Composite aerogel with multi-scale porous structure and method for producing the same, seawater desalination apparatus

The pulsed laser-based method for creating silicon-containing composite aerogels with milli-micro-nano multiscale pores addresses the limitations of single-scale structures by enhancing mechanical strength and flame retardancy, improving water transport and light absorption for efficient solar energy applications.

JP2024139672AActive Publication Date: 2024-10-09OCEAN UNIV OF CHINA
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2023197611
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-27
Filing Date
2023-11-21
Publication Date
2024-10-09
Estimated Expiration
2043-11-21

AI Technical Summary

Technical Problem

Existing aerogel materials with single-scale pore structures face limitations in water transport, light absorption, heat conduction, and energy utilization, and methods for creating multiscale pore structures are complex, requiring template agents that complicate the process and affect morphology.

Method used

A pulsed laser-based method using silicon-containing nano-inorganic materials, polyvinyl alcohol, agar, and glutaraldehyde to form a composite aerogel, followed by pulsed laser processing to create customizable milli-micro-nano multiscale pores without a template, enhancing mechanical strength and flame retardancy.

Benefits of technology

The method allows precise control over pore structure and distribution, improving water transport, light absorption, and mechanical properties, enabling efficient solar energy-driven seawater desalination and sewage treatment with enhanced evaporation rates and flame resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024139672000001_ABST
    Figure 2024139672000001_ABST
Patent Text Reader

Abstract

To provide silicon-containing inorganic-organic composite aerogels having a reproducible multi-scale pore structure that is used in materials for converting and utilizing solar energy, and methods for preparing them.SOLUTION: Using silicon-containing nano-inorganic materials as a freezing motif, biomass polymers as a cross-linking agent, and deionized water as the solvent, these three are mixed uniformly, allowing the mixture to leave to solidify to form a hydrogel. The hydrogel is frozen to form a cryohydrate. Then, using freeze-drying technology, the cryohydrate is removed to form a micro-nano scale porous aerogel. Finally, using a pulsed laser technology, the resultant micro-nano scale aerogel is subjected to customized punching of milli-pores to finally obtain a milli-micro-nano multi-scale pore structure aerogel.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the technical field of aerogel material preparation, in particular to the technical field of aerogel material preparation for solar energy conversion and utilization, specifically to a method for preparing and using silicon-containing inorganic-organic composite aerogel with a multi-scale pore structure that can be customized with vertically aligned millipores and three-dimensionally interconnected micro-nanopores. [Background technology]

[0002] As the consumption of non-renewable energy increases, the utilization of renewable energy for energy conversion has become an important development trend in the future. Solar energy is characterized by abundant resources, cleanness and no pollution. The utilization and conversion of solar energy to replace the consumption of some fossil energy is of great significance to environmental protection and sustainable development. The design and development of lightweight, highly efficient and mass-producible solar energy conversion and utilization materials is an important way to realize the practical application of solar energy.

[0003] Aerogel materials have excellent characteristics such as low linear density, light weight, low thermal conductivity, large specific surface area, high porosity, etc., and are widely used in life and production. Aerogel materials are usually formed under supercritical drying or freeze-drying conditions, and have a three-dimensional porous network skeleton structure, and its pore structure characteristics are often affected by both the frozen motif and the crosslinking strength. In order to ensure the strength of aerogel, chemical crosslinking or physical crosslinking is commonly used. Chemical crosslinking means that monomers cause polycondensation or copolymerization reactions under the action of chemical crosslinking agents to form covalent bonds and build a three-dimensional network structure. Physical crosslinking means a three-dimensional polymer network formed by bond crosslinking through physical forces such as hydrogen bonds, coordination bonds, van der Waals forces, and intermolecular entanglement. By selecting crosslinking agents with different characteristics, the pore structure and crosslinking strength of aerogel can be controlled to meet the needs of various use environments. Polyvinyl alcohol is a water-soluble polymer with abundant hydroxyl groups and wide range of uses. It has good film-forming properties, thermal stability, adhesion, wear resistance, self-repairing properties and good mechanical strength. It also has excellent biocompatibility, biodegradability and non-toxicity and harmless properties, and has unique advantages in the field of environmental protection. Agar, as a polysaccharide material with excellent biocompatibility, contains abundant carboxyl groups, can be dissolved at a water temperature of 90°C and hardened at room temperature, and has excellent recyclability. Therefore, by selecting an appropriate crosslinking agent and utilizing multiple crosslinking mechanisms, the crosslinking strength of aerogel can be effectively improved.

[0004] Aerogel materials have the characteristics of controllable pore structure and high porosity. When used in the field of solar energy-driven water evaporation, they can not only provide a significant light absorption area in terms of solar absorption, but also provide abundant passages for water transport and vapor escape. Therefore, aerogel materials have broad application prospects in the fields of seawater desalination, sewage treatment, photothermal catalysis and other fields by solar energy-driven interfacial water evaporation. However, the internal pore size of aerogels is often mesopores with a diameter of 2-50 nm, and aerogels with single pore structure have many limitations in water transport, light absorption, heat conduction, energy utilization, etc., whereas aerogels with multi-scale pore structure can provide a larger specific surface area to absorb solar light, and at the same time, can exert capillary action by controlling the pore size to improve the water supply rate. In addition, by constructing a through-hole structure inside the aerogel, it is possible to use the difference in salt concentration in the longitudinal direction to form a surface tension gradient, exert the Marangoni effect, and promote the migration of salt ions, thereby realizing the design of the anti-salting function of aerogel materials. The synergistic use of the light absorption and material exchange capabilities of the milli-micro-nano multi-scale pore structure provides more application possibilities for aerogels in environmental protection fields such as seawater desalination, wastewater treatment, air purification, etc. Therefore, to ensure structural properties while achieving multifunctionality, the pore size distribution and pore structure of aerogels need to be further controlled and optimized.

[0005] At present, aerogels that have been developed relatively maturely include polymer-based aerogels, biomass aerogels, etc., but such organic aerogels are easily combustible, their pore formation technology and application are severely limited, and it is difficult to precisely control and optimize the pore size. In the reported methods for constructing multi-scale pore structures, one or two pore formation methods are usually used in combination. For example, the preparation method of nitrogen-doped hierarchical pore graphene aerogel disclosed in Patent Document 1 (China Patent Publication No. 109243849) uses CaCO 3 @Polydopamine particles were used as templates, and CaCO was prepared by acid washing. 3However, in this method, a template agent is introduced and the template agent needs to be removed in a subsequent step, which is not only complicated but also does not help to control the pore morphology and structure. Patent Document 2 (China Patent Publication No. 110064347) discloses an inorganic nanofiber / organic polymer composite aerogel prepared by a freeze casting molding method, which has a "layer-stack-layer" structure, but can only provide micro-channels, and has certain limitations in terms of water and gas flux, material exchange and movement. Patent Document 3 (China Patent Publication No. 113578282) discloses an emulsion template method for preparing aerogel materials, but this method has poor controllability over the pore size distribution and pore structure of the aerogel, and is difficult to accurately control the number and distribution of various pore types. Therefore, the development of a technology that does not require a pore-forming template, is simple in process, can be efficiently prepared, and can precisely control the characteristics and distribution of the pore structure to prepare aerogels with multi-scale pore structures and optimized pore sizes is of great significance for improving the efficiency of solar-energy-driven water evaporation and expanding its scope of application. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] China Patent Publication No. 109243849 [Patent Document 2] China Patent Application Publication No. 110064347 [Patent Document 3] China Patent Application Publication No. 113578282 Summary of the Invention [Problem to be solved by the invention]

[0007] In order to precisely control the properties and distribution of the pore structure of aerogels, the present invention provides a pulsed laser-based multi-scale pore aerogel, which not only has three scales of pore size, millimeter-micrometer-nano, simultaneously, but also does not require a pore-forming agent template during preparation. [Means for solving the problem]

[0008] The present invention also provides a method for preparing and using the aerogel.

[0009] In order to achieve the above objectives, the overall idea of ​​the technical solution adopted by the present invention is as follows: First, by utilizing the advantages of the high melting point, excellent high temperature stability and high temperature oxidation resistance of silicon-containing nano-inorganic materials, polyvinyl alcohol, agar and glutaraldehyde as crosslinking agents, and synergistically utilizing physical and chemical crosslinking mechanisms such as hydrogen bonding and polycondensation reaction, a silicon-containing nano-inorganic-organic composite porous double-network aerogel is prepared, which not only ensures the mechanical properties of the aerogel by utilizing the strength and toughness of the polymer material, but also improves the hardness and flame retardant ability of the polyvinyl alcohol / agar aerogel by utilizing the properties of the inorganic material, and provides it with processing versatility based on its enhanced ablation resistance. Second, after preparing the flame-retardant silicon-containing nano-inorganic-organic aerogel, the pulse laser technology with high pulse energy and high processing efficiency is used to produce a simple and efficient process, with the number and distribution of millipores being precisely controlled, and the pore pattern being customizable.

[0010] The specific technical solution is as follows: a multi-scale pore structure aerogel based on pulsed laser, in which silicon-containing nano-inorganic material is used as a freezing motif, biomass polymer is used as a crosslinking agent, and deionized water is used as a solvent, and the three are uniformly mixed and left to solidify to form a silicon-containing inorganic-organic composite hydrogel, and then frozen to form ice crystals, and then freeze-drying technology is used to remove the ice crystals to form a micro-nanoscale silicon-containing inorganic-organic composite aerogel; finally, pulsed laser technology is used to perform customized punching of millipores on the obtained micro-nanoscale silicon-containing inorganic-organic composite aerogel, and the high speed, high energy and designable punching pattern characteristics of the laser are used to design the pore size, pore shape and pore number of the millipores of the aerogel, to obtain a milli-micro-nanoscale multi-scale pore silicon-containing inorganic-organic composite aerogel with a controllable process and capable of meeting the needs of multiple scenes and complex use environments.

[0011] Furthermore, the silicon-containing nano-inorganic material is MoSi 2 , SiO 2 , Si 3 N 4 These include, but are not limited to:

[0012] Furthermore, the cross-linking agent includes at least polyvinyl alcohol, agar, and glutaraldehyde.

[0013] Hereinafter, a method for preparing aerogel with multi-scale pore structure based on the above pulsed laser is provided, which includes steps 1 to 3. Step 1: Preparation of silicon-containing inorganic-organic hybrid hydrogel First, polyvinyl alcohol and agar are weighed, deionized water is added and the mixture is heated to dissolve the two powders into a homogeneous solution, and then a glutaraldehyde solution is added to the solution to crosslink the two powders. Silicon-containing nano-inorganic powder is added to the crosslinking liquid to obtain a homogeneous silicon-containing inorganic-organic composite sol. The silicon-containing inorganic-organic composite sol is allowed to stand and solidify, forming a silicon-containing inorganic-organic hydrogel with a certain toughness. Furthermore, the concentration of the polyvinyl alcohol in the silicon-containing inorganic-organic composite sol system is 1 to 4 wt%, the concentration of the agar in the silicon-containing inorganic-organic composite sol system is 1 to 2 wt%, and the concentration of the silicon-containing nano-inorganic powder in the silicon-containing inorganic-organic composite sol system is 0.02 to 1 wt%. Furthermore, the concentration of the glutaraldehyde solution is 50 wt %. Step 2: Preparation of micro- and nano-scale silicon-containing inorganic-organic composite aerogels The silicon-containing inorganic-organic composite hydrogel obtained in step 1 is frozen to obtain ice crystals, which are then vacuum freeze-dried to obtain micro-nanoscale silicon-containing inorganic-organic composite aerogels; Furthermore, the freezing temperature range of the silicon-containing inorganic-organic composite hydrogel is −30 to −80° C., and the lower the freezing temperature, the smaller the pore size becomes, and the higher the temperature, the larger the pore size becomes. Step 3: Synthesis of silicon-containing inorganic-organic hybrid aerogels with multiscale pores at milli-, micro-, and nano-scales Using pulsed laser processing technology, the resulting micro-nanoscale silicon-containing inorganic-organic composite aerogel is subjected to millipore structure processing. The specific processing method is as follows: The frequency of the pulsed laser is set to 20, the pulse width to 5000, the scanning speed to 50-150 mm / s, the laser power to 3-8%, the laser spot to 1 mm, the shape of the millipores is designed, and the matrix punching programming is performed. Then, the laser light source performs the millipore punching process from top to bottom on the micro-nanoscale silicon-containing inorganic-organic composite aerogel, and the pore size, pore shape, pore number, etc. of the millipores of the aerogel are designed by utilizing the high efficiency, high speed, high energy, and designable characteristics of the punching pattern of the laser, to obtain the milli-micro-nanoscale multi-scale pore silicon-containing inorganic-organic composite aerogel with vertically oriented millipore shape, adjustable porosity. In principle, the pore size of the millipores is controlled by self-programming and is not limited, and the number of millipores is determined by the pore density and the area of ​​the aerogel, and is controlled by self-programming and is not limited. The porosity may be greater than 98%.

[0014] Furthermore, the shape of the millipores includes, but is not limited to, square, circular, and polygonal, and the distribution pattern of the millipores is not limited.

[0015] The multi-scale pore structure aerogel based on the pulsed laser of the present invention can be used in solar energy-driven seawater desalination. The method of use is to combine the aerogel with polystyrene foam and fibrous water-absorbing paper to assemble an evaporator. The silicon-containing inorganic-organic composite aerogel absorbs and converts solar energy to evaporate seawater to obtain fresh water, the polystyrene foam acts as an insulating layer to perform thermal management and suppress the heat conduction loss during the photothermal evaporation process, and the hydrophilic fiber paper transports seawater by capillary force.

[0016] The method for testing the seawater desalination rate of the evaporator is to place the evaporator on an analytical balance, irradiate it with a simulated xenon lamp light source, and continuously record the mass change of the evaporator at different times through a computer connected to the balance, monitor the mass loss, and calculate the evaporation rate. Effect of the Invention

[0017] Compared with the prior art, the technical solution provided by the present invention has the following beneficial effects: (1) The present invention uses polyvinyl alcohol, agar and glutaraldehyde as crosslinking agents, polyvinyl alcohol has a large amount of hydroxyl functional groups on the molecular chain, agar contains a large amount of carboxyl functional groups, hydroxyl groups and carboxyl groups form hydrogen bonds between molecular chains to form a physical crosslinked network, and carboxyl groups and aldehyde groups also undergo polycondensation reaction to form covalent bonds to form a chemical crosslinked network, and the double network structure can not only form a stable three-dimensional porous structure during freeze-drying, but also further improve the strength of the aerogel. These properties not only help ensure the macro-moldability of the aerogel and avoid volumetric shrinkage, but also can increase the compressive strength, improve the swelling resistance, and achieve excellent mechanical properties. (2) The present invention prepares inorganic-organic composite aerogel, and improves the flame retardancy of the aerogel by adding silicon-containing inorganic nanomaterials, and endows it with pulsed laser processability. Compared with the prior art, the pulsed laser shock is used for the first time to perform customized optimization and control of millimeter-scale pores in the aerogel, and is not limited by the size and shape of the template. Diverse designs of millimeter pores can be realized with just simple programming, the method is simple, the process is stable, the reproducibility is good, it is simple and efficient, the cost is low, it is environmentally friendly and pollution-free, the control range of the pore structure is wide, and accurate structure matching design can be performed according to different use scenarios, which has good commercial application prospects in multiple fields and has the potential for large-scale popular application. (3) The present invention obtains a silicon-containing inorganic-organic composite aerogel with a milli-micro-nano multi-scale pore structure that combines vertical alignment and three-dimensional interconnection by blending multi-component materials and combining them with ingenious multi-scale pore structure design, optimizing the pore size distribution, increasing the specific surface area, improving its swelling resistance, and improving water transport performance, material exchange efficiency and self-cleaning function. It has a good evaporation rate in the field of solar energy-driven seawater desalination, and shows the prospect of application in the field of solar energy conversion and utilization, including but not limited to the fields of seawater desalination and wastewater treatment. [Brief description of the drawings]

[0018] In order to more clearly describe the technical solutions of the embodiments of the present invention, the drawings that need to be used in the embodiments are briefly described below. The drawings described below are only some embodiments of the present invention, and those skilled in the art can obtain other drawings based on these drawings without any creative efforts.

[0019] [Figure 1] FIG. 1 is a schematic diagram of the preparation process of milli-micro-nano multi-scale pore structure MoSi2 aerogel of the present invention. [Diagram 2] 1 is a macroscopic photograph of a MoSi2 aerogel with a milli-micro-nano multi-scale pore structure before and after pulse laser punching in Examples 1 to 3 of the present invention. [Diagram 3] FIG. 1 is a SEM image of the multi-scale pore structure MoSi2 aerogel in Example 1 of the present invention, which is composed of four photographs a, b, c, and d, in which photograph a shows the micro-nanoscale pore structure on the surface of MoSi2 aerogel, photograph b shows the microscopic structure in the millimeter-scale pore channel of MoSi2 aerogel after laser punching, photograph c shows the internal pore structure of the original MoSi2 aerogel, and photograph d is an enlarged view of the microscopic structure in the millimeter-scale pore channel of MoSi2 aerogel. [Figure 4]FIG. 2 is a density diagram of the original MoSi2 aerogel of the present invention and the MoSi2 aerogels with multi-scale pore structures synthesized in Examples 1 to 3. [Diagram 5] FIG. 1 shows the swelling performance of the original MoSi2 aerogel of the present invention and the multi-scale pore structure MoSi2 aerogels synthesized in Examples 1 to 3. [Figure 6a] FIG. 2 is an actual diagram of a flame retardancy test of an aerogel before the addition of the MoSi2 nanomaterial of the present invention. [Figure 6b] FIG. 1 is an actual diagram of the flame retardancy test of the aerogel after the addition of MoSi2 nanomaterial of the present invention. [Figure 7a] FIG. 14 is a graph showing the mass loss and evaporation rate of the multi-scale pores of the original MoSi2 aerogel of the present invention at 1x solar intensity within 60 min. [Figure 7b] FIG. 1 is a graph showing the mass loss and evaporation rate of the multi-scale pore MoSi2 aerogels of Examples 1 to 3 of the present invention at 1x solar intensity within 60 min. [Figure 8] FIG. 2 is a photographic illustration of salt self-dissolution over time for the original MoSi2 aerogel of the present invention and the multi-scale pore MoSi2 aerogels of Examples 1 to 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings, in order to make the advantages and features of the present invention easily understandable to those skilled in the art, and to more clearly define the protection scope of the present invention.

[0021] It should be noted that the original MoSi 2 Aerogel is a micro-nanoscale MoSi that does not require laser punching. 2 This refers to aerogel.

[0022] Example 1 Example 1 is a MoSi matrix with 5×5 circular macropores. 2 Taking the preparation of aerogel as an example, referring to FIG. 1, the present invention uses a multi-scale pore structure of milli-micro-nano MoSi2 The preparation method and use of the aerogel are described, including Steps 1 to 3 below. Step 1: MoSi 2 1. Preparation of Hydrogels First, 2 wt% agar and 1 wt% polyvinyl alcohol powder were weighed and placed in a beaker, 100 ml of deionized water was added, heated to 90 °C, and magnetic stirring was maintained for 1 h to dissolve the two powders and obtain a homogeneous solution. Next, 100 μl of glutaraldehyde solution with a concentration of 50 wt% was added to the solution and stirring was continued for 10 minutes. Next, MoSi 2 The powder was weighed and slowly added to the above solution with magnetic stirring until a homogenous black solution was obtained. The black solution obtained above was poured into a prefabricated mold with dimensions of 100 x 100 x 10 mm, and after leaving it to stand for 5 minutes, the solution solidified to produce MoSi 2 A hydrogel was formed. Step 2: MoSi with micro-nanoscale pore structure 2 Preparation of aerogels The MoSi obtained in step 1 2 The hydrogel was placed in a refrigerator at -80 °C and frozen for 24 h to allow ice crystals to solidify. The frozen gel was then taken out and placed in a freeze dryer at -80 °C for 48 h to vacuum dry it, after which it was taken out and the MoSi 2 Aerogel was obtained. Step 3: Milli-micro-nano multi-scale pore MoSi 2 Synthesis of aerogel The aerogel in step 2 was cut to obtain a square aerogel with a size of 30 × 30 mm. The resulting micro-nanoscale MoSi 2 Customized punching process of millipore pattern was carried out on aerogel. The frequency of the laser was set to 20, the pulse width to 5000, the speed to 100 mm / s, the laser power to 8%, the pore shape to 1 mm diameter circle, the pore spacing to set, and the programming design of 5 × 5 matrix circular pores was carried out. Then, the laser was started. The laser source was MoSi2 The aerogel was punched from top to bottom to create millipores. After about 30 seconds, the laser punching was completed, and the aerogel was formed into a P5×5 pattern as shown in Figure 2, and a vertically oriented millipore pattern with through holes and three-dimensionally interconnected micro-nano multi-scale pores as shown in Figure 3. 2 Aerogel was obtained. (5) Use of photovoltaic seawater desalination Through testing, the P5×5 multi-scale pore MoSi 2 The water evaporation rate of aerogel is 1.39 kg m -2 h -1 It was.

[0023] Example 2 Example 2 is a MoSi matrix with 6 x 6 circular millipores. 2 Taking the preparation of aerogel as an example, the preparation method is basically the same as in Example 1, with the difference being that, under the condition of ensuring that the macroscopic shape does not collapse, in order to verify the adjustable mesh number of the millipores of the aerogel in the present invention, the programming design of the 5×5 matrix of circular pores in step 3 in Example 1 is changed to the programming of the 6×6 matrix of circular pores, and other parameters and operation steps of the pulsed laser are not changed, and a multi-scale pore aerogel with a mesh number of P6×6 millipores is obtained, as shown in Figure 2. Through testing, the P6×6 multi-scale pore MoSi 2 The water evaporation rate of aerogel is 1.26 kg m -2 h -1 It was.

[0024] Example 3 Example 3 is a MoSi matrix with 7×7 square pores. 2Taking the preparation of aerogel as an example, the preparation method is basically the same as that in Example 1, with the difference being that in order to verify that the millimeter-scale pore pattern of the aerogel in the present invention can be accurately customized, the programming design of the 5×5 matrix of circular pores in step 3 in Example 1 is changed to the programming design of the 7×7 matrix of square pores, and other parameters and operation steps of the pulsed laser are not changed, and a multi-scale pore aerogel with a mesh number of P7×7 millipores is obtained, as shown in Figure 2. Through testing, the P7×7 multi-scale pore MoSi 2 The water evaporation rate of aerogel is 1.13 kg m -2 h -1 It was. FIG. 2 shows the millimeter-micro-nano multiscale pore structure MoSi before and after pulse laser punching in Examples 1 to 3 of the present invention. 2 1 is a macroscopic photograph of the aerogel. As can be seen from the figure, the MoSi 2 Aerogel has good macroscopic moldability, no cracks or obvious shrinkage deformation on the surface, and good cutting processing properties. After pulsed laser punching, aerogel does not suffer from ablation, structural collapse and other destructive phenomena. With the increase in the mesh number of millipores and the change in pore shape, aerogel still retains the stable macroscopic structural characteristics, and can realize the advantages of customized processing of millipore patterns, adjustable mesh number, controllability of pore size distribution and so on. Multi-scale pore structure MoSi 2 When the aerogel was immersed in water, the surface color turned black, which was due to the removal of gelation. However, no collapse phenomenon occurred in the shape of the pores, and no destruction occurred in the macroscopic shape of the aerogel, proving that the multi-scale pore aerogel retains excellent strength and toughness. FIG. 3 shows the multi-scale pore structure MoSi 2 SEM images of the aerogels. Photo a in the figure shows the MoSi 2It can be seen that the surface of the aerogel has an elliptical micropore structure, and a large number of nanopores are uniformly distributed in the constructed network skeleton. From photo b in the figure, it can be seen that after pulsed laser processing, the pore skeleton of the through hole is carbonized at high temperature, the surface turns black, the cross-linking bonds are broken, and a microscopic structure stacked in layers is formed. Photo d in the figure is a local enlarged view of photo b, and as can be seen from the figure, there are wrinkles on the surface of the pore skeleton after fracture, and it has a gap structure assembled by layers. Photo c in the figure shows the MoSi without laser punching. 2 This is the internal pore structure of the aerogel. As can be seen from the figure, the aerogel skeleton has grown large and has through-holes in one direction. FIG. 4 shows the original MoSi 2 Aerogels and multiscale pore MoSi of Examples 1 to 3 2 A density diagram of aerogel. The densities are 0.039, 0.036, 0.034, and 0.033 g / cm3, respectively. 3 As can be seen from the figure, with the increase in the mesh number of the millipores of the aerogel, its density gradually decreases, but the difference is small, indicating that the impact of laser punching on the quality of the aerogel is small. FIG. 5 shows the original MoSi 2 Aerogels and multiscale pore MoSi of Examples 1 to 3 2 The figure shows the swelling ratio of aerogels. The swelling ratios are 17.3%, 18.8%, 19.3%, and 21.4%, respectively. As can be seen from the figure, with the increase in the mesh size of the millipores of the aerogel, the swelling ratio gradually increases, proving that the water absorption ability of the aerogel is enhanced and the water saturation degree is increased. The reason is that the original MoSi 2 Compared with aerogels, the presence of millipores provides more penetration paths for aqueous solutions, and the breaking of cross-linking bonds reduces the penetration resistance of aqueous solutions, promoting the multiscale pore structure aerogels with more millipores to absorb more water in the same time. 6a and 6b are diagrams showing the MoSi 2The flame retardancy test of aerogel before and after adding nanomaterials. As can be seen from the figure, MoSi 2 Before the addition of nanomaterials, the polyvinyl alcohol / agar aerogel continued to burn within 14 s, whereas the polyvinyl alcohol / agar / MoSi 2 The aerogel self-stopped when the combustion proceeded to 14 s, and MoSi 2 It was demonstrated that the addition of nanomaterials improved the flame retardancy of aerogel. This was due to the addition of MoSi 2 This is because it has high temperature stability, acts as a thermal insulator, and forms a good physical barrier during the combustion process, effectively preventing adjacent parts from continuing to burn. 7a and 7b are the original MoSi 2 Aerogels and multiscale pore MoSi of Examples 1 to 3 2 Figure 7 shows the mass loss and evaporation rate diagrams of the aerogels at 1x solar intensity within 60 min. As can be seen from the mass loss diagram in Figure 7a and the evaporation rate diagram in Figure 7b, the original MoSi 2 The aerogels maintained fast mass loss within the first 30 min of evaporation, but the mass loss clearly slowed within 30–60 min, which was consistent with the original MoSi 2 This is because the water supply is slow due to the large cross-linking degree of the aerogel, and the water supply rate is far behind the evaporation rate. However, when the number of millimeter-scale through-holes is P5×5, the evaporation rate increases significantly, which is due to the faster water supply rate. If the number of millimeter-scale through-holes is further increased, the evaporation rate decreases, which is due to the increase in the number of millimeter-scale meshes, which leads to a decrease in the light absorption area. As can be seen from the above, by controlling the appropriate number of millimeter-scale meshes, and minimizing the area loss under the premise of improving the water supply rate and ensuring the water supply capacity, it is possible to develop a multi-scale pore structure MoSi 2 It can effectively improve the solar energy evaporation performance of aerogel. FIG. 8 shows the original MoSi 2 Aerogels and multiscale pore MoSi of Examples 1 to 3 2The actual diagram of salt self-dissolution in aerogel. As can be seen from the diagram, when salt is deposited on the surface of different aerogels, the salt dissolution efficiency over time is P7×7>P6×6>P5×5>original MoSi 2 aerogels, and compared to the original micro-nanostructured aerogels, the increase in the number of millipore meshes results in the formation of MoSi 2 The internal mass transport efficiency of the aerogel was improved and endowed with self-cleaning capability, further demonstrating the need to design and construct milli-micro-nano multi-scale pore structure aerogels.

[0025] The above are merely specific examples of the present invention, and the scope of protection of the present invention is not limited thereto, and any modifications or replacements that can be conceived without creative efforts should be included within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be based on the scope of protection defined by the claims.

Claims

1. A pulsed laser-based multi-scale pore structure aerogel, comprising: a silicon-containing nano-inorganic material as a frozen motif; a biomass polymer as a crosslinking agent; and deionized water as a solvent; the three are uniformly mixed and allowed to stand to solidify to form a silicon-containing inorganic-organic composite hydrogel; the mixture is then frozen to form ice crystals; the ice crystals are then removed using freeze-drying technology to form a micro-nanoscale silicon-containing inorganic-organic composite aerogel; and finally, the pulsed laser technology is used to perform customized punching of millipores on the obtained micro-nanoscale silicon-containing inorganic-organic composite aerogel; the high speed, high energy and designable punching pattern characteristics of the laser are used to design the pore size, pore shape and number of the millipores of the aerogel, to obtain a milli-micro-nanoscale multi-scale pore structure aerogel, which is process-controllable and can meet the needs of multiple scenes and complex use environments.

2. The silicon-containing nano-inorganic material is MoSi 2 , SiO 2 and Si 3 N 4 2. The pulsed laser based multi-scale pore structure aerogel of claim 1, including, but not limited to:

3. 2. The pulsed laser-based multi-scale pore structure aerogel of claim 1, wherein the cross-linking agent comprises at least polyvinyl alcohol, agar and glutaraldehyde.

4. A method for preparing a multi-scale pore structure aerogel based on pulsed laser according to any one of claims 1 to 3, comprising steps 1 to 3: Step 1: Preparation of silicon-containing inorganic-organic composite hydrogel First, polyvinyl alcohol and agar are weighed, deionized water is added and the mixture is heated to dissolve the two powders into a homogeneous solution, a glutaraldehyde solution is added to the solution to crosslink the two powders, and a homogeneous silicon-containing inorganic-organic composite sol is obtained by adding silicon-containing nano-inorganic powder to the crosslinking liquid. The silicon-containing inorganic-organic composite sol is allowed to stand and solidify, forming a silicon-containing inorganic-organic composite hydrogel with a certain toughness. Step 2: Preparation of micro- and nano-scale silicon-containing inorganic-organic composite aerogels The silicon-containing inorganic-organic composite hydrogel obtained in step 1 is frozen to obtain ice crystals, and then vacuum freeze-dried to obtain a micro-nanoscale silicon-containing inorganic-organic composite aerogel; Step 3: Synthesis of silicon-containing inorganic-organic composite aerogels with milli-, micro-, and nano-scale multi-scale pores Using pulsed laser processing technology, the resulting micro-nanoscale silicon-containing inorganic-organic composite aerogel is subjected to millipore structure processing. The specific processing method is as follows: The method for preparing aerogel with multi-scale pore structure based on pulse laser according to any one of claims 1 to 3, characterized in that: the frequency of the pulse laser is set to 20, the pulse width is set to 5000, the scanning speed is set to 50-150 mm / s, the laser power is set to 3-8%, and the laser spot is set to 1 mm, the shape of the millipore is designed, and the matrix punching program is performed; and then, the laser light source performs the millipore punching process from top to bottom on the micro-nano scale silicon-containing inorganic-organic composite aerogel; and by utilizing the high efficiency, high speed, high energy, and punching pattern designable characteristics of the laser, the pore size, pore shape, and pore number of the millipore of the aerogel are designed, so as to obtain a silicon-containing inorganic-organic composite aerogel with milli-micro-nano multi-scale pores having a shape of the vertically oriented millipores and a tunable porosity.

5. 5. The method for preparing aerogel with multi-scale pore structure based on pulsed laser according to claim 4, characterized in that in step 1, the concentration of said polyvinyl alcohol in the silicon-containing inorganic-organic composite sol system is 1-4 wt%, the concentration of agar in the silicon-containing inorganic-organic composite sol system is 1-2 wt%, and the concentration of silicon-containing nano-inorganic powder in the silicon-containing inorganic-organic composite sol system is 0.02-1 wt%.

6. The method for preparing multi-scale pore structure aerogel based on pulsed laser according to claim 4, characterized in that in step 2, the freezing temperature range of the silicon-containing inorganic-organic composite hydrogel is -30 to -80°C.

7. The method for preparing multi-scale pore structure aerogel based on pulsed laser according to claim 4, characterized in that the shape of the millipores includes but is not limited to square, circular and polygonal.

8. A method for converting and utilizing solar energy, comprising using the pulsed laser-based multi-scale pore structure aerogel according to any one of claims 1 to 3.

Citation Information

Patent Citations

  • Three-dimensional structure body and method of manufacturing same

    JP2007233418A

  • Processing method of aerogel

    JP2019171446A

  • Method for producing hydrophobic aerogel composite gel-like substance having cold resistance and heat insulating property, and related product thereof

    JP2021172566A

  • Nitrogen-doped graded pore graphene aerogel for supercapacitor and preparation method thereof

    CN109243849A

  • Porous aerogel based on bionic vascular bundle microstructure and preparation method and application thereof