Metal pressure brazing with a core having a high coefficient of thermal expansion

The brazing process with a thermally expanding core addresses the challenges of assembling parts with high thermal expansion, providing reliable, cost-effective assembly and precise geometry maintenance, especially for sandwich structures, by using a high-expansion coefficient core and clamping system.

FR3148537A1Pending Publication Date: 2024-11-15SAFRAN NACELLES
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
FR2023004686
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

Existing brazing processes are expensive, unreliable, and unsuitable for industrial-scale assembly of parts with high thermal expansion coefficients, particularly sandwich structures, requiring costly pre-assembly and pressurized gas, and lack the ability to maintain desired geometry and braze thin external skins on a light internal core.

Method used

A brazing process using a core with a high thermal expansion coefficient that expands during heating to apply mechanical pressure on parts, ensuring reliable assembly and maintaining geometry, combined with a clamping system to secure parts, and a heating process that maintains the core's pressure until the solder melts.

Benefits of technology

Enables efficient, cost-effective assembly of parts with high thermal expansion, particularly sandwich structures, by maintaining desired geometry and allowing reuse of the core, reducing the need for pre-assembly and pressurized gas, and achieving precise geometric tolerances.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Metal pressure brazing with a core having a high coefficient of thermal expansion. Brazing process comprising the following steps: - supply of a first part (2) to be assembled, - application of a brazing layer (5) to a brazing face (6) of the first part to be assembled, - application of a second part (3) onto the brazing layer, - application of a core (1) at a distance from a bearing face (7) of the first part, - heating of the assembly to a temperature above the melting point of the brazing layer, but below that of the parts, - maintaining the heating, thermal expansion of the core and pressing of the core against the bearing face of the first part with a pressure force, - pressing of the bearing face of the first part against the second part under the effect of the pressure force, - cooling of the assembly and contraction of the core, - removal of the core. Figure to be published with the abbreviation: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Metal pressure brazing with a core with a high coefficient of thermal expansion TECHNICAL FIELD OF THE INVENTION

[0001] The technical field of the invention is that of brazing, and more particularly of pressure brazing using a filler metal also referred to as brazing.

[0002] The present invention relates to a new brazing method particularly suitable for assembling parts with a high coefficient of thermal expansion, and in particular sandwich structures. TECHNOLOGICAL BACKGROUND OF THE INVENTION

[0003] When brazing, it is sometimes necessary to apply pressure to the parts to be joined to press them together, preferably while the brazing is in the molten state. This pressure can be applied either by pre-assembly under stress or by the use of a pressurized gas, which is very expensive.

[0004] There is therefore a need for a new brazing process, using a new brazing tool, making it possible to apply pressure to the parts to be assembled and which is reliable, inexpensive and which can be used satisfactorily in the context of the manufacture of parts on an industrial scale.

[0005] Whatever the shape of the parts to be assembled, such a brazing process must allow the pre-assembled parts to be fitted cold, or allow the parts to be pre-assembled directly on the brazing tool, while also allowing the brazed parts to be demolded.

[0006] This brazing process must provide good brazing quality and allow the desired geometry to be maintained for the final part obtained.

[0007] It must also make it possible to braze sandwich structures comprising two thin outer skins onto a light inner core of different heights, in which the material constituting the core is a material having high compressive strength and low density, in particular a material having a honeycomb-type structure. Summary of the invention

[0008] The invention offers a solution to the problems mentioned above, by providing a brazing tool comprising a core designed to expand when the parts to be assembled are heated in order to exert mechanical pressure on the part with which it comes into contact. A clamping system may be necessary to immobilize the parts to be assembled during brazing.

[0009] One aspect of the invention relates to a method of brazing at least two parts to be assembled, said method comprising the following steps: • supply of a first part to be assembled, • placing a layer of solder on a face called the soldering face of the first part to be assembled, • placing a second part to be assembled on the solder layer, the method further comprising the following steps: • placing a core at a distance D from a face called the support face of the first part to be assembled, • heating the core, the parts to be assembled and the solder layer to a temperature T higher than the melting point of the solder layer, but lower than the melting point of the parts to be assembled, • maintaining the heating at temperature T for a duration C of between 1 and 40 minutes, thermal expansion of the core and support of the core on the support face of the first part to be assembled with a pressure F, • pressing the support face of the first part to be assembled against the second part to be assembled under the effect of pressure F, • cooling of the core, the parts to be assembled and the solder layer, and shrinkage of the core, • removal of the core.

[0010] In addition to the characteristics which have just been mentioned in the preceding paragraph, the method according to one aspect of the invention may have one or more complementary characteristics among the following, considered individually or according to all technically possible combinations: • the core has a thermal expansion coefficient a that is at least 4 x 106 °C 1 higher than that of the parts to be assembled having the highest thermal expansion coefficient. • distance D is less than 2 millimeters. • the duration C of heating at temperature T is between 2 and 15 minutes. • the process includes the next step planned before the implementation step of a core: pre-assembly of the parts to be assembled by creating holding points between them. • the method comprises, before the heating step, a step of locking the parts to be assembled in position. • the method comprises, before the heating step, a step of locking the core in position. • the heating step is carried out at a temperature T at least 20°C, preferably at least 60°C, higher than the melting point of the layer of solder. • the heating maintenance step is carried out at a temperature T at least 50°C, preferably at least 70°C, lower than the melting point of the parts to be assembled. • the cooling step is carried out under an inert atmosphere. • the cooling step is carried out at a cooling rate between 1 and 10°C / min. • the pressure F exerted by the core on the parts to be assembled during its expansion is between 0.2 and 0.5 bar. • the heating step is carried out at a pressure less than or equal to 1.13 x 103 mbar.

[0011] It will be noted that by the creation of holding points between parts we mean the creation of electric microwelds or fusion welds.

[0012] The use of a core capable of expanding during heating advantageously makes it possible to exert mechanical pressure on the parts to be assembled at a face thereof which may be difficult to access, in particular in the case of brazing parts of revolution, for example cylindrical, conical or truncated cone-shaped, or in the shape of a barrel or half-barrel.

[0013] The external profile of the core, intended to exert pressure on one of the faces of the parts to be assembled, can be chosen to have - in the expanded state - a shape complementary to that desired for the part with which it comes into contact, which advantageously makes it possible to maintain the desired geometry for the final part obtained and to anticipate with precision the volume occupied by the core when it is in the expanded state so as not to damage the parts to be assembled, in particular in the case of brazing sandwich structures.

[0014] Since the core material is designed not to be irreversibly damaged or deformed during brazing, particularly during heating, said core can advantageously be reused.

[0015] The fact that the core returns to its initial shape after cooling advantageously facilitates the demolding of the brazed parts.

[0016] The brazing method of the invention is all the more efficient if the core has a coefficient of thermal expansion much higher than that of the parts to be assembled, particularly in the case where the parts to be assembled have a high coefficient of thermal expansion.

[0017] The distance D between the core and the nearest part to be assembled advantageously makes it possible to take into account geometric defects in said part, to have sufficient assembly clearance to be able to fit the parts to be assembled onto the core and to have brazing clearance for assembling the parts to be assembled.

[0018] In the case where a counter-pressure part is provided in the immediate vicinity or in contact with the external face of the second part to be assembled, the latter has an internal profile having a shape complementary to that desired for the second part to be assembled with which it comes into contact under pressure during the thermal expansion of the core, which advantageously makes it possible to use the brazing method of the invention to further conform the brazed parts according to a desired profile according to a hot-forming type method. Such hot-forming advantageously makes it possible to dispense with a possible preliminary cold hydroforming operation, which makes it possible to limit the phenomena of elastic return and therefore to obtain more precise geometric tolerances for the final part obtained.

[0019] The invention and its various applications will be better understood by reading the following description and examining the accompanying figures. BRIEF DESCRIPTION OF THE FIGURES

[0020] The figures are presented for information purposes only and in no way limit the invention.

[0021] [Fig.l][Fig.2][Fig.3] are schematic cross-sectional views illustrating the process of the invention applied to the brazing of revolution parts having a flat surface.

[0022] [Fig. Ibis] is an enlargement of the circled portion in [Fig. 1].

[0023] [Fig.4][Fig.5][Fig.6] are schematic cross-sectional views illustrating the method of the invention applied to the brazing of half-cylinder shaped parts.

[0024] [Fig.4bis] is an enlargement of the circled part in [Fig.4].

[0025] [Fig.7][Fig.8][Fig.9] are schematic views in longitudinal section illustrating the method of the invention applied to the brazing of hollow truncated cone-shaped parts having a sandwich structure.

[0026] [Fig.7bis] is an enlargement of the circled part in [Fig.7]. DETAILED DESCRIPTION

[0027] Unless otherwise specified, the same element appearing in different figures has a single reference.

[0028] The principle of the invention is based on the use of a brazing tool comprising a core 1 which expands during the heating step in a brazing process, this core 1 then applying mechanical pressure to the parts to be assembled 2, 3, 4 during its increase in volume.

[0029] Conventionally, this method firstly comprises a pre-assembly operation consisting of placing, layer by layer, the parts to be assembled 2, 3, 4 with a layer of solder 5 between them, the nature of which is chosen in the usual way according to the constituent materials of the parts to be assembled 2, 3, 4. The face of a part to be assembled on which a layer of solder 5 is deposited is designated as brazing face 6. For N parts to be assembled 2, 3, 4 by brazing, we thus count Nl brazing faces 6.

[0030] For large surfaces to be brazed, the brazing layer 5 is preferably in the form of a strip or tape, while for smaller surfaces, the brazing layer 5 is preferably in the form of a paste, powder, wire, rods or ring.

[0031] During this pre-assembly operation, the parts to be assembled 2, 3, 4 are held together during their handling. This holding is preferably done by making small welding or fusion points between the parts to be assembled 2, 3, 4.

[0032] The pre-assembly operation can be carried out directly on the tooling. Otherwise, after the pre-assembly operation, the parts to be assembled 2, 3, 4 are moved to the brazing tooling.

[0033] Depending on their conformation, the parts to be assembled 2, 3, 4 are then positioned on the core 1 or the core 1 is introduced inside the parts to be assembled 2, 3, 4 (see [Fig.1], [Fig.4] and [Fig.7]).

[0034] The core 1 is then positioned at a distance D from a face called the support face 7 of the part to be assembled 2 closest to the core 1, which is usually the part to be assembled constituting the first layer and / or the lower layer of the parts to be assembled 2, 3, 4. The support face 7 of the part to be assembled 2 is the face of this part which is closest to the core 1 when the latter is put in place. The distance D is preferably less than 2 millimeters, which makes it possible to take into account the geometry defects of the parts to be assembled 2, 3, 4 (usually from 0.5 to 1.3 mm), to have sufficient assembly clearance to be able to fit the parts to be assembled onto the core (approximately 0.5 mm at the radius for parts of revolution) and to have a brazing clearance for the assembly of the parts to be assembled (approximately 0.2 mm for a sheet / honeycomb type assembly and approximately 0.1 mm for a sheet / sheet type assembly).

[0035] Once the core 1 is correctly positioned relative to the parts to be assembled 2, 3, 4, the brazing tool and the parts to be assembled 2, 3, 4 are mutually immobilized by an immobilization device (not shown). This immobilization device preferably comprises keying clamping means, but any other immobilization device can be used.

[0036] The assembly formed by the core 1, the parts to be assembled 2, 3, 4 and the brazing layer(s) 5 is then heated to a temperature T higher than the melting point of the brazing layers 5, but lower than the melting point of the parts to be assembled 2, 3, 4. This heating is preferably carried out in a temperature range between 1000°C and 1200°C, for example for brazing parts based on steel or nickel, but it can also be carried out in a temperature range between 800 °C and 1000 °C, for example for brazing titanium-based parts. The heating is also preferably carried out at a temperature T at least 20 °C higher, preferably at least 60 °C, than the melting point of the brazing layer 5, and carried out at a temperature T at least 50 °C lower, preferably at least 70 °C lower, than the melting point of the parts to be assembled 2, 3, 4. Using the lowest possible brazing temperature T increases the service life of the core 1 and consumes less energy.

[0037] Heating can be achieved by placing the core 1 and the parts to be assembled 2, 3, 4 in an oven, or by heating the core 1 by induction

[0038] The heating is maintained for a duration C, allowing the core 1 to expand under the effect of the heat and to exert pressure on the parts to be assembled 2, 3, 4. The heating duration C is between 1 and 40 minutes, preferably between 2 and 15 minutes.

[0039] During the expansion of the core 1, its external surface 8 is pressed against the bearing face 7 of the first part to be assembled 2 with a pressure F, and exerts a mechanical pressure on it, in order to deform it orthogonally with respect to the external surface 8 of the core 1 (see [Fig.2], [Fig.5] and [Fig.8]). The pressure F exerted by the core 1 on the parts to be assembled 2, 3, 4 during its expansion is for example between 0.2 and 0.5 bar.

[0040] Thus, in the case where the core 1 is housed in a hollow part to be assembled 2, by expanding the core 1 exerts a mechanical pressure on the internal face of said part to be assembled 2, aiming to deform it outwards. The core 1 therefore exerts a docking pressure on the nearest part to be assembled 2. This pressure must be at least 0.2 bars to ensure sufficient plastic deformation of said part to be assembled 2 and ensure good brazing of the parts to be assembled 2, 3, 4, but must preferably not exceed the buckling resistance of the parts to be assembled 2, 3, 4, and be much lower than the mechanical resistance of the core 1 when hot. For example, a titanium honeycomb structure buckles from 0.5 bars of pressure at 980°C.

[0041] In order to expand in the same way over the entire bearing face 7 of the first part to be assembled, the core 1 is preferably in the form of a mattress of constant thickness. Indeed, a constant thickness of the mattress allows in particular thermal homogeneity in the core 1, which increases the service life of the core 1 by limiting its internal deformations of the tooling. It is preferably between 30 and 40 mm. This thickness must be sufficient to guarantee good resistance over time but not too great to limit the thermal inertia of the mattress and therefore limit the duration of the brazing cycle and energy consumption. The surface condition of the core 1 must preferably have a maximum arithmetic mean roughness Ra of 1.6 and form tolerances of the order of 0.2 mm. When designing core 1, a thermal simulation can be carried out to identify stress concentrations and remove them.

[0042] Although not shown in the drawings, the parts to be assembled 2, 3, 4 are also likely to expand during the heating step. Consequently, in order to ensure that the core 1 can exert sufficient pressure on the parts to be assembled 2, 3, 4, it preferably has a thermal expansion coefficient a that is at least 4 x 106 °C 1 higher than that of the parts to be assembled 2, 3, 4. In this respect, it will be noted that the more sinuous the profile of the parts to be assembled 2, 3, 4 and the smaller their diameter, and consequently the greater the delta in thermal expansion coefficient a between the core 1 and the parts to be assembled 2, 3, 4 must be.

[0043] The core 1 is preferably made of a material having a coefficient of thermal expansion a of at least 22.4 x 106 °C 1 in a temperature range between 1000 °C and 1200 °C, this plate corresponding to a preferred temperature range for the process. The ASTM E228 or ISO 11359-2 standards can for example be used to measure the coefficient of thermal expansion a of the tooling.

[0044] In order not to be irreversibly deformed during heating, the core 1 is preferably made of a material such that it is not deformed by fining. The NF A 03-355 standard can for example be used to measure the fining of the tool.

[0045] During heating, the core 1 expands and the parts to be assembled 2, 3, 4 are pressed against each other, while the molten material of the solder layer 5 is distributed substantially uniformly between them.

[0046] After this heating, the assembly still needs to be cooled. This cooling is carried out, for example, at a cooling rate of between 1 and 10°C / min. It is preferably carried out at a cooling rate of approximately 2°C / min and then, once the brazing has solidified, at a faster cooling rate, for example approximately 7°C / min. The cooling rate can, for example, be controlled by regulating the temperature drop of the heating means and / or by cooling the core 1 and the parts to be assembled 2, 3, 4 using a cold source.

[0047] During cooling, the core 1 returns to its initial dimensions and the material of the brazing layer 5 solidifies to assemble the parts to be assembled 2, 3, 4 (see [Fig.3], [Fig.6] and [Fig.9]). The core 1 can then be removed from the final part obtained. In order to be able to carry out this cooling quickly, the core 1 is preferably made of a material which is not damaged when it is cooled to a cooling rate greater than or equal to 75°C per minute. Cooling is preferably carried out under an inert atmosphere, for example under an atmosphere of argon, nitrogen or hydrogen.

[0048] Brazing is preferably carried out under vacuum, for example at a minimum secondary vacuum level of 1.13 x 103 mbar, in a humidity-free environment, with parts to be assembled 2, 3, 4 clean and degreased or pickled.

[0049] The parts to be assembled 2, 3, 4 can have many shapes, some of which are illustrated by way of example in the figures. They can be conical, cylindrical, of revolution or not, with or without an apex (top of a cone) or a combination of concave / convex shapes.

[0050] During the expansion of the core 1, depending on their shape, the parts to be assembled 2, 3, 4 may have a tendency to want to move relative to each other and / or relative to the core 1. Similarly, the core 1 may also have a tendency to want to move relative to the parts to be assembled 2, 3, 4. This occurs in particular when the parts to be assembled 2, 3, 4 are conical, truncated or half-barrel shaped.

[0051] In this case, it is necessary to lock the parts to be assembled 2, 3, 4 and / or the core 1 in position before the heating step in order to keep them in place during their respective expansion. This locking can for example be achieved by means of a clamping system 9 which immobilizes the parts to be assembled 2, 3, 4 and / or the core 1, or by means of a system of shims 10 which prevents their movement. The locking means used depend on the shape of the parts to be assembled 2, 3, 4 and the core 1. As there are very many possible shapes, it is therefore necessary to use clamping systems 9 and shims 10 adapted to each situation, but without this presenting any real difficulty for the person skilled in the art.

[0052] If the parts to be assembled 2, 3, 4 and the core 1 do not have a shape likely to cause their displacement during the expansion of the core 1, by expanding in all directions, the expansion of the core 1 can generate an automatic centering of the parts to be assembled 2, 3, 4 with the core 1. In this case, it is not necessary to lock or hold the parts to be assembled 2, 3, 4 and / or the core 1. This is particularly the case when the parts to be assembled 2, 3, 4 and the core 1 are of substantially cylindrical or barrel-shaped shape, with the core 1 housed substantially in the center of the parts to be assembled 2, 3, 4.

[0053] The core 1 is preferably a single piece, but it can also be in several parts, for example in order to facilitate the demolding of the brazed parts, in particular if the parts to be assembled 2, 3, 4 have an apex or an undercut shape. For example, a core 1 comprising movable and / or removable keys can be used in order to braze parts having a strong undercut.

Claims

Claims

1. Method for brazing at least two parts (2, 3, 4) to be assembled, said method comprising the following steps: - providing a first part (2) to be assembled, - placing a brazing layer (5) on a face called the brazing face (6) of the first part (2) to be assembled, - placing a second part (3) to be assembled on the brazing layer (5), - the method being characterized in that it further comprises the following steps: - placing a core (1) at a distance D from a face called the bearing face (7) of the first part (2) to be assembled, said core (1) having a thermal expansion coefficient (a) greater than that of the parts (2, 3, 4) to be assembled, - heating the core (1), the parts to be assembled (2, 3, 4) and the brazing layer (5) to a first temperature (T) greater than the melting point of the brazing layer (5), but lower than the melting point of the parts to be assembled (2, 3, 4),- maintaining the heating at a second temperature (T) for a duration (C) of between 1 and 40 minutes, thermal expansion of the core (1) and pressing the core (1) on the bearing face (7) of the first part (2) to be assembled with a pressure (F), - pressing the bearing face (7) of the first part (2) to be assembled against the second part (3) to be assembled under the effect of the pressure F, - cooling the core (1), the parts to be assembled (2, 3, 4) and the brazing layer (5), and shrinking the core (1), - removing the core (1).,

2. Method according to claim 1, characterized in that the core (1) has a thermal expansion coefficient (a) at least 4 x 106 °C 1 higher than that of the parts (2, 3, 4) to be assembled having the highest thermal expansion coefficient.

3. Method according to claim 1 or 2, characterized in that the distance (D) is less than 2 millimeters.

4. Method according to any one of the preceding claims, characterized in that the duration (C) of heating to the temperature (T) is between 2 and 15 minutes.

5. Method according to any one of the preceding claims, characterized in that it comprises, before the heating step, a step of locking in position the parts to be assembled (2, 3, 4).

6. Method according to any one of the preceding claims, characterized in that it comprises, before the heating step, a step of locking the core (1) in position.

7. A method according to any one of the preceding claims, characterized in that the cooling step is carried out at a cooling rate of between 1 and 10°C / min.

8. Method according to any one of the preceding claims, characterized in that the pressure (F) exerted by the core (1) on the parts to be assembled (2, 3, 4) during its expansion is between 0.2 and 0.5 bar.

9. Method according to any one of the preceding claims, characterized in that the heating step is carried out at a temperature (T) at least 20°C, preferably at least 60°C, higher than the melting point of the solder layer (5).

10. Method according to any one of the preceding claims, characterized in that the heating maintenance step is carried out at a temperature (T) at least 50°C, preferably at least 70°C, lower than the melting point of the parts to be assembled (2, 3, 4).

Citation Information

Patent Citations

  • Double-sleeve internal pressure applying brazing method and double-sleeve welding assembly

    CN112756723A

  • Bonded composite constructing inside of metal and outside of ceramic and production thereof

    JP1992321571A

  • Tooling adapted for brazing a set of parts

    US20170274466A1

  • Method of making a ribbed panel

    US3747197A