "front", "back", "top", "bottom", "left", "right", etc., or relative position qualifiers, such as the terms "above", "below", "upper", "lower", etc., or to orientation qualifiers, such as the terms "horizontal", "vertical", etc., reference is made unless otherwise specified to the orientation of the figures.

[0035] Unless otherwise specified, the expressions "about", "approximately", "substantially", and "of the order of" mean to within 10%, preferably to within 5%.

[0036] Figures 1 to 10 illustrate, schematically and partially, devices or structures obtained at the end of successive steps of an example of a method for manufacturing an image sensor.

[0037] More particularly, [Fig. 1] corresponds to a starting structure comprising a semiconductor substrate 11, for example a silicon substrate, in which photodetectors 12 have been previously formed. By way of example, the photodetectors 12 are photodiodes, for example, adapted to capture infrared radiation, visible and / or ultraviolet. For example, the photodetectors 12 are photodetectors made in CMOS technology (from the English "Complementary Metal Oxide Semiconductor" - complementary metal oxide semiconductor).

[0038] In this example, the substrate 11 is intended to be illuminated by its upper face 11. The starting structure illustrated in [Fig. 1] further comprises one or more contact pads 13 located on the side of the upper face of the substrate 11. The pads 13 are intended to be connected to an external device, for example by means of electrically conductive wires, for example metal wires. The pads 13 are arranged out of line with the photodetectors 12 so as not to mask the photodetectors 12. By way of example, in top view, the photodetectors 12 are located in a central region of the substrate 11, and the pads 13 are located opposite a peripheral region of the substrate 11.

[0039] By way of example, the contact recovery pads 13 are connected to one or more metallization levels arranged on the lower face side of the substrate 11, by insulated conductive vias (not detailed in the figures) passing vertically through the substrate 11. By way of example, the contact recovery pads 13 are made of a metallic material, for example aluminum.

[0040] Figures 2 to 4 illustrate devices obtained at the end of steps of forming a layer of microlenses on the side of the upper face of the substrate 11, opposite the photodetectors 12.

[0041] [Fig.2] illustrates a device obtained at the end of a step of forming a resin layer 15 on the side of the upper face of the substrate 11.

[0042] The layer 15 is, for example, deposited in full wafer form over the entire surface of the upper face of the substrate 11. The layer 15 thus covers the contact recovery pads 13, and the photodetectors 12. The layer 15 is made of a resin transparent to the detection wavelengths of the sensor. The layer 15 has, for example, a thickness of between 1 μm and 6 μm, for example of the order of 4 μm.

[0043] The resin of layer 15 is, for example, a crosslinked resin which cannot be dissolved in the usual liquid solvents for developing and / or etching resins. The resin of layer 15 is, for example, a non-photosensitive resin. For example, the resin of layer 15 has a flat upper face. For example, the resin of layer 15 is chosen so that it can be crosslinked, for example by UV rays or from a certain temperature, for example, of the order of 200°C. For example, the resin of layer 15 is chosen so that it can be etched using an oxygen-based physical plasma. For example, the resin of layer 15 comprises a polymer, for example of the acrylic type.

[0044] [Fig. 3] illustrates a device obtained at the end of a step of forming an etching mask 19 on the upper face of the resin layer 15. The mask 19 comprises microlens-shaped structures, intended to be transferred into the resin layer 15 during a subsequent etching step, so as to form microlenses in the layer 15.

[0045] By way of example, the mask 19 is formed from a layer of photosensitive resin. The resin of the mask 19 is for example first deposited full plate, on and in contact with the upper face of the layer 15. At this stage, the resin of the mask 19 has for example a substantially uniform thickness over the entire surface of the structure. The deposition of the resin of the mask 19 can be done by a spin coating technique or by any other suitable deposition technique. The resin layer of the mask 19 is then structured, for example by photolithography, so as to form, opposite the photodetectors 12, separate resin pads 21. In this example, an individual resin pad 21 is provided opposite each photodetector 12 of the sensor. A finishing annealing is then carried out, during which the resin pads 21 deform to take the form of microlenses. After finishing, the resin pads 21 are, for example, separated.The embodiments described are however not limited to this particular case. The pads 21 have for example a thickness less than the thickness of the layer 15.

[0046] [Fig.4] illustrates a device obtained at the end of a physical etching step of the layer 15 and the mask 19, leading to the transfer of the pattern of the mask 19 into an upper part of the layer 15. The etching is for example stopped when all the resin of the mask 19 has been consumed.

[0047] Thus, in the device illustrated in [Fig.4], the layer 15 comprises microlenses 23 facing the photodetectors 12. By way of example, the microlenses 23 have a height of between 0.5 pm and 3 pm.

[0048] At this stage, the connection pads 13 remain covered by the resin of the layer 15.

[0049] Figures 5 to 7 illustrate devices obtained after steps of removing the resin of layer 15 opposite the pads 13, to allow electrical contact to be reestablished on the pads 13.

[0050] [Fig. 5] illustrates a device obtained at the end of a step of forming a masking layer 25 of resin on the upper face of the layer 15.

[0051] By way of example, the layer 25 is first deposited full plate on the upper face of the layer 15, for example in contact with the upper face of the layer 15. The layer 25 is then removed, for example by photolithography, opposite the pads 13, so as to expose the portion of the resin layer 15 coating the pads 13. The resin of the layer 25 is, for example, a photosensitive resin.

[0052] By way of example, the layer 25 has a thickness greater than the thickness of the layer 15. By way of example, the layer 25 has a thickness of between 4 μm and 10 μm, for example of the order of 5 μm.

[0053] [Fig.6] illustrates a device obtained at the end of a step of etching layer 15 through layer 25. During this step, layer 25 is used as an etching mask.

[0054] More particularly, during this step, the part of the layer 15 not covered by the layer 25 is removed so as to reveal the upper face of the contact recovery pads 13.

[0055] The etching carried out during this step is a physical etching by plasma, called etching by ion bombardment, reactive dry etching or spray etching ("dry etching" in English). Such etching results in a removal of material by bombardment, for example, using a dioxygen-based plasma. The plasma used during this etching step has, for example, a different composition from the plasma used during the etching leading to the formation of the microlenses 23.

[0056] During the above-mentioned step, layers 25 and 15 are consumed simultaneously.

[0057] The etching step is for example stopped when the contact pads 13 are completely cleared and there are no more residues of the layer 15 on their surface. At this stage, a part of the layer 25 remains on the surface of the layer 15 opposite the microlenses 23.

[0058] [Fig.7] illustrates a device obtained at the end of a step of removing the remaining part of the layer 25 so as to release the upper face of the microlenses 23. This removal step is for example carried out by wet etching using a solvent, using an etching solution making it possible to selectively etch the material of the layer 25 relative to the material of the layer 15.

[0059] [Fig.8] illustrates a device obtained at the end of a step of depositing a protective layer 29 made of an electrically insulating material on the surface of the device illustrated in [Fig.7],

[0060] The layer 29 extends for example continuously over the entire upper surface of the device of [Fig.7]. Thus, the layer 29 covers in particular the microlenses 23 and the pads 13.

[0061] For example, layer 29 is made of a material which protects layer 15 from humidity. Layer 29 is, for example, made of an oxide, for example silicon oxynitride (SiON).

[0062] By way of example, the protective layer 29 is deposited, by a conformal deposition method on the upper face of the device illustrated in [Fig.7], for example by chemical vapor deposition, for example plasma-enhanced chemical vapor deposition (PECVD).

[0063] The layer 29 has, for example, a thickness of between 50 nm and 500 nm, for example of the order of 300 nm.

[0064] Figures 9 and 10 illustrate devices obtained at the end of steps of localized removal of the protective layer 29 directly above all or part of each of the contact resumption pads 13, to allow the resumption of electrical contact on the pads 13.

[0065] [Fig. 9] illustrates a device obtained at the end of a step of depositing a resin layer 31 on the upper face of the device of [Fig. 8], and of forming, in the resin layer 31, a through opening 33 opening onto the protective layer 29 opposite the pad 13. The opening 33 is for example formed by photolithography.

[0066] [Fig. 10] illustrates a device obtained at the end of a step of etching the protective layer 29 at the bottom of the opening 33, using the resin layer 31 as an etching mask. At the end of this etching, the layer 31 is removed.

[0067] A disadvantage of the method described above is that, in the step described in relation to [Fig. 6], the etching by ion bombardment of the layers 15 and 25 leads to the formation of polymer fibers or filaments on the sides of the layer 15. These filaments are, for example, made of crosslinked carbon including, for example, sputtered silicon. These filaments may in particular extend beyond the upper face of the layer 15. The polymer fibers or filaments cover the side of the layer 15 in a non-homogeneous manner. Thus, the layer 29 deposited in the step described in relation to [Fig. 8] has in particular thickness irregularities which may lead to sealing and integrity defects which are problematic for the subsequent manufacturing steps and for the reliability of the device. Cleaning of the polymer filaments by wet etching may be provided between the step described in relation to [Fig.7] and the step described in relation to [Fig.8].However, this step generates additional costs and does not allow total removal of the polymer fibers without damaging the microlenses 23. .

[0068] Figures 11 to 13 illustrate, schematically and partially, devices obtained at the end of successive steps of an example of a method of manufacturing an image sensor according to one embodiment.

[0069] The initial steps of the method are for example identical or similar to what has been described above in relation to figures 1 to 5 and will not be detailed again below.

[0070] According to one aspect of an embodiment, it is planned to replace the step of etching by ion bombardment (so-called physical and therefore anisotropic etching) of the resin layer 15 described in relation to [Fig. 6], by a step of plasma etching, totally chemical, and therefore isotropic (process sometimes designated by the English terms "dry-stripping" or "dry-ashing"). This chemical etching is based on the use of free radicals generated by remote plasmas. Such etching puts using equipment different from that used for the physical etching step described in relation to [Fig.6]. This etching technique is usually used to remove, recycle or strip, full plate, resin layers. This technique is also sometimes used to carry out, full plate, chemical treatments on the exposed materials. It is proposed here to use it, in an unusual way, to carry out a localized etching of the resin layer 15 through the mask formed by the resin layer 25. This technique has the advantage of being less aggressive than physical etching, and does not generate polymer fibers or filaments on the sides of the layer 15.

[0071] [Fig. 11] illustrates a device obtained at the end of the chemical plasma etching step of the resin layer 15 through the mask formed by the resin layer 25.

[0072] The chemical plasma etching implemented so as to obtain the device illustrated in [Fig. 11] consumes the layers 25 and 15 simultaneously and isotropically. Thus, at the end of the etching step, the layers 15 and 25 have an inclined flank 35 (non-vertical). For example, the inclination of the flank 35 of the layers 25 and 15 can be controlled in particular by controlling the etching time.

[0073] The chemical etching plasma used preferably comprises dioxygen. For example, the chemical etching plasma comprises dioxygen, dinitrogen and dihydrogen. For example, the temperature of the etched material during this step is between 80°C and 250°C, for example of the order of 150°C.

[0074] The aforementioned etching is stopped when the contact recovery pads 13 are revealed and there are no more residues of the layer 15 on their surface. At this stage, a part of the layer 25 remains on the surface of the layer 15 opposite the microlenses 23.

[0075] [Fig. 12] illustrates a device obtained at the end of a step of removing the remaining part of the layer 25 so as to release the upper face of the microlenses 23. This removal step is for example carried out by wet etching, using a solvent-type solution making it possible to selectively remove the material of the layer 25 relative to the material of the layer 15.

[0076] The steps illustrated in figures 11 and 12 are, for example, followed by steps of depositing a protective layer 29, then opening the protective layer 29 opposite the pads 13, identical or similar to what has been described above in relation to figures 8 to 10.

[0077] [Fig. 13] illustrates the device obtained at the end of these steps.

[0078] An advantage of this embodiment is that the chemical plasma etching described in relation to [Fig. 11] does not generate polymer fibers unlike the physical etching of the step of [Fig. 6]. The layer 29 is therefore deposited in a conforms to the surface of layer 15 which allows it to fulfill its role of protecting layer 15. It is also possible to do without a specific step of cleaning the polymer fibers before depositing layer 29.

[0079] Another advantage of this embodiment is that the chemical etching step is very selective and makes it possible not to consume the material of the substrate 11.

[0080] Another advantage of this embodiment is that the step of chemical etching of the layer 15 results in the formation of a slope in this same layer 15 opposite the pads 13, this slope being adjustable in order to increase the conformity and the resistance of the encapsulation layer 29 which covers it.

[0081] Various embodiments and variations have been described. Those skilled in the art will understand that certain features of these various embodiments and variations could be combined, and other variations will occur to those skilled in the art. In particular, the described embodiments are not limited to the examples of dimensions and materials mentioned above.

[0082] Finally, the practical implementation of the embodiments and variants described is within the reach of those skilled in the art from the functional indications given above.

Claims

Claims

1. A method of manufacturing an image sensor comprising: a) forming a plurality of microlenses (23) of a first resin, in a layer (15) of said first resin; b) after step a), forming a mask (25) of a second resin, on and in contact with said layer (15); and c) after step b), chemical plasma etching of said layer (15), through the mask (25).

2. A method according to claim 1, wherein said layer (15) covers one face of a semiconductor substrate (11) in which a plurality of photodetectors (12) have been previously formed.

3. Method according to claim 2, wherein said layer (15) further covers a contact recovery pad (13) previously formed on the substrate (11).

4. Method according to claim 3, in which during step c), the contact recovery pad (13) is exposed.

5. A method according to any one of claims 1 to 4, wherein, in step a), the formation of the microlenses (23) comprises a step d) of forming microlens-shaped structures (21) in a layer (19) of a third resin, followed by a step e) of transferring said structures (21) into the layer (15) of the first resin by physical etching.

6. A method according to claim 5, wherein, in step d), the structures (21) are formed by photolithography and finishing.

7. Method according to any one of claims 1 to 6, comprising, after step c), a step of depositing a protective and insulating layer (29) on the surface and on the sides of the layer (15) made of the first resin.

8. A method according to any one of claims 1 to 7, wherein, after step c), the mask (25) is removed using a solvent.

9. A method according to any one of claims 1 to 8, wherein the layer (15) of the first resin is crosslinked.

10. A method according to any one of claims 1 to 9, wherein the layer (15) of the first resin is non-photosensitive.

11. A method according to any one of claims 1 to 10, wherein the plasma comprises dioxygen.