End sealing method
The method uses laser welding with controlled parameters to seal pipe ends and fastening holes, addressing the issues of water ingress and edge burn-through, ensuring secure fastening and maintaining surface flatness.
Patent Information
- Application Number
- JP2023047869
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-04
AI Technical Summary
Existing pipe sealing technologies fail to effectively seal fastening portions and fastening holes, leading to potential water ingress and corrosion, while also risking burn-through of the welded edge and compromising the flatness of the contact surface.
A method involving laser welding with specific parameters such as ring mode, defocus distances, pulse oscillation, and controlled angles to seal the flat end and fastening hole of a pipe without melting through the edges, ensuring a stable and flat contact surface.
Prevents water ingress and air leakage, maintains the flatness of the contact surface, and prevents burn-through, allowing for secure fastening and stable axial force without damaging adjacent components.
Smart Images

Figure 2024136682000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for sealing an end of a pipe part to prevent water from entering or air from entering or exiting the end of the pipe part. [Background technology]
[0002] Conventionally, Japanese Patent Application Laid-Open No. 2002-035850 (Patent Document 1) discloses a method of sealing a pipe in which an oblong beam of laser light is irradiated over the entire area of the sealed portion of the flattened and crushed end face of the tip of the pipe, thereby welding and sealing the entire sealed portion in one go, completely sealing the tip of an oil-filled pipe with a single shot of irradiation.
[0003] Furthermore, JP 2003-145220 A (Patent Document 2) discloses a method for manufacturing a pipe-shaped collision reinforcement material, which includes a sealing step in which both ends or their vicinity of a straight metal pipe material are crushed and the crushed portions are welded to seal both ends or their vicinity of the metal pipe material, thereby making the inside of the metal pipe material into an airtight space. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2002-035850 A [Patent Document 2] JP 2003-145220 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, the technology disclosed in Patent Document 1 is a method for sealing a pipe for filling oil. Therefore, there is no fastening portion for fastening the end of the pipe to other parts, and there is no fastening hole into which a bolt or the like is inserted. Therefore, there is no description about sealing the fastening hole. In addition, since the end of the pipe is not used as a contact surface with other parts, there is no description about the quality of the welded part. The same is true for the technology disclosed in Patent Document 2.
[0006] The present invention has been made in consideration of the above points, and has an object to provide an end sealing method that can completely prevent the intrusion of water, etc. into a pipe end by sealing the tip of a fastening part and also sealing the end face of a fastening hole into which a bolt, etc. is inserted. Another object of the present invention is to provide an end sealing method that produces a pipe part that does not burn through the edge part of the welded end face and maintains the flatness of the fastening seat surface that abuts against another part. [Means for solving the problem]
[0007] The end sealing method of the present invention includes the steps of: A method for sealing an end of a pipe part, the method comprising: a fastening portion having a fastening seat surface formed by flattening a pipe end and adapted to abut against another part; a flat end portion formed at a tip of the fastening seat surface; and a fastening hole provided in the fastening seat surface, a flat end sealing process in which an end surface of the flat end is irradiated with a laser beam in the axial direction of the pipe to weld the end surface of the flat end without melting the edge of the end surface; a fastening hole sealing process in which a laser beam is irradiated at an inclination angle to an end surface of the fastening hole to weld the end surface of the fastening hole, thereby sealing the end surface of the fastening hole without burning through the edge of the fastening hole; The present invention is characterized by comprising:
[0008] According to the end sealing method of the present invention, the end face of the flat end and the end face of the fastening hole are sealed by laser welding. Therefore, there is no ingress of water or ingress of air into or out of the pipe, let alone around the fastening hole. This prevents corrosion inside the pipe. In addition, there is no melting through of the edge of the end face due to laser welding. Therefore, when the fastening part is abutted against another part with a fastener such as a bolt to fasten it, the fastening part and the other part are in close contact and the other part is not damaged. In addition, the flatness of the fastening seat surface is maintained, so a stable axial force of the bolt can be obtained.
[0009] A preferred example of the end sealing method of the present invention is The laser light is irradiated in a ring mode in which the cross section of the laser light is ring-shaped.
[0010] A preferred example of the end sealing method of the present invention is The laser light is irradiated onto the end surface of the flat end portion at a defocus distance of 5 to 8% of the focal length of the condenser lens, The laser light is irradiated to the end face of the fastening hole with a defocus distance of 4 to 6% added to the focal length of the condenser lens.
[0011] A preferred example of the end sealing method of the present invention is The laser light is pulse-oscillated under control.
[0012] A preferred example of the end sealing method of the present invention is The condition of the pulse oscillation control is The laser light irradiated to the end surface of the flat end portion has an oscillation frequency of 20 to 30 Hz and a duty ratio of 20 to 30%, The laser light irradiated to the end surface of the fastening hole has an oscillation frequency of 5 to 10 Hz and a duty ratio of 10 to 20%.
[0013] A preferred example of the end sealing method of the present invention is The processing speed of the laser light is The laser light irradiated to the end surface of the flat end portion is 40 to 60 cm / min. The laser light is irradiated onto the end surface of the fastening hole at a rate of 10 to 20 cm / min.
[0014] A preferred example of the end sealing method of the present invention is The wall thickness of the pipe used in the pipe part is 1.2 to 1.6 mm; The output of the laser light irradiated onto the end surface of the flat end portion is 1700 to 1900 watts; The output of the laser light irradiated to the end surface of the fastening hole is 1400 to 1600 watts.
[0015] According to these preferred examples of the end sealing method of the present invention, the conditions of the laser light are optimized, making it possible to more effectively prevent the edges at the end faces from being burned through. Effect of the Invention
[0016] As described above, according to the end sealing method of the present invention, it is possible to completely prevent the intrusion of water, etc. into the pipe end by sealing the tip of the fastening part and also the fastening hole into which the bolt, etc. is inserted. In addition, it is possible to obtain a pipe part in which the edge part of the welded end face does not burn through and the flatness of the fastening seat surface that abuts against other parts is maintained. [Brief description of the drawings]
[0017] [Figure 1] FIG. 4 is a plan view of a fastening portion of the pipe part. [Diagram 2] FIG. 2 is a side view of a fastening portion of the pipe part. [Diagram 3] FIG. 2 is a front view of a fastening portion of the pipe part. [Figure 4] FIG. 1 is a diagram showing a schematic diagram of laser welding. [Diagram 5] FIG. 13 is a diagram illustrating a defocus distance. [Figure 6] FIG. 4 is a diagram illustrating pulse oscillation control of laser light. [Figure 7]10 is a diagram showing a schematic diagram of a state in which a flat end portion is irradiated with a pulse-oscillation-controlled laser beam. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, an embodiment of an end sealing method according to the present invention will be described in detail with reference to the accompanying drawings.
[0019] First, the structure of a pipe part 1, which is a workpiece, will be described with reference to Figs. 1 to 3. The pipe part 1 has a fastening portion 10 at its end, which is fastened to another part 40. The fastening portion 10 has a fastening seat surface 11, a flat end portion 12, a fastening hole 13, and a standing edge portion 14. The fastening seat surface 11 is formed by flattening the pipe end portion, with which the other part 40 and its wide surface ws (back surface) come into contact. The flat end portion 12 is provided at the tip of the fastening seat surface 11, and is formed in a straight line shape when viewed from the front. The fastening hole 13 is a through hole provided at the approximate center of the fastening seat surface 11, through which a bolt 41 or the like is passed. A seat portion 15 is provided around the fastening hole 13, against which a bolt 41, a nut, or a washer 42 comes into contact. However, the seat portion 15 does not differ in structure from the other parts of the fastening seat surface 11, and is represented by hatching for convenience. The vertical edge 14 is a rib-like portion provided on both the left and right ends of the fastening seat surface 11. The vertical edge 14 is formed halfway up the fastening seat surface 11. The material of the pipe part 1 used in this embodiment is, for example, a metal containing iron as a main component, such as steel. The wall thickness t (see FIG. 4(B)) of the pipe part 1 is 1.2 to 1.6 mm. Therefore, the thickness of the flat end portion 12 itself is 2.4 to 3.2 mm, which is twice the wall thickness t.
[0020] Next, an embodiment of an end sealing method will be described with reference to Figures 1 to 6. The end sealing method of this embodiment includes a flat end sealing step and a fastening hole sealing step. Either the flat end sealing step or the fastening hole sealing step can be performed first.
[0021] In the flat end sealing process, the end face of the flat end 12 is irradiated with a laser beam 31 emitted from a torch 30 in the axial direction of the pipe to weld the end face, and the end face 24 of the flat end 12 is sealed without burning through the edges 20, 21. The axial direction refers to the direction along the wide surface of the flat end 12, as shown by the arrow a in FIG. 2 and FIG. 4(A). In the fastening hole sealing process, the end face 25 of the fastening hole 13 is irradiated with a laser beam 31 emitted from a torch 30 at an inclination angle to weld the end face, and the end face 25 of the fastening hole 13 is sealed without burning through the edges 22, 23. The inclination angle is, as shown in FIG. 4(B), an angle θ with respect to the fastening seat surface 11 so that the laser beam 31 is not irradiated to the edge 22 of the fastening hole 13 on the opposite side to the side to be welded. In this embodiment, the angle θ is 40 degrees. It is preferable to make this angle θ small within a range that does not affect the end face edge 22 on the opposite side of the fastening hole 13. The reason is that when the angle θ becomes large, the laser light 31 irradiated to the end face 25 of the fastening hole 13 is irradiated over a wide area, which may cause the edges 22, 23 to burn through or make it impossible to ensure flatness of the fastening seat surface 11 around the fastening hole 13.
[0022] Next, detailed conditions of the flat end sealing process and the fastening hole sealing process will be explained. This is because, in the laboratory level or in small-scale production, the end faces 24, 25 of the pipe part 1 often have a relatively beautiful shape. Furthermore, by a craftsman holding a hand torch and performing appropriate welding according to each end face 24, 25, it is possible to seal the end faces 24, 25 without burning through the edges 20, 21, 22, 23. However, in an actual mass production line, the end faces 24, 25 of the pipe part 1 are often rough or there are gaps between the pressed upper and lower plates, and welding is performed using a robot that has been taught the same operation. For this reason, a certain degree of condition is required to seal the end faces 34, 25 without burning through the edges 20, 21, 22, 23. In this embodiment, the FLW3000EN manufactured by Amada Co., Ltd. is used as the laser welding machine.
[0023] In this embodiment, the ring mode is used in both the flat end sealing process and the fastening hole sealing process, in which the cross section of the laser light 31 is irradiated in a ring shape. This is because in the normal mode, in which the spot of the laser light 31 is circular, the center of the spot has the highest energy density. Therefore, even if the laser light 31 is irradiated with the defocus distances d1 and d2 described below, the shape of the end faces 24 and 25 may be distorted or the flatness of the fastening seat surface 11 may be roughened. On the other hand, by using the ring mode for the laser light 31, the energy density is made uniform over the entire spot of the laser light 31. As a result, sealing can be performed while maintaining the shape of the end faces 24 and 25 of the flat end 12 and the fastening hole 13, and the flatness of the fastening seat surface 11.
[0024] In addition, in both the flat end sealing process and the fastening hole sealing process, the laser light 31 is irradiated to the workpieces w1 and w2 in a state shifted from the focal distance. In detail, as shown in FIG. 5(A), in the flat end sealing process, the laser light 31 irradiated to the end face 24 (workpiece w1) of the flat end 12 is irradiated in a state in which the defocus distance d1 is added to the focal distance d of the condenser lens 32 by 5 to 8%. In this embodiment, the condenser lens 32 has a focal distance d of 300 mm, and the defocus distance d1 is 15 to 24 mm. This is because if the defocus distance d1 is short, the laser light 31 may melt the fastening seat surface 11 deeply, which may affect the flatness of the fastening seat surface 11. On the other hand, if the defocus distance d1 is too long, the end face edges 20 and 21 are likely to burn through, or the welding itself becomes difficult (similar to the fastening hole sealing process).
[0025] As shown in FIG. 5(B), in the fastening hole sealing process, the laser light 31 irradiated to the end surface 25 (workpiece w2) of the fastening hole 13 is irradiated in a state in which a defocus distance d2 of 4 to 6% is added to the focal distance d of the condenser lens 32. Since the focal distance d of the condenser lens 32 is also 300 mm, the defocus distance d2 is 12 to 18 mm. Since the laser light 31 is irradiated with a tilt angle θ (see FIG. 4(B)) in the fastening hole sealing process, the defocus distance d2 is measured at the center of the laser light 31. The spot diameter of the laser light 31 at the focal distance d of the condenser lens 32 of the laser welding machine used in this embodiment is about 0.24 mm. In addition, the spot diameter in this embodiment when the defocus distances d1 and d2 are added is about 2.5 mm.
[0026] Next, the pulse oscillation control of the laser light 31 will be described. In this embodiment, the laser light 31 irradiated in the flat end sealing process and the fastening hole sealing process is pulse oscillation controlled. The conditions will be described with reference to Figs. 6 and 7. Fig. 6 is a diagram showing the ON and OFF of the laser light 31, where the line is on the top when it is ON and the line is on the bottom when it is OFF. One ON and OFF is one cycle, and the ratio of the time that the light is ON in one cycle is represented as the duty ratio. For example, if the time of one cycle is 100 ms (milliseconds) and the ON time is 20 ms, the duty ratio is 20%.
[0027] In the flat end sealing process, the laser light 31 irradiated to the end surface 24 of the flat end 12 has an oscillation frequency of 20 to 30 Hz and a duty ratio of 20 to 30%. The processing speed of the laser light 31 irradiated to the end surface 24 of the flat end 12 is 40 to 60 cm / min. In this way, the oscillation frequency and the duty ratio are relatively low, and the processing speed is also relatively slow, so that the end 24 is reliably sealed while preventing the edges 20, 21 from being burned through. In addition, no weaving is performed when irradiating the laser light 31. For these reasons, the laser light 31 shows a trajectory such as that shown in FIG. 7.
[0028] In the fastening hole sealing process, the laser light 31 irradiated to the end face 25 of the fastening hole 13 has an oscillation frequency of 5 to 10 Hz and a duty ratio of 10 to 20%. In addition, the processing speed of the laser light 31 irradiated to the end face 25 of the fastening hole 13 is 10 to 20 cm / min. In this way, in the fastening hole sealing process, the oscillation frequency and duty ratio are lower than in the flat end sealing process, and the processing speed is also slower to prevent the edges 22, 23 of the end face 25 from being burned through. In addition, no weaving of the laser light 31 is performed in the fastening hole sealing process either.
[0029] Next, the output of the laser light 31 will be described. In the flat end sealing step, the output of the laser light 31 irradiated to the end face 24 of the flat end 12 is preferably 1700 to 1900 watts. In the fastening hole sealing step, the output of the laser light 31 irradiated to the end face 25 of the fastening hole 13 is preferably 1400 to 1600 watts. This is because if the output of the laser light 31 is too small, sealing will not be possible, and if the output is too large, the edges 20, 21, 22, and 23 of the end face will melt away.
[0030] As described above, according to the end sealing method of the present embodiment, even in a mass production line using a robot, the end face 24 of the flat end 12 and the end face 25 of the fastening hole 13 can be sealed. This completely prevents water from entering the pipe end, and prevents corrosion of the pipe part 1. In addition, the front and back of the fastening seat surface 11 that comes into contact with the other part 40 are not deformed by welding. Furthermore, the edges 20, 21, 22, and 23 do not melt through the end face 24 of the flat end 12 and the end face 25 of the fastening hole 13. Therefore, the fastening seat surface 11 and the other part 40 can be in close contact with each other, and the bolt 41 and the like do not float on the seat part 15. As a result, the fastening between the pipe part 1 and the other part 40 can be ensured.
[0031] In addition, by employing a ring mode for the laser beam 31 and irradiating the laser beam 31 with defocus distances d1 and d2 added, the heat input by the laser beam 31 becomes wide and shallow, and it is possible to effectively prevent the edges 20, 21, 22, and 23 from burning through at the end faces 24 and 25. Generally, in laser welding, a narrow range is deeply melted to produce welding with little distortion, but in this embodiment, the laser beam 31 is irradiated widely and shallowly to achieve both reliable sealing of the end faces 24 and 25 and prevention of the edges 20, 21, 22, and 23 from burning through.
[0032] In addition, the laser light 31 is pulse-oscillated, so that the oscillation frequency per unit time is relatively low and the duty ratio is relatively low. Furthermore, the welding processing speed is relatively slow. Therefore, after the end faces 24, 25 are melted and sealed, time for cooling can be taken. Furthermore, the output of the laser light 31 is set to be optimal for the wall thickness of the pipe. As a result, it is possible to further prevent the edges 20, 21, 22, 23 from being burned through at the end faces 24, 25. [Explanation of symbols]
[0033] 1. Pipe parts, 10... fastening section, 11... fastening seat surface, 12... flat end, 13... fastening hole, 14... standing edge section, 15... seat surface section, ws... wide surface, 20, 21·· Edge (flat end), 22, 23·· Edge (fastening hole), 24·· End face (flat end), 25·· End face (fastening hole), 30 torch, 31 laser light, 32 focusing lens 40... Other parts, 41... Bolt, 42... Washer, w1, w2: Work,
Claims
1. A method for sealing an end of a pipe part, the method comprising: a fastening portion having a fastening seat surface formed by flattening a pipe end and adapted to abut against another part; a flat end portion formed at a tip of the fastening seat surface; and a fastening hole provided in the fastening seat surface, a flat end sealing process in which an end surface of the flat end is irradiated with a laser beam in the axial direction of the pipe to weld the end surface of the flat end without melting the edge of the end surface; a fastening hole sealing process in which a laser beam is irradiated at an inclination angle to an end surface of the fastening hole to weld the end surface of the fastening hole, thereby sealing the end surface of the fastening hole without burning through the edge of the fastening hole; An end sealing method comprising:
2. The method for sealing edges according to claim 1 , wherein the laser light is irradiated in a ring mode in which the cross section of the laser light is ring-shaped.
3. The laser light is irradiated onto the end surface of the flat end portion in a state where a defocus distance is added to a condenser lens focal length of 5 to 8%; The end sealing method according to claim 1 or 2, wherein the laser light irradiated to the end face of the fastening hole is irradiated at a defocusing distance of 4 to 6% of the focal length of a focusing lens.
4. The method for sealing an edge according to claim 3, wherein the laser light is pulse-oscillated.
5. The condition of the pulse oscillation control is The laser light irradiated to the end surface of the flat end portion has an oscillation frequency of 20 to 30 Hz and a duty ratio of 20 to 30%, 5. The end sealing method according to claim 4, wherein the laser light irradiated to the end surface of the fastening hole has an oscillation frequency of 5 to 10 Hz and a duty ratio of 10 to 20%.
6. The processing speed of the laser light is The laser light irradiated to the end surface of the flat end portion is 40 to 60 cm / min, The method for sealing an end portion according to claim 5, wherein the laser light irradiated to the end surface of the fastening hole is 10 to 20 cm / min.
7. The wall thickness of the pipe used in the pipe part is 1.2 to 1.6 mm; The output of the laser light irradiated onto the end surface of the flat end portion is 1700 to 1900 watts; The method for sealing an end portion according to claim 6, wherein the output of the laser light irradiated to the end surface of the fastening hole is 1400 to 1600 watts.
Citation Information
Patent Citations
JP1975029149A
Sealing method for oil-filling pipe of liquid-seal type pressure sensor
JP2002035850A
Method of sealing tube plate and heat transfer tube of heat exchanger and heat exchanger
JP2013230476A
Pipe part
JP2017087251A
Method for manufacturing tubular reinforcing material against collision
JP2003145220A