Security label manufacturing method
The method enhances security labels by using a peel-off detection layer and controlled adhesive properties to ensure the release layer separates from the cellophane base, enabling reliable detection of unauthorized peeling.
Patent Information
- Application Number
- JP2023048378
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-24
- Publication Date
- 2024-10-04
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional security labels using cellophane as a base material fail to reliably detect unauthorized peeling due to the release layer separating with the base material, making it difficult to visually identify illicit removal.
A method involving a peel-off detection layer printed on one side of the label member, an adhesive layer formed on the separator, and specific drying and adhesive properties to ensure the release layer peels off from the base material when the label is removed, using cellophane as the base material.
Ensures reliable detection of unauthorized peeling by ensuring the release layer remains on the adherend, allowing visual confirmation of tampering.
Smart Images

Figure 2024137028000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a security label that is affixed to an object to seal an opening or the like and is capable of detecting unauthorized removal of the security label. [Background technology]
[0002] A method of attaching an adhesive label to an adherend is widely used as a means for sealing an opening of an adherend such as a box or container, or as a means for displaying attribute information of the adherend. However, with a normal label, when a person with a nefarious purpose such as stealing contents or falsifying attribute information removes the label from the adherend and then reattaches it, it is difficult to detect tampering from its appearance. Therefore, a so-called security label has been proposed that can detect tampering by leaving a trace of removal on the adherend. The sheet-like substrate constituting this security label is generally made of a synthetic resin such as polyethylene terephthalate (PET), but it is also known to be made of naturally derived cellophane (see, for example, paragraph number
[0013] of the specification of Patent Document 1).
[0003] This security label is manufactured by laminating a label member and a separator (release paper). In detail, first, a peel detection layer for detecting peeling is printed on the back surface of the substrate. Next, an adhesive is applied to cover this peel detection layer and dried to form an adhesive layer. This produces a label member. Next, a separator is laminated to the adhesive layer of this label member, thereby integrating the label member and the separator. This completes the security label.
[0004] When this security label is used, the label member is peeled off from the separator together with the adhesive layer and attached to the adherend. If the label member is peeled off from the adherend by a person with illicit purposes, the peel layer constituting the peel detection layer peels off from the substrate and remains on the surface of the adherend. By visually checking this peel layer, a user can detect that the label member has been illicitly peeled off. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2002-40946 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, in the conventional security label manufacturing method, when a cellophane substrate is used, the produced security label may have a peeling detection layer that is not fully peeled from the substrate, and the peeling layer that should remain on the surface of the adherend may be separated from the adherend along with the substrate, resulting in a problem that unauthorized peeling cannot be reliably detected.
[0007] The present invention has been devised in light of these circumstances, and its object is to provide a method for manufacturing a security label in which, even when a base material made of cellophane is used, the release layer is reliably peeled off from the base material when the label member is peeled off from the substrate, and unauthorized peeling can be reliably detected. [Means for solving the problem]
[0008] A method for manufacturing a security label according to one embodiment of the present invention is a method for manufacturing a security label in which a label member and a separator are integrated via an adhesive layer, and includes the following steps: a first step in which a peel detection layer for detecting peeling from an adherend is printed on one side of a sheet-like substrate made of cellophane to produce the label member; a second step in which an adhesive is applied to one side of the separator to form the adhesive layer; a third step in which the adhesive layer is dried at a predetermined drying temperature; and a fourth step in which the peel detection layer and the adhesive layer are bonded together to integrate the label member and the separator.
[0009] In addition, in one embodiment of the method for manufacturing a security label of the present invention, the first step may include a fifth step in which a peel layer constituting the peel detection layer is printed on a part of one side of the substrate, and a sixth step in which an ink layer constituting the peel detection layer is printed on the remainder of one side of the substrate.
[0010] In addition, in the method for producing a security label according to one aspect of the present invention, the ink layer may be printed on the remaining portion of one surface of the substrate, covering the release layer.
[0011] In the method for producing a security label according to one aspect of the present invention, the drying temperature in the third step may be 50°C or higher and 130°C or lower.
[0012] In the method for producing a security label according to one aspect of the present invention, the drying temperature in the third step may exceed 130°C.
[0013] In the method for producing a security label according to one embodiment of the present invention, the pressure-sensitive adhesive layer has a basis weight (weight per square meter) of 18.3 g / m 2 It may be the following.
[0014] In the method for producing a security label according to one embodiment of the present invention, the pressure-sensitive adhesive layer has a basis weight of 8.7 g / m 2 It may be the following.
[0015] In addition, in the method for manufacturing a security label according to one embodiment of the present invention, the ink constituting the release layer may have a viscosity, measured using a Zahn Cup No. 3, of 15 seconds or more and 19 seconds or less, and the ink constituting the ink layer may have a viscosity, measured using a Zahn Cup No. 4, of 34 seconds or more and 36 seconds or less. Effect of the Invention
[0016] According to one aspect of the method for manufacturing a security label of the present invention, even when a substrate made of cellophane is used, the release layer is reliably peeled off from the substrate when the label member is peeled off from the substrate, making it possible to reliably detect unauthorized peeling. [Brief description of the drawings]
[0017] [Figure 1] 1 is a schematic cross-sectional view showing the configuration of a security label 1 produced by a method for producing a security label according to an embodiment of the present invention. [Diagram 2] FIG. 1 is a schematic diagram showing a printing line 10 used in a method for producing a security label according to an embodiment of the present invention. [Diagram 3] FIG. 1 is a schematic diagram showing a lamination line 20 used in a method for producing a security label according to an embodiment of the present invention. [Figure 4] 2 is a flowchart showing a flow of a method for manufacturing a security label according to an embodiment of the present invention. [Diagram 5] 10 is a flowchart showing a detailed flow of a label member producing step S1. [Figure 6] 13 is a table showing the results of an experiment confirming the relationship between the basis weight of the adhesive layer 3 and the degree of character loss in the peel detection layer 6. [Figure 7]13 is a table showing the results of an experiment conducted to confirm the relationship between the drying temperature of the dryer 28 and the degree of character loss in the peel detection layer 6. [Figure 8] FIG. 2 is an explanatory diagram for explaining a procedure for using the security label 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, a method for producing a security label according to an embodiment of the present invention will be described with reference to the drawings.
[0019] (Security Label Configuration) First, the configuration of a security label manufactured by a security label manufacturing method according to an embodiment of the present invention will be described. Fig. 1 is a schematic cross-sectional view showing the configuration of a security label 1 according to an embodiment of the present invention. As shown in Fig. 1, the security label 1 comprises a label member 2, an adhesive layer 3, and a separator 4. For ease of explanation, each part of the security label 1 is illustrated in Fig. 1 at a scale different from the actual one.
[0020] As shown in Fig. 1, the label member 2 has a substrate 5, a peel detection layer 6, and an information display layer 7. Of these, the substrate 5 is a sheet-like member made of cellophane. The cellophane according to the present invention is also called cellophane, and is known as a transparent film made mainly of pulp. That is, this cellophane is manufactured by chemically treating pulp obtained by crushing wood to produce a solution called viscose, and then molding this viscose into a thin film and solidifying it.
[0021] The peel detection layer 6 serves to detect that the label member 2 has been peeled off from the adherend H (see FIG. 8). As shown in FIG. 1, the peel detection layer 6 has a peel layer 8 and an ink layer 9. Of these, the peel layer 8 peels off from the substrate 5 and remains on the surface of the adherend H when the label member 2 is peeled off. The peel layer 8 is printed on the back surface of the substrate 5 so as to form so-called superimposed characters. That is, the peel layer 8 is printed so as to be superimposed on a part of the back surface of the substrate 5, and forms characters (for example, the characters "Opened") in a planar view. The peel layer 8 may form figures, symbols, etc. in a planar view.
[0022] On the other hand, when the label member 2 is peeled off, most of the ink layer 9 is separated from the adherend H (see FIG. 8) together with the substrate 5. The ink layer 9 is printed so as to cover the release layer 8 and to be laminated on the remaining part of the back surface of the substrate 5. Here, the adhesion between the ink layer 9 and the release layer 8 (the energy required to peel them off) is set to be greater than the adhesion between the release layer 8 and the substrate 5. Although not shown in detail in the figure, the ink layer 9 has the same color as the release layer 8. The ink layer 9 may be printed on the remaining part of the back surface of the substrate 5 so as to fill the gaps in the release layer 8 without covering the release layer 8. The ink layer 9 may have a color different from that of the release layer 8.
[0023] The information display layer 7 plays a role in displaying information related to the attributes and contents of the adherend H. This information display layer 7 is printed on the surface of the substrate 5 so as to form so-called superimposed characters. That is, the information display layer 7 is printed so as to be partially laminated on the surface of the substrate 5, and this printed portion itself forms characters or the like (for example, a company name or a company logo) in a planar view. In addition, although not shown in detail in the figure, this information display layer 7 has a color different from that of the substrate 5. The information display layer 7 may be printed on the back surface of the substrate 5, or the information display layer 7 may not be provided.
[0024] The adhesive layer 3 adheres the separator 4 to the label member 2 when the security label 1 is unused, and adheres the label member 2 to the adherend H when the security label 1 is used. The adhesive layer 3 is made of a so-called acrylic adhesive, and is provided between the label member 2 and the separator 4 with a substantially constant thickness, as shown in FIG. 1. The adhesive layer 3 has a larger adhesion force between the adhesive layer 3 and the ink layer 9 than the adhesion force between the peeling layer 8 and the substrate 5. The adhesive layer 3 has a property that the adhesion force between the adhesive layer 3 and the separator 4 is smaller than the adhesion force between the adhesive layer 3 and the peeling detection layer 6. The adhesive layer 3 has a property that the adhesion force between the adhesive layer 3 and the separator 4 is smaller than the adhesion force between the substrate 5 and the peeling detection layer 6. The adhesive layer 3 has a property that the adhesion force between the adhesive layer 3 and the adherend H is smaller than the adhesion force between the adhesive layer 3 and the peeling detection layer 6. The adhesive layer 3 has a property that the adhesion force between the adhesive layer 3 and the adherend H is larger than the adhesion force between the substrate 5 and the peeling layer 8, and smaller than the adhesion force between the substrate 5 and the ink layer 9. The adhesive layer 3 may be made of a conventionally known adhesive such as a urethane resin-based, silicone-based, natural rubber-based, or synthetic rubber-based adhesive instead of an acrylic adhesive.
[0025] The separator 4 serves to prevent the adhesive strength of the adhesive layer 3 from decreasing due to exposure to the outside. Although not shown in detail in the figure, the separator 4 is a so-called laminated paper, which is formed by subjecting one side of the paper to a release treatment using a release agent such as a silicone-based, acrylic-based, or PVA-based release agent. It is also possible to form the separator 4 by subjecting a woven fabric, plastic film, or the like to a release treatment instead of paper. The separator 4 thus formed is provided by bonding the release-treated surface to the adhesive layer 3.
[0026] (Printing line) Next, a printing line used in the method for manufacturing the security label 1 according to the embodiment of the present invention will be described. FIG. 2 is a schematic diagram showing a printing line 10. The printing line 10 has a first conveying path 11, a first unwinding device 12, a first winding device 13, a peel detection layer printer 14, and an information display layer printer 15. The first conveying path 11 is a path along which the base material 5 is conveyed (the conveying direction is indicated by an arrow in FIG. 2). The first unwinding device 12 holds the base material 5 in a wound state and serves to send the base material 5 to the first conveying path 11. The first unwinding device 12 is configured to be able to wind the base material 5 around it, and is provided at the most upstream part of the first conveying path 11. Meanwhile, the first winding device 13 serves to recover the base material 5 from the first conveying path 11 by winding up the base material 5 after the printing process has been completed. The first winding device 13 has a configuration similar to that of the first unwinding device 12, and is provided at the most downstream part of the first conveying path 11.
[0027] The peel detection layer printer 14 serves to print the peel layer 8 and the ink layer 9 of the peel detection layer 6 on the back surface of the substrate 5. As shown in FIG. 2, the peel detection layer printer 14 is provided at a position downstream of the first unwinding device 12 on the first conveying path 11. Although not shown in detail in the figure, a printer for printing the peel layer 8 and a printer for printing the ink layer 9 may be provided separately. On the other hand, the information display layer printer 15 serves to print the information display layer 7 on the front surface of the substrate 5. The information display layer printer 15 is provided at a position downstream of the peel detection layer printer 14 on the first conveying path 11. The information display layer printer 15 may be provided at a position upstream of the peel detection layer printer 14 on the first conveying path 11. Alternatively, the peel detection layer printer 14 may be provided with a function of printing the information display layer 7 without providing the information display layer printer 15.
[0028] (Laminating line) Next, a bonding line used in the manufacturing method of the security label 1 according to the embodiment of the present invention will be described. Fig. 3 is a schematic diagram showing a bonding line 20. The bonding line 20 has a second conveying path 21, a third conveying path 22, a fourth conveying path 23, a second unwinding device 24, a third unwinding device 25, a second winding device 26, a coating device 27, a dryer 28, and a bonding device 29.
[0029] The second conveying path 21 is a path along which the separator 4 is conveyed. The third conveying path 22 is a path along which the label material 2 is conveyed. The fourth conveying path 23 is a path along which the finished security label 1 is conveyed. The conveying directions of each path are indicated by arrows in FIG. 3. The most downstream portion of the second conveying path 21, the most downstream portion of the third conveying path 22, and the most upstream portion of the fourth conveying path 23 join together at a junction 30 shown in FIG. 3. Note that conveying rollers or the like that send the conveyed object downstream are appropriately provided on each path.
[0030] The second unwinding device 24 holds the separator 4 in a wound state and sends the separator 4 to the second conveying path 21. As shown in FIG. 3, the second unwinding device 24 is configured to be able to wind the separator 4 around it and is provided at the most upstream part of the second conveying path 21. The third unwinding device 25 holds the label material 2 that has passed through the printing line 10 in a wound state and sends the label material 2 to the third conveying path 22. The third unwinding device 25 is configured to be able to wind the label material 2 around it and is provided at the most upstream part of the third conveying path 22. On the other hand, the second winding device 26 plays a role of recovering the security label 1 from the fourth conveying path 23 by winding up the security label 1 that has completed the bonding process. The second winding device 26 is configured to be able to wind the security label 1 around it and is provided at the most downstream part of the fourth conveying path 23.
[0031] The coating device 27 serves to form an adhesive layer 3 by applying an acrylic adhesive to the surface of the separator 4. This coating device 27 is provided at a position downstream of the second unwinding device 24 on the second conveying path 21. The dryer 28 serves to heat the separator 4 to dry the adhesive layer 3 formed on the surface to a certain degree. This dryer 28 is provided at a position downstream of the coating device 27 on the second conveying path 21. The bonding device 29 serves to integrate the separator 4 and the label member 2 by bonding them together. This bonding device 29 is configured with a pair of bonding rollers 31, and the pair of bonding rollers 31 are provided so as to face each other across the junction 30.
[0032] (Security label manufacturing method and its effects) Next, a method for producing a security label according to an embodiment of the present invention will be described. Fig. 4 is a flow chart showing the flow of the method for producing a security label. The method for producing a security label includes a label member producing step S1 (corresponding to the "first step" of the present invention), an adhesive layer forming step S2 (corresponding to the "second step" of the present invention), an adhesive layer drying step S3 (corresponding to the "third step" of the present invention), and a laminating step S4 (corresponding to the "fourth step" of the present invention). The method for producing a security label may include other steps in addition to these steps.
[0033] The label member production process S1 is a process for producing a label member 2 from a substrate 5 by the above-mentioned printing line 10. FIG. 5 is a flow chart showing a detailed flow of the label member production process S1 (see FIG. 4). The label member production process S1 includes a peeling layer printing process S5 (corresponding to the "fifth process" according to the present invention), an ink layer printing process S6 (corresponding to the "sixth process" according to the present invention), and an information display layer printing process S7. Note that the label member production process S1 may include other processes besides these.
[0034] The peeling layer printing step S5 is a step of printing the above-mentioned peeling layer 8 (see FIG. 1) on the back surface of the substrate 5. That is, in this peeling layer printing step S5, first, the substrate 5 held around the first unwinding device 12 shown in FIG. 2 is sent to the first conveying path 11. Here, the substrate 5 is cellophane having a thickness of about 35 to 38 μm. Then, the peeling detection layer printer 14 provided on the first conveying path 11 prints the peeling layer 8 composed of a predetermined ink so as to form a predetermined superimposed character and to be laminated on the back surface of the substrate 5. Here, as the ink constituting the peeling layer 8, an ink having a viscosity measured at room temperature using a Zahn cup No. 3 of 15 seconds or more and 19 seconds or less is used. Note that the thickness of the substrate 5 and the ink constituting the peeling layer 8 are not limited to the present embodiment and can be changed arbitrarily.
[0035] The ink layer printing step S6 is a step of printing the ink layer 9 (see FIG. 1) on the back surface of the substrate 5 on which the peeling layer 8 is printed. That is, in this ink layer printing step S6, the ink layer 9 composed of a predetermined ink is printed by the peeling detection layer printer 14 shown in FIG. 2 so as to be laminated on the back surface of the peeling layer 8 while covering the characters placed on the peeling layer 8. Here, as the ink constituting the ink layer 9, an ink having a viscosity measured at room temperature using a Zahn cup No. 4 of 34 seconds or more and 36 seconds or less is used. Note that the ink layer 9 may be printed on the back surface of the substrate 5 so as to fill the gaps of the characters placed on the peeling layer 8 without covering the peeling layer 8. Note that the ink constituting the ink layer 9 is not limited to the present embodiment and can be changed arbitrarily.
[0036] The information display layer printing step S7 is a step of printing the above-mentioned information display layer 7 (see FIG. 1) on the surface of the substrate 5. That is, in this information display layer printing step S7, the information display layer 7 composed of a predetermined ink is printed by the information display layer printer 15 shown in FIG. 2 so as to form predetermined superimposed characters on the surface of the substrate 5 that has passed through the peel detection layer printer 14. Then, the substrate 5 that has passed through the information display layer printer 15 is collected from the first transport path 11 by being wound up by the first winding device 13.
[0037] The adhesive layer forming step S2 is a step of forming the above-mentioned adhesive layer 3 (see FIG. 1) on the surface of the separator 4. That is, in this adhesive layer forming step S2, first, the separator 4 held around itself is sent to the second transport path 21 by the second unwinding device 24 shown in FIG. 3. Then, the adhesive layer 3 composed of an acrylic adhesive is formed on the surface of the separator 4 by a coating device 27 provided on the second transport path 21. This adhesive layer 3 has a thickness of 18.3 g / m 2 and preferably 8.7 g / m 2 It has the following basis weight: The basis weight of the pressure-sensitive adhesive layer 3 is not limited to that in this embodiment and can be changed as desired.
[0038] The adhesive layer drying step S3 is a step of drying the adhesive layer 3 to a certain degree. That is, in this adhesive layer drying step S3, the separator 4 that has passed through the coating device 27 shown in Fig. 3 is transported downstream through the second transport path 21, and its surface is heated by the dryer 28. As a result, the adhesive layer 3 formed on the surface of the separator 4 and in a low-viscosity state is dried to a certain degree by being heated, and its viscosity is increased to a certain degree. Here, the drying temperature of the dryer 28 is set to a temperature of 50°C or higher, more preferably a temperature exceeding 130°C.
[0039] The lamination step S4 is a step of laminating the label member 2 and the separator 4 together to form an integrated unit. That is, in this lamination step S4, first, the label member 2 produced in the above-mentioned label member production step S1 and held around the third unwinding device 25 shown in FIG. 3 is sent to the third conveying path 22 by the third unwinding device 25. Meanwhile, the separator 4 that has passed through the above-mentioned dryer 28 is conveyed further downstream on the second conveying path 21. Then, when the label member 2 and the separator 4 reach the junction 30, the peel detection layer 6 (see FIG. 1) constituting the label member 2 and the adhesive layer 3 formed on the surface of the separator 4 are laminated to each other as they pass between a pair of laminating rollers 31 constituting the lamination device 29. As a result, the label member 2 and the separator 4 are integrated to produce the security label 1. The produced security label 1 is sent to the fourth conveying path 23 by the lamination device 29. This security label 1 is wound up by the second winding device 26 and is collected from the fourth transport path 23. With the above, the production of the security label 1 is completed.
[0040] As described above, according to the method for manufacturing a security label of an embodiment of the present invention, cellophane is used as the base material 5, and this cellophane is made primarily from pulp, a renewable resource, so that it can contribute to the SDGs (Sustainable Development Goals) from the perspective of moving away from plastic.
[0041] In addition, in this embodiment, as a method for integrating the label member 2 and the separator 4 via the adhesive layer 3, a so-called transfer method is adopted in which the adhesive layer 3 is formed on the surface of the separator 4, and the adhesive layer 3 and the peel detection layer 6 of the label member 2 are bonded to each other. According to this method, it is the separator 4 that passes through the dryer 28 in the adhesive layer drying step S3, and the label member 2 does not pass through the dryer 28 as in the conventional security label manufacturing method. Therefore, the substrate 5 and the peel detection layer 6 constituting the label member 2 are prevented from being denatured or deformed by heating in the dryer 28. As a result, even when cellophane is used as the substrate 5, when the label member 2 is peeled off from the adherend H, the peel layer 8 of the peel detection layer 6 is reliably peeled off from the substrate 5 and remains on the surface of the adherend H. Therefore, a user can reliably detect unauthorized peeling of the label member 2 by visually checking this peel layer 8.
[0042] In this embodiment, the pressure-sensitive adhesive layer 3 is 18.3 g / m 2 The following grammage is more preferable: 8.7 g / m 2 The basis weight is set as follows. This is because the degree of character loss of the peel detection layer 6, i.e., the degree of peeling of the peel layer 8 from the substrate 5, is better as the basis weight of the adhesive layer 3 is smaller. FIG. 6 is a table showing the results of an experiment confirming the relationship between the basis weight of the adhesive layer 3 and the degree of character loss of the peel detection layer 6. In the experiment, a substrate 5 made of cellophane was used, the drying temperature of the dryer 28 was set to 130° C., and the basis weight of the adhesive layer 3 was changed in various ways to produce experimental samples of the security label 1. Then, these experimental samples were attached to a stainless steel plate as the adherend H, and after 10 minutes, each was peeled off from the stainless steel plate. At this time, the peel angle (the angle between the peel direction and the extension direction of the stainless steel plate) was 180°, and the peel speed was 300 mm / min. Each image shown in the table of FIG. 6 was taken from the back side of the substrate 5 peeled off from the stainless steel plate. According to this, the degree of character loss in the peel detection layer 6 is as follows: 2When the thickness is less than 8.7 g / m, the security label 1 can be used satisfactorily. 2 From the above, it was confirmed that the adhesive layer 3 exhibited better results when the basis weight was 18.3 g / m 2 Setting the basis weight of the adhesive layer 3 to 8.7 g / m or less has the advantage that unauthorized removal of the security label 1 can be detected with a high degree of certainty. 2 Setting the value below has the advantage that unauthorized removal of the security label 1 can be reliably detected, and the amount of acrylic adhesive used can be reduced, thereby reducing manufacturing costs.
[0043] In this embodiment, the drying temperature of the dryer 28 in the adhesive layer drying step S3 is set to a temperature of 50° C. or higher, and more preferably to a temperature exceeding 130° C. This is because the higher the drying temperature of the dryer 28, the better the degree of character loss in the peel detection layer 6. FIG. 7 is a table showing the results of an experiment confirming the relationship between the drying temperature of the dryer 28 and the degree of character loss in the peel detection layer 6. In the experiment, a base material 5 made of cellophane was used, and the adhesive layer 3 had a basis weight of 18.3 g / m2. 2 After setting the drying temperature at 50° C. or higher, the drying temperature of the dryer 28 was varied to produce experimental samples of the security label 1. These experimental samples were then attached to a stainless steel plate as the adherend H, and after 10 minutes had passed, each was peeled off from the stainless steel plate. At this time, the peeling angle was 180°, and the peeling speed was 300 mm / min. Each image shown in the table of FIG. 7 is an image taken from the back side of the substrate 5 peeled off from the stainless steel plate. It was confirmed that the character loss of the peel detection layer 6 was good enough to be usable as a security label 1 when the drying temperature was 50° C. or higher, and was even better when the drying temperature exceeded 130° C.
[0044] As described above, setting the drying temperature at a temperature exceeding 130°C has the advantage of being able to reliably detect unauthorized removal of the security label 1. On the other hand, setting the drying temperature at a low temperature, at least 50°C and no more than 130°C, has the advantages of being able to detect unauthorized removal of the security label 1 with a fair degree of certainty, reducing denaturation and deformation of the separator 4, reducing manufacturing costs by reducing electricity costs, and reducing carbon dioxide emissions.
[0045] In this embodiment, the ink constituting peel layer 8 of peel detection layer 6 is an ink having a viscosity of 15 seconds or more and 19 seconds or less, measured at room temperature using Zahn cup No. 3, and the ink constituting ink layer 9 is an ink having a viscosity of 34 seconds or more and 36 seconds or less, measured at room temperature using Zahn cup No. 4. This is because the degree of character loss in peel detection layer 6 is improved when the ink is used after the basis weight of adhesive layer 3 and the drying temperature of dryer 28 are set as described above.
[0046] (Procedure for using security labels and their effects) Next, a description will be given of the procedure for using the security label 1 and its effects. Figure 8 is an explanatory diagram for explaining the procedure for using the security label 1. For ease of explanation, each part of the security label 1 is illustrated in Figure 8 at a scale different from the actual size.
[0047] A user who uses the security label 1 first peels off the separator 4 from the security label 1 as shown in FIG. 8(a). At this time, as described above, the adhesive layer 3 interposed between the separator 4 and the label member 2 has a property that the adhesive strength between the separator 4 and the peel detection layer 6 is smaller than the adhesive strength between the separator 4 and the peel detection layer 6. Therefore, when the separator 4 is peeled off, the adhesive layer 3 is not peeled off from the label member 2 along with the separator 4, but is integrated with the label member 2 while adhering to the peel detection layer 6. Furthermore, as described above, the adhesive strength between the adhesive layer 3 and the separator 4 is set to be smaller than the adhesive strength between the substrate 5 and the peel detection layer 6. Therefore, when the separator 4 is peeled off, the peel detection layer 6 is not separated from the substrate 5. Then, the adhesive layer 3 integrated with the label member 2 is exposed to the outside on the side opposite to the label member 2, i.e., the side that was adhered to the separator 4.
[0048] Next, as shown in Fig. 8(b), the user attaches the label member 2 to an adherend H such as a box or a container. That is, the user attaches the label member 2 to the adherend H by adhering the surface of the adhesive layer 3 integrated with the label member 2, which is exposed to the outside, to the adherend H. This completes the attachment of the label member 2. At this time, the information displayed by the information display layer 7 is visible to the user, while the characters placed thereon formed by the peeling layer 8 of the peel detection layer 6 are not visible to the user.
[0049] Thereafter, the label member 2 may be peeled off from the adherend H by a person with an illegal purpose. Here, as described above, the adhesive layer 3 has a property that the adhesion force between the adhesive layer 3 and the adherend H is smaller than the adhesion force between the peel detection layer 6. Furthermore, as described above, the adhesion force between the adhesive layer 3 and the adherend H is set to be larger than the adhesion force between the substrate 5 and the release layer 8 and smaller than the adhesion force between the substrate 5 and the ink layer 9. Therefore, when such an illegal peeling is performed, as shown in FIG. 8(c), in the label member 2, in the portion where the release layer 8 does not exist, the adhesive layer 3 is separated from the adherend H, and the ink layer 9 and the adhesive layer 3 are separated from the adherend H together with the substrate 5. On the other hand, in the portion where the release layer 8 of the label member 2 exists, the release layer 8 is peeled off from the substrate 5, and the release layer 8, the ink layer 9 and the adhesive layer 3 remain on the surface of the adherend H.
[0050] Then, the peel-off layer 8 is peeled off from the base material 5 and exposed to the outside, thereby displaying characters (for example, the characters "Opened") corresponding to the placed characters in a planar view. In addition, it is extremely difficult for a person with illicit intentions to return the label member 2, once peeled off, to its original state. Therefore, by visually checking the characters displayed by the peel-off layer 8, the user can reliably detect that the security label 1 has been peeled off from the adherend H in an unauthorized manner.
[0051] (Modification) The technical scope of the present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit of the present invention as defined by the claims. For example, the following modifications are possible as embodiments of the present invention.
[0052] In this embodiment, as shown in Fig. 4, the label member producing step S1 is performed before the adhesive layer forming step S2. However, the label member producing step S1 may be performed between the adhesive layer forming step S2 and the adhesive layer drying step S3, or between the adhesive layer drying step S3 and the laminating step S4.
[0053] In this embodiment, as shown in FIG. 5, the information display layer printing step S7 is performed after the ink layer printing step S6. However, the information display layer printing step S7 may be performed before the release layer printing step S5, or between the release layer printing step S5 and the ink layer printing step S6. Also, the information display layer printing step S7 may be omitted. Also, in this embodiment, the release layer printing step S5 is performed before the ink layer printing step S6. However, when the ink layer 9 is provided without covering the release layer 8, the release layer printing step S5 may be performed after the ink layer printing step S6.
[0054] 1, in this embodiment, the peeling detection layer 6 is partially printed on the back surface of the substrate 5 to form predetermined overlay characters, while the ink layer 9 is printed on the back surface of the substrate 5 so as to cover the peeling layer 8. However, the peeling layer 8 may be printed on the back surface of the substrate 5 so as to partially form voids to form predetermined cut-out characters, while the ink layer 9 may be printed on the back surface of the substrate 5 so as to fill the voids in the peeling layer 8. [Industrial Applicability]
[0055] The security label 1 produced by the security label manufacturing method of the present invention can be used not only to detect removal by persons with fraudulent purposes, but also to detect accidental removal by general users. [Explanation of symbols]
[0056] 1 Security Label 2 Label material 3 Adhesive layer 4. Separator 5 Base material 6 Peeling detection layer 8 Release layer 9 Ink Layer H Adherent S1 Label material manufacturing process (first process) S2 Adhesive layer formation process (second process) S3 Adhesive Layer Drying Process (Third Process) S4 Laminating Process (Fourth Process) S5 Release Layer Printing Process (Fifth Process) S6 Ink Layer Printing Process (Sixth Process) S7 Information Display Layer Printing Process (Seventh Process)
Claims
1. A method for producing a security label in which a label member and a separator are integrated via an adhesive layer, comprising the steps of: a first step of producing the label member by printing a peel detection layer for detecting peeling from an adherend on one surface of a sheet-like substrate made of cellophane; a second step of applying an adhesive to one surface of the separator to form the adhesive layer; a third step in which the pressure-sensitive adhesive layer is dried at a predetermined drying temperature; a fourth step of bonding the peel detection layer and the adhesive layer together to integrate the label member and the separator; A method for producing a security label, comprising:
2. The first step comprises: A fifth step in which a peeling layer constituting the peel detection layer is printed on a part of one surface of the base material; a sixth step of printing an ink layer constituting the peel detection layer on a remaining portion of one surface of the substrate; 2. The method of claim 1, further comprising:
3. The method of claim 2, wherein the ink layer is printed over the release layer and onto the remainder of one side of the substrate.
4. 4. The method for manufacturing a security label according to claim 1, wherein the drying temperature in the third step is 50° C. or higher and 130° C. or lower.
5. 4. The method for producing a security label according to claim 1, wherein the drying temperature in the third step is greater than 130°C.
6. The pressure-sensitive adhesive layer has a basis weight of 18.3 g / m 2 4. The method for producing a security label according to claim 1, wherein:
7. The pressure-sensitive adhesive layer has a basis weight of 8.7 g / m 2 4. The method for producing a security label according to claim 1, wherein:
8. 4. The method for producing a security label according to claim 2 or 3, wherein the ink constituting the release layer has a viscosity of 15 seconds or more and 19 seconds or less, as measured by Zahn Cup No. 3, and the ink constituting the ink layer has a viscosity of 34 seconds or more and 36 seconds or less, as measured by Zahn Cup No. 4.
Citation Information
Patent Citations
One-off sealing tag
CN201004296Y
Tamper instruction label
JP1995234636A
Label which prevents re-sticking and illegal use
JP2002040946A
Seal for confirming unsealing
JP2003131576A
Hologram label
JP2014126799A