Phase modulator and manufacturing method for the same

By using transparent electrodes and cavities to separate electrodes from optical waveguides, the phase modulator reduces optical loss, enabling a wider scan angle and smaller optical phased arrays for LiDAR applications.

JP2024134348APending Publication Date: 2024-10-03KK TOYOTA CHUO KENKYUSHO +3
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2023044606
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-20
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Reducing the pitch distance between adjacent optical waveguides in a phase modulator to widen the scan angle of a light beam leads to increased optical loss due to absorption by electrodes.

Method used

Incorporating transparent electrodes and securing a distance between electrodes and optical waveguides using cavities, reducing the pitch distance while minimizing optical loss.

Benefits of technology

The solution allows for a wider scan angle and smaller optical phased array by suppressing optical loss, enabling long-distance measurement in LiDAR devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024134348000001_ABST
    Figure 2024134348000001_ABST
Patent Text Reader

Abstract

To provide a technique of suppressing the absorption of propagation light in an electrode in a phase modulator.SOLUTION: A phase modulator includes a semiconductor layer including an optical waveguide, a clad layer provided on the semiconductor layer and including a first cavity and a second cavity, a first electrode in contact with an upper surface of the semiconductor layer through the first cavity, and a second electrode in contact with the upper surface of the semiconductor layer through the second cavity. The first electrode includes a first transparent electrode provided in at least a part of the first cavity. The second electrode includes a second transparent electrode provided in at least a part of the second cavity.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The technology disclosed in this specification relates to a phase modulator used in an optical phased array (OPA). [Background technology]

[0002] Patent Documents 1 to 3 disclose an example of a phase modulator used in an optical phased array. One example of this type of phase modulator includes a semiconductor layer including an optical waveguide and an electrode in contact with the semiconductor layer. The electrode includes a first electrode in contact with the semiconductor layer and a second electrode in contact with the semiconductor layer and disposed away from the first electrode. The optical waveguide is configured such that its refractive index or optical absorptance changes when a voltage is applied between the first electrode and the second electrode. When the refractive index or optical absorptance changes, the phase of the propagating light propagating through the optical waveguide changes.

[0003] The optical phased array is configured to generate a plurality of propagating lights having a phase difference between each other by using such a phase modulator, and to output each of the plurality of propagating lights from a corresponding transmitting antenna. The plurality of propagating lights output from the transmitting antenna become a light beam having a specific deflection angle. The deflection angle of the light beam depends on the phase difference of the plurality of propagating lights. For this reason, the optical phased array having the phase modulator can scan the output light beam by controlling the voltage applied between the first electrode and the second electrode. In this way, the optical phased array having the phase modulator has a feature that the deflection angle of the light beam can be changed without using, for example, a mechanical mirror structure. Such an optical phased array can be mounted on, for example, a LiDAR (Light Detection and Ranging) device. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] U.S. Patent Publication No. 2021 / 0026216 [Patent Document 2] Patent Publication No. 2021-103147 [Patent Document 3] JP 2020-166061 A Summary of the Invention [Problem to be solved by the invention]

[0005] In order to widen the scan angle of the light beam emitted from the transmitting antenna, the pitch distance between adjacent optical waveguides must be reduced. However, according to the study by the present inventors, it has been found that when the pitch distance between adjacent optical waveguides is reduced, a problem occurs in which a part of the propagating light propagating through the optical waveguide is absorbed by the electrodes, resulting in increased optical loss. This specification provides a technology for suppressing the absorption of propagating light by the electrodes in a phase modulator. [Means for solving the problem]

[0006] The phase modulator disclosed in the present specification may include a semiconductor layer including an optical waveguide, a cladding layer provided on the semiconductor layer, the cladding layer including a first cavity exposing a part of the upper surface of the semiconductor layer and a second cavity exposing another part of the upper surface of the semiconductor layer, a first electrode contacting the upper surface of the semiconductor layer through the first cavity, and a second electrode contacting the upper surface of the semiconductor layer through the second cavity. The optical waveguide may be disposed between a position where the first electrode contacts the upper surface of the semiconductor layer and a position where the second electrode contacts the upper surface of the semiconductor layer, and may be configured such that a phase of propagating light changes when a voltage is applied between the first electrode and the second electrode. The first electrode may include a first transparent electrode provided in at least a part of the first cavity. The second electrode may include a second transparent electrode provided in at least a part of the second cavity. According to this phase modulator, since at least a portion of each of the first electrode and the second electrode includes a transparent electrode, it is possible to suppress absorption of propagating light by the first electrode and the second electrode.

[0007] The method for manufacturing a phase modulator disclosed in the present specification may include an optical waveguide forming step of forming an optical waveguide in a semiconductor layer, a cladding layer forming step of forming a cladding layer on the semiconductor layer, the cladding layer having a first cavity exposing a part of the upper surface of the semiconductor layer and a second cavity exposing another part of the upper surface of the semiconductor layer, and a transparent electrode film forming step of forming a transparent electrode film on the cladding layer, the transparent electrode film having a first transparent electrode provided in at least a part of the first cavity and a second transparent electrode provided in at least a part of the second cavity. According to this manufacturing method, a phase modulator in which absorption of propagating light is suppressed can be manufactured. [Brief description of the drawings]

[0008] [Figure 1]FIG. 1 is a schematic perspective view of a main part of an optical phased array. [Diagram 2] 4 is a cross-sectional view of a main portion of an embodiment of a phase modulator, and is a schematic cross-sectional view of a main portion corresponding to line II-II in FIG. [Diagram 3] FIG. 2 is a schematic plan view of a main portion of a phase modulator; [Figure 4] 3A to 3C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 2 during a manufacturing process. [Diagram 5] 3A to 3C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 2 during a manufacturing process. [Figure 6] 3A to 3C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 2 during a manufacturing process. [Figure 7] 3A to 3C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 2 during a manufacturing process. [Figure 8] 3A to 3C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 2 during a manufacturing process. [Figure 9] 3A to 3C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 2 during a manufacturing process. [Figure 10] FIG. 1 is a schematic cross-sectional view of a main portion of an embodiment of a phase modulator. [Figure 11] 11A to 11C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 10 during the manufacturing process. [Figure 12] 11A to 11C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 10 during the manufacturing process. [Figure 13] 11A to 11C are schematic cross-sectional views of a main part of the phase modulator shown in FIG. 10 during the manufacturing process. [Figure 14] 11 is a schematic cross-sectional view of a main part of the phase modulator shown in FIG. 10 during the manufacturing process; [Figure 15] FIG. 1 is a schematic cross-sectional view of a main portion of an embodiment of a phase modulator. [Figure 16] 16A to 16C are diagrams each showing a cross section of a main part of the phase modulator shown in FIG. 15 during a manufacturing process. [Figure 17]16A to 16C are diagrams each showing a cross section of a main part of the phase modulator shown in FIG. 15 during a manufacturing process. [Figure 18] FIG. 1 is a schematic cross-sectional view of a main portion of an embodiment of a phase modulator. [Figure 19] FIG. 1 is a schematic cross-sectional view of a main portion of an embodiment of a phase modulator. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] (Optical phased array configuration) 1, the optical phased array 1 includes an optical waveguide 4, a distributor 6, a phase modulator 8, and a transmitting antenna 9. The optical waveguide 4, distributor 6, phase modulator 8, and transmitting antenna 9 are configured on a substrate 2 as an optical integrated circuit.

[0010] The distributor 6 is configured to split the optical waveguide 4 into a plurality of beams, and splits the propagating light input to the optical waveguide 4 into a plurality of propagating lights of the same phase. Each of the split propagating lights is phase-modulated by the phase modulator 8. The phase-modulated propagating lights are input to the transmitting antenna 9. The transmitting antenna 9 includes a diffraction grating provided corresponding to each of the optical waveguides 4, and outputs the phase-modulated propagating lights as a light beam toward the outside. The phase modulator 8 of the optical phased array 1 can control the phase difference between the propagating lights and adjust the deflection angle of the output light beam. Such an optical phased array 1 is mounted, for example, in a LiDAR device, although it is not particularly limited thereto.

[0011] (Structure of phase modulator) Hereinafter, the phase modulator 8 will be described with reference to the drawings. For clarity of illustration, reference numerals may be attached only to some of the repeatedly arranged structures.

[0012] As shown in Figs. 1 to 3, the phase modulator 8 includes a plurality of optical waveguides 4 formed on a substrate 2. The optical waveguides 4 are arranged adjacent to each other in the x direction. Each of the optical waveguides 4 extends between the distributor 6 and the transmitting antenna 9 along the y direction. The x direction indicates one direction parallel to the main surface 2S of the substrate 2, the y direction indicates a direction parallel to the main surface 2S of the substrate 2 and perpendicular to the x direction, and the z direction indicates a direction perpendicular to the main surface 2S of the substrate 2 (perpendicular to each of the x direction and the y direction). As shown in Fig. 2, the portion surrounded by the dashed line is a unit 10 constituting the phase modulator 8. The distance between adjacent optical waveguides 4 is referred to as a pitch distance 10D. Hereinafter, the unit 10 will be described as a phase modulator 8.

[0013] The phase modulator 8 includes a substrate 2, a cladding layer 16 provided on the substrate 2, a first electrode 40, and a second electrode 50. The substrate 2 includes an insulating layer 12 and a semiconductor layer 14 laminated on the insulating layer 12. The material of the insulating layer 12 is not particularly limited, but may be, for example, silicon oxide (SiO 2 ) The material of the semiconductor layer 14 is not particularly limited, but may be, for example, silicon. The semiconductor layer 14 has an optical waveguide 4, a p-type semiconductor region 22, and an n-type semiconductor region 32.

[0014] The optical waveguide 4 is provided at a position exposed to one of the principal surfaces 2S of the semiconductor layer 14. In this example, the optical waveguide 4 is a non-doped region formed as a part of the semiconductor layer 14. Alternatively, the optical waveguide 4 may be formed of a semiconductor material different from that of the semiconductor layer 14, for example, silicon nitride. The optical waveguide 4 is disposed between the first electrode 40 and the second electrode 50 when viewed from the z-axis direction (hereinafter, referred to as "when viewed in a plan view"). The optical waveguide 4 is also provided between the p-type semiconductor region 22 and the n-type semiconductor region 32 when viewed in a plan view. The optical waveguide 4 has a protruding portion 4A protruding from the principal surface 2S of the semiconductor layer 14. When the optical waveguide 4 has the protruding portion 4A, the protruding portion 4A is covered with the cladding layer 16, and the propagating light is effectively confined within the optical waveguide 4. The protruding portion 4A may not be formed as necessary.

[0015] The p-type semiconductor region 22 is provided at a position exposed on one main surface 2S of the semiconductor layer 14, and is disposed between the first electrode 40 and the optical waveguide 4. The p-type semiconductor region 22 contacts both the first electrode 40 and the optical waveguide 4. When viewed in a plan view, the p-type semiconductor region 22 extends along the direction in which the optical waveguide 4 extends, i.e., the y direction. The p-type semiconductor region 22 may have a high concentration region in which the p-type impurity concentration is adjusted to be high in a portion in contact with the first electrode 40.

[0016] The n-type semiconductor region 32 is provided at a position exposed to one main surface 2S of the semiconductor layer 14, and is disposed between the second electrode 50 and the optical waveguide 4. The n-type semiconductor region 32 contacts both the second electrode 50 and the optical waveguide 4. When viewed in a plan view, the n-type semiconductor region 32 extends along the direction in which the optical waveguide 4 extends, i.e., the y direction. The n-type semiconductor region 32 may have a high concentration region in which the n-type impurity concentration is adjusted to be high in a portion in contact with the second electrode 50.

[0017] The cladding layer 16 is provided so as to cover one main surface 2S of the semiconductor layer 14. The cladding layer 16 is made of a material having a smaller refractive index than the optical waveguide 4. The material of the cladding layer 16 is not particularly limited, but may be, for example, silicon oxide (SiO 2). The cladding layer 16 has a first cavity 24 and a second cavity 34 formed therein. The first cavity 24 penetrates the cladding layer 16 and is formed so as to expose a part of the range of one main surface 2S of the semiconductor layer 14 where the p-type semiconductor region 22 is formed. The first cavity 24 extends along the direction in which the optical waveguide 4 extends, i.e., the y direction, when viewed in a plan view. The second cavity 34 penetrates the cladding layer 16 and is formed so as to expose a part of the range of one main surface 2S of the semiconductor layer 14 where the n-type semiconductor region 32 is formed. The second cavity 34 extends along the direction in which the optical waveguide 4 extends, i.e., the y direction, when viewed in a plan view. Both the first cavity 24 and the second cavity 34 are formed in a tapered shape from the upper surface of the cladding layer 16 toward one main surface 2S of the semiconductor layer 14.

[0018] The first electrode 40 and the second electrode 50 are disposed apart in the x-axis direction with the optical waveguide 4 therebetween, and are electrically insulated. The first electrode 40 is formed on the cladding layer 16. When viewed in a plan view, the first electrode 40 extends in the direction in which the optical waveguide 4 extends, i.e., along the y-axis direction. The second electrode 50 is also formed on the cladding layer 16. When viewed in a plan view, the second electrode 50 extends in the direction in which the optical waveguide 4 extends, i.e., along the y-axis direction.

[0019] The first electrode 40 has a first transparent electrode 42 and a first wiring electrode 44. The first transparent electrode 42 is provided in the first cavity 24 of the cladding layer 16 and is in contact with the p-type semiconductor region 22. In this example, only the first transparent electrode 42 is provided in the first cavity 24. The first transparent electrode 42 also extends outside the first cavity 24 of the cladding layer 16 and on the upper surface of the cladding layer 16. The first wiring electrode 44 is provided outside the first cavity 24 of the cladding layer 16 and is provided on a part of the first transparent electrode 42 extending on the upper surface of the cladding layer 16. The first wiring electrode 44 is electrically connected to the p-type semiconductor region 22 via the first transparent electrode 42. In this way, the first wiring electrode 44 is located away from the protrusion 4A of the optical waveguide 4 in the stacking direction (z-axis direction) and the surface direction (x-axis direction).

[0020] The second electrode 50 has a second transparent electrode 52 and a second wiring electrode 54. The second transparent electrode 52 is provided in the second cavity 34 of the cladding layer 16 and is in contact with the n-type semiconductor region 32. In this example, only the second transparent electrode 52 is provided in the second cavity 34. The second transparent electrode 52 also extends outside the second cavity 34 of the cladding layer 16 and on the upper surface of the cladding layer 16. The second wiring electrode 54 is provided outside the second cavity 34 of the cladding layer 16 and is provided on a part of the second transparent electrode 52 extending on the upper surface of the cladding layer 16. The second wiring electrode 54 is electrically connected to the n-type semiconductor region 32 via the second transparent electrode 52. In this way, the second wiring electrode 54 is located away from the protrusion 4A of the optical waveguide 4 in the stacking direction (z-axis direction) and the surface direction (x-axis direction).

[0021] The first transparent electrode 42 of the first electrode 40 and the second transparent electrode 52 of the second electrode 50 are made of a material that is transparent to the light propagating through the optical waveguide 4. The material of the transparent electrodes 42, 52 may be a transparent conductive oxide (TCO). The transparent conductive oxide (TCO) is not particularly limited, and may be, for example, an indium oxide (InO)-based, tin oxide (SnO)-based, or zinc oxide (ZnO)-based material. The impurities doped into these oxide semiconductors may include at least one selected from the group consisting of indium (In), gallium (Ga), aluminum (Al), antimony (Sb), fluorine (F), tin (Sn), yttrium (Y), cadmium (Cd), arsenic (As), niobium (Nb), tantalum (Ta), germanium (Ge), molybdenum (Mo), titanium (Ti), zirconium (Zr), hafnium (Hf), tungsten (W), tellurium (Te), boron (B), scandium (Sc), vanadium (V), and silicon (Si).

[0022] The first wiring electrode 44 of the first electrode 40 is connected to a wiring for electrically connecting a control terminal (not shown) provided in the optical phased array 1 and the first transparent electrode 42. The material of the first wiring electrode 44 is made of a metal, and is not particularly limited, but may be, for example, aluminum (Al). As shown in FIG. 3, the first wiring electrode 44 may be formed to extend from one end to the other end of the first transparent electrode 42 along the y-axis direction in a planar view. Instead of this example, the first wiring electrode 44 may be formed to contact only a part of the first transparent electrode 42 in the y-axis direction in a planar view.

[0023] The second wiring electrode 54 of the second electrode 50 is connected to a wiring for electrically connecting a control terminal (not shown) provided in the optical phased array 1 and the second transparent electrode 52. The material of the second wiring electrode 54 is made of a metal, and is not particularly limited, but may be, for example, aluminum (Al). As shown in FIG. 3, the second wiring electrode 54 may be formed to extend from one end to the other end of the second transparent electrode 52 along the y-axis direction in a planar view. The second wiring electrode 54 may be formed to contact only a part of the second transparent electrode 52 in the y-axis direction in a planar view.

[0024] (Operation of phase modulator) When a voltage that is more positive than the second electrode 50 is applied to the first electrode 40, a current flows from the first electrode 40 to the second electrode 50 via the p-type semiconductor region 22, the optical waveguide 4, and the n-type semiconductor region 32. This increases the carrier concentration in the optical waveguide 4, and changes the phase of the propagating light propagating through the optical waveguide 4. The phase modulator 8 adjusts the phase of the propagating light propagating through the optical waveguide 4, and outputs the phase-modulated propagating light to the transmitting antenna 9 (see FIG. 1).

[0025] The distribution of the propagating light propagating through the optical waveguide 4 is a range including the periphery of the optical waveguide 4. A part of the propagating light propagating through the optical waveguide 4 contacts the first transparent electrode 42 of the first electrode 40 and the second transparent electrode 52 of the second electrode 50. For example, if these contacting parts are opaque metal electrodes, a part of the propagating light is absorbed by the metal electrodes, and the optical loss increases. On the other hand, in the phase modulator 8, since these contacting parts are composed of the transparent electrodes 42 and 52, such optical loss is suppressed. Therefore, the phase modulator 8 can output the propagating light to the transmitting antenna 9 (see FIG. 1) while maintaining the intensity of the propagating light. As a result, when the optical phased array 1 (see FIG. 1) is mounted on a LiDAR device, the LiDAR device can measure long distances.

[0026] In addition, when the optical phased array 1 (see FIG. 1) is mounted on a LiDAR device, in order to widen the scan angle of the light beam emitted from the transmitting antenna 9, the pitch distance 10D between adjacent optical waveguides 4 must be reduced. For example, in order to emit a light beam with a wavelength of 1550 nm at a scan angle of 60°, the pitch distance 10D between adjacent optical waveguides 4 must be 1.55 μm or less. However, when the pitch distance 10D between the optical waveguides 4 is reduced, the above-mentioned problem of a part of the propagating light being absorbed by the metal electrode and increasing the light loss becomes apparent. The phase modulator 8 having the transparent electrodes 42 and 52 can suppress such an increase in light loss. As a result, the LiDAR device mounted with the optical phased array 1 including the phase modulator 8 can reduce the pitch distance 10D between adjacent optical waveguides 4 while suppressing the increase in light loss, and therefore the scan angle can be widened. Furthermore, since the pitch distance 10D of the optical waveguides 4 can be reduced, the optical phased array 1 can also be made smaller.

[0027] In addition, in the phase modulator 8, the first wiring electrode 44 of the first electrode 40 is disposed on the side farther from the optical waveguide 4 with the first cavity 24 therebetween. Similarly, in the phase modulator 8, the second wiring electrode 54 of the second electrode 50 is disposed on the side farther from the optical waveguide 4 with the second cavity 34 therebetween. In this way, a distance is ensured between the wiring electrodes 44, 54 and the optical waveguide 4, so that an increase in optical loss due to a part of the propagating light being absorbed by the wiring electrodes 44, 54 is suppressed. Note that, if the film thickness of the cladding layer 16 is sufficiently ensured, the wiring electrodes 44, 54 may be disposed inside the cavity 24, 34. In this case, the pitch distance 10D of the optical waveguide 4 can be reduced, so that the optical phased array 1 can be miniaturized.

[0028] (Method of manufacturing phase modulator) A method for manufacturing the phase modulator 8 will be described below with reference to Fig. 4 to Fig. 9. First, as shown in Fig. 4, a substrate 2 on which an insulating layer 12 and a semiconductor layer 14 are laminated is prepared.

[0029] 5, a part of the semiconductor layer 14 is removed by etching to form a convex portion 4A of the optical waveguide 4. Next, p-type impurities and n-type impurities are introduced into a part of the semiconductor layer 14 by ion implantation, and the introduced impurities are activated to form a p-type semiconductor region 22 and an n-type semiconductor region 32.

[0030] 6, a film formation technique is used to form the cladding layer 16 on the semiconductor layer 14. On the upper surface of the cladding layer 16, projections and recesses corresponding to the projections 4A of the optical waveguide 4 are formed.

[0031] Next, as shown in Fig. 7, a first cavity 24 and a second cavity 34 are formed in the cladding layer 16 using photolithography and reactive ion etching techniques. Both the first cavity 24 and the second cavity 34 are formed in a tapered shape from the upper surface of the cladding layer 16 toward one main surface 2S of the semiconductor layer 14. In this specification, the process shown in Figs. 6 and 7 is referred to as a cladding layer formation process.

[0032] 8, a transparent electrode film 70 is formed in the cavities 24, 34 and on the cladding layer 16 by using a sputtering technique. Since the sputtering technique has good step coverage, the transparent electrode film 70 is formed conformally. Furthermore, since the cavities 24, 34 are formed in a tapered shape, the transparent electrode film 70 is formed well in these cavities 24, 34. Note that instead of the sputtering technique, the transparent electrode film 70 may be formed by using a CVD (Chemical Vapor Deposition) technique or an ALD (Atomic Layer Deposition) technique.

[0033] Next, a heat treatment process is carried out to adjust the extinction coefficient and electrical resistance of the transparent electrode film 70. This heat treatment process is composed of a combination of heating in an oxygen atmosphere and heating in a non-oxygen atmosphere. In this example, first, oxygen (O 2 ) atmosphere, and then nitrogen (N 2 Heating is carried out in an oxygen (O 2The heating of the atmosphere is not particularly limited, but is performed, for example, at 400° C. for 20 minutes. 2 The heating of the atmosphere is carried out under conditions of, but not limited to, 500° C. and 60 minutes.

[0034] The properties required for the transparent electrode film 70 are a low extinction coefficient and a low electrical resistance. In the transparent conductive oxide (TCO), which is the material of the transparent electrode film 70, its oxygen defects (oxygen vacancies and interstitial oxygen) act as carriers. The carriers in the transparent conductive oxide (TCO) have electrical conductivity and inhibit light transmission. When the transparent conductive oxide (TCO) is heated in an oxygen atmosphere, the oxygen defects are filled, and the electrical resistance increases and the extinction coefficient decreases due to the disappearance of carriers. On the other hand, when the transparent conductive oxide (TCO) is heated in a non-oxygen atmosphere, oxygen is removed and the electrical resistance decreases and the extinction coefficient increases due to the generation of carriers. The upper and lower limits of the extinction coefficient and the upper and lower limits of the electrical resistance depend on the conditions of heating in an oxygen atmosphere and heating in a non-oxygen atmosphere. In this way, the extinction coefficient and electrical resistance of the transparent conductive oxide (TCO) can be adjusted by combining heating in an oxygen atmosphere and heating in a non-oxygen atmosphere. In this example, the conditions of heating in an oxygen atmosphere and heating in a non-oxygen atmosphere are adjusted so that the electrical resistance value ensures the necessary electrical conductivity while suppressing an increase in the extinction coefficient due to oxygen defects. In addition to adjusting the extinction coefficient and electrical resistance value, this heat treatment can also eliminate other types of defects other than oxygen defects formed in the transparent electrode film 70 during film formation. The order of performing heating in an oxygen atmosphere and heating in a non-oxygen atmosphere is not particularly limited.

[0035] Next, as shown in FIG. 9, an opening is formed in the transparent electrode film 70 using photolithography and reactive ion etching techniques, and the first transparent electrode 42 and the second transparent electrode 52 are formed. The width of the opening is not particularly limited as long as the first transparent electrode 42 and the second transparent electrode 52 are electrically insulated. For example, the opening of the transparent electrode film 70 above the protrusion 4A of the optical waveguide 4 may extend to the ends of the first cavity 24 and the second cavity 34. In this example, the above-mentioned heat treatment is performed before forming the opening in the transparent electrode film 70, but instead of this example, the above-mentioned heat treatment may be performed after forming the opening in the transparent electrode film 70. In this specification, the process shown in FIG. 8 and FIG. 9 is referred to as a transparent electrode film forming process.

[0036] Thereafter, an aluminum electrode film is formed using a sputtering technique, and then the electrode film is processed using a photolithography technique and a wet etching technique to form the first wiring electrode 44 and the second wiring electrode 54. Through these steps, the phase modulator 8 can be manufactured.

[0037] (Modification of Phase Modulator) The following describes some modified examples of the phase modulator 8. Components common to the phase modulator 8 shown in Fig. 2 and Fig. 3 are given the same reference numerals, and descriptions thereof will be omitted.

[0038] (First Modification of Phase Modulator) 10 is characterized in that the upper surface of the cladding layer 16 is flattened, and the first cavity 24 and the second cavity 34 are formed substantially vertically. With this configuration, the widths of the first cavity 24 and the second cavity 34 can be narrowed, so that the pitch distance 10D of the optical waveguides 4 is reduced, and the optical phased array 1 can be miniaturized.

[0039] (Manufacturing method of the first modified phase modulator) First, the above-mentioned steps shown in Fig. 4 to Fig. 6 are carried out. Next, as shown in Fig. 11, the upper surface of the cladding layer 16 is planarized using a CMP (Chemical Mechanical Polishing) technique. In this manner, in this manufacturing method, a planarization process is added to the cladding layer formation step.

[0040] 12, a first cavity 24 and a second cavity 34 are formed in the cladding layer 16 using photolithography and reactive ion etching techniques. Both the first cavity 24 and the second cavity 34 are formed substantially perpendicularly from the upper surface of the cladding layer 16 toward one main surface 2S of the semiconductor layer 14. Since the upper surface of the cladding layer 16 has been flattened, pattern formation by photolithography becomes easy.

[0041] Next, as shown in Fig. 13, a transparent electrode film 70 is formed in the cavities 24, 34 and on the cladding layer 16 using a sputtering technique. The transparent electrode film 70 is formed thick enough to completely fill the cavities 24, 34. Next, a heat treatment consisting of a combination of heating in an oxygen atmosphere and heating in a non-oxygen atmosphere is performed to adjust the extinction coefficient and electrical resistance value of the transparent electrode film 70. Note that this heat treatment may be performed after forming an opening in the transparent electrode film 70.

[0042] Next, as shown in FIG. 14, the upper surface of the transparent electrode film 70 is planarized using CMP technology, and then openings are formed in the transparent electrode film 70 using photolithography technology and reactive ion etching technology to form the first transparent electrode 42 and the second transparent electrode 52.

[0043] Thereafter, an aluminum electrode film is formed using a sputtering technique, and then the electrode film is processed using a photolithography technique and a wet etching technique to form the first wiring electrode 44 and the second wiring electrode 54. Through these steps, the first modified example of the phase modulator 8 can be manufactured.

[0044] (Second Modification of Phase Modulator) 15 is characterized in that a first transparent electrode 42 and a first wiring electrode 44 are arranged in a stacked manner in the first cavity 24, and a second transparent electrode 52 and a second wiring electrode 54 are arranged in a stacked manner in the second cavity 34. With such a configuration, it is not necessary to secure a large space outside the cavities 24, 34 for arranging the wiring electrodes 44, 54, and therefore the pitch distance 10D of the optical waveguides 4 is reduced, and the optical phased array 1 can be made smaller.

[0045] (Manufacturing method of the second modified phase modulator) The process up to forming the cavities 34, 24 in the cladding layer 16 is the same as that of the first modified example. Next, as shown in FIG. 16, a transparent electrode film 70 is formed in the cavities 24, 34 and on the cladding layer 16 using a sputtering technique. The transparent electrode film 70 is formed thinly so as not to fill the cavities 24, 34. Next, a heat treatment consisting of a combination of heating in an oxygen atmosphere and heating in a non-oxygen atmosphere is performed to adjust the extinction coefficient and electrical resistance value of the transparent electrode film 70. This heat treatment may be performed after removing the transparent electrode film 70 formed on the cladding layer 16.

[0046] 17, the transparent electrode film 70 formed on the cladding layer 16 is removed using an etching technique or a CMP technique. As a result, the first transparent electrode 42 remains in the first cavity 24, and the second transparent electrode 52 remains in the second cavity 34.

[0047] Thereafter, an aluminum electrode film is formed using a sputtering technique, and then the electrode film is processed using a photolithography technique and a wet etching technique to form the first wiring electrode 44 and the second wiring electrode 54. Through these steps, the second modified example of the phase modulator 8 can be manufactured.

[0048] (Third Modification of Phase Modulator) In the third modification of the phase modulator 8 shown in FIG. 18, the first transparent electrode 42 provided in the first cavity 24 has a high-concentration transparent electrode 42a and a low-concentration transparent electrode 42b. The high-concentration transparent electrode 42a is adjusted to have a higher concentration of impurities to be doped than the low-concentration transparent electrode 42b, and a higher carrier concentration. In the third modification of the phase modulator 8, the second transparent electrode 52 provided in the second cavity 34 also has a high-concentration transparent electrode 52a and a low-concentration transparent electrode 52b. The configuration of the second transparent electrode 52 is the same as that of the first transparent electrode 42. Only the first transparent electrode 42 will be described below, but the second transparent electrode 52 is similar.

[0049] The high-concentration transparent electrode 42a and the low-concentration transparent electrode 42b are laminated in this order. The high-concentration transparent electrode 42a is provided between the p-type semiconductor region 22 and the low-concentration transparent electrode 42b formed in the semiconductor layer 14, and is in contact with both the p-type semiconductor region 22 and the low-concentration transparent electrode 42b. The thickness of the low-concentration transparent electrode 42b in the z-axis direction is greater than the thickness of the high-concentration transparent electrode 42a in the z-axis direction.

[0050] When the carrier concentration of the transparent electrode 42 is low, the absorption of the propagating light is suppressed. On the other hand, when the carrier concentration of the transparent electrode 42 is low, the contact resistance with the p-type semiconductor region 22 increases. In the third modified example of the phase modulator 8, the high-concentration transparent electrode 42a having a high carrier concentration is provided, so that the contact resistance between the p-type semiconductor region 22 and the transparent electrode 42 decreases. On the other hand, the low-concentration transparent electrode 42b has a low carrier concentration, so that the absorption of the propagating light in the low-concentration transparent electrode 42b is suppressed. In this way, in the third modified example of the phase modulator 8, it is possible to suppress both the absorption of the propagating light and the increase in the contact resistance.

[0051] (Fourth Modification of Phase Modulator) The fourth modification of the phase modulator 8 shown in FIG. 19 is characterized in that a third electrode 60 is provided on the clad layer 16 covering the convex portion 4A of the optical waveguide 4. The third electrode 60 has a third transparent electrode 62 and a third wiring electrode 64. The third transparent electrode 62 faces the convex portion 4A of the optical waveguide 4 via the clad layer 16, and is disposed at a position overlapping the convex portion 4A of the optical waveguide 4 when viewed in a plan view. The third transparent electrode 62 extends in the direction in which the optical waveguide 4 extends, that is, along the y-axis direction when viewed in a plan view. The carrier concentration of the third transparent electrode 62 is lower than the carrier concentration of the first transparent electrode 42 and the second transparent electrode 52. The third wiring electrode 64 is provided on the third transparent electrode 62. The third wiring electrode 64 is composed of a pair of electrodes, and the pair of electrodes is disposed apart in the y-axis direction when viewed in a plan view. The third transparent electrode 62 is provided between the pair of electrodes constituting the third wiring electrode 64. Therefore, when a voltage is applied between the pair of electrodes constituting the third wiring electrode 64, a current flows through the third transparent electrode 62. Since the carrier concentration of the third transparent electrode 62 is adjusted to be low, when a current flows through the third transparent electrode 62, the third transparent electrode 62 generates heat due to Joule heat. The fourth modified example of the phase modulator 8 can adjust the phase of the propagating light by the heat generated by the third electrode 60, in addition to adjusting the phase of the propagating light using the first electrode 40 and the second electrode 50. Therefore, the fourth modified example of the phase modulator 8 can adjust the phase of the propagating light with higher precision.

[0052] The features of the technology disclosed in this specification are summarized below. Note that the technical elements described below are independent technical elements that exhibit technical usefulness alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing.

[0053] (First feature) 1. A phase modulator comprising: a semiconductor layer including an optical waveguide; a cladding layer provided on the semiconductor layer, the cladding layer having a first cavity and a second cavity that expose a portion of an upper surface of the semiconductor layer; a first electrode in contact with the top surface of the semiconductor layer via the first cavity; a second electrode in contact with the top surface of the semiconductor layer through the second cavity, the optical waveguide is disposed between a position where the first electrode contacts the upper surface of the semiconductor layer and a position where the second electrode contacts the upper surface of the semiconductor layer, and is configured such that a phase of propagating light changes when a voltage is applied between the first electrode and the second electrode; the first electrode includes a first transparent electrode disposed in at least a portion of the first cavity; The second electrode includes a second transparent electrode disposed at least partially within the second cavity.

[0054] (Second feature) The semiconductor layer is a first semiconductor region of a first conductivity type in contact with the first electrode; a second semiconductor region of a second conductivity type in contact with the second electrode, 2. The phase modulator of claim 1, wherein the optical waveguide is disposed between the first semiconductor region and the second semiconductor region.

[0055] (Third feature) Only the first transparent electrode is provided in the first cavity, 3. The phase modulator according to claim 2, wherein only the second transparent electrode is provided within the second cavity.

[0056] (Fourth feature) the first electrode includes a first wiring electrode electrically connected to the first semiconductor region via the first transparent electrode; the first wiring electrode is provided outside the first cavity, the second electrode includes a second wiring electrode electrically connected to the second semiconductor region via the second transparent electrode, 4. The phase modulator according to feature 3, wherein the second wiring electrode is provided outside the second cavity.

[0057] (Fifth feature) 5. The phase modulator according to any one of Features 1 to 4, wherein the first transparent electrode and the second transparent electrode are made of a transparent conductive oxide (TCO).

[0058] (6th feature) A method for manufacturing a phase modulator, comprising the steps of: an optical waveguide forming step of forming an optical waveguide in the semiconductor layer; a cladding layer forming step of forming a cladding layer on the semiconductor layer, the cladding layer having a first cavity and a second cavity that expose a part of an upper surface of the semiconductor layer; a transparent electrode film forming process for forming a transparent electrode film on the cladding layer, the transparent electrode film having a first transparent electrode provided in at least a portion of the first cavity and a second transparent electrode provided in at least a portion of the second cavity.

[0059] (7th feature) The method further includes a heat treatment step of heat treating the transparent electrode film, The transparent electrode film is a transparent conductive oxide (TCO), 7. The method for manufacturing a phase modulator according to claim 6, wherein the heat treatment includes heating in an oxygen atmosphere and heating in a non-oxygen atmosphere.

[0060] (8th feature) The transparent electrode film forming step includes: forming the transparent electrode film on the cladding layer including within the first cavity and the second cavity; forming an opening in a portion of the transparent electrode film to insulate the first transparent electrode provided in the first cavity from the second transparent electrode provided in the second cavity; 8. The method for manufacturing a phase modulator according to claim 7, wherein the heat treatment is performed before forming the opening in the portion of the transparent electrode film or after forming the opening in the portion of the transparent electrode film.

[0061] (9th Feature) 9. The method for manufacturing a phase modulator according to any one of Features 6 to 8, wherein the cladding layer forming step includes flattening an upper surface of the cladding layer.

[0062] Although specific examples of the present invention have been described above in detail, these are merely examples and do not limit the scope of the claims. The technology described in the claims includes various modifications and variations of the specific examples exemplified above. Furthermore, the technical elements described in this specification or drawings exhibit technical utility alone or in various combinations, and are not limited to the combinations described in the claims at the time of filing. Furthermore, the technology exemplified in this specification or drawings can achieve multiple objectives simultaneously, and achieving one of these objectives is itself technically useful. [Explanation of symbols]

[0063] 2: substrate, 4: optical waveguide, 4A: convex portion, 8: phase modulator, 10: unit, 10D: pitch distance, 12: insulating layer, 14: semiconductor layer, 16: cladding layer, 22: p-type semiconductor region, 24: first cavity, 32: n-type semiconductor region, 34: second cavity, 40: first electrode, 42: first transparent electrode, 44: first wiring electrode, 50: second electrode, 52: second transparent electrode, 54: second wiring electrode,

Claims

1. 1. A phase modulator comprising: a semiconductor layer including an optical waveguide; a cladding layer provided on the semiconductor layer, the cladding layer having a first cavity exposing a portion of an upper surface of the semiconductor layer and a second cavity exposing another portion of the upper surface of the semiconductor layer; a first electrode in contact with the top surface of the semiconductor layer through the first cavity; a second electrode in contact with the top surface of the semiconductor layer through the second cavity, the optical waveguide is disposed between a position where the first electrode contacts the upper surface of the semiconductor layer and a position where the second electrode contacts the upper surface of the semiconductor layer, and is configured such that a phase of propagating light changes when a voltage is applied between the first electrode and the second electrode; the first electrode includes a first transparent electrode disposed in at least a portion of the first cavity; The second electrode comprises a second transparent electrode disposed at least partially within the second cavity.

2. The semiconductor layer is a first semiconductor region of a first conductivity type in contact with the first electrode; a second semiconductor region of a second conductivity type in contact with the second electrode, The phase modulator according to claim 1 , wherein the optical waveguide is disposed between the first semiconductor region and the second semiconductor region.

3. Only the first transparent electrode is provided in the first cavity, 3. The phase modulator according to claim 2, wherein only the second transparent electrode is provided within the second cavity.

4. the first electrode includes a first wiring electrode electrically connected to the first semiconductor region via the first transparent electrode; the first wiring electrode is provided outside the first cavity, the second electrode includes a second wiring electrode electrically connected to the second semiconductor region via the second transparent electrode, The phase modulator according to claim 3 , wherein the second wiring electrode is provided outside the second cavity.

5. 5. The phase modulator according to claim 1, wherein the first transparent electrode and the second transparent electrode are transparent conductive oxides (TCOs).

6. A method for manufacturing a phase modulator, comprising the steps of: an optical waveguide forming step of forming an optical waveguide in the semiconductor layer; a cladding layer forming step of forming a cladding layer on the semiconductor layer, the cladding layer having a first cavity exposing a portion of an upper surface of the semiconductor layer and a second cavity exposing another portion of the upper surface of the semiconductor layer; A method for manufacturing a phase modulator, comprising: a transparent electrode film formation process for forming a transparent electrode film, the transparent electrode film having a first transparent electrode provided in at least a portion of the first cavity and a second transparent electrode provided in at least a portion of the second cavity.

7. The method further includes a heat treatment step of heat treating the transparent electrode film, the transparent electrode film is a transparent conductive oxide (TCO); The method for manufacturing a phase modulator according to claim 6 , wherein the heat treatment includes heating in an oxygen atmosphere and heating in a non-oxygen atmosphere.

8. The transparent electrode film forming step includes: forming the transparent electrode film on the cladding layer including within the first cavity and the second cavity; forming an opening in a portion of the transparent electrode film to insulate the first transparent electrode provided in the first cavity from the second transparent electrode provided in the second cavity; The method for manufacturing a phase modulator according to claim 7 , wherein the heat treatment is performed before forming the opening in a portion of the transparent electrode film or after forming the opening in a portion of the transparent electrode film.

9. The method for manufacturing a phase modulator according to claim 6 , wherein the cladding layer forming step includes planarizing an upper surface of the cladding layer.

Citation Information

Patent Citations

  • Optical scanning device

    JP2020166061A

  • Optical antenna

    JP2021103147A

  • Optical Phase Shifter Device

    US20210026216A1