Light-emitting element and manufacturing method for the same

The manufacturing method for UVC light emitting elements with Ru p-electrodes and V/Al/Ti n-electrodes, combined with a heat treatment process, addresses the low power efficiency issue by enhancing light extraction and reducing contact resistance, resulting in improved power efficiency.

JP2024136698AInactive Publication Date: 2024-10-04TOYODA GOSEI CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023047893
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-04
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

UVC light emitting devices have low power efficiency, necessitating improvements in light extraction efficiency and reduction of forward voltage, which have been difficult to achieve.

Method used

A manufacturing method for UVC light emitting elements using Group III nitride semiconductors with specific electrode configurations and materials, including a p-electrode made of Ru and an n-electrode with a V/Al/Ti structure, along with a heat treatment process to reduce contact resistance and activate p-type impurities, ensuring a high ratio of p-electrode area to total area of the hole and p-layer.

Benefits of technology

The solution increases ultraviolet ray reflection, enhances light extraction efficiency, and reduces contact resistance, thereby improving the power efficiency of the UVC light emitting elements.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024136698000001_ABST
    Figure 2024136698000001_ABST
Patent Text Reader

Abstract

To provide a manufacturing method for a light-emitting element of UVC with high power efficiency.SOLUTION: A manufacturing method for a light-emitting element including Group-III nitride semiconductor containing Al and having an emission wavelength of 200 to 280 nm includes a p-electrode forming step of forming a p-electrode 15 including a Ru layer in contact with a p-layer 14 on the p-layer 14, an n-electrode forming step of forming an n-electrode 16 including a V layer of V with a thickness of 5 nm or more and 15 nm or less in contact with an n-layer 11 on the n-layer 11 exposed at a bottom surface of a hole 23, and an Al layer of Al on and in contact with the V layer, and a thermal processing step of performing a thermal process at 500 to 650°C for 1 to 10 minutes to reduce the contact resistance of the p-electrode 15 and the n-electrode 16 and activate p-type impurities in the p-layer 14. The patterns of the hole 23 and the p-electrode 15 are set so that the ratio of the area of the p-electrode 15 to the total area of the hole 23 and the p-layer 14 becomes 70% or more.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a light-emitting device and a method for manufacturing the same. [Background technology]

[0002] In recent years, UV LEDs have been attracting attention for their use in sterilizing and disinfecting water and air, and there has been active research and development into improving the efficiency of UV LEDs.

[0003] In conventional light-emitting devices made of III-nitride semiconductors, ITO and Ni / Au are widely used as the p-electrode in contact with the p-layer. These materials have low reflectance in UVC (200 to 280 nm). Therefore, in UVC light-emitting devices, the use of Rh or Ru, which has high reflectance, as the p-electrode has been considered (Patent Document 1). In addition, Ti / Al is widely used as the n-electrode in contact with the n-layer, and it is also known to use V as in Patent Document 2. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2020-64955 A [Patent Document 2] JP 2003-77862 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, UVC light-emitting elements have low power efficiency, and there has been a demand for improvement. To increase power efficiency, it is necessary to simultaneously improve the light extraction efficiency and reduce the forward voltage Vf, which has been difficult to achieve.

[0006] The present invention has been made in view of the above background, and aims to provide a UVC light-emitting element with high power efficiency and a method for manufacturing the same. [Means for solving the problem]

[0007] One aspect of the present invention is A method for producing a light-emitting device made of an Al-containing Group III nitride semiconductor having an emission wavelength of 200 to 280 nm, comprising the steps of: a semiconductor layer formation step of laminating an n-layer, a light-emitting layer, and a p-layer on a substrate in this order; a hole forming step of forming holes in a predetermined region on the surface of the p-layer, the holes having a depth reaching the n-layer; a p-electrode formation step of forming a p-electrode on the p-layer, the p-electrode having a Ru layer in contact with the p-layer; an n-electrode formation process for forming an n-electrode on the n-layer exposed at the bottom of the hole, the n-electrode having a V layer of 5 nm to 15 nm in thickness in contact with the n-layer and made of V or a metal mainly composed of V, and an Al layer of Al or a metal mainly composed of Al in contact with the V layer; a heat treatment step of performing a heat treatment at a temperature of 500 to 650° C. for 1 to 10 minutes to reduce the contact resistance of the p-electrode and the n-electrode and to activate the p-type impurity of the p-layer; The method for manufacturing a light-emitting device includes setting a pattern of the hole and the p-electrode so that a ratio of an area of ​​the p-electrode to a total area of ​​the hole and the p-layer is 70% or more.

[0008] Another aspect of the present invention is A light emitting device made of an Al-containing Group III nitride semiconductor having an emission wavelength of 200 to 280 nm, A substrate; A semiconductor layer in which an n-layer, a light-emitting layer, and a p-layer are stacked in this order on a substrate; a hole provided in a predetermined region on the surface of the p-layer and having a depth reaching the n-layer; a p-electrode having a Ru layer provided on and in contact with the p-layer; a hole provided on the n-layer exposed at the bottom surface of the hole and positioned in contact with the n-layer; x or Al having a higher Al composition than the n-layer y Ga 1-y N xand a second layer located on and in contact with the first layer, the second layer being made of a metal mainly containing Al and containing V, and the second layer having a thickness of 50 nm or more and 500 nm or less. In the light-emitting device, the patterns of the holes and the p-electrode are set so that the ratio of the area of ​​the p-electrode to the total area of ​​the holes and the p-layer is 70% or more. Effect of the Invention

[0009] According to the above embodiment, by increasing the area of ​​the p-electrode made of Ru, the reflection of ultraviolet light by the p-electrode can be increased, and the light extraction efficiency can be improved. In addition, both the p-electrode and the n-electrode have low contact resistance, and the forward voltage can be reduced. Therefore, the power efficiency of the UVC light-emitting element can be improved. [Brief description of the drawings]

[0010] [Figure 1] FIG. 2 is a cross-sectional view perpendicular to a substrate, showing the configuration of a light-emitting element according to an embodiment. [Diagram 2] FIG. 2 is a diagram showing a planar pattern of an electrode. [Diagram 3] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 4] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Diagram 5] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 6] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 7] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 8] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 9] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 10] 5A to 5C are diagrams illustrating a manufacturing process of the light emitting element according to the embodiment. [Figure 11] 1 is a graph showing IV characteristics of a light-emitting element. [Figure 12] A graph (scatter plot) showing the emission wavelength and power efficiency of a light-emitting element. [Figure 13] FIG. 13 is a diagram showing an electrode pattern of the first modified example. [Figure 14] FIG. 11 is a cross-sectional view perpendicular to the substrate, showing a configuration of Modification 2 of the light-emitting device in the embodiment. [Figure 15] FIG. 13 is a diagram showing an electrode pattern of Modification 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] The method for manufacturing a light-emitting device is a method for manufacturing a light-emitting device made of a group III nitride semiconductor containing Al and having an emission wavelength of 200 to 280 nm. The method includes a semiconductor layer forming step of sequentially stacking an n-layer, a light-emitting layer, and a p-layer on a substrate, a hole forming step of forming a hole in a predetermined region of the surface of the p-layer to a depth reaching the n-layer, a p-electrode forming step of forming a p-electrode having a Ru layer in contact with the p-layer on the p-layer, an n-electrode forming step of forming an n-electrode on the n-layer exposed at the bottom of the hole, the n-electrode having a V layer that is in contact with the n-layer and is a metal containing V or V as a main component and has a thickness of 5 nm to 15 nm, and an Al layer that is a metal containing Al as a main component and is in contact with the V layer, and a heat treatment step of performing a heat treatment at a temperature of 500 to 650°C for 1 to 10 minutes to reduce the contact resistance of the p-electrode and the n-electrode and to activate the p-type impurity of the p-layer. The patterns of the holes and the p-electrode are set so that the ratio of the area of ​​the p-electrode to the total area of ​​the holes and the p-layer is 70% or more.

[0012] A plurality of the holes may be formed, the holes may be arranged in a square lattice pattern, a regular triangular lattice pattern, or a honeycomb pattern, and the n-electrode may be formed on the bottom surface of each of the holes.

[0013] After the heat treatment step, the method may further include a pn electrode formation step of forming a first pn electrode and a second pn electrode on the p electrode and the n electrode, respectively; a protective film formation step of forming a protective film, which is an insulator, so as to cover the entire top surface of the element; and a pad electrode formation step of providing holes at predetermined positions in the protective film and forming, on the protective film, a p pad electrode connected to the first pn electrode through the hole, and an n pad electrode connected to the second pn electrode through the hole and spaced apart from the p pad electrode.

[0014] The light-emitting device is made of a group III nitride semiconductor containing Al and has an emission wavelength of 200 to 280 nm. The light-emitting device also includes a substrate, a semiconductor layer in which an n-layer, a light-emitting layer, and a p-layer are laminated on the substrate in this order, a p-electrode having a hole provided in a predetermined region on the surface of the p-layer, the hole having a depth reaching the n-layer, and a Ru layer provided on and in contact with the p-layer, and an AlN x or Al having a higher Al composition than the n-layer y Ga 1-y N x and an n-electrode having a first layer having a thickness of 1 nm or more and 3 nm or less, and a second layer located on and in contact with the first layer, made of a metal mainly containing Al and containing V, and having a thickness of 50 nm or more and 500 nm or less. The patterns of the holes and the p-electrode are set so that the ratio of the area of ​​the p-electrode to the total area of ​​the holes and the p-layer is 70% or more.

[0015] A plurality of the holes may be formed, the holes may be arranged in a lattice pattern, and the n-electrode may be formed on the bottom surface of each of the holes.

[0016] The device may further include a first pn electrode and a second pn electrode provided on the p electrode and the n electrode, respectively, a protective film which is an insulator covering the entire top surface of the element, a p pad electrode provided on the protective film and connected to the first pn electrode through a hole provided in the protective film, and an n pad electrode provided on the protective film, connected to the second pn electrode through a hole provided in the protective film, and provided at a distance from the p pad electrode.

[0017] (Embodiment) Fig. 1 is a diagram showing the configuration of a light-emitting element in an embodiment, and is a cross-sectional view perpendicular to a substrate. Fig. 2 is a diagram showing a planar pattern of an electrode of the light-emitting element in an embodiment. The light-emitting element in the embodiment is a flip-chip type ultraviolet light-emitting element, and emits light having a UVC emission wavelength of, for example, 200 to 280 nm.

[0018] 1. Structure of the light-emitting element 1, the light-emitting device in the embodiment has a substrate 10, an n-layer 11, a light-emitting layer 12, an electron blocking layer 13, a p-layer 14, a p-electrode 15, an n-electrode 16, pn-electrodes 17A and 17B, a protective film 18, a reflective film 19, a p-pad electrode 20, an n-pad electrode 21, and an anti-reflective film 22. Each component will be described below.

[0019] The substrate 10 is a substrate made of sapphire with a c-plane as the main surface. Any material other than sapphire may be used as long as it has a high transmittance for the emission wavelength and allows a Group III nitride semiconductor to be grown thereon.

[0020] An anti-reflection film 22 is provided on the back surface of the substrate 10 (the surface opposite to the n-layer 11 side, the light extraction side). By providing the anti-reflection film 22, ultraviolet light is prevented from being reflected on the back surface of the substrate 10 and returning to the element side, improving light extraction. The anti-reflection film 22 is, for example, SiO2 with a thickness of ¼ of the emission wavelength.

[0021] The n-layer 11 is located on the substrate 10 via a buffer layer (not shown). The n-layer 11 is made of n-AlGaN. The n-type impurity is Si, and the Si concentration is 5×10 18 ~5×10 19 / cm 3 The n-layer 11 may be composed of multiple layers.

[0022] The light emitting layer 12 is located on the n-layer 11. The light emitting layer 12 has an MQW structure in which well layers and barrier layers are alternately and repeatedly stacked. The number of repetitions is, for example, 2 to 5. The well layers are made of AlGaN, and the Al composition is set according to the desired emission wavelength. The barrier layers are AlGaN with a higher Al composition than the well layers. They may also be AlGaInN with a higher band gap energy than the well layers. The light emitting layer 12 may also have an SQW structure.

[0023] The electron blocking layer 13 is located on the light emitting layer 12. The electron blocking layer 13 is made of p-AlGaN having a higher Al composition ratio than the barrier layer of the light emitting layer 12. The electron blocking layer 13 prevents the electrons injected from the n-electrode 16 from diffusing beyond the light emitting layer 12 toward the p-layer 14.

[0024] The p-layer 14 is located on the electron blocking layer 13. The p-layer 14 is made of p-AlGaN. In the light emitting device of the embodiment, all the semiconductor layers from the n-layer 11 to the p-layer 14 are made of AlGaN, which suppresses the absorption of ultraviolet light by the semiconductor layers. The Al composition of the p-layer 14 is, for example, 5 to 80%. The p-type impurity is Mg. The Mg concentration is 1×10 19 / cm 3 That is all. The p-layer 14 may be composed of multiple layers with different Al compositions or Mg concentrations. In that case, the layer in contact with the p-electrode 15 may be p-AlGaN with an Al composition of 5 to 80%. The p-layer 14 is not limited to AlGaN, and may be any III-nitride semiconductor containing Al, such as AlGaInN.

[0025] Holes 23 are formed in a portion of the surface of p-layer 14, with a depth reaching n-layer 11. Holes 23 are dot-shaped, and a plurality of holes 23 are arranged in a lattice pattern (see FIG. 2). However, holes 23 are not provided in the region below p-electrode 15. N-layer 11 is exposed at the bottom of holes 23. By arranging holes 23 for exposing n-layer 11 in a dot-shaped pattern, uniformity of light emission within the surface is ensured, while the reduction in the light-emitting area (area of ​​p-layer 14) due to holes 23 is minimized, thereby improving light output.

[0026] The planar pattern of each hole 23 is, for example, a circle. Alternatively, it may be a polygon such as a regular hexagon. In the case of a regular hexagon, it is preferable that the side surface of the hole 23 be an m-plane. The arrangement pattern of the holes 23 is a regular triangular lattice. Alternatively, it may be, for example, a square lattice or a honeycomb pattern.

[0027] The p-electrode 15 is provided on the p-layer 14. The p-electrode 15 is provided on the surface of the p-layer 14 excluding areas where the holes 23 are not provided and the vicinity of the edges of the p-layer 14 (see FIG. 2), thereby making the light-emitting area large. The p-electrode 15 is a reflective electrode that reflects ultraviolet light emitted from the light-emitting layer 12 toward the substrate 10 to increase the light extraction efficiency. The material of the p-electrode 15 is Ru. An alloy mainly composed of Ru may also be used. Ru has high reflectance in UVC light and has low contact resistance with the p-AlGaN p-layer 14, making it suitable for the p-electrode 15 in a UVC light-emitting element.

[0028] The ratio of the area of ​​the p electrode 15 to the area of ​​the top surface of the element (the total area of ​​the holes 23 and the p layer 14) is set to 70% or more. The planar patterns of the holes 23 and the p electrode 15 are set to satisfy this. For example, the diameter, number of arrangements, and arrangement intervals of the holes 23 are adjusted. By increasing the area of ​​the p electrode 15 made of Ru, it is possible to increase the reflection of ultraviolet light by the p electrode 15 and improve the light extraction efficiency. It is more preferable that the ratio is 75% or more.

[0029] The n-electrodes 16 are provided on the n-layer 11 exposed at the bottom of each hole 23. Therefore, the n-electrodes 16 are also arranged in a dot pattern (see FIG. 2). The material of the n-electrodes 16 is a structure obtained by heat-treating V / Al / Ti. Other materials that can be used include Ti / Al / Ti. The structure obtained by heat-treating V / Al / Ti is specifically AlN x The structure is one in which a layer made of Al, a layer made of a metal mainly containing Al and also V and Ti, and a layer made of Ti are laminated in this order.

[0030] AlN xThe layer consisting of... has a thickness of 1 to 3 nm. x is, for example, 0.4 to 0.7. Also, x may decrease as it moves away from the n-layer 11 in the thickness direction. In this case, the average of x in the thickness direction is 0.4 to 0.7. Also, there may be diffusion of Ga from the n-layer 11 side. In that case, it is Al with an Al composition ratio higher than that of the n-layer 11. y Ga 1-y N x (0.4 ≤ x ≤ 0.7). If the Al composition ratio of the n-layer 11 is a, then a < y ≤ 1. y is, for example, 0.7 or more. Also in this case, x may decrease as it moves away from the n-layer 11 in the thickness direction, and y may increase as it moves away from the n-layer 11 in the thickness direction.

[0031] The layer made of a metal mainly composed of Al and containing V and Ti has a thickness of 50 to 500 nm. The ratios of Al, V, and Ti are, for example, 50 to 85 mol% for Al, 5 to 20 mol% for V, and 10 to 30 mol% for Ti.

[0032] In the n-electrode 16 with the above structure, the contact resistance to the n-layer 11 is reduced. For example, the contact resistivity of the n-electrode 16 to the n-layer 11 is 4×10 ―4 Ω·cm 2 or less. The reason is, firstly, considered to be that the layer consisting of AlN x functions as a good contact layer to the n-layer 11. Secondly, it is considered that nitrogen vacancies are generated on the surface of the n-layer 11 and the contact resistance is reduced due to n-type formation.

[0033] The layer made of Ti is provided as a cover to suppress the evaporation of Al in the n-electrode 16 during alloying. In addition to Ti, TiN, Ni, Pt, Au, etc. can also be used.

[0034] Pn electrodes 17A and 17B are provided on p-electrode 15 and n-electrode 16, respectively. The planar pattern of pn electrode 17A is similar to that of p-electrode 15. The planar pattern of pn electrode 17B is similar to that of n-electrode 16, and is a pattern in which a plurality of dots are arranged. The material of pn electrodes 17A and 17B is, for example, Ti / Ni / Au / Al.

[0035] The protective film 18 is provided so as to cover the entire upper surface of the element, that is, it is provided continuously on the side surfaces and surface of the p-electrode 15 and the n-electrode, the surface and side surfaces of the semiconductor layer, the side surfaces of the element isolation trench 26, and the inside of the hole 23.

[0036] The protective film 18 is an insulator, such as SiO2. Other materials that can be used include SiN, Al2O3, TiO2, and AlN. A laminate of a plurality of materials may also be used.

[0037] A reflective film 19 made of Al is provided in the protective film 18. The reflective film 19 is provided over the entire surface except for areas where holes 24 and 25, which will be described later, exist. The reflective film 19 reflects light toward the substrate 10, improving the light extraction efficiency. It also improves the heat dissipation of the protective film 18. The reflective film 19 is embedded in the protective film 18 to prevent migration.

[0038] The material of the reflective film 19 is not limited to Al, but may be any material having a high reflectance at the emission wavelength, or may be an alloy mainly containing Al.

[0039] The p-pad electrode 20 and the n-pad electrode 21 are provided spaced apart on the protective film 18. The p-pad electrode 20 is connected to the p-n electrode 17A through a hole 24 formed in the protective film 18. The n-pad electrode 21 is connected to each of the p-n electrodes 17B through holes 25 formed in the protective film 18. The material of the p-pad electrode 20 and the n-pad electrode 21 is, for example, Ti / Pt / Au / AuSn.

[0040] The planar patterns of the p pad electrode 20 and the n pad electrode 21 are formed by dividing a rectangular pattern slightly inside the rectangular pattern of the element in half at the corner of the rectangle by a linear region of width W along a straight line L that forms an angle of 45° with respect to the side of the rectangle, with the one side forming an isosceles right triangle pattern being the p pad electrode 20 and the other (a pentagon with the corners of the rectangle rounded off) being the n pad electrode 21.

[0041] The angle of the linear region is not limited to 45°, but is preferably close to 45° in order to maximize the sum of the areas of the p-pad electrode 20 and the n-pad electrode 21, and is preferably, for example, 30 to 60°, and more preferably 40 to 50°.

[0042] Moreover, the position and width W of the linear region are preferably set so that the sum of the areas of the p pad electrode 20 and the n pad electrode 21 is 90% or more of the light emitting area (area of ​​the p electrode 15). Of course, the width W is set so as not to cause a short circuit between the p pad electrode 20 and the n pad electrode 21. For example, the width W is 100 μm or more. Moreover, the p pad electrode 20 is set to a size that allows good bonding to the submount side. For example, the lengths of the two equal sides in the right-angled isosceles triangle of the p pad electrode 20 are 200 μm or more.

[0043] By configuring the planar patterns of the p-pad electrode 20 and the n-pad electrode 21 as described above, the sum of the areas of the p-pad electrode 20 and the n-pad electrode 21 can be made large, thereby improving heat dissipation.

[0044] As described above, in the light emitting device of the embodiment, Ru is used as the material of the p electrode 15, and the ratio of the area of ​​the p electrode 15 to the area of ​​the upper surface of the device is set to 70% or more, which can improve light extraction. In addition, both the p electrode 15 and the n electrode 16 have low contact resistance, which can reduce the forward voltage. Therefore, the power efficiency of the light emitting device can be improved.

[0045] 2. Light-emitting device manufacturing process A manufacturing process of the light emitting device according to the embodiment will be described with reference to the drawings.

[0046] First, a substrate 10 made of sapphire is prepared. Then, an n-layer 11, a light-emitting layer 12, an electron blocking layer 13, and a p-layer 14 are formed in this order on the substrate 10 by MOCVD (see FIG. 3).

[0047] Next, predetermined regions of p-layer 14 are dry etched to form a plurality of holes 23 having a depth reaching n-layer 11 (see FIG. 4).

[0048] Next, p-electrode 15 is formed on p-layer 14 by sputtering or vapor deposition (see FIG. 5). Next, a V layer, an Al layer, and a Ti layer are laminated in this order by sputtering or vapor deposition on n-layer 11 exposed at the bottom of hole 23 to form n-electrode 16 (see FIG. 6). Although n-electrode 16 may be formed before p-electrode 15, in order to form p-electrode 15 while the surface of p-layer 14 is as clean as possible, in this embodiment, p-electrode 15 is formed first.

[0049] Next, a heat treatment is performed at a temperature of 500 to 650° C. for 1 to 10 minutes. The heat treatment is preferably performed under reduced pressure in an inert gas atmosphere such as nitrogen, for example, at a pressure of 1×10 2 ~1×10 4 The heat treatment temperature is preferably 500 to 560°C.

[0050] This heat treatment serves both as a Mg activation treatment for p-layer 14 and as a reduction in the contact resistance of p-electrode 15 and n-electrode 16 .

[0051] In the embodiment, the heat treatment temperature is reduced by using V / Al / Ti as n-electrode 16, and the number of heat treatments is reduced by simultaneously performing the Mg activation treatment of p-layer 14 and the reduction of the contact resistance of p-electrode 15 and n-electrode 16 in a common manner. As a result of lowering the heat treatment temperature and reducing the number of heat treatments, it is possible to suppress deterioration of the electrical characteristics of the light-emitting element.

[0052] Here, the n-electrode 16 changes to the following structure by the above heat treatment. In the V / Al / Ti n-electrode 16, the V diffuses into the Al, but does not diffuse into the n-layer 11 or Ti. As a result of this diffusion, the V layer disappears. Also, the Al in the V / Al / Ti reacts with the N in the n-layer 11, and AlN is formed at the interface between the n-layer 11 and the Al layer. x It is believed that V acts like a catalyst to promote the reaction between Al and N. As a result of this heat treatment, the structure of the n-electrode 16 becomes AlN. x The structure changes to a three-layer structure consisting of a layer made of Al, a layer made of metal mainly containing V and Ti, and a layer made of Ti.

[0053] By changing the n-electrode 16 to such a structure, the contact resistance of the n-electrode 16 with the n-layer 11 is reduced. The reasons for this are as already mentioned. That is, first, AlN x It is believed that the layer made of AlN functions as a good contact layer for the n-layer 11. x It is believed that the formation of nitrogen vacancies in n layer 11 facilitates the conversion of n layer 11 to n-type.

[0054] Next, pn electrodes 17A and 17B are formed on p-electrode 15 and n-electrode 16, respectively, by sputtering or vapor deposition (see FIG. 7).

[0055] Next, the element isolation trenches 26 are formed. The element isolation trenches 26 are deep enough to expose the substrate 10. Next, the protective film 18 is formed to cover the entire upper surface of the element (see FIG. 8). The protective film 18 is formed by deposition, sputtering, CVD, or the like. Sputtering and CVD are preferred because of the denseness of the film.

[0056] Next, a reflective film 19 made of Al is formed on the protective film 18 except for the areas where holes 24 and 25 are to be formed later (see FIG. 9). The reflective film 19 is formed by deposition or sputtering, and patterned by wet etching.

[0057] Next, the protective film 18 is formed again on the protective film 18 and the reflective film 19 (see FIG. 10). This results in a structure in which the reflective film 19 is embedded in the protective film 18. It is preferable that the protective film 18 is not formed on the bottom surface of the element isolation groove 26, and that the protective film 18 is separated for each element. This is to prevent force from being applied to the protective film 18 and to prevent fluctuations in the stress of the protective film 18 when dividing the device into individual elements.

[0058] Next, a predetermined region of the protective film 18 is dry etched to form holes 24 and 25 reaching the pn electrodes 17A and 17B. Then, the p pad electrode 20 and the n pad electrode 21 are formed on the protective film 18, respectively, so that the p pad electrode 20 is connected to the pn electrode 17A through the hole 24, and the n pad electrode 21 is connected to the pn electrode 17B through the hole 25. The patterns of the p pad electrode 20 and the n pad electrode 21 are as shown in FIG. 2. The p pad electrode 20 and the n pad electrode 21 are formed by deposition or sputtering, and patterned by lift-off. Next, an anti-reflection film 22 is formed on the back surface of the substrate 10. Next, the substrate 10 is divided into individual elements. In this manner, the light-emitting device in the embodiment shown in FIG. 1 is manufactured.

[0059] 3. Experimental Results Various experimental results relating to the embodiment will be described.

[0060] (Experiment 1) A light emitting device according to the embodiment was fabricated with an emission wavelength of 275 nm and Ru as the p-electrode 15. For comparison, a light emitting device was also fabricated in which the p-electrode 15 was changed from Ru to Rh.

[0061] Fig. 11 is a graph showing the IV characteristics of the light-emitting device. As shown in Fig. 11, it was found that the driving voltage can be reduced more when Ru is used as the p-electrode 15 than when Rh is used. This is because Ru has a lower contact resistance with the p-layer 14 than Rh.

[0062] (Experiment 2) A number of light-emitting devices according to the embodiment were fabricated in which the composition of the light-emitting layer 12 was set so as to give an emission wavelength of 275 nm, and the p-electrode 15 was made of Ru. For comparison, a number of light-emitting devices were also fabricated in which the material of the p-electrode 15 was changed from Ru to Rh.

[0063] FIG. 12 is a graph (scatter plot) showing the emission wavelength and power efficiency of the light-emitting element. The power efficiency is a value normalized by setting the average power efficiency when the p-electrode 15 is Rh as 100%. As shown in FIG. 12, it was found that the power efficiency tends to be higher when Ru is used as the p-electrode 15 than when Rh is used. This is thought to be because the ultraviolet reflectance is high for both Ru and Rh, but the contact resistance is lower for Ru than for Rh. It was also found that the variation in power efficiency is smaller for Ru than for Rh. The results of Experiments 1 and 2 showed that Ru is more preferable than Rh as the p-electrode 15 for UVC light-emitting elements.

[0064] 4. Modifications of the embodiment Various modifications of the light emitting element in the embodiment will be described.

[0065] (Variation 1) The electrode pattern shown in the embodiment is just an example, and other patterns may be used as long as the ratio of the area of ​​the p-electrode 15 to the area of ​​the upper surface of the element is 70% or more. For example, a pattern like the following modified example 1 may be used.

[0066] Variation 1 of the light-emitting element in the embodiment has a changed electrode pattern as follows: instead of the p-electrode 15, n-electrode 16, p-pad electrode 120, n-pad electrode 121, and hole 23 in the embodiment, a p-electrode 115, an n-electrode 116, a p-pad electrode 120, an n-pad electrode 121, and a hole 123 are provided.

[0067] Fig. 13 is a diagram showing an electrode pattern of a first modified example of a light emitting device in an embodiment. As shown in Fig. 13, the p-pad electrode 120 and the n-pad electrode 121 are patterns obtained by dividing a pattern slightly inside the rectangular pattern of the element into two by a strip-shaped linear region along a straight line parallel to the side of the rectangle. The linear region is located near one side of the rectangle, and of the two patterns divided by the linear region, the one with the smaller area is the p-pad electrode 120, and the one with the larger area is the n-pad electrode 121.

[0068] Holes 123 provided in place of holes 23 are located below n-pad electrode 121, and a plurality of holes 123 are arranged in a triangular lattice pattern. They are not arranged in the region below p-pad electrode 120. An n-electrode 116 and a pn-electrode 17B are provided in this order on the bottom surface of hole 123, and pn-electrode 17B and n-pad electrode 121 are connected via holes 25 opened in protective film 18. The pattern of holes 25 is almost the same as the pattern of n-electrode 116, and is omitted from FIG. 13.

[0069] Moreover, p electrode 115 provided in place of p electrode 15 has a pattern obtained by removing holes 123 from the pattern of p layer 14. A pn ​​electrode 17A is provided on p electrode 115, and pn electrode 17A is connected to p pad electrode 120 via holes 24. Holes 24 connecting pn electrode 17A to p pad electrode 120 are circular, and a plurality of holes 24 are arranged along the sides of a rectangle. The circular pattern outside the circle of holes 24 indicates the boundary of reflective film 19.

[0070] (Variation 2) Modification 2 of the light emitting device in the embodiment has a different electrode structure and electrode pattern, and is otherwise similar to the light emitting device in the embodiment.

[0071] Fig. 14 is a diagram showing the configuration of the light emitting device according to the embodiment, which is a cross-sectional view perpendicular to the main surface of the substrate. Fig. 15 is a diagram showing the electrode pattern of the light emitting device according to the embodiment, which is a cross-sectional view perpendicular to the main surface of the substrate. Fig. 15 shows the planar patterns of the p-electrode 215, the n-electrode 216, the p-pad electrode 220, and the n-pad electrode 221.

[0072] 14 and 15, holes 223 are provided instead of holes 23. Holes 223 are circular and arranged in a regular triangular lattice pattern. N-electrode 216 and pn-electrode 217B are provided in this order on the bottom surface of holes 223. Unlike the cases of FIGS. 2 and 13, holes 223 are arranged over the entire surface, and holes 223 are also provided below p-pad electrode 220. p-electrode 215 is formed in a pattern obtained by excluding the area of ​​holes 223 from the rectangular pattern of p-layer 14. In addition, pn-electrode 217B is provided on p-electrode 215 in the same planar pattern as p-electrode 215.

[0073] Moreover, a protective film 218 is provided in place of the protective film 18. The protective film 218 has a structure in which a first protective film 218A and a second protective film 218B are laminated in this order. The first protective film 218A and the second protective film 218B may be made of the same material or different materials.

[0074] Intermediate electrodes 219A and 219B are provided between first protective film 218A and second protective film 218B. Note that intermediate electrodes 219A and 219B are not shown in Fig. 15. Intermediate electrode 219A is connected to p-electrode 15 via a hole provided in first protective film 218A. Intermediate electrode 219B is connected to each dot-shaped n-electrode 16 via a hole provided in first protective film 218A. These holes are also not shown in Fig. 15.

[0075] The p-pad electrode 220 and the n-pad electrode 221 are provided on the protective film 218B with a space therebetween. The p-pad electrode 220 is connected to the intermediate electrode 219A through a hole formed in the second protective film 218B. The n-pad electrode 221 is connected to the intermediate electrode 219B through a hole formed in the second protective film 218B. These holes are also omitted in FIG. 15. As shown in FIG. 15, the p-pad electrode 220 and the n-pad electrode 221 are patterns obtained by dividing a pattern slightly inside the rectangular pattern of the element into two equal parts by a strip-shaped linear region along a straight line parallel to the side of the rectangle.

[0076] In the second modification, the holes 223 can be arranged over the entire surface, improving the in-plane uniformity of light emission. In addition, intermediate electrodes 219A and 219B are interposed between the p-electrode 15 and the n-electrode 16 and the p-pad electrode 220 and the n-pad electrode 221, allowing the patterns of the p-pad electrode 220 and the n-pad electrode 221 to be freely set. [Explanation of symbols]

[0077] 10: Substrate 11:n layer 12: Light-emitting layer 13: Electron block layer 14:p layer 15:p electrode 16:n electrode 17A, 17B: pn electrode 18:Protective film 19: Reflective film 20:p pad electrode 21:n pad electrode

Claims

1. A method for manufacturing a light-emitting device made of an Al-containing Group III nitride semiconductor having an emission wavelength of 200 to 280 nm, comprising the steps of: a semiconductor layer forming step of stacking an n-layer, a light emitting layer, and a p-layer on a substrate in this order; a hole forming step of forming holes in a predetermined region on the surface of the p-layer, the holes having a depth reaching the n-layer; a p-electrode formation step of forming a p-electrode on the p-layer, the p-electrode having a Ru layer in contact with the p-layer; an n-electrode formation process for forming an n-electrode on the n-layer exposed at the bottom of the hole, the n-electrode having a V layer of 5 nm to 15 nm in thickness in contact with the n-layer and made of V or a metal mainly composed of V, and an Al layer of Al or a metal mainly composed of Al in contact with the V layer; a heat treatment process for performing a heat treatment at a temperature of 500 to 650° C. for 1 to 10 minutes to reduce the contact resistance of the p-electrode and the n-electrode and to activate the p-type impurity of the p-layer; a pattern of the holes and the p-electrode is set so that a ratio of an area of ​​the p-electrode to a total area of ​​the holes and the p-layer is 70% or more.

2. 2. The method for manufacturing a light-emitting element according to claim 1, wherein a plurality of the holes are formed, the holes are arranged in a square lattice pattern, a regular triangular lattice pattern, or a honeycomb pattern, and the n-electrode is formed on a bottom surface of each of the holes.

3. a pn electrode formation step of forming a first pn electrode and a second pn electrode on the p electrode and the n electrode, respectively, after the heat treatment step; a protective film forming step of forming an insulating protective film so as to cover the entire upper surface of the element; a pad electrode forming process for forming a p-pad electrode on the protective film, the p-pad electrode being connected to the first p-n electrode through the hole, and an n-pad electrode being connected to the second p-n electrode through the hole and spaced apart from the p-pad electrode; The method for producing a light-emitting device according to claim 1 or 2, further comprising:

4. A light emitting device made of an Al-containing Group III nitride semiconductor having an emission wavelength of 200 to 280 nm, A substrate; a semiconductor layer including an n-layer, a light-emitting layer, and a p-layer stacked in this order on a substrate; a hole provided in a predetermined region on the surface of the p-layer and having a depth reaching the n-layer; a p-electrode having a Ru layer provided on and in contact with the p-layer; a hole provided on the n-layer exposed at a bottom surface of the hole and positioned in contact with the n-layer; x or an Al layer having a higher Al composition than the n-layer; y G 1-y N x and a second layer located on and in contact with the first layer, the second layer being made of a metal mainly containing Al and containing V, and the second layer having a thickness of 50 nm or more and 500 nm or less. a pattern of the holes and the p-electrode is set so that a ratio of an area of ​​the p-electrode to a total area of ​​the holes and the p-layer is 70% or more.

5. The light-emitting element according to claim 4 , wherein a plurality of the holes are formed, the holes are arranged in a lattice pattern, and the n-electrode is formed on a bottom surface of each of the holes.

6. a first pn electrode and a second pn electrode provided on the p electrode and the n electrode, respectively; a protective film which is an insulator covering the entire upper surface of the element; a p-pad electrode provided on the protective film and connected to the first pn electrode through a hole provided in the protective film; an n-pad electrode provided on the protective film, connected to the second pn-electrode through a hole provided in the protective film, and spaced apart from the p-pad electrode; The light-emitting device according to claim 4 or 5, further comprising:

Citation Information

Patent Citations

  • Manufacturing GAN semiconductor element

    JP1998112555A

  • Gallium nitride compound semiconductor device

    JP1998270758A

  • Light-emitting element and light-emitting device using the same

    JP2017034231A

  • P-ohmic contact structure and light emitting device using the same

    US20220102588A1

  • Semiconductor light-emitting element

    WO2020137470A1