Manufacturing method of piezoelectric device
The method enhances piezoelectric device output by forming a thick vibration region with connecting portions and gaps, addressing limitations in adjusting resonance frequency and signal strength in conventional devices.
Patent Information
- Application Number
- JP2023050224
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
AI Technical Summary
Conventional piezoelectric devices face challenges in adjusting resonance frequency and output signal strength due to limitations in changing the rigidity and thickness of the vibration region, leading to reduced displacement and output when the length of the vibration region is shortened.
A manufacturing method that involves forming a piezoelectric device with a thick vibration region by incorporating connecting portions and gaps between layers, allowing for easier removal of sacrificial layers and maintaining low rigidity, thereby enhancing displacement and output.
The method enables the formation of a high-output piezoelectric device with increased displacement and suppressed rigidity, facilitating improved resonance characteristics and signal strength.
Smart Images

Figure 2024139334000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a piezoelectric device, and more particularly to a method for manufacturing a high-output piezoelectric device. [Background technology]
[0002] Piezoelectric devices equipped with a thin film (piezoelectric film) of piezoelectric material can detect voltage changes caused by displacement of the piezoelectric film that constitutes the vibration region, or can displace the piezoelectric film by applying a voltage to it, and can be used as piezoelectric sensors, piezoelectric actuators, etc.
[0003] For example, a conventional piezoelectric device employs a cantilever structure in which one end of a vibration region is bonded to a support substrate and supported by the support substrate. This type of piezoelectric device is disclosed in, for example, Patent Document 1. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 5936154 Summary of the Invention [Problem to be solved by the invention]
[0005] FIG. 12 shows a schematic cross-sectional view for explaining a conventional piezoelectric device. As shown in FIG. 12, in a conventional piezoelectric device 300, a first piezoelectric film 3a and a second piezoelectric film 3b are laminated on a support substrate 1 via an insulating film 2, a first electrode 4a and a second electrode 4b are arranged on either side of the first piezoelectric film 3a, and a second electrode 4b and a third electrode 4c are arranged on either side of the second piezoelectric film 3b. A cavity 5 is formed in the support substrate 1, and the first piezoelectric film 3a, the second piezoelectric film 3b, and the first to third electrodes 4a to 4c on the cavity 5 are partitioned by slits 6 (FIG. 13), thereby forming a vibration region 7 whose one end is joined to and supported by the support substrate 1. 8a and 8b are lead electrodes, and the lead electrode 8a is connected to the first electrode 4a and the third electrode 4c, and the lead electrode 8b is connected to the second electrode 4b.
[0006] Fig. 13 is a schematic plan view illustrating an example of the arrangement of the slits 6 in the piezoelectric device 300 in Fig. 12. When the slits 6 are arranged as shown in Fig. 13, a piezoelectric device 300 having two vibration regions 7 with a cantilever structure is formed. Note that the cross-sectional view taken along line BB in Fig. 13 corresponds to Fig. 12, and Fig. 13 does not show the third electrode 4c, the extraction electrodes 8a and 8b, etc., shown in Fig. 12, but shows only the arrangement of the slits 6 penetrating the first piezoelectric film 3a and the second piezoelectric film 3b, etc., covering the cavity 5.
[0007] 12 and 13, the resonant frequency of the vibrating region 7 can be adjusted by the rigidity and length of the vibrating region 7. Specifically, the resonant frequency increases when the rigidity of the vibrating region 7 is increased, and the resonant frequency increases when the length L of the vibrating region 7 is decreased. Note that the length L of the vibrating region 7 is the length from the joint end with the support substrate 1 to the open end, as shown in FIG.
[0008] In order to form a piezoelectric film with good film quality, the thickness of the piezoelectric film formed by sputtering or CVD (Chemical Vapor Deposition) is usually set to 0.5 to 1.0 μm, and it is difficult to significantly change the thickness of the piezoelectric film. Since the rigidity of the vibration region 7 is determined once the type and thickness of the piezoelectric material constituting the piezoelectric film are determined, it is difficult to significantly change the rigidity of the vibration region 7 in order to adjust the resonance frequency of the vibration region 7. Therefore, the resonance frequency of the vibration region 7 is generally adjusted by changing the length of the vibration region 7.
[0009] 12 and 13 is used as an ultrasonic transmitter / receiver for obstacle detection or ultrasonic diagnosis, it is necessary to adjust the length of the vibration region 7 to be short and increase the resonance frequency of the vibration region 7. When the length of the vibration region 7 is shortened in this way, the displacement of the piezoelectric film constituting the vibration region 7 becomes small, resulting in a problem of a decrease in the output signal.
[0010] The present applicant has proposed a high-output piezoelectric device. FIG. 1 is a schematic cross-sectional view illustrating the high-output piezoelectric device proposed by the present applicant. In the piezoelectric device 100 shown in FIG. 1, a first electrode 4a, a first piezoelectric film 3a, and a second electrode 4b are laminated on a support substrate 1 via an insulating film 2, and a fourth electrode 4d, a second piezoelectric film 3b, and a third electrode 4c are further laminated via connecting parts 9 and 9a. The first piezoelectric film 3a, the second piezoelectric film 3b, and the first to fourth electrodes 4a to 4d on a cavity 5 formed in the support substrate 1 are partitioned by slits 6, and a vibration region 7 is formed, one end of which is joined to and supported by the support substrate 1. 8a and 8b are extraction electrodes.
[0011] Fig. 2 is a schematic plan view illustrating an example of the arrangement of the slits 6 and the connecting portions 9a of the piezoelectric device 100 of Fig. 1. By arranging the slits 6 and the connecting portions 9a as shown in Fig. 2, it is possible to configure the piezoelectric device 100 having two vibration regions 7 with a cantilever structure. Note that the cross-sectional view taken along line AA in Fig. 2 corresponds to Fig. 1, and Fig. 2 does not show the third electrode 4c, the extraction electrodes 8a and 8b, etc. shown in Fig. 1, but only shows the arrangement of the slits 6 and the columnar connecting portions 9a penetrating the first piezoelectric film 3a and the second piezoelectric film 3b, etc., covering the cavity 5.
[0012] The piezoelectric device 100 thus configured has a thick vibration region 7 due to the provision of the connecting portions 9a. Furthermore, because the columnar connecting portions 9a are spaced apart from each other and gaps 10 are provided, the rigidity of the vibration region 7 is smaller than that of a vibration region of the same thickness configured from a single piezoelectric film, and does not change significantly compared to the rigidity of a structure in which the first piezoelectric film 3a and the second piezoelectric film 3b are laminated without any connecting portions as shown in Fig. 12. As a result, the displacement of the first piezoelectric film 3a and the second piezoelectric film 3b is large, making it possible to configure a high-output piezoelectric device.
[0013] In the piezoelectric device 100 having the connecting portion 9a and the void 10, the following steps can be considered as a manufacturing process for the connecting portion 9a and the void 10. First, the first electrode 4a, the first piezoelectric film 3a, and the second electrode 4b are sequentially laminated on the entire surface of the support substrate 1 via the insulating film 2. The connecting portion 9a is formed on the second electrode 4b, and a sacrificial layer is filled in the region that becomes the void portion 10 between the adjacent connecting portions 9a to flatten it. Furthermore, the fourth electrode 4d, the second piezoelectric film 3b, and the third electrode 4c are sequentially laminated on the entire surface. After that, a slit 6 is formed that penetrates the first piezoelectric film 3a, the second piezoelectric film 3b, the first to fourth electrodes 4a to 4d, and the sacrificial layer, etc., to expose a part of the sacrificial layer. The sacrificial layer is removed from the slit 6, and the void 10 is formed.
[0014] In the manufacturing process described above, it is necessary to reliably remove the sacrificial layer near the joint with the support substrate 1, which is an area where the displacement of the vibration region 7 is large. However, since the vicinity of the joint is far from the slit 6, there is a problem that it takes a long time to remove the sacrificial layer or that it is difficult to remove. This problem occurs not only in piezoelectric devices with a cantilever structure, but also in piezoelectric devices with a bridge structure in which two opposing sides of the vibration region are supported by being joined to a support substrate.
[0015] SUMMARY OF THE PRESENT EMBODIMENTS An object of the present invention is to provide a manufacturing method that can easily form a high-output piezoelectric device. [Means for solving the problem]
[0016] A method for manufacturing a piezoelectric device of the present invention includes the steps of: forming a first laminate in which a first electrode, a first piezoelectric film, and a second electrode are stacked in sequence on a first support substrate; forming a second laminate in which a third electrode, a second piezoelectric film, and a fourth electrode are stacked in sequence on a second support substrate; forming connecting portions spaced apart from each other on at least an area on the second electrode of the first laminate where a vibration region is to be formed, the connecting portions being joined to the second laminate; joining the connecting portions to the fourth electrode of the second laminate, to form a third laminate in which the first laminate and the second laminate are stacked with a gap between the connecting portions by the connecting portions; removing the second support substrate of the third laminate; and removing the first support substrate in an area of the third laminate corresponding to the area where the vibration region is to be formed, to form a vibration region. Effect of the Invention
[0017] According to the method for manufacturing a piezoelectric device of the present invention, a first laminate including a first piezoelectric film and a second laminate including a second piezoelectric film are formed, and at least the vibration region is laminated via a plurality of connecting parts arranged at a distance from each other, so that it is possible to form connecting parts having voids without forming a sacrificial layer that is difficult to remove. As a result, it is possible to easily form a piezoelectric device having a thick vibration region and high output by suppressing an increase in the rigidity of the vibration region. [Brief description of the drawings]
[0018] [Figure 1] 1 is a schematic cross-sectional view illustrating a high-output piezoelectric device proposed by the present applicant. [Diagram 2] 2 is a diagram illustrating an example of an arrangement of slits and connecting portions in the piezoelectric device shown in FIG. 1. [Diagram 3] 3A to 3C are diagrams illustrating an embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to the present invention. [Figure 4] 3A to 3C are diagrams illustrating an embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to the present invention. [Diagram 5] 3A to 3C are diagrams illustrating an embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to the present invention. [Figure 6] 3A to 3C are diagrams illustrating an embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to the present invention. [Figure 7] 3A to 3C are diagrams illustrating an embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to the present invention. [Figure 8] 5A to 5C are diagrams illustrating an embodiment of a manufacturing process in another method for manufacturing a piezoelectric device according to the present invention. [Figure 9] 5A to 5C are diagrams illustrating an embodiment of a manufacturing process in another method for manufacturing a piezoelectric device according to the present invention. [Figure 10] 6A to 6C are diagrams illustrating one embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to another embodiment of the present invention. [Figure 11] 6A to 6C are diagrams illustrating one embodiment of a manufacturing process in a method for manufacturing a piezoelectric device according to another embodiment of the present invention. [Figure 12] FIG. 1 is a schematic cross-sectional view of a conventional piezoelectric device. [Figure 13] FIG. 11 is a schematic plan view illustrating an example of an arrangement of slits in a conventional piezoelectric device. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] The method for manufacturing a piezoelectric device of the present invention will be described with reference to the drawings, but the present invention is not limited to these embodiments, and the members, materials, etc. described below can be modified in various ways within the scope of the present invention. Furthermore, the same reference numerals in the drawings indicate equivalent or identical items, and the size and positional relationship between each component are for the sake of convenience and do not strictly reflect the actual situation.
[0020] Hereinafter, an embodiment of the method for manufacturing a piezoelectric device of the present invention will be described, which is a manufacturing method in which an assembly of a plurality of piezoelectric devices is formed and then separated into individual pieces to simultaneously form a plurality of piezoelectric devices.
[0021] (Manufacturing method for piezoelectric devices 1) 3 to 7 are explanatory diagrams of one embodiment of the manufacturing method of the piezoelectric device of the present invention. First, a first laminate 10A is formed on a first support substrate 1a made of, for example, a silicon substrate, with a first insulating film 2a made of, for example, a thermal oxide film, and a first electrode 4a, a first piezoelectric film 3a, and a second electrode 4b laminated thereon (FIG. 3). Similarly, a second laminate 10B is formed on a second support substrate 1b made of, for example, a silicon substrate, with a third electrode 4c, a second piezoelectric film 3b, and a fourth electrode 4d laminated thereon with a second insulating film 2b made of, for example, a thermal oxide film, and a second laminate 10B is formed on a second support substrate 1b made of, for example, a silicon substrate, with a third insulating film 2b made of, for example, a thermal oxide film, and a fourth electrode 4d laminated thereon. Since the second laminate 10B has the same shape as the first laminate 10A shown in FIG. 3, it is not shown in the figure, and the corresponding reference numerals in FIG. 3 are written in parentheses. The first to fourth electrodes 4a to 4d are made of, for example, molybdenum, and the first piezoelectric film 3a and the second piezoelectric film 3b are made of, for example, aluminum nitride, zinc oxide, PZT (lead zirconate titanate), and the like. The first electrode 4a and the third electrode 4c can be formed simultaneously by placing the first support substrate 1a on which the insulating film 2a is formed and the second support substrate 1b on which the insulating film 2b is formed in a reaction device used for sputtering, for example. Furthermore, the first piezoelectric film 3a and the second piezoelectric film 3b can be formed simultaneously in a reaction device used for sputtering or CVD (Chemical Vapor Deposition). The piezoelectric films formed simultaneously in this manner are preferably piezoelectric films with uniform orientation and piezoelectric characteristics. The first laminate 10A and the second laminate 10B can be configured to include a plurality of regions on which piezoelectric devices are to be formed, but the following description will be given with reference to one region on which piezoelectric devices are to be formed.
[0022] Next, as shown in FIG. 4, a connecting portion 9 made of, for example, polysilicon is formed on the second electrode 4b of the first laminate 10A, and at least a part of the connecting portion 9 in the region where the vibration region is to be formed is removed to form the connecting portion 9a. The connecting portion 9a may have a cylindrical structure. The connecting portions 9a are arranged apart from each other as shown in FIG. 2. Note that 9b is a connecting portion formed together with the connecting portion 9a by removing a part of the connecting portion 9, but the connecting portion 9b is arranged in a region where a slit is to be formed, which will be described later, and is removed by forming the slit (FIG. 4). Also, the second laminate 10B shown in FIG. 4 shows a state in which the surface of the second laminate 10B is arranged facing the surface side of the connecting portion 9 and the like formed on the surface of the first laminate 10A.
[0023] As shown in Fig. 4, the first laminate 10A and the second laminate 10B are arranged, and the surfaces of the connecting portions 9, 9a, and 9b formed on the first laminate 10A are joined to the surface of the fourth electrode 4d of the second laminate 10B to form the third laminate 10C (Fig. 5). This joining forms gaps 10 between the multiple connecting portions 9a. The joining of the surfaces of the connecting portions 9, 9a, and 9b to the surface of the fourth electrode 4d of the second laminate 10B can be performed by indirect joining using a resin such as polyimide or epoxy resin as an adhesive, or by direct joining such as metal joining.
[0024] Thereafter, the second support substrate 1b and the second insulating film 2b are removed from the third laminate 10C to expose the third electrode 4c. The exposed third electrode 4c is patterned, and the second piezoelectric film 3b, the fourth electrode 4d, the connecting portion 9, the second electrode 4b, and a portion of the first piezoelectric film 3a are appropriately removed to form the lead-out electrode 8a connected to the first electrode 4a and the third electrode 4c, and the lead-out electrode 8b connected to the second electrode 4b and the fourth electrode 4d. In FIG. 6, 11 is an insulating film that insulates the lead-out electrode 8a from the second electrode 4b and the fourth electrode 4d. If the second electrode 4b and the fourth electrode 4d are patterned in advance so as not to come into contact with the lead-out electrode 8a, the insulating film 11 is not necessary.
[0025] To form the slits 6, the third electrode 4c, the second piezoelectric film 3b, the fourth electrode 4d, the connecting portion 9b, the second electrode 4b, the first piezoelectric film 3a, and the first electrode 4a are partially removed to expose the surface of the first insulating film 2a. Then, the first support substrate 1a and the first insulating film 2a are partially removed to form a cavity 5. The formation of this cavity 5 forms a vibration region 7. To separate the assembly of the plurality of piezoelectric devices thus formed, cutting grooves 12 are formed in a lattice pattern (FIG. 7), making it possible to simultaneously form a plurality of piezoelectric devices 100 shown in FIG. 1.
[0026] The connecting parts 9a are arranged so that the vibration region 7 has the desired vibration characteristics. As an example, as shown in Figs. 1 and 2, the connecting parts 9a are arranged in a row from the joint part with the support substrate 1 supporting the vibration region 7 to the end of the vibration region 7 in a direction parallel to at least the short side of the rectangular vibration region 7, so that the first piezoelectric film 3a and the second piezoelectric film 3b can be configured to vibrate as one body. Furthermore, by arranging the connecting parts 9a in this way, the gap 10 is also arranged in a direction parallel to the short side of the vibration region 7, and the rigidity of the vibration region 7 is smaller than that of a vibration region of the same thickness constituted by a single piezoelectric film, and is not larger than that of a structure in which the first piezoelectric film 3a and the second piezoelectric film 3b are stacked without the connecting parts 9a in between. In order to obtain the desired vibration characteristics, it is preferable to appropriately change the arrangement of the connecting parts 9a, as well as the shape, the number of connecting parts 9a, the material constituting the connecting parts 9a, etc.
[0027] As described above, the piezoelectric device 100 formed by the manufacturing method of this embodiment can simultaneously form the first piezoelectric film 3a and the second piezoelectric film 3b that constitute the vibration region 7, making it possible to suppress variations in orientation and piezoelectric characteristics. In addition, the first piezoelectric film 3a and the second piezoelectric film 3b are configured to be joined via the connecting portion 9a, and the vibration region 7 can be configured to be thick. Furthermore, by configuring the vibration region 7 to have a gap 10 between the connecting portions 9a, an increase in the rigidity of the vibration region 7 is suppressed, and the gap 10 can be arranged in the vicinity of the joint portion with the support substrate 1 where the displacement of the vibration region 7 is particularly large, and a piezoelectric device with large displacement of the first piezoelectric film 3a and the second piezoelectric film 3b and high output can be easily formed.
[0028] (Manufacturing method for piezoelectric devices 2) Next, an embodiment of a method for manufacturing another piezoelectric device of the present invention will be described. In the above-mentioned method for manufacturing a piezoelectric device 1, as described in Figs. 4 and 5, the connection portion 9a etc. formed on the first laminate 10A is bonded to the fourth electrode 4d of the second laminate 10B, but the shape of the connection portion 9a etc. can be changed in various ways. For example, as shown in Fig. 8, connection portions 9-1, 9a-1 and 9b-1 (corresponding to the first connection portion) made of, for example, polysilicon, and having half the height of the connection portions 9, 9a and 9b described above are formed on the second electrode 4b of the first laminate 10A, and similarly, connection portions 9-2, 9a-2 and 9b-2 (corresponding to the second connection portion) made of, for example, polysilicon, and having half the height of the connection portions 9, 9a and 9b described above are formed on the fourth electrode 4d of the second laminate 10B. The connection portions 9-2, 9a-2 and 9b-2 (corresponding to the second connection portion) are made of, for example, polysilicon, and having half the height of the connection portions 9, 9a and 9b described above, and constitute a connection portion together with the connection portions 9-1, 9a-1 and 9b-1.
[0029] When forming the third laminate 10C, the connecting portion 9-1 is joined to the connecting portion 9-2, the connecting portion 9a-1 is joined to the connecting portion 9a-2, and the connecting portion 9b-1 is joined to the connecting portion 9b-2 (FIG. 9). Since the connecting portions after joining have the same shapes as the connecting portions 9, 9a, and 9b, respectively, the shape of the third laminate 10C is the same as the shape of the third laminate 10C shown in FIG.
[0030] Thereafter, similarly to the above-described piezoelectric device manufacturing method 1, the second support substrate 1b and the second insulating film 2b are removed from the third laminate 10C to expose the third electrode 4c. The third electrode 4c is patterned, and the second piezoelectric film 3b, the fourth electrode 4d, the connecting portions 9-2 and 9-1, the second electrode 4b, and a portion of the first piezoelectric film 3a are appropriately removed to form an extraction electrode 8a connected to the first electrode 4a and the third electrode 4c, and an extraction electrode 8b connected to the second electrode 4b and the fourth electrode 4d.
[0031] To form the slits 6, the third electrode 4c, the second piezoelectric film 3b, the fourth electrode 4d, the connecting portions 9b-1 and 9b-2, the second electrode 4b, the first piezoelectric film 3a, and the first electrode 4a are partially removed to expose the surface of the first insulating film 2a. Then, the first support substrate 1a and the first insulating film 2a are partially removed to form a cavity 5. The formation of this cavity 5 forms a vibration region 7. To separate the assembly of multiple piezoelectric devices, cut grooves 12 are formed in a lattice pattern (FIG. 10). In this way, in the method for manufacturing a piezoelectric device 2, multiple piezoelectric devices 200 shown in FIG. 11 can also be formed simultaneously.
[0032] Although the embodiment of the manufacturing method of the piezoelectric device of the present invention has been described above, the present invention is not limited to these. For example, the shapes of the connecting parts 9a and 9b are not limited to a shape in which two cylindrical shapes are joined. For example, a shape in which a truncated cone is joined, a shape in which a wall shape or a wall-like structure is joined, etc. are also possible, and these shapes can be combined. The arrangement and size of the connecting parts 9a, etc. are arranged so that the vibration region 7 vibrates as desired, and the material constituting the connecting parts 9a, etc. may also be appropriately selected.
[0033] The first to fourth electrodes 4a to 4d do not necessarily need to be formed over the entire surface of the vibration region 7, but may be arranged to sandwich at least the region where the displacement of the first piezoelectric film 3a and the second piezoelectric film 3b occurs. The arrangement of the slits 6 can also be changed, and a bridge structure or a membrane structure can be used in addition to a cantilever structure.
[0034] (summary) (1) In one embodiment of a method for manufacturing a piezoelectric device of the present invention, the method can include the steps of: forming a first laminate in which a first electrode, a first piezoelectric film, and a second electrode are stacked in sequence on a first support substrate; forming a second laminate in which a third electrode, a second piezoelectric film, and a fourth electrode are stacked in sequence on a second support substrate; forming connecting portions spaced apart from each other on at least an area on the second electrode of the first laminate where a vibration region is to be formed, the connecting portions being joined to the second laminate; joining the connecting portions to the fourth electrode of the second laminate to form a third laminate in which the first laminate and the second laminate are stacked with a gap between the connecting portions by the connecting portions; removing the second support substrate of the third laminate; and removing the first support substrate in an area of the third laminate corresponding to the area where the vibration region is to be formed, thereby forming a vibration region.
[0035] (2) By configuring the process to include a step of forming a first connecting portion on the first laminate, the first connecting portion constituting part of the connecting portion in place of the connecting portion, and a step of forming a second connecting portion on the second laminate, the second connecting portion constituting the connecting portion together with the first connecting portion, and the step of forming the third laminate includes a step of joining the first connecting portion and the second connecting portion, and stacking the first laminate and the second laminate by the connecting portion constituted by the first connecting portion and the second connecting portion, it is possible to easily form connecting portions of different shapes.
[0036] (3) The third laminate formed by stacking the first laminate and the second laminate via the connecting portion includes a plurality of piezoelectric device formation regions, and by configuring the process to include a process of forming a plurality of piezoelectric device assemblies and then dicing them into individual piezoelectric devices, a plurality of piezoelectric devices can be easily formed. [Explanation of symbols]
[0037] 100~300 Piezoelectric devices 1a 1st support board 1b Second support board 2. Insulating film 3a First piezoelectric film 3b Second piezoelectric film 4a to 4d, first to fourth electrodes 5, cavity 6, slit 7, vibration region 8a, 8b, lead-out electrodes 9, 9a, 9a-1, 9a-2, 9b, 9b-1, 9b-2, connection parts 10, gap 10A to 10C, first to third laminates 11, insulating film 12, cutting groove
Claims
1. forming a first laminate in which a first electrode, a first piezoelectric film, and a second electrode are laminated in this order on a first support substrate; forming a second laminate in which a third electrode, a second piezoelectric film, and a fourth electrode are laminated in this order on a second support substrate; forming connecting portions spaced apart from each other in at least a region on the second electrode of the first laminate where a vibration region is to be formed, the connecting portions being joined to the second laminate; a step of joining the connecting portion to the fourth electrode of the second stack, and forming a third stack in which the first stack and the second stack are stacked by the connecting portion with a gap between the connecting portions; removing the second support substrate of the third stack; removing the first support substrate from a region of the third laminate corresponding to a region where the vibration region is to be formed, thereby forming a vibration region; A method for manufacturing a piezoelectric device comprising the steps of:
2. forming a first connecting portion on the first laminate in place of the connecting portion and constituting a part of the connecting portion; forming a second connecting portion on the second laminate, the second connecting portion constituting the connecting portion together with the first connecting portion; The step of forming the third stack includes: a step of joining the first connecting portion and the second connecting portion, and stacking the first laminate and the second laminate by the connecting portion constituted by the first connecting portion and the second connecting portion, A method for manufacturing the piezoelectric device according to claim 1.
3. the third laminate formed by stacking the first laminate and the second laminate by the connecting portion includes a plurality of piezoelectric device forming regions, and a step of forming a plurality of piezoelectric device assemblies and then singulating them into individual piezoelectric devices is included. A method for manufacturing the piezoelectric device according to claim 1 or 2.