Laminate

The laminate with a synthetic resin base layer and a metal-filled coloring layer with a dielectric constant of 4.0 or more addresses the issue of filler content decrease, ensuring electromagnetic wave permeability and enhancing appearance in vehicle components.

JP2024137120AActive Publication Date: 2024-10-07TOYODA GOSEI CO LTD

Patent Information

Application Number
JP2023048512
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-07
Estimated Expiration
2043-03-24

AI Technical Summary

Technical Problem

Conventional vehicle components with metal fillers in the coating film to ensure electromagnetic wave permeability face a decrease in filler content, leading to insufficient metallic luster and poor appearance.

Method used

A laminate comprising a base layer of synthetic resin and a coloring layer with a metal filler, having a dielectric constant of 4.0 or more, to increase filler content and maintain electromagnetic wave permeability while improving appearance.

Benefits of technology

The laminate ensures both sufficient electromagnetic wave permeability and improved appearance by optimizing the filler content and thickness of the coloring layer, maintaining good appearance and transmission properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024137120000001_ABST
    Figure 2024137120000001_ABST
Patent Text Reader

Abstract

To provide a laminate that can improve an external appearance while securing electromagnetic wave transmissivity.SOLUTION: A vehicle component 13 is applied to a vehicle 11 on which a millimeter-wave radar device 12 that sends and receives a millimeter-wave is mounted, is arranged ahead a transmission direction of a millimeter-wave in the millimeter-wave radar device 12, and transmits the millimeter-wave. The vehicle component 13 comprises a synthetic-resin substrate layer 14, and a color-developing layer 16 in which metal filler is dispersed on a coating film. The color-developing layer 16 has millimeter-wave transmissivity and has a dielectric constant of 4.0 or more.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a laminate that is transparent to electromagnetic waves. [Background technology]

[0002] Conventionally, a vehicle part as shown in Patent Document 1, for example, has been known as a laminate. Such a vehicle part has a substrate and a coating film. From the viewpoint of ensuring electromagnetic wave permeability of the vehicle part, it is considered preferable that the relative dielectric constants of the substrate and the coating film are equal to each other and are 3.0 or less. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 4158646 Summary of the Invention [Problem to be solved by the invention]

[0004] However, in the above-mentioned vehicle parts, if the paint film contains metallic filler and the relative dielectric constant of the paint film is set to 3.0 or less to ensure electromagnetic wave permeability, the content of the filler in the paint film will be insufficient, and therefore the paint film will not have a sufficient metallic luster, which may result in poor appearance. [Means for solving the problem]

[0005] Various aspects of the laminate for solving the above problems will be described below. [Embodiment 1] A laminate that is electromagnetically transparent, comprising a base layer made of synthetic resin and a color-developing layer containing a metal filler, the color-developing layer being electromagnetically transparent and having a relative dielectric constant of 4.0 or more.

[0006] The inventors of the present application have found that there is a positive linear relationship between the amount of filler contained in the color-forming layer [(weight of filler contained in the color-forming layer / total weight of the color-forming layer after drying)×100%] and the relative dielectric constant of the color-forming layer. Therefore, according to the above configuration, by setting the relative dielectric constant of the color-forming layer having electromagnetic wave transparency to 4.0 or more, the filler content of the color-forming layer is increased, thereby improving the appearance. Therefore, the appearance can be improved while ensuring electromagnetic wave transparency.

[0007] [Aspect 2] The laminate according to [Aspect 1], wherein the thickness of the color-developing layer is in the range of 3 μm or more and 75 μm or less. According to the above configuration, by making the thickness of the coloring layer 75 μm or less, sufficient electromagnetic wave permeability can be ensured even when a coloring layer with a relative dielectric constant of 4.0 or more is used. On the other hand, by making the thickness of the coloring layer 3 μm or more, the coloring of the coating film is ensured, so that a good appearance can be maintained. Therefore, a good appearance can be maintained while ensuring sufficient electromagnetic wave permeability.

[0008] [Aspect 3] The laminate according to [Aspect 2], characterized in that the amount of the filler contained in the color-developing layer is 2.0% or more, and the relative dielectric constant of the color-developing layer is 8.0 or more. According to the above-mentioned configuration, the amount of the filler contained in the color-forming layer is set to 2.0% or more and the relative dielectric constant of the color-forming layer is set to 8.0 or more, so that the amount of the filler contained in the color-forming layer can be further increased, which contributes to further improving the appearance. Effect of the Invention

[0009] The present invention has an effect of improving the appearance while ensuring electromagnetic wave transparency. [Brief description of the drawings]

[0010] [Figure 1] 1 is a schematic cross-sectional view showing a vehicle component according to an embodiment; [Diagram 2] FIG. 2 is a schematic diagram of a color layer in a vehicle part. [Diagram 3]1 is a graph showing the relationship between the amount of aluminum and the relative dielectric constant in color-developing layers A to E. [Figure 4] 13 is a graph showing the results of calculating the relationship between the thickness of the base material layer and the attenuation of the transmitted millimeter wave in each of a vehicle part having a coloring layer A and a vehicle part having a coloring layer E. [Diagram 5] 13 is a graph showing the results of a comparison of the amount of attenuation of millimeter waves when the thickness of the base layer is optimized and the amount of attenuation of millimeter waves when the thickness of the base layer is not optimized, for a vehicle part having a coloring layer A and a vehicle part having a coloring layer E. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] An embodiment in which the laminate is embodied in a vehicle part will be described below with reference to the drawings. In the following description, the forward direction of the vehicle is defined as the front, and the reverse direction is defined as the rear. As shown in Fig. 1, a millimeter wave radar device 12 for monitoring the front is mounted on the front end of a vehicle 11 as an example of a radar device that transmits and receives electromagnetic waves. The millimeter wave radar device 12 has a function of transmitting millimeter waves of electromagnetic waves toward the front outside the vehicle and receiving millimeter waves reflected by an object outside the vehicle. The millimeter wave is a radio wave with a wavelength of 1 mm to 10 mm and a frequency of 30 GHz to 300 GHz.

[0012] As described above, the millimeter wave radar device 12 transmits millimeter waves toward the front of the vehicle 11, and therefore the transmission direction of millimeter waves by the millimeter wave radar device 12 is a direction from the rear to the front of the vehicle 11. The front in the transmission direction of millimeter waves roughly coincides with the front of the vehicle 11, and the rear in the transmission direction of millimeter waves roughly coincides with the rear of the vehicle 11. For this reason, in the following description, the front in the transmission direction of millimeter waves will be simply referred to as "front", "front", etc., and the rear in the transmission direction of millimeter waves will be simply referred to as "rear", "rear", etc.

[0013] <Vehicle parts 13> 1, a substantially plate-shaped vehicle part 13 as an example of a laminate that transmits millimeter waves (electromagnetic waves) is disposed in front of the millimeter wave radar device 12. The vehicle part 13 is formed, for example, of an emblem, a front grille, a front bumper, etc. of the vehicle 11. The vehicle part 13 is disposed in an upright state such that its front surface faces the front of the vehicle 11 and its rear surface faces the rear of the vehicle 11. The front surface of the vehicle part 13 constitutes the design surface of the vehicle part 13.

[0014] The vehicle part 13 includes a base layer 14 made of synthetic resin, a primer layer 15 provided on the front surface of the base layer 14, a color-developing layer 16 provided on the front surface of the primer layer 15, and a clear coat layer 17 provided on the front surface of the color-developing layer 16. The primer layer 15 is formed of a coating film for undercoating. The clear coat layer 17 is formed of a colorless and transparent coating film for topcoating.

[0015] <Base material layer 14> 1, the base layer 14 is formed into a plate shape by, for example, injection molding using a synthetic resin material having millimeter wave permeability (electromagnetic wave permeability). The synthetic resin material used to form the base layer 14 may be transparent or opaque.

[0016] Examples of synthetic resin materials used to form the base layer 14 include polypropylene (PP) resin, polycarbonate (PC) resin, acrylonitrile-butadiene-styrene copolymer (ABS) resin, acrylonitrile-ethylene-propylene-diene-styrene (AES) resin, polymethyl methacrylate (PMMA) resin, acrylonitrile-styrene-acrylate copolymer (ASA) resin, and PMMA resin containing ASA resin.

[0017] <Coloring layer 16> As shown in Fig. 2, the coloring layer 16 is formed by dispersing a plurality of metallic (aluminum in this example) fillers 18 in an intermediate coating film 19. That is, the coloring layer 16 contains a plurality of metallic fillers 18. Gaps are formed between the fillers 18. Therefore, the coloring layer 16 has millimeter wave transparency (electromagnetic wave transparency). The coloring layer 16 is set so that its relative dielectric constant is 4.0 or more.

[0018] The thickness of the color-forming layer 16 is preferably set in the range of 3 μm to 75 μm. The thickness of the color-forming layer 16 is more preferably set in the range of 5 μm to 75 μm. If the thickness of the color-forming layer 16 is less than 3 μm, the color of the coating film 19 constituting the color-forming layer 16 may be insufficient. On the other hand, if the thickness of the color-forming layer 16 exceeds 75 μm, the millimeter wave transmittance of the color-forming layer 16 may be reduced.

[0019] 3, the inventors of the present application discovered that there is a positive linear relationship between the amount of aluminum, which is the amount of filler 18 contained in color-forming layer 16, and the relative dielectric constant of color-forming layer 16. The amount of aluminum (amount of filler 18) contained in color-forming layer 16 is expressed as [(weight of aluminum (filler 18) contained in color-forming layer 16 / total weight of color-forming layer 16 after drying)×100%].

[0020] 3 is a graph showing the relationship between the amount of aluminum and the relative dielectric constant for five types of color layers A to E (color layers 16) having coating films 19 of different colors. It can be seen from the graph in FIG. 3 that there is a positive linear relationship between the amount of aluminum contained in the color layer 16 and the relative dielectric constant of the color layer 16.

[0021] 3, it can be seen that the coloring layers A to E all have an aluminum content (amount of filler 18) of 2.0% or more and a relative dielectric constant of 8.0 or more. For this reason, it is more preferable that the coloring layer 16 in the vehicle part 13 has an aluminum content of 2.0% or more and a relative dielectric constant of 8.0 or more.

[0022] <Setting the Thickness of the Base Layer 14> The thickness of the base material layer 14 in the vehicle part 13 is preferably set in the range of 1.0 mm or more and 2.5 mm or less. The thickness of the base material layer 14 in the vehicle part 13 is more preferably set in the range of 2.0 mm or more and 2.5 mm or less. However, from the viewpoint of improving the millimeter wave transmittance of the vehicle part 13, it is most preferable to optimize the thickness of the base material layer 14 according to the coloring layers A to E (see FIG. 3) used.

[0023] Fig. 4 is a graph showing the results of calculating the relationship between the thickness of the base material layer 14 and the attenuation of the transmitted millimeter wave in each of the vehicle part 13 having the coloring layer A and the vehicle part 13 having the coloring layer E. From the graph in Fig. 4, it can be seen that the optimal thickness of the base material layer 14 that minimizes the attenuation of the millimeter wave in the vehicle part 13 having the coloring layer A is 2.35 mm. From the graph in Fig. 4, it can be seen that the optimal thickness of the base material layer 14 that minimizes the attenuation of the millimeter wave in the vehicle part 13 having the coloring layer E is 2.10 mm.

[0024] Fig. 5 is a graph showing the results of comparing the amount of attenuation of millimeter waves when the thickness of the base layer 14 is optimized and when the thickness of the base layer 14 is not optimized in each of the vehicle part 13 having the coloring layer A and the vehicle part 13 having the coloring layer E. In Fig. 5, the thickness of the base layer 14 when not optimized is set to 2.5 mm in both the vehicle part 13 having the coloring layer A and the vehicle part 13 having the coloring layer E.

[0025] In addition, in Fig. 5, the thicknesses of the base material layer 14 optimized in the vehicle part 13 having the coloring layer A and the vehicle part 13 having the coloring layer E are set to 2.35 mm and 2.10 mm, respectively, from the graph in Fig. 4. It can be seen from the graph in Fig. 5 that in both the vehicle part 13 having the coloring layer A and the vehicle part 13 having the coloring layer E, when the thickness of the base material layer 14 is not optimized, the attenuation of the millimeter wave is less than the required value of -0.85 dB, and the required value is not met.

[0026] 5, in both the vehicle part 13 having the coloring layer A and the vehicle part 13 having the coloring layer E, when the thickness of the base layer 14 is optimized, the attenuation of millimeter waves becomes equal to or greater than the required value of -0.85 dB, thereby satisfying the required value. Therefore, in the vehicle part 13, the attenuation of millimeter waves can be minimized by optimizing the thickness of the base layer 14 according to the selected color of the coating film 19 of the coloring layer 16.

[0027] <Function of vehicle part 13> 1 , the millimeter waves are transmitted through each layer of the vehicle part 13. The transmitted millimeter waves are reflected by objects in front of the vehicle 11, including a preceding vehicle and pedestrians, and then transmitted again through each layer of the vehicle part 13 to be received by the millimeter wave radar device 12.

[0028] In this case, the coloring layer 16 in the vehicle part 13 has millimeter wave transparency. In addition, since the relative dielectric constant of the coloring layer 16 in the vehicle part 13 is 4.0 or more, the content of the filler 18 in the coloring layer 16 is further increased. This improves the appearance of the vehicle part 13. Therefore, it is possible to ensure the millimeter wave transparency of the vehicle part 13 while improving the appearance at the same time.

[0029] The millimeter wave radar device 12 recognizes an object and detects the distance and relative speed between the object and the vehicle 11 based on the transmitted and received millimeter waves. <Effects of the embodiment> According to the embodiment described above in detail, the following effects are achieved.

[0030] (1) The vehicle component 13 includes a synthetic resin base layer 14 and a coloring layer 16 having aluminum filler 18 dispersed in a coating film 19. The coloring layer 16 is permeable to millimeter waves and has a relative dielectric constant of 4.0 or more.

[0031] The inventors of the present application found that there is a positive linear relationship between the amount of filler 18 contained in the coloring layer 16 [(weight of filler 18 contained in the coloring layer 16 / total weight of the coloring layer 16 after drying)×100%] and the relative dielectric constant of the coloring layer 16. From this, according to the above configuration, by setting the relative dielectric constant of the coloring layer 16 having millimeter wave transmissibility to 4.0 or more, the content of the filler 18 in the coloring layer 16 increases, so that the appearance of the vehicle part 13 can be improved. Therefore, the millimeter wave transmissibility of the vehicle part 13 can be ensured while the appearance of the vehicle part 13 can be improved. In other words, it is possible to ensure the millimeter wave transmissibility of the vehicle part 13 and improve the appearance at the same time.

[0032] (2) In the vehicle component 13, the thickness of the coloring layer 16 is in the range of 3 μm to 75 μm. According to the above configuration, by setting the thickness of the coloring layer 16 to 75 μm or less, the millimeter wave transmittance of the vehicle part 13 can be sufficiently ensured even if a coloring layer 16 having a relative dielectric constant of 4.0 or more is used for the vehicle part 13. On the other hand, by setting the thickness of the coloring layer 16 to 3 μm or more, the coloring of the coating film 19 is ensured, so that a good appearance can be maintained. Therefore, the millimeter wave transmittance of the vehicle part 13 can be sufficiently ensured while maintaining a good appearance of the vehicle part 13.

[0033] (3) In the vehicle component 13, the amount of the filler 18 contained in the coloring layer 16 is 2.0% or more, and the relative dielectric constant of the coloring layer 16 is 8.0 or more. According to the above-mentioned configuration, by making the amount of the filler 18 contained in the coloring layer 16 2.0% or more and making the relative dielectric constant of the coloring layer 16 8.0 or more, it is possible to further increase the amount of the filler 18 contained in the coloring layer 16. This can contribute to further improving the appearance of the vehicle part 13.

[0034] <Example of change> The above embodiment can be modified as follows: The above embodiment and the following modifications can be combined with each other as long as they are not technically inconsistent.

[0035] The coloring layer 16 may be made of a film of transparent resin mixed with multiple fillers 18 and paint. In this way, the coloring layer 16 can be directly attached to the base layer 14 of the vehicle part 13, so that the primer layer 15 and the clear coat layer 17 can be omitted.

[0036] The color-developing layer 16 may contain a coloring agent such as a dye. In the vehicle component 13, the amount of the filler 18 contained in the coloring layer 16 does not necessarily have to be 2.0% or more, and the relative dielectric constant of the coloring layer 16 does not necessarily have to be 8.0 or more.

[0037] In the vehicle component 13, the thickness of the color-developing layer 16 does not necessarily have to be in the range of 3 μm or more and 75 μm or less. The millimeter wave radar device 12 that transmits and receives millimeter waves (electromagnetic waves) for detecting objects outside the vehicle may be a device for monitoring the rear of the vehicle in addition to monitoring the front of the vehicle.

[0038] The radar device may be an infrared radar device that transmits and receives infrared rays (electromagnetic waves). The laminate is not limited to the vehicle part 13, but may be a consumer part. That is, the laminate may be applied to a consumer product equipped with a radar device that transmits and receives electromagnetic waves other than the vehicle 11. Examples of such consumer products include an automatic cleaning robot, a robot for transporting or serving food, a drone, etc.

[0039] When the laminate is a consumer part having the same layer structure as the vehicle part 13, it is preferable to set the thickness of the base layer 14 in the range of 1.0 mm or more and 2.5 mm or less, and the thickness of the color-developing layer 16 in the range of 3 μm or more and 75 μm or less. [Explanation of symbols]

[0040] 11…Vehicle 12... Millimeter wave radar device as an example of a radar device 13... Vehicle parts as an example of laminates 14...Base material layer 15...Primer layer 16, A~E…Coloring layer 17…Clear coat layer 18…Filler 19...Paint film

Claims

1. A laminate that transmits electromagnetic waves, The inkjet recording medium has a base layer made of synthetic resin and a color-developing layer containing a metal filler, The color-developing layer is electromagnetically transparent and has a relative dielectric constant of 4.0 or more.

2. 2. The laminate according to claim 1, wherein the color-developing layer has a thickness in the range of 3 [mu]m to 75 [mu]m.

3. The amount of the filler contained in the color-developing layer is 2.0% or more, 3. The laminate according to claim 2, wherein the color-developing layer has a relative dielectric constant of 8.0 or more.

Citation Information

Patent Citations

  • Radio wave transmitting exterior component and its manufacturing method

    JP2002135030A

  • Molded product for use in radar device beam passage

    JP2005212745A

  • Electromagnetic wave transmissive brilliant coating resin product and its manufacturing method

    JP2010030075A

  • Decorative coated film

    JP2019111707A

  • Millimeter wave transmission garnish

    JP2022183556A

Cited By

  • Electromagnetic wave transmissive laminate and electromagnetic wave radar system

    JP2026079210A