A composition of sustainable one-part alkali-activated mortar and brick masonry and method of preparation thereof
Patent Information
- Application Number
- IN202421017986
- Authority / Receiving Office
- IN · IN
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-03-13
- Publication Date
- 2026-10-26
- Estimated Expiration
- 2044-03-13
AI Technical Summary
Current construction materials, such as cement and clay bricks, have environmental and economic drawbacks due to their reliance on non-renewable resources and generation of industrial waste, necessitating the development of sustainable alternatives with enhanced physical and mechanical properties.
A composition and method for sustainable one-part alkali-activated mortar and brick masonry using industrial rejects like fly ash, ground granulated blast furnace slag, and waste foundry sand, activated with sodium metasilicate, which are optimized through mix design and performance evaluations to improve strength, durability, and reduce waste.
The resulting materials demonstrate superior compressive strength, density, and durability, suitable for non-load-bearing structures, while reducing environmental impact and offering economic benefits by utilizing locally available industrial waste, thus promoting sustainable construction practices.
Smart Images

Figure 00000013_0000
Abstract
Description
TECHNICAL FIELD OF INVENTIONThe present invention is related to the field of civil engineering. More specifically, it relates to a composition of sustainable one-part alkali-activated mortar and brick masonry.BACKGROUND OF THE INVENTIONThe background information herein below relates to the present disclosure but is not necessarily prior art.US20100320641A1 related to a process for obtaining basic construction elements formed by cement and residual material for building basic artifacts for civil construction, involving, cement aggregated to mineral residues, the process includes the following steps: accumulation of raw material: formed by cement material found in nature or derived from mining and industrial processes and in this case, there is no single field; homogenization or mixture: is performed manually or by machinery, such as front-end loaders, according to percentage of each raw material used, obtaining an unique and homogenous plaster; disintegration of raw material such as cement, lamination, homogenization, involving specific machinery with a new purge of residual rejects and finally, a temporary bulk storage.US9802865B1 discloses a nano-modified dry-mixed alkali-activated cementitious, or one-part geopolymer cement (OPgC), material with high early strength is provided for rapid repair of cement-based infrastructure components. The OPgC may include an aluminosilicate rich material, an alkali material and a nano modifier, and optionally include other functional admixtures and fibers. The OPgC can be freshly mixed with water to obtain a repairing material. The OPgC may mix with water and fine or coarse aggregate to form mortar or concrete. The OPgC can be an alternative binding matrix for the development of an environmentally friendly and cost-effective rapid repair material.CN105461265B describe a kind of modified alkali-activated carbonatite binder materials and preparation method thereof, It is an object of the invention to provide a kind of modified alkali-activated carbonatite binder materials and preparation method thereof, wherein, according to the mass fraction, the raw material of the binder materials is included Fly ash and 2~parts of 100 parts of slag compound, 25~50 parts of alkali-activator, 0.5~2 part of retarder and polymer glue powder The solid content of wherein described alkali-activator is 30~40%;The method that the present invention is modified using polymer glue powder to alkali activated carbonatite binder materials, compared with the method being modified using polymer emulsion to alkali-activated carbonatite fly-ash mine residue material, there is the present invention simple production process, metering to prepare the features such as accurate, storage transportation safety, construction usage are convenient, product condenses fast, adhesion strength height, good acid-fast alkali proof, excellent in the pins of durability. There are various drawbacks to prior art and existing technology. Hence, there was a long-felt need in the art.OBJECTIVE OF THE INVENTIONThe primary objective of the present invention is to provide a composition and method of preparation of sustainable one-part alkali-activated mortar and brick masonry.Yet another objective of the invention is to develop sustainable building materials by utilizing industrial rejects such as fly ash, ground granulated blast furnace slag (GGBS), and waste foundry sand (WFS).Yet another objective of the invention is to enhance the physical and mechanical properties of the materials.Yet another objective of the invention is to create environmentally friendly alternatives to traditional construction materials.SUMMARY OF THE INVENTIONAccordingly, the following invention provides a composition and method of preparation of sustainable one-part alkali-activated mortar and brick masonry. The invention focuses on the development of sustainable building materials through the utilization of industrial rejects, including fly ash, ground granulated blast furnace slag (GGBS), and waste foundry sand (WFS). By repurposing these materials, the invention aims to create environmentally friendly alternatives to traditional construction materials like cement mortar and clay bricks. Through a systematic approach involving raw material collection, feasibility assessment, mix design trials, and performance evaluations, the invention strives to enhance the physical and mechanical properties of the developed materials. This includes achieving superior compressive strength, density, and durability, making them suitable for use in non load-bearing structures. Additionally, the invention seeks to promote sustainability in the construction industry by providing builders and construction professionals with viable alternatives that contribute to reducing environmental impact while maintaining structural integrity and performance standards.By optimizing mix designs and conducting comprehensive performance evaluations, the invention demonstrates the feasibility and effectiveness of utilizing industrial rejects for sustainable construction. The resulting one-part alkali-activated mortar (OPAM) and brick masonry (OPAB) exhibit promising properties, surpassing those of conventional materials in terms of strength and durability. Furthermore, the utilizing locally available industrial waste as precursors offers economic and environmental benefits by reducing waste generation and reliance on conventional raw materials. Overall, the invention presents a viable solution for enhancing sustainability in construction practices, offering builders and construction professionals the opportunity to contribute to environmental conservation efforts while meeting the demands for durable and high-performance building materials.BRIEF DESCRIPTION OF DRAWINGThis invention is described by way of example with reference to the following drawings where,Figure 1 of sheet 1 illustrated the flowchart of proposed invention. Where,101 denotes the collection of raw materials,102 denotes checking the feasibility of the material.103 denotes the mix design trail for OPAM.104 denotes the performance evaluation of OPAM,105 denotes the end product from the optimum mix.106 denotes the performance evaluation of OPAB.Figure 2 of sheet 1 shows the particle size distribution curve of the WFS.Figure 3 of sheet 2 shows the SEM observation on OPAM at magnifications of 1k, 10k, 50k and 100k.Figure 4 of sheet 2 shows the EDS point analysis.DETAILED DESCRIPTION OF THE INVENTIONAs used in the description herein and throughout the claims that follow, the meaning of "a," "an," and "the" includes plural reference unless the context clearly dictates otherwise. Also, as used in the description herein, the meaning of "in" includes "in" and "on" unless the context clearly dictates otherwise.The present invention is related to a composition and method of preparation of sustainable one-part alkali-activated mortar and brick masonry. This invention focuses on developing one-part alkali-activated materials to improve traditional two-part systems. The aim is to create sustainable binders that can be used to make paste, mortar, and concrete. In particular, the study looks at the design and development of one-part alkali-activated mortar (OPAM) and brick masonry (OPAB) using locally available industrial waste, such as fly ash (FA) and ground granulated blast furnace slag (GGBS), as a precursor. The activator used is sodium metasilicate, while waste foundry sand (WFS) is used as a partial replacement of fine aggregate obtained from Truform Techno Products Ltd. GGBS and FA are used as sources of alumina and silica obtained from industries in nearby Nagpur, India areas. WFS was chosen because of its high silica content. The physical and chemical characteristics of the source material were determined to clarify the material's suitability for use in the development of the building product. Physical parameters such as sieve analysis, specific gravity, bulk density, water absorption, and chemical analysis such as X-ray fluorescence were determined. Basic characteristics of the produced samples, including consistency, density, and compressive strength, were evaluated. The investigation results show that OPAM and OPAB test samples demonstrate better physic-mechanical properties compared to fly ash bricks, clay bricks, and commonly used cement mortar. It is advised to use the created samples for non-load-bearing structures.Figure 1 shows (101) Fly Ash, GGBS, Sodium metasilicate, River Sand, Waste Foundry Sand. (102) Particle size distribution, Specific Gravity, Bulk Density, Water Absorption, X-ray fluorescence. (103) Fly Ash and GGBS in different %, Sodium metasilicate- 10, and % of binder, Water to binder ratio - 0.40, Binder to Fine aggregate ratio - 1:2, Substitute River sand with WFS. (104) Standard consistency, initial setting and final setting time of binder, Workability of OPAM, Density, Compressive strength test. (105) Dimension of Brick (mm) 2*100 *80, (106) Density of OPAB, Compressive strength test, Water Absorption Test, Efflorescence.The physical properties and chemical composition of the raw materials utilized in this innovation are shown in Tables 1 and 2, respectively. The particle size distribution curve of the WFS is shown in Figure 2.Table 1: Physical properties of materialsTable 2: Chemical composition of materialsOne Part Alkali Activated Mortar (OPAM):The process of determining the optimal mix design can involve multiple trials. In this case, the process involved two specific trials: Trial A and Trial B. Trial A was carried out to establish a control mix design, which would serve as a reference point for subsequent testing. Once the control mix design had been established, Trial B was performed to refine the mix and determine the optimum mix design. For trial A, the samples were named Mix 1 to Mix and all contained GGBS and FA in varying weight percentages. Based on the total weight of the binder, the activator percentage was added to the mortar samples in the range of to weight percent. The water-to-binder ratio was fixed at 0.40 for all mixes, while the binder-to sand ratio was kept uniform at 1 to 2. Table 3 provides more details on the contents of one-part alkali-activated mortars.Table 2: Trial A for Control Mix DesignThe experiment involved the preparation of test samples using raw materials such as FA, GGBS, sodium metasilicate, and river sand. These materials were first weighed and dry-mixed for 3 minutes. Then, the dry mix was blended with a specific amount of water and poured into moulds. The mixture was leveled, compacted, and left to rest for about 24 hours at room temperature. The standard consistency and initial and final setting time of the binder were determined using the Vicat apparatus (IS 4031, IS 269). The Flow Table Test (IS: 5512-1983) was used to assess the workability of the OPAM. To determine the mechanical strength and characteristics, the density and compressive strength of the hardened mortar were measured after 7 and 28 days. The test results indicated that the OPAM had a quick setting time, with initial and final setting times of 40 to 50 minutes and 250 to 350 minutes, respectively. The results obtained from trial A are detailed in Table 4.Table 4: Test Results of Trial A for Control Mix DesignDuring the initial phase, sample Mix showed the highest compressive strength of 17.70 N / mm2, followed by samples Mix 14 and Mix 13 with 10.55 N / mm2 and 6.80 N / mm2 respectively. However, after 28 days, there were slight differences in compressive strength. Mortar gains 90-95% strength in 7 days due to immediate geopolymerization when water is applied. Trial B was conducted after selecting Mix as the control mix design for OPAM. In this trial, river sand was replaced by WFS at intervals of 25%, 50%, 75%, and 100%. The proportion of the Trial B mix design is given in Table 5. These mixtures underwent the same tests as those in Trial A. The workability, density, and compressive strength of each mix design are shown in Table 6.According to the compressive strength results shown in Table 6, up to 50% of the fine aggregate in OPAM can be replaced with waste foundry sand.Table 5: Trial B for Optimum Mix DesignTable 6: Test Results of Trial B for Optimum Mix DesignMicrostructural characterization:For the microstructural characterization, a Field Emission Scanning Electron Microscope fitted with an Oxford energy dispersive spectroscopy system was used. The samples were viewed at magnifications of 1k, 10k, 50k and 100k. An accelerating voltage of 3 to 5 keV and a probe current of 50 pA were used for the elemental analysis. SEM observation equipped with EDS point analysis and the corresponding result are shown in Fig. 3 and 4.One Part Alkali Activated Brick (OPAB):The brick test samples were cast, cured, and evaluated for density and compressive strength at 28 days of age, using Optimum Mix design M17 and following the guidelines of IS 3495: 1992. The design matrix for the experimental work is presented in Table 7, while the results of the density, compressive strength, water absorption, and efflorescence of the developed brick test samples at 28 days of age can be found in Table 8.Table 7: Design matrix for OPAB per cubic meterTable 8: Test result of OPABAccording to IS 3495-Part 1-1992, the first-class brick should have a minimum compressive strength of MPa after 28 days. The M17 mix design showed a compressive strength of more than MPa after 28 days of age, making the trial M17 the optimal mix. The end product was designed to have a density of around 2000-2100 kg / m3 while using locally available industrial waste as a substitute for conventional raw materials like cement and fine aggregate. No water was necessary for the curing process. Early strength gain was achieved in 7 days. Thus, making the designed masonry product a sustainable solution.Best method of performing the invention: In the preferred embodiment of the present invention, a method for preparation of composition of sustainable one-part alkali-activated mortar and brick masonry, comprising of; Mixing 560 kg / m3 of ground granulated blast furnace slag and 140 kg / m3 of sodium metasilicate, 700 kg / m3 of river sand;Followed by addition of 700 kg / m3 of waste foundry sand; and Adding with continuous mixing, 40 kg / m3 of water in the mixture obtained through step (b).While various embodiments of the present disclosure have been illustrated and described herein, it will be clear that the disclosure is not limited to these embodiments only. Numerous modifications, changes, variations, substitutions, and equivalents will be apparent to those skilled in the art, without departing from the spirit and scope of the disclosure, as described in the claims.
Claims
1. A composition of sustainable one-part alkali-activated mortar and brick masonry, consisting of; 560 kg / m3 of ground granulated blast furnace slag; 140 kg / m3 of sodium metasilicate; 700 kg / m3 of river sand; 700 kg / m3 of waste foundry sand; and 40 kg / m3 of water.
2. A method for preparation of composition of sustainable one-part alkali activated mortar and brick masonry, comprising of; a) Mixing 560 kg / m3 of ground granulated blast furnace slag and 140 kg / m3 of sodium metasilicate, 700 kg / m3 of river sand; b) Followed by addition of 700 kg / m3 of waste foundry sand; and c) Adding with continuous mixing, 40 kg / m3 of water in the mixture obtained through step (b).