An avalanche photodiode device

GB2629561APending Publication Date: 2024-11-06PHLUX TECH LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
GB2023005699
Authority / Receiving Office
GB · GB
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-11-06

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

An avalanche photodiode (APD) sub-assembly comprises: a substrate 401; a first contact layer 403 formed on the substrate; a second contact layer 402; and an avalanche layer 406 comprising antimony disposed between the first contact layer and the second contact layer. The first contact layer is an n-type contact layer. The second contact layer comprises a p-type contact region 450 formed by diffusing zinc. The p-type contact region has a smaller cross-sectional area than the avalanche layer, the cross-sectional area being perpendicular to a direction from the substrate to the second contact layer. The avalanche layer may comprise AlGaAsAb, InAlAsSb or AlAsSb. Between the avalanche layer and the second contact layer there may be an absorption layer 417. Between the absorption layer and the second contact layer there may be at least one stopper layer 460, which has a lower diffusivity of zinc than the second contact layer. An APD device and a method of manufacturing the APD sub-assembly are also disclosed.
Need to check novelty before this filing date? Find Prior Art

Claims

1. An avalanche photodiode (APD) sub-assembly comprising:a substrate;a first contact layer formed on the substrate;a second contact layer; andan avalanche layer comprising antimony, the avalanche layer being disposed between the first contact layer and the second contact layer;wherein the first contact layer is an n-type contact layer;wherein the second contact layer comprises a p-type contact region formed by diffusing zinc;wherein the p-type contact region has a smaller cross-sectional area than the avalanche layer, the cross-sectional area being perpendicular to a direction from the substrate to the second contact layer.

2. An APD sub-assembly according to claim 1, wherein the avalanche layer comprises AIGaAsSb, InAIAsSb or AlAsSb.

3. An APD sub-assembly according to any one of the preceding claims, wherein the distance between a sidewall of the avalanche layer and an edge of the p-type contact region in the direction perpendicular to a direction from the substrate to the second contact layer is at least 7.5 pm.

4. An APD sub-assembly according to any one of the preceding claims, wherein the avalanche layer has a thickness of from 100 nm to 1500 nm or from 300 nm to 1000 nm.

5. An APD sub-assembly according to any one of the preceding claims, comprising a first cladding layer having a thickness of at least 1 pm disposed between the avalanche layer and the second contact layer, wherein the second contact layer is formed in the cladding layer.

6. An APD sub-assembly according to claim 5, wherein the first cladding layer comprises a zinc diffusion area, the zinc diffusion area having a smaller cross-sectional area than the avalanche layer, the cross-sectional area being perpendicular to a direction from the substrate to the second contact layer.

7. An APD sub-assembly according to claim 6, wherein the distance between a sidewall of the avalanche layer and an edge of the zinc diffusion area in the first cladding layer in a direction perpendicular to a direction from the substrate to the second contact layer is at least 7.5 pm.

8. An APD sub-assembly according to claim 6 or 7, wherein zinc diffusion area comprises a localized region of the first cladding layer.

9. An APD sub-assembly according to any one of the preceding claims, comprising an absorption layer disclosed between the avalanche layer and the second contact layer.

10. An APD sub-assembly according to claim 9, wherein the absorption layer comprises InGaAs, GaAsSb, InGaAIAs, InGaAsP, or an InGaAs / GaAsSb type-ll superlattice.

11. An APD sub-assembly according to claim 9 or 10, comprising at least one stopper layer disposed between the absorption layer and second contact layer, wherein the at least one stopper layer has a lower diffusivity of zinc than the second contact layer.

12. An APD sub-assembly according to claim 11, wherein the at least one stopper layer comprises InGaAs or InGaAIAs and / or wherein the at least one stopper layer is intrinsic.

13. An APD sub-assembly according to any one of claims 9 to 12, comprising a transition portion disposed between the avalanche layer and the absorption layer; wherein the transition portion comprises a first grading layer of InAIGaAs or InGaAsP, and a charge sheet disposed between the first grading layer and the avalanche layer; wherein the charge sheet has a bandgap between the bandgap of the absorption layer and the bandgap of the avalanche layer.

14. An APD sub-assembly according to claim 13, wherein the charge sheet is p-doped and / or wherein the charge sheet comprises InAIAs or InP15. An APD sub-assembly according to claim 13 or 14, comprising a second grading layer of InAIGaAs or InGaAsP disposed between the charge sheet and the avalanche layer.

16. An APD sub-assembly according to any one of the preceding claims, wherein the APD subassembly is a quasi-planar sub-assembly.

17. An APD sub-assembly according to any one of the preceding claims, wherein the p-type contact region comprises a localized region of the second contact layer.

18. An APD sub-assembly according to any one of the preceding claims, wherein the second contact layer comprises an outer first portion and an inner second portion, wherein the first portion is separated from the second portion and the second portion comprises the p-type contact region.

19. An APD device comprising the APD sub-assembly according to any one of the preceding claims and, optionally, wherein the APD device comprises an electrode formed on each of the p-type contact layer and the n-type contact layer.

20. A method of manufacturing an APD sub-assembly, the method comprising: providing a substrate;forming a first contact layer on the substrate, wherein the first contact layer is an n-type contact layer;layering a plurality of layers on the first contact layer, the plurality of layers comprising an avalanche layer comprising antimony and a second contact layer, such that the avalanche layer is disposed between the first and second contact layers; andcreating a p-type contact region in the second contact layer by diffusing zinc into the second contact layer; wherein the p-type contact region has a smaller cross-sectional area than the avalanche layer, the cross-sectional area being perpendicular to a direction from the substrate to the second contact layer.

21. A method according to claim 20, wherein creating the p-type contact region comprises a single zinc diffusion.

22. A method according to claim 20 or 21, comprising, prior to creating the p-type contact region, etching the second contact layer to separate the second contact layer into an outer first portion and an inner second portion; andapplying a mask over the first portion of the second contact layer to inhibit zinc diffusion into the first portion.

23. A method according to claim 22, wherein creating the p-type contact region comprises etching the second portion of the second contact layer to provide the p-type contact region after the zinc diffusion.

24. A method according to any one of claims 20 to 23, comprising etching the plurality of layers such that a distance between a sidewall of the avalanche layer and an edge of the p-type contact region in a direction perpendicular to a direction from the substrate to the second contact layer is at least 7.5 pm.

25. A method according to any one of claims 20 to 24, wherein the plurality of layers comprises a first cladding layer disposed between the avalanche layer and the second contact layer; andwherein creating the p-type contact region creates a zinc diffusion area in the first cladding layer.

26. A method according to claim 15, when dependent on claim 24, wherein etching the plurality of layers is such that a distance between the sidewall of the avalanche layer and an edge of the zinc diffusion area in the first cladding layer in the direction perpendicular to a direction from the substrate to the second contact layer is at least 7.5 pm.

Citation Information

Patent Citations

  • Avalanche photodiode structure and method