Manufacturing method for insert molded body and manufacturing device for insert molded body

Heating the metal member during insert molding, combined with optional preheating, enhances bonding strength by maintaining resin fluidity and penetration into metal surface unevenness, addressing the bonding challenges in existing methods.

JP2024136282AInactive Publication Date: 2024-10-04MITSUI CHEMICALS INC +1
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023047360
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-23
Publication Date
2024-10-04
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing insert molding methods struggle to achieve sufficient bonding strength between metal and resin members due to increased pressure transmission loss and difficulty of resin penetration into fine uneven structures formed by chemical etching, which compromises airtightness and bonding effectiveness.

Method used

A method involving heating the metal member from placement in a first mold until a second mold faces the first mold, using a movable heater, and optionally preheating, to maintain resin fluidity and enhance bonding strength, even with fine surface unevenness.

Benefits of technology

The method produces an insert molded body with excellent bonding strength between metal and resin members, ensuring resin penetration into uneven structures and improving work efficiency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

To provide a manufacturing method for an insert molded body that can obtain an insert molded body with excellent joining strength between metal members and resin members, and a manufacturing device for an insert molded body that can obtain the insert molded body with excellent joining strength between the metal members and the resin members.SOLUTION: A manufacturing method for an insert molded body comprises the steps of placing a metal member in a first metal mold and placing a second metal mold opposite to the first metal mold to form a space for injecting a resin material around the metal member, and the metal member is heated from the time the metal member is placed in the first metal mold to the time the second metal mold is placed opposite to the first metal mold.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method and an apparatus for manufacturing an insert molded body. [Background technology]

[0002] Insert molding is a method for forming an article (insert molded product) in which a resin part is integrated with a different part such as a metal part. In insert molding, a dissimilar material such as a metal is generally placed in a cavity formed in a mold, and a resin material is brought into contact with the surface. In this state, the resin material is solidified or cured to obtain an insert molded product.

[0003] As a measure for increasing the airtightness at the interface between a metal member and a resin member, a method of roughening the surface of the metal member by chemical etching has been proposed (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2001-225352 A Summary of the Invention [Problem to be solved by the invention]

[0005] Paragraph

[0010] of Patent Document 1 cites that the mechanism for improving airtightness is that the surface area of ​​the metal is increased by finely roughening the metal surface by chemical etching, and the area of ​​the metal / resin interface is increased, which increases the pressure transmission loss when gas or liquid passes through the interface and penetrates into the inside of the part. On the other hand, it becomes difficult for the resin material to penetrate into the fine uneven structure formed by chemical etching, and there is a risk that the effect of increasing the bonding strength, such as airtightness, may not be fully obtained.

[0006] In view of the above circumstances, an object of the present disclosure is to provide a manufacturing method for an insert molded body that can obtain an insert molded body having excellent bonding strength between a metal member and a resin member, and a manufacturing apparatus for an insert molded body that can obtain an insert molded body having excellent bonding strength between a metal member and a resin member. [Means for solving the problem]

[0007] Means for solving the above problems include the following embodiments. <1> placing a metal member in a first mold; and a step of forming a space for injecting a resin material around the metal member by disposing a second mold opposite the first mold. A method for producing an insert molded product, comprising heating the metal member after the metal member is placed in a first mold and before a second mold is placed so as to face the first mold. <2> placing a metal member and a resin material in a first mold; and disposing the second mold so as to face the first mold. A method for manufacturing an insert molded body, comprising heating the metal member after the metal member and the resin material are placed in a first mold and before a second mold is placed opposite the first mold. <3> The heating is performed using a movable heater. <1> or <2> A method for producing the insert molding according to claim 1. <4> Further comprising a step of preheating the metal member before being placed in the first mold. <1> or <2> A method for producing the insert molding according to claim 1. <5> A first mold for disposing a metal member; A second mold that can be arranged to face the first mold and forms a space for injecting a resin material around the metal member; and a heater for heating the metal member from the time the metal member is placed in a first mold until the time a second mold is placed opposite the first mold. <6> a first mold for disposing a metal member and a resin material; A second mold that can be arranged to face the first mold; an insert molding apparatus comprising: a heater for heating the metal member from the time when the metal member and the resin material are placed in a first mold until the time when a second mold is placed opposite the first mold. <7> The heater is movable. <5> or <6> The insert molding apparatus according to claim 1 . <8> Further comprising a mechanism for preheating the metal member before it is placed in the first mold. <5> or <6> The insert molding apparatus according to claim 1 . Effect of the Invention

[0008] According to the present disclosure, there is provided a method for manufacturing an insert molded body, which provides an insert molded body having excellent bond strength between a metal member and a resin member, and an apparatus for manufacturing an insert molded body, which provides an insert molded body having excellent bond strength between a metal member and a resin member. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] In the present disclosure, a numerical range indicated using "~" indicates a range that includes the numerical values ​​before and after "~" as the minimum and maximum values, respectively. In the numerical ranges described in stages in this disclosure, the upper or lower limit value described in a certain numerical range may be replaced by the upper or lower limit value of another numerical range described in stages, or may be replaced by a value shown in the examples. In this disclosure, when a material contains multiple substances corresponding to each component, the amount of each component in the material means the total amount of the multiple substances present in the material, unless otherwise specified.

[0010] First Embodiment A first embodiment of the present disclosure includes a step of placing a metal member in a first mold; and a step of forming a space for injecting a resin material around the metal member by disposing a second mold opposite the first mold. This is a method for producing an insert molded product, in which the metal member is heated during the period from when the metal member is placed in a first mold until when a second mold is placed so as to face the first mold.

[0011] According to the above method, an insert molded body having excellent bonding strength between a metal member and a resin member can be obtained. In particular, even if a fine uneven structure is formed on the surface of the metal member, an insert molded body having excellent bonding strength between the metal member and the resin member can be obtained. The reason for this is thought to be that the metal member is heated from when it is placed in the first mold until when the second mold is placed so as to face the first mold, so that the temperature drop of the resin material when in contact with the metal member is suppressed, and a state in which it is easy to penetrate into the uneven structure of the metal member is maintained.

[0012] The metal member is heated during the period from when the metal member is placed in the first mold until when the second mold is placed so as to face the first mold, i.e., the metal member is heated during the period when the molds are in an open state.

[0013] The method for heating the metal member placed in the first mold is not particularly limited. From the viewpoint of ease of heating the metal member when the second mold is not disposed so as to face the first mold (i.e., when the mold is in an open state), it is preferable to heat the metal member using a movable heater. By using a movable heater, for example, when the mold is in an open state, the heater can be disposed at the position of the second mold when the second mold is disposed so as to face the first mold (hereinafter also referred to as the reference position) to heat the metal member, and when the mold is closed, the heater can be moved from the reference position to place the second mold at the reference position. When the heater is movable, the entire heater may be movable, or only a part of the heater (such as the heater head) may be movable.

[0014] The heating of the metal member may be performed evenly over the entire metal member, or may be performed intensively on the portion of the metal member where the temperature is likely to decrease. For example, when the metal member is not in contact with the first mold, the portion is exposed to the outside air and the temperature is likely to decrease when the mold is in an open state. Therefore, the heating of the metal member may be performed intensively on the portion of the metal member that is not in contact with the first mold.

[0015] The method may further include the step of preheating the metal member before it is placed in the first mold. By preheating the metal member, the fluidity of the resin material when it comes into contact with the metal member can be more reliably ensured, and the work efficiency of the insert molding can be improved.

[0016] There are no particular limitations on the method for preheating the metal member before it is placed in the first mold, and it can be performed using known heating means such as an oven or a heater.

[0017] In the above method, the temperature of the metal member when it is heated or preheated is not particularly limited. From the viewpoint of ensuring the fluidity of the resin material when it comes into contact with the metal member and preventing deterioration of the resin material, it is preferable that the temperature of the metal member when it is heated or preheated is a temperature T (°C) that satisfies the following formula: Tm-A≦T≦Tm+B In the formula, Tm is the melting point or softening point (° C.) of the resin material, and A and B are each independently a number from 0 to 50, preferably 0 to 25, and more preferably 0 to 10.

[0018] In the above method, the method of injecting the resin material into the space around the metal member is not particularly limited, and can be carried out by any known method.

[0019] <Second embodiment> A second embodiment of the present disclosure includes a step of placing a metal member and a resin material in a first mold; and disposing the second mold so as to face the first mold. This is a method for manufacturing an insert molded body, in which the metal member is heated after the metal member and the resin material are placed in a first mold and before a second mold is placed opposite the first mold.

[0020] The above method is suitable, for example, when the resin material placed in the first mold is solid. Examples of the form of the solid resin material include sheet, film, tape, and particles.

[0021] In the second embodiment, details and preferred aspects of the heating or preheating of the metal member are similar to those of the first embodiment.

[0022] <Third embodiment> A third embodiment of the present disclosure includes a first mold for arranging a metal member; A second mold that can be arranged to face the first mold and forms a space for injecting a resin material around the metal member; and a heater for heating the metal member from the time the metal member is placed in the first mold until the time the second mold is placed opposite the first mold.

[0023] The manufacturing apparatus is used, for example, in the method for manufacturing the insert molded article of the first embodiment. The first mold, the second mold, and the heater constituting the production apparatus are not particularly limited, and known means can be used.

[0024] In the above manufacturing apparatus, the heater may be movable. The manufacturing apparatus may further include a mechanism for preheating the metal member before it is placed in the first mold. The mechanism for preheating the metal member is not particularly limited, and may be any known heating means such as an oven or a heater.

[0025] <Fourth embodiment> A fourth embodiment of the present disclosure includes a first mold for arranging a metal member and a resin material; A second mold that can be arranged to face the first mold; and a heater for heating the metal member from the time when the metal member and the resin material are placed in a first mold until the time when a second mold is placed opposite the first mold.

[0026] The above-mentioned manufacturing apparatus is used, for example, in the method for manufacturing the insert molded article of the second embodiment. The first mold, the second mold, and the heater constituting the production apparatus are not particularly limited, and known means can be used.

[0027] In the above manufacturing apparatus, the heater may be movable. The manufacturing apparatus may further include a mechanism for preheating the metal member before it is placed in the first mold. The mechanism for preheating the metal member is not particularly limited, and may be any known heating means such as an oven or a heater.

[0028] (Metal parts) The type of metal member used in the manufacturing method of the insert molded article of the present disclosure is not particularly limited, and can be selected depending on the application of the insert molded article, etc. From the viewpoint of electrical conductivity and heat dissipation, it is preferable that the metal member contains at least one metal selected from copper, aluminum, copper alloys, and aluminum alloys. The metal member may contain only one metal or two or more metals. In addition, at least a part of the surface may have a plating layer.

[0029] The metal member produced by the method of the present disclosure has at least a part of its surface bonded to the resin member. In the present disclosure, "bonded" means that the metal member is fixed to the resin member without using an adhesive, screws, or the like.

[0030] The metal member may have an uneven structure on its surface. When the metal member has an uneven structure on its surface, the molten or softened resin material is solidified in a state where it has entered the uneven structure, thereby exerting an anchor effect, and the resin member is firmly bonded to the surface of the metal member.

[0031] From the viewpoint of bonding with the resin member, the Rz of the surface of the metal member is preferably 2 μm or more, more preferably 5 μm or more, and even more preferably 10 μm or more. In this disclosure, Rz of the surface of a metal member is a parameter in the height direction called "maximum height", which is calculated by extracting a part of the roughness curve measured by a roughness meter over a reference length (500 μm) and calculating it as the sum of the highest part (maximum peak height: Rp) and the deepest part (maximum valley depth: Rv). And ask.

[0032] The true surface area (m2) of the surface of a metal component measured by the krypton adsorption method 2 ) to the geometric surface area (m 2 ) may be 4 or more, 6 or more, or 10 or more. A larger roughness index means that the microscopic surface area of ​​the metal member is larger and the contact area with the resin material is larger.

[0033] In the present disclosure, the true surface area of ​​the surface of a metal component is determined by the BET method using krypton gas as an adsorbate. That is, the BET specific surface area (m 2 / g) multiplied by the mass (g) of the object to be measured is the true surface area (m 2 The true surface area of ​​the surface of the metal component is determined by pretreating the measurement target by vacuum heating and degassing (100°C), then measuring the adsorption isotherm by krypton gas adsorption at liquid nitrogen temperature (77K) using a specific surface area measuring device (e.g., BELSORP-max, manufactured by Microtrack-Bell Corporation), and then determining the area from the measurement results. In this disclosure, the geometric surface area of ​​the surface of a metal component is a value calculated from the dimensions of the object to be measured. For example, if the object to be measured is a rectangular parallelepiped with length X, width Y, and height Z, the geometric surface area S can be calculated as S = 2XY + 2YZ + 2ZX.

[0034] The metal member may be subjected to a roughening treatment to form an uneven structure on the surface. Methods for roughening metal members include chemical etching methods as disclosed in JP 2001-225352 A; methods using lasers as disclosed in JP 4020957 A; methods of immersing the surface of a metal member in an aqueous solution of an inorganic base such as NaOH or an inorganic acid such as HCl or HNO3; methods of treating the surface of a metal member by anodization as disclosed in JP 4541153 A; and methods of using an acid-based etching agent (preferably an inorganic acid, Examples of such methods include a displacement crystallization method in which etching is performed with an acid-based etching solution containing ferric ions or cupric ions) and, if necessary, manganese ions, aluminum chloride hexahydrate, sodium chloride, etc.; a method in which the surface of a metal member is immersed in an aqueous solution of one or more compounds selected from hydrazine hydrate, ammonia, and water-soluble amine compounds (NMT method) as disclosed in International Publication No. 2009 / 31632; a hot water treatment method as disclosed in Japanese Patent Application Laid-Open No. 2008-162115; and roughening treatments such as blasting.

[0035] When a concave-convex structure is formed on the surface of a metal member, the average pore size of the concaves in the concave-convex structure may be, for example, 5 nm to 250 μm, preferably 10 nm to 150 μm, and more preferably 15 nm to 100 μm. The average pore depth of the recesses in the relief structure may be, for example, 5 nm to 250 μm, preferably 10 nm to 150 μm, and more preferably 15 nm to 100 μm. When either or both of the average pore size and the average pore depth of the recesses in the uneven surface structure are within the above numerical ranges, stronger bonding tends to be obtained.

[0036] The average pore size and average pore depth of the recesses in the uneven structure can be determined by using an electron microscope or a laser microscope. Specifically, the surface and cross section of the surface of the metal member are photographed. From the obtained photograph, 50 recesses are arbitrarily selected, and the average pore size and average pore depth of the recesses can be calculated as arithmetic average values ​​from the pore size and pore depth of the recesses.

[0037] The metal member may have a plating layer. The material of the plating layer is not particularly limited, and known materials such as tin (Sn), zinc (Zi), nickel (Ni), and chromium (Cr) can be used. The thickness of the plating layer is not particularly limited. For example, it may be in the range of 10 nm to 2,000 μm.

[0038] (Resin material) The type of resin material used in the method for producing an insert molded article according to the present disclosure is not particularly limited, and can be selected depending on the application of the insert molded article, etc. In the present disclosure, a resin material means a material that essentially contains a resin and optionally contains materials other than resin. The resin contained in the resin material may be a thermoplastic resin, a thermosetting resin, a thermoplastic elastomer, a thermosetting elastomer, or the like.

[0039] Thermoplastic resins include polyethylene (PE), polypropylene (PP), polystyrene (PS), acrylonitrile / styrene resin (AS), acrylonitrile / butadiene / styrene resin (ABS), methacrylic resin (PMMA), polyvinyl chloride (PVC), polyamide (PA), polyacetal (POM), ultra-high molecular weight polyethylene (UHPE), polybutylene terephthalate (PBT), polyethylene terephthalate (PET), polymethylpentene (TPX), polycarbonate (PC), and modified polyphenylene ether. Examples of suitable materials include polyphenylene sulfide (PPE), polyphenylene sulfide (PPS), polyether ether ketone (PEEK), liquid crystal resin (LCP), polytetrafluoroethylene (PTFE), polyetherimide (PEI), polyarylate (PAR), polysulfone (PSF), polyethersulfone (PES), polyamideimide (PAI), polybutylene sulfide (PBS), polycyclohexylene dimethylene terephthalate (PCT), thermoplastic polyimide (TPI), polyphthalamide (PPA), and polyimide (PI).

[0040] Examples of the thermosetting resin include phenol resin, urea resin, melamine resin, unsaturated polyester, alkyd resin, epoxy resin, and diallyl phthalate resin.

[0041] Examples of the thermoplastic elastomer include styrene-based thermoplastic elastomers, polyester-based thermoplastic elastomers, urethane-based thermoplastic elastomers, and amide-based thermoplastic elastomers.

[0042] Examples of thermosetting elastomers include diene rubbers such as natural rubber (NR), isoprene rubber (IR), butadiene rubber (BR), styrene-butadiene copolymer rubber (SBR), chloroprene rubber (CR), and acrylonitrile-butadiene copolymer rubber (NBR), as well as non-diene rubbers such as butyl rubber (IIR), ethylene-propylene rubber (EPM), urethane rubber, silicone rubber, and acrylic rubber. The resins contained in the resin material may be used alone or in combination of two or more kinds.

[0043] From the viewpoint of bonding strength to metal members, the resin contained in the resin material is preferably polyamide, polyphenylene sulfide, polybutylene sulfide, or polycyclohexylene dimethylene terephthalate. From the viewpoints of heat resistance (heat resistance temperature of 150°C or higher) and oil resistance, the resin contained in the resin material is preferably polyether ether ketone, liquid crystal resin, polyether sulfone, thermoplastic polyimide, polyphthalamide, polyimide, polyamide, or polyphenylene sulfide.

[0044] The resin material may contain various additives in addition to the resin, such as fillers such as glass fiber and inorganic powder, heat stabilizers, antioxidants, pigments, weather resistance agents, flame retardants, plasticizers, dispersants, lubricants, release agents, and antistatic agents.

[0045] When the resin material contains components other than resin, the proportion of the resin in the entire resin material is preferably 10% by mass or more, more preferably 20% by mass or more, and even more preferably 30% by mass or more. The upper limit of the proportion of the resin in the entire resin material is not particularly limited, and may be 100% by mass.

[0046] (Insert molding) The insert molded article produced by the method of the present disclosure is an object including at least a metal member and a resin member. The resin member is formed from the resin material used in the method of the present disclosure. The insert molded article produced by the method of the present disclosure can be used for various applications, such as electrical and electronic devices, automobile parts, daily necessities, furniture, etc.

[0047] The insert molded body produced by the method of the present disclosure is also suitable when copper is used as the metal member. Copper has excellent electrical conductivity and is widely used as a material for conductive members such as bus bars, but has high thermal conductivity and is prone to temperature drop during the molding process. The method of the present disclosure suppresses the drop in temperature of the metal member during the molding process. Therefore, the insert molded body produced by the method of the present disclosure has excellent bonding strength with the resin member even when copper is used as the metal member.

Claims

1. placing a metal member in a first mold; and a step of forming a space for injecting a resin material around the metal member by disposing a second mold opposite to the first mold, A method for manufacturing an insert molded product, comprising heating the metal member after the metal member is placed in a first mold and before a second mold is placed so as to face the first mold.

2. placing a metal member and a resin material in a first mold; and disposing a second mold so as to face the first mold. A manufacturing method for an insert molded body, comprising heating the metal member after the metal member and the resin material are placed in a first mold and before a second mold is placed opposite the first mold.

3. The method for producing an insert molded article according to claim 1 or 2, wherein the heating is performed by using a movable heater.

4. The method for producing an insert molded body according to claim 1 or 2, further comprising a step of preheating the metal member before being placed in the first mold.

5. A first mold for disposing a metal member; a second mold that can be arranged to face the first mold and that forms a space around the metal member for injecting a resin material; a heater for heating the metal member from the time the metal member is placed in a first mold until the time a second mold is placed opposite the first mold.

6. a first mold for disposing a metal member and a resin material; A second mold that can be arranged to face the first mold; a heater for heating the metal member from the time when the metal member and the resin material are placed in a first mold until the time when a second mold is placed opposite the first mold.

7. The insert molding apparatus according to claim 5 or claim 6, wherein the heater is movable.

8. The insert molding apparatus according to claim 5 or 6, further comprising a mechanism for preheating the metal member before it is placed in the first mold.

Citation Information

Patent Citations

  • Method for manufacturing metal insert resin composite molded article

    JP2001225352A