Wiring sheet

The wiring sheet design with a low water absorption base material and specific resin layer properties addresses deformation issues, ensuring flatness and functionality in harsh environments, making it suitable for sensor heaters.

JP2024141479APending Publication Date: 2024-10-10LINTEC CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023053162
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Existing wiring sheets used in high temperature and high humidity conditions are prone to deformation, which can lead to sensor malfunctions.

Method used

A wiring sheet design featuring a low water absorption base material layer, a wiring body with conductive linear bodies, a resin layer, and electrodes, where the base material layer has a water absorption rate of 0.3% or less and the resin layer has a storage modulus of 5.0×10^6 Pa to 1.0×10^10 Pa, ensuring the sheet remains flat and functional.

Benefits of technology

The design prevents deformation of the wiring sheet under high temperature and high humidity conditions, maintaining flatness and functionality, suitable for use as a heater in sensors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

To provide a wiring sheet which can prevent deformation of the wiring sheet.SOLUTION: A wiring sheet 100 includes: a low water absorption rate base material layer 1; a wiring body 2 in which a plurality of conductive filaments 21 are disposed at intervals; a resin layer 3 supporting the wiring body 2 directly or indirectly; and a pair of electrodes 4 which directly contacts with the conductive filaments 21.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wiring sheet. [Background technology]

[0002] As an example of a wiring sheet that can be used for a sheet heater, Patent Document 1 discloses a heat generating film in which a transparent resin layer having a recess is disposed on a transparent supporting substrate, and a conductive portion is provided in the recess of the resin layer. In this heat generating film, the transparent supporting substrate is made of a polyester resin, a polyimide resin, a cellulose resin, or the like. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2021 / 157532 Summary of the Invention [Problem to be solved by the invention]

[0004] The heat generating film described in Patent Document 1 makes it possible to manufacture a heater that prevents the bones of the wiring from being exposed. However, it has been found that the wiring sheet described in Patent Document 1 may be deformed when used under high temperature and high humidity conditions. When this planar heat generating film is used as a heater for a sensor, this deformation may cause the sensor to malfunction.

[0005] An object of the present invention is to provide a wiring sheet capable of preventing deformation of the wiring sheet. [Means for solving the problem]

[0006] [1] A low-water-absorption substrate layer, a wiring body in which a plurality of conductive linear bodies are arranged at intervals, a resin layer that directly or indirectly supports the wiring body, and a pair of electrodes that directly contact the conductive linear bodies. Wiring sheet.

[0007] [2] The wiring sheet according to [1], The low water absorption rate base layer has a water absorption rate of 0.3% or less when left for 48 hours at a temperature of 85°C and a humidity of 85% RH. Wiring sheet.

[0008] [3] The wiring sheet according to [1] or [2], The resin layer has a water absorption rate of 0.8% or more when left for 48 hours at a temperature of 85°C and a humidity of 85% RH. Wiring sheet.

[0009] [4] The wiring sheet according to any one of [1] to [3], The storage modulus of the resin layer at 23° C. is 5.0×10 6 Pa or more, 1.0×10 10 Pa or less, Wiring sheet.

[0010] [5] The wiring sheet according to any one of [1] to [4], The low water absorption base layer has a thickness of 0.5 mm or more. Wiring sheet.

[0011] [6] The wiring sheet according to any one of [1] to [5], The transmittance of near-infrared light with a wavelength of 1000 nm is 70% or more. Wiring sheet.

[0012] [8] The wiring sheet according to any one of [1] to [7], Used as a heater for sensors Wiring sheet. Effect of the Invention

[0013] Advantageous Effects of Invention According to one aspect of the present invention, it is possible to provide a wiring sheet capable of preventing deformation of the wiring sheet. [Brief description of the drawings]

[0014] [Figure 1] 1 is a schematic diagram showing a wiring sheet according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view showing the II-II cross section of FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] [Embodiment] Hereinafter, the present invention will be described with reference to the drawings, taking an embodiment as an example. The present invention is not limited to the contents of the embodiment. In the drawings, some parts are illustrated enlarged or reduced in size for ease of explanation.

[0016] (Wiring sheet) As shown in FIGS. 1 and 2, wiring sheet 100 according to this embodiment includes low water absorption substrate layer 1, wiring body 2, resin layer 3, and a pair of electrodes 4. The wiring body 2 is formed by arranging a plurality of conductive linear bodies 21 at intervals. The resin layer 3 directly or indirectly supports the wiring body 2. The electrode 4 is in direct contact with the conductive linear bodies 21.

[0017] The present inventors surmise that the reason why wiring sheet 100 according to this embodiment can prevent deformation of the wiring sheet is as follows. That is, the inventors presume that the reason why the wiring sheet 100 is deformed is that the surface of the substrate in contact with the resin layer 3 swells due to moisture, and the substrate warps due to the dimensional difference with the surface not in contact with the resin layer 3. Specifically, for example, when the resin layer 3 is made of a resin with relatively high water absorption, the moisture in the resin layer 3 comes into contact with the substrate for a long time and penetrates, so that the substrate surface in contact with the resin layer 3 is likely to swell. On the other hand, the substrate surface not in contact with the resin layer 3 is in contact with a gas containing moisture, but the moisture does not penetrate easily and hardly swells. Then, the substrate warps due to the dimensional difference between the surfaces. In contrast, in this embodiment, the substrate is a low water absorption substrate layer 1. This low water absorption substrate layer 1 is difficult to penetrate with moisture and difficult to swell even on the surface in contact with the resin layer 3. Therefore, even when the wiring sheet 100 is used in a high temperature and high humidity environment, the wiring sheet 100 can be prevented from deforming.

[0018] (Low water absorption base material layer) The low water absorption base layer 1 can directly or indirectly support the wiring body 2. Furthermore, the low water absorption base layer 1 can protect one surface of the wiring body 2. From the viewpoint of preventing deformation of wiring sheet 100, the water absorption rate of the low water absorption base layer when left for 48 hours at a temperature of 85° C. and a humidity of 85% RH is preferably 0.35% or less, more preferably 0.3% or less, even more preferably 0.2% or less, and particularly preferably 0.1% or less. This water absorption rate may be 0.0001% or more. This water absorption rate can be measured by the method described in the examples below.

[0019] The material for the low water absorption base layer 1 is preferably resin, glass, or the like, from the viewpoints of strength and handling properties. Examples of the resin include polyethylene, polypropylene, polystyrene, polycarbonate, and polyacetal. Low water absorption base layer 1 may contain a colorant, which can adjust the transmittance of visible light and near infrared light in wiring sheet 100 to within a desired range.

[0020] The thickness of the low water absorption base layer 1 is preferably 0.05 mm or more, more preferably 0.25 mm or more, more preferably 0.5 mm or more, even more preferably 1.0 mm or more, and particularly preferably 1.5 mm or more. The thickness of the low water absorption base layer 1 is preferably 10 mm or less, more preferably 5 mm or less, and even more preferably 3 mm or less. By having the thickness of the low water absorption base layer in this range, deformation when used under high temperature and high humidity can be prevented.

[0021] The flatness of the wiring sheet 100 when used under high temperature and high humidity is preferably 0.3 mm or less, more preferably 0.2 mm or less, even more preferably 0.1 mm or less, and particularly preferably 0.07 mm or less. If the flatness is within this range, the wiring sheet can be used satisfactorily without malfunctioning even when used as a heater for a sensor. A method for measuring the flatness is shown in the examples.

[0022] (Wiring body) The wiring body 2 has a structure in which a plurality of conductive linear bodies 21 are arranged at intervals from one another. The wiring body 2 also has a structure in which a plurality of conductive linear bodies 21 are arranged in a direction intersecting the axial direction of the conductive linear bodies 21.

[0023] The conductive linear body 21 may be linear or wavy in plan view of the wiring sheet 100. Examples of the wave shape include a sine wave, a rectangular wave, a triangular wave, and a sawtooth wave. For example, if the wiring body 2 has such a structure, breakage of the conductive linear body 21 can be suppressed when the wiring sheet 100 is stretched in the axial direction of the conductive linear body 21.

[0024] The volume resistivity of the conductive linear body 21 is 1.0×10 -9 It is preferable that the resistance is Ω·m or more, and 3.0×10 -9 More preferably, it is 1.0×10 -8 The volume resistivity of the conductive linear body 21 is preferably 1.0×10-3 It is preferable that the resistance is Ω·m or less, and 1.0×10 -4 It is more preferable that the resistance is 1.0×10 -5 It is more preferable that the volume resistivity is Ω·m or less. When the volume resistivity of the conductive linear body 21 is in the above range, the surface resistance of the wiring body 2 tends to decrease. The volume resistivity of the conductive linear body 21 was measured as follows. Silver paste was applied to the end of the conductive linear body 21 and a portion 40 mm from the end, and the resistance of the end and a portion 40 mm from the end was measured. Then, the cross-sectional area (unit: m 2 ) is multiplied by the resistance value and the obtained value is divided by the measured length (0.04 m) to calculate the volume resistivity of the conductive linear body 21.

[0025] The cross-sectional shape of the conductive linear body 21 is not particularly limited and may be polygonal, flat, elliptical, circular, etc. From the viewpoint of compatibility with the resin layer 3, etc., the cross-sectional shape of the conductive linear body 21 is preferably elliptical or circular.

[0026] When the cross section of the conductive linear member 21 is circular, the diameter D (see FIG. 2) of the conductive linear member 21 is preferably 3 μm or more and 200 μm or less. From the viewpoints of suppressing an increase in sheet resistance and improving the heat generation efficiency and dielectric breakdown resistance characteristics of the wiring sheet 100, the diameter D of the conductive linear member 21 is more preferably 4 μm or more, and even more preferably 5 μm or more. The diameter D of the conductive linear member 21 is more preferably 150 μm or less, even more preferably 100 μm or less, particularly preferably 50 μm or less, and extremely preferably 20 μm or less. When the cross section of the conductive linear body 21 is elliptical, it is preferable that the major axis is in the same range as the diameter D described above.

[0027] The diameter D of the conductive linear body 21 is determined by observing the conductive linear body 21 using a digital microscope, measuring the diameter of the conductive linear body 21 at five randomly selected points, and averaging the measured values.

[0028] The interval L (see FIG. 2) between the conductive linear members 21 is preferably 0.3 mm or more, more preferably 0.5 mm or more, even more preferably 0.8 mm or more, and particularly preferably 1.5 mm or more. The interval L between the conductive linear members 21 is preferably 50 mm or less, more preferably 30 mm or less, even more preferably 20 mm or less, and particularly preferably 5 mm or less. If the spacing between conductive linear bodies 21 is within the above range, the conductive linear bodies are relatively densely packed, which improves the function of wiring sheet 100, such as maintaining the resistance of wiring body 2 low.

[0029] The interval L between the conductive linear bodies 21 is measured by, for example, observing the conductive linear bodies 21 of the wiring body 2 using a digital microscope and measuring the interval between two adjacent conductive linear bodies 21. The interval between two adjacent conductive linear bodies 21 is the length along the direction in which the conductive linear bodies 21 are arranged, and is the length between opposing portions of the two conductive linear bodies 21 (see FIG. 2). When the conductive linear bodies 21 are arranged at uneven intervals, the interval L is the average value of the intervals between all adjacent conductive linear bodies 21.

[0030] The conductive linear body 21 may be produced by any method, such as etching, screen printing, or inkjet printing, but may be a linear body including a metal wire (hereinafter also referred to as a "metal wire linear body"). Metal wires have high thermal conductivity, high electrical conductivity, and high handling properties. The metal wire linear body can greatly reduce resistance, and even if the diameter of the metal wire linear body is extremely small, it can pass a current required for heating the wiring sheet 100. This makes it possible to make the conductive linear body 21 less visible. That is, when a metal wire linear body is used as the conductive linear body 21, the resistance value of the wiring body 2 can be reduced while the light transmittance can be improved. In addition, the wiring sheet 100 can easily generate heat quickly. Furthermore, as described above, a linear body having a small diameter can be easily obtained. In addition, examples of the conductive linear body 21 include a linear body containing a carbon nanotube and a linear body in which a conductive coating is applied to a thread, in addition to a metal wire linear body.

[0031] The metal wire linear body may be a linear body made of a single metal wire, or may be a linear body made of a plurality of twisted metal wires. Examples of the metal wire include wires containing metals such as copper, aluminum, tungsten, iron, molybdenum, nickel, titanium, silver, and gold, or alloys containing two or more metals (for example, steels such as stainless steel and carbon steel, brass, phosphor bronze, zirconium copper alloys, beryllium copper, iron nickel, nichrome, nickel titanium, Kanthal, Hastelloy, and rhenium tungsten). The metal wire may be plated with gold, tin, zinc, silver, nickel, chromium, nickel chromium alloys, or solder, or may be coated with a carbon material or polymer, which will be described later. In particular, wires containing one or more metals selected from tungsten and molybdenum, and alloys containing these metals, are preferred from the viewpoint of low volume resistivity. The metal wire may be a metal wire coated with a carbon material. When the metal wire is coated with a carbon material, the metallic luster is reduced, and the presence of the metal wire can be easily made less noticeable. In addition, when the metal wire is coated with a carbon material, metal corrosion is also suppressed. Examples of the carbon material that coats the metal wire include amorphous carbon such as carbon black, activated carbon, hard carbon, soft carbon, mesoporous carbon, and carbon fiber; graphite, fullerene, graphene, and carbon nanotubes.

[0032] The conductive linear body 21 may be a linear body having a conductive coating applied to the thread. Examples of the thread include threads spun from resins such as nylon or polyester. Examples of the thread include threads of metal fibers, carbon fibers, or ion-conductive polymer fibers. Examples of the conductive coating include coatings of metals, conductive polymers, or carbon materials. The conductive coating can be formed by plating, vapor deposition, or the like. A linear body having a conductive coating applied to the thread can improve the conductivity of the linear body while maintaining the flexibility of the thread. In other words, it becomes easier to reduce the resistance of the wiring body 2.

[0033] (Resin layer) The resin layer 3 directly or indirectly supports the wiring body 2. In addition, the resin layer 3 can stabilize the resistance value of the wiring body 2. That is, the resin layer 3 can fix the conductive linear body 21 and stabilize the contact between the conductive linear body 21 and the electrode 4, making it difficult for an increase in the resistance value to occur. From the viewpoint of stabilizing the resistance value of the wiring body 2, the storage modulus of the resin layer 3 at 23° C. is set to 5.0×10 6 Pa or more, 1.0×10 10 From the same viewpoint, the storage modulus of the resin layer 3 at 23° C. is preferably 5.0×10 7 More preferably, the pressure is 5.0×10 Pa or more. 8 The storage modulus of the resin layer at 23° C. is preferably 7.0×10 Pa or more. 9 Pa or less, and more preferably 4.0×10 9 It is more preferable that the pressure is 0.1 Pa or less. From the same viewpoint, the storage modulus of the resin layer 3 at 105° C. is 5.0×10 7 Pa or more, and 5.0×10 8 The storage modulus of the resin layer 3 at 105° C. is preferably 7.0×10 9 Pa or less, and 4.0×10 9 It is more preferable that the pressure is 0.1 Pa or less. The storage modulus can be measured by the method described in the Examples below.

[0034] The water absorption rate of the resin layer 3 when left for 48 hours at a temperature of 85°C and a humidity of 85%RH is preferably 0.8% or more, more preferably 1.2% or more, and even more preferably 1.6% or more. The higher the water absorption rate, the more likely the wiring sheet 100 is to deform, but since the wiring sheet 100 has water-absorbing functional groups, it is possible to obtain a wiring sheet 100 that is excellent in processability during manufacturing, durability, and handling. In this embodiment, since the low water absorption rate base layer 1 is used, even if the water absorption rate of the resin layer 3 is within the above range, the wiring sheet 100 can be prevented from deforming. The water absorption rate may be 10% or less. The water absorption rate can be measured by the method described in the examples described later.

[0035] The thickness of the resin layer 3 is not particularly limited. The thickness of the resin layer 3 may be equal to or greater than the diameter D of the conductive linear body 21, or may be less than the diameter D of the conductive linear body 21. If the thickness of the resin layer 3 is equal to or greater than the diameter D of the conductive linear body 21, the wiring body 2 can be included in the resin layer 3. If the thickness of the resin layer 3 is less than the diameter D of the conductive linear body 21, the wiring body 2 is exposed from the resin layer 3. In addition, when the wiring body 2 is exposed from the resin layer 3, the wiring body 2 may be exposed on the side of the low water absorption base layer 1, or may be exposed on the opposite side of the low water absorption base layer 1. The thickness of the resin layer 3 is preferably 1 μm or more, more preferably 5 μm or more, and even more preferably 10 μm or more. The thickness of the resin layer 3 is preferably 100 μm or less, more preferably 50 μm or less, and even more preferably 30 μm or less.

[0036] From the viewpoint of setting the storage modulus within the above range, the resin layer 3 is preferably a layer made of a cured product of a curable adhesive. Examples of the curable adhesive include a thermosetting adhesive that is cured by heat, and an energy ray curable adhesive. Examples of the energy ray include ultraviolet rays, visible energy rays, infrared rays, and electron beams. Note that "energy ray curing" also includes heat curing by heating using energy rays.

[0037] The thermosetting adhesive preferably contains a thermosetting resin. The thermosetting resin is not particularly limited, and specifically includes epoxy resin, phenol resin, melamine resin, urea resin, polyester resin, urethane resin, acrylic resin, benzoxazine resin, phenoxy resin, amine-based compound, and acid anhydride-based compound. These can be used alone or in combination of two or more. Among these, from the viewpoint of suitability for curing using an imidazole-based curing catalyst, it is preferable to use epoxy resin, phenol resin, melamine resin, urea resin, amine-based compound, and acid anhydride-based compound, and particularly from the viewpoint of showing excellent curing properties, it is preferable to use epoxy resin, phenol resin, a mixture thereof, or a mixture of epoxy resin and at least one selected from the group consisting of phenol resin, melamine resin, urea resin, amine-based compound, and acid anhydride-based compound, and it is preferable to use epoxy resin.

[0038] As the epoxy resin, a cyclic one such as an aromatic epoxy resin or an alicyclic epoxy resin is preferable from the viewpoint of increasing the storage modulus of the resin layer 3. An epoxy resin having a flexible segment such as an oxyalkylene chain tends to decrease the storage modulus of the resin layer 3.

[0039] The energy ray curable adhesive preferably contains an energy ray curable resin. Examples of the energy ray curable resin include a compound having at least one polymerizable double bond in the molecule, and an acrylate compound having a (meth)acryloyl group is preferable.

[0040] Examples of the acrylate compounds include dicyclopentadiene diacrylate, trimethylolpropane tri(meth)acrylate, tetramethylolmethane tetra(meth)acrylate, pentaerythritol tri(meth)acrylate, pentaerythritol tetra(meth)acrylate, dipentaerythritol monohydroxypenta(meth)acrylate, dipentaerythritol hexa(meth)acrylate, 1,4-butylene glycol di(meth)acrylate, and 1,6-hexanediol di(meth)acrylate. acrylate and other linear aliphatic skeleton-containing (meth)acrylates; dicyclopentanyl di(meth)acrylate and other cyclic aliphatic skeleton-containing (meth)acrylates; polyethylene glycol di(meth)acrylate and other polyalkylene glycol (meth)acrylates; oligoester (meth)acrylates, urethane (meth)acrylate oligomers, epoxy-modified (meth)acrylates, polyether (meth)acrylates other than polyalkylene glycol (meth)acrylates, and itaconic acid oligomers.

[0041] The weight average molecular weight (Mw) of the energy ray curable resin is preferably 100 or more, and more preferably 300 or more. Moreover, this weight average molecular weight is preferably 30,000 or less, and more preferably 10,000 or less. In this specification, the weight average molecular weight is a value measured by gel permeation chromatography (GPC) in terms of standard polystyrene.

[0042] The adhesive may contain one type of energy ray curable resin or two or more types. When the adhesive contains two or more types of energy ray curable resins, the combination and ratio thereof can be selected arbitrarily.

[0043] When an energy ray curable resin or a thermosetting resin is used, it is preferable to use a photopolymerization initiator, a thermal polymerization initiator, etc. By using a photopolymerization initiator, a thermal polymerization initiator, etc., the polymerization reaction of the curable resin can be easily initiated, and the curing reaction can be easily controlled.

[0044] Examples of the photopolymerization initiator include photoradical polymerization initiators such as benzophenone, acetophenone, benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin isopropyl ether, benzoin isobutyl ether, benzoin benzoic acid, benzoin methyl benzoate, benzoin dimethyl ketal, 2,4-diethylthioxanthone, 1-hydroxycyclohexyl phenyl ketone, benzyl diphenyl sulfide, tetramethylthiuram monosulfide, azobisisobutyronitrile, 2-chloroanthraquinone, diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide, and bis(2,4,6-trimethylbenzoyl)-phenyl-phosphine oxide.

[0045] In addition to the photoradical polymerization initiator, the photocationic polymerization initiator can be used. The photocationic polymerization initiator is a compound that generates cationic species when irradiated with energy rays and initiates the curing reaction of a cationic curable compound, and is composed of a cationic moiety that absorbs energy rays and an anionic moiety that serves as an acid generating source.

[0046] Examples of the photocationic polymerization initiator include sulfonium salt compounds, iodonium salt compounds, phosphonium salt compounds, ammonium salt compounds, antimony salt compounds, diazonium salt compounds, selenium salt compounds, oxonium salt compounds, bromine salt compounds, etc. Among these, from the viewpoints of excellent compatibility and excellent storage stability of the resulting adhesive, sulfonium salt compounds are preferred, and aromatic sulfonium salt compounds having an aromatic group are more preferred.

[0047] Examples of the sulfonium salt compounds include triphenylsulfonium hexafluorophosphate, triphenylsulfonium hexafluoroantimonate, and triphenylsulfonium tetrakis(pentafluorophenyl)borate.

[0048] Examples of iodonium salt compounds include diphenyliodonium tetrakis(pentafluorophenyl)borate, diphenyliodonium hexafluorophosphate, and (tricumyl)iodonium tetrakis(pentafluorophenyl)borate.

[0049] Examples of the phosphonium salt compounds include tri-n-butyl(2,5-dihydroxyphenyl)phosphonium bromide and hexadecyltributylphosphonium chloride.

[0050] Examples of the ammonium salt compound include benzyltrimethylammonium chloride, phenyltributylammonium chloride, and benzyltrimethylammonium bromide.

[0051] Examples of antimonate compounds include triphenylsulfonium hexafluoroantimonate, p-(phenylthio)phenyldiphenylsulfonium hexafluoroantimonate, and diaryliodonium hexafluoroantimonate.

[0052] Examples of the thermal polymerization initiator include peroxodisulfates such as hydrogen peroxide, ammonium peroxodisulfate, sodium peroxodisulfate, and potassium peroxodisulfate; azo compounds such as 2,2'-azobis(2-amidinopropane) dihydrochloride, 4,4'-azobis(4-cyanovaleric acid), 2,2'-azobisisobutyronitrile, and 2,2'-azobis(4-methoxy-2,4-dimethylvaleronitrile); and thermal radical polymerization initiators such as organic peroxides such as benzoyl peroxide, lauroyl peroxide, peracetic acid, persuccinic acid, di-t-butyl peroxide, t-butyl hydroperoxide, and cumene hydroperoxide.

[0053] In addition to the above-mentioned thermal radical polymerization initiator, the thermal cationic polymerization initiator can be used as the thermal polymerization initiator. The thermal cationic polymerization initiator is a compound that can generate cationic species that initiate polymerization by heating. The thermal cationic polymerization initiator can be a sulfonium salt, a quaternary ammonium salt, a phosphonium salt, a diazonium salt, an iodonium salt, or the like. Among these, the sulfonium salt is preferred from the viewpoints of easy availability and easy production of a product with superior adhesion and transparency.

[0054] Examples of the sulfonium salt include triphenylsulfonium tetrafluoroborate, triphenylsulfonium hexafluoroantimonate, and triphenylsulfonium hexafluoroarsinate.

[0055] Examples of the quaternary ammonium salt include tetrabutylammonium tetrafluoroborate, tetrabutylammonium hexafluorophosphate, and tetrabutylammonium hydrogen sulfate. Examples of the phosphonium salt include ethyltriphenylphosphonium hexafluoroantimonate and tetrabutylphosphonium hexafluoroantimonate.

[0056] Examples of the diazonium salt include benzene diazonium chloride, etc. Examples of the iodonium salt include diphenyl iodonium hexafluoroarsinate, bis(4-chlorophenyl) iodonium hexafluoroarsinate, bis(4-bromophenyl) iodonium hexafluoroarsinate, phenyl(4-methoxyphenyl) iodonium hexafluoroarsinate, etc.

[0057] These polymerization initiators can be used alone or in combination of two or more. When these polymerization initiators are used to form a crosslinked structure, the amount used is preferably 0.1 parts by mass or more and 30 parts by mass or less, more preferably 0.3 parts by mass or more and 20 parts by mass or less, and particularly preferably 0.5 parts by mass or more and 10 parts by mass or less, relative to 100 parts by mass of the energy ray-curable resin or the thermosetting resin.

[0058] When a thermosetting resin is used, a curing catalyst such as an imidazole-based curing catalyst may be used.

[0059] In this embodiment, the curable adhesive may contain a flexibility adjusting component together with the energy ray curable resin or the thermosetting resin in order to easily maintain the sheet shape before curing. Examples of polymers used as the flexibility adjusting component include phenoxy resin, polyolefin resin or modified product thereof, polyamideimide resin, polyimide resin, rubber resin, and acrylic resin.

[0060] These flexibility adjusting components may be used alone or in combination of two or more.

[0061] When the curable adhesive used in this embodiment contains a flexibility adjusting component, the total amount of the energy ray curable resin and the thermosetting resin contained in the adhesive is preferably 15 parts by mass or more and 300 parts by mass or less, more preferably 30 parts by mass or more and 250 parts by mass or less, and even more preferably 60 parts by mass or more and 200 parts by mass or less, relative to 100 parts by mass of the flexibility adjusting component, from the viewpoint of adjusting the storage modulus of the resin layer 3 to the above-mentioned range. In addition, when the adhesive contains an energy ray curable resin or a thermosetting resin but does not contain a flexibility adjusting component, the storage modulus of the resin layer 3 tends to be too high.

[0062] In this embodiment, it is preferable that the curable adhesive does not contain a filler. When the adhesive does not contain a filler, it is possible to prevent the storage modulus of the resin layer 3 at 23° C. from becoming too high. However, the curable adhesive may contain a filler as long as the storage modulus of the resin layer 3 at 23° C. can be adjusted to fall within the above range.

[0063] Examples of the filler include inorganic powders such as silica, alumina, talc, calcium carbonate, titanium white, red iron oxide, silicon carbide, and boron nitride; beads obtained by sphering inorganic powders, single crystal fibers, and glass fibers. Among these, silica filler and alumina filler are preferred. The filler may be used alone or in combination of two or more.

[0064] In this embodiment, the curable adhesive may contain a colorant, which can adjust the transmittance of visible light and near-infrared light through wiring sheet 100 to within a desired range. In this embodiment, a colored layer may be provided in addition to the low water absorption base layer 1, the wiring body 2, and the resin layer 3. By providing a colored layer, the transmittance of visible light and near infrared light in the wiring sheet 100 can be adjusted to within a desired range. The composition of the colored layer is not particularly limited, but by using an infrared transmitting ink, the transmittance of visible light and near infrared light in wiring sheet 100 can be adjusted to fall within a desired range.

[0065] The curable adhesive may contain other components, such as well-known additives, such as organic solvents, coupling agents, flame retardants, tackifiers, UV absorbers, antioxidants, preservatives, fungicides, plasticizers, defoamers, and wettability adjusters.

[0066] (electrode) The electrodes 4 are used to supply a current to the conductive linear body 21. The electrodes 4 are in a pair. The electrodes 4 are in direct contact with the conductive linear body 21. The electrodes 4 are disposed so as to be electrically connected to both ends of the conductive linear body 21. The electrode 4 can be formed using a known electrode material. Examples of the electrode material include a conductive paste such as silver paste, a metal foil such as copper foil, and a metal wire. When the electrode material is a metal wire, the metal wire may be one piece, but is preferably two or more pieces.

[0067] When the electrode material is a metal foil or metal wire, the metal of the metal foil or metal wire may be copper, aluminum, tungsten, iron, molybdenum, nickel, titanium, silver, gold, or other metals; or alloys containing two or more metals such as stainless steel, carbon steel, or other steel, brass, phosphor bronze, zirconium copper alloy, beryllium copper, iron nickel, nichrome, nickel titanium, Kanthal, Hastelloy, and rhenium tungsten. The metal foil or metal wire may be plated with gold, tin, zinc, silver, nickel, chrome, nickel chrome alloy, solder, or the like.

[0068] The width of at least one of the electrodes 4 is preferably 10 mm or less, and more preferably 3 mm or less, in a plan view of the wiring sheet 100. The width of this electrode is preferably 0.1 mm or more. When at least one of the electrodes is a metal wire, the width of the electrode is the diameter of the metal wire, and when two or more metal wires are used, the width of one electrode refers to the sum of the diameters of the metal wires when the metal wires are arranged side by side, or refers to the long diameter of the bundle of metal wires when viewed in a plan view.

[0069] The thickness of the electrode 4 is preferably 2 μm or more, more preferably 5 μm or more, and even more preferably 10 μm or more. The thickness of the electrode 4 is preferably 200 μm or less, more preferably 100 μm or less, even more preferably 50 μm or less, and particularly preferably 25 μm or less. If the thickness of the electrode 4 is within the above range, the electrical conductivity is high and the resistance is low, and the resistance value with the wiring body 2 can be kept low. In addition, sufficient strength as an electrode is obtained. In addition, when the electrode is a metal wire, the thickness of the electrode is the diameter of the metal wire.

[0070] (Wiring sheet) In the wiring sheet 100 according to this embodiment, the transmittance of near-infrared light with a wavelength of 1000 nm is preferably 70% or more, more preferably 80% or more, and even more preferably 85% or more. When this transmittance is equal to or greater than the lower limit, the wiring sheet 100 can be used as a heater for an optical sensor. The transmittance may be less than 100%. The transmittance can be measured by the method described in the examples below. Moreover, the transmittance of visible light in the wavelength range of 380 nm to 780 nm is not particularly limited. For example, in the case of a transparent wiring sheet 100, this transmittance is preferably high. On the other hand, in the case of a non-transparent wiring sheet 100, this transmittance is preferably 10% or less, and more preferably 5% or less. When this transmittance is equal to or less than the upper limit, the wiring sheet 100 can be used as a black planar heater. This transmittance may be more than 0%. This transmittance can be measured by the method described in the examples below.

[0071] The wiring sheet 100 according to the present embodiment can be suitably used, for example, as a planar heater. Since the wiring sheet 100 according to the present embodiment can prevent deformation as described above, it can be particularly suitably used as a heater that requires high flatness even when used in harsh environments such as high temperature and high humidity. Examples of such applications include sensors.

[0072] (Method of manufacturing wiring sheet) There are no particular limitations on the method for manufacturing interconnect sheet 100 according to this embodiment. Interconnect sheet 100 can be manufactured, for example, by the following steps. First, a process for producing a wiring film including the wiring body 2 is performed. In this process, a thermosetting adhesive for forming the resin layer 3 is applied onto a release film to form a coating film. Next, the coating film is dried to produce an adhesive layer. Next, the conductive linear bodies 21 are arranged on the adhesive layer to form the wiring body 2. For example, in a state where an adhesive layer with a release film is arranged on the outer circumferential surface of a drum member, the conductive linear bodies 21 are wound spirally on the adhesive layer while rotating the drum member. Then, the bundle of conductive linear bodies 21 wound spirally is cut along the axial direction of the drum member. This forms the wiring body 2 and places it on the adhesive layer. In this way, a wiring film in which the wiring body 2 is formed on the adhesive layer with a release film is obtained. According to this method, for example, by moving the unwinding portion of the conductive linear bodies 21 along a direction parallel to the axis of the drum member while rotating the drum member, it is easy to adjust the interval L between adjacent conductive linear bodies 21 in the wiring body 2. Next, a step is performed to provide a pair of electrodes 4 on the low water absorption base layer 1. In this step, for example, a conductive paste or the like is printed in a predetermined arrangement on the low water absorption base layer 1, and then dried, so that the pair of electrodes 4 can be provided. Next, a process is performed in which a wiring film is placed on the low water absorption base layer 1 provided with the pair of electrodes 4, and the thermosetting adhesive is cured. In this process, the wiring film is bonded onto the low water absorption base layer 1 provided with the pair of electrodes 4 so that the pair of electrodes 4 contact both ends of the conductive linear body 21 in the wiring body 2 of the wiring film. Then, after removing the release film, a predetermined heat treatment is performed on the thermosetting adhesive to form a resin layer 3, and the wiring sheet 100 is produced.

[0073] (Effects of the First Embodiment) According to this embodiment, the following advantageous effects can be obtained. (1) According to the present embodiment, deformation of wiring sheet 100 can be prevented even when used in a high-temperature and high-humidity environment. (2) According to this embodiment, the resin layer 3 can fix the conductive linear body 21, suppress deformation in the thickness direction inside the wiring sheet 100, stabilize the contact between the conductive linear body 21 and the electrode 4, and stabilize the resistance value of the wiring body 2. (3) According to this embodiment, the storage modulus of the resin layer 3 at 23° C. is set to 5.0×10 6 Pa or more, 1.0×10 10 By setting the pressure to be equal to or less than Pa, when wiring sheet 100 is deformed, conductive linear body 21 can be fixed while preventing the connection portion between conductive linear body 21 and electrode 4 from being destroyed. (4) According to the present embodiment, by making the transmittance of wiring sheet 100 to near-infrared rays at a wavelength of 1000 nm 70% or more, wiring sheet 100 can be used as a heater for an optical sensor.

[0074] [Modifications of the embodiment] The present invention is not limited to the above-described embodiment, and any modifications or improvements that can achieve the object of the present invention are included in the present invention. For example, in the above-described embodiment, the wiring sheet 100 is used as a film-like planar heater, but is not limited thereto. For example, the wiring sheet 100 may be attached to an adherend. In this case, it is preferable to attach the wiring film to the adherend with an adhesive for forming the resin layer 3, and then harden the adhesive to produce an adherend to which the wiring sheet 100 is attached. EXAMPLES

[0075] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples in any way. Moreover, the wiring sheets obtained in the examples were evaluated as follows.

[0076] [Water absorption measurement] A resin layer sheet was prepared from the same composition as that forming the resin layer to be measured, and used as a sample. In addition, a substrate to be measured was prepared, and used as a sample. These samples were left standing for 48 hours under high temperature and high humidity conditions of a temperature of 85°C and a humidity of 85RH%, and then the masses of these samples before and after being left standing under high temperature and high humidity were measured, and the water absorption rate was calculated from the following formula. Water absorption rate=(W2-W1) / W1×100(%) W1: Mass of the sample before placing it under high temperature and high humidity W2: Mass of the sample after being left in a high temperature and high humidity environment

[0077] [Flatness evaluation] The wiring sheet was left to stand for 48 hours under conditions of a temperature of 85°C and a humidity of 85 RH%, and then the flatness of the wiring sheet was measured by placing the wiring sheet on a JIS standard class 0 (JIS B7513:1992) granite precision plate and sliding it over the plate with a constant pressure thickness gauge "PG-02J" manufactured by Techclock Corporation attached to the edge, and recording the fluctuation range of the thickness gauge value using the maximum deflection type flatness measurement method.

[0078] [Storage modulus measurement] A cylindrical test sample with a diameter of 8 mm and a thickness of 1 mm was prepared from the same composition as the composition forming the layer to be measured. The storage modulus of the test sample was measured using a viscoelasticity measuring device (manufactured by Anton Paar, device name "MCR300") with a parallel plate with a diameter of 8 mm as a measuring jig under the conditions of a test start temperature of -20°C, a test end temperature of 150°C, a heating rate of 3°C / min, and a frequency of 1 Hz.

[0079] [Transmittance measurement] The transmittance of the wiring sheet to near-infrared light (1000 nm) was measured using an ultraviolet-visible-near-infrared spectrophotometer (manufactured by Shimadzu Corporation, product name "UV-VIS-NIR SPECTROPHOTOMETER UV-3600").

[0080] [Preparation Example 1] A curable adhesive was obtained by blending 100 parts by mass of a phenoxy resin (manufactured by Mitsubishi Chemical Corporation, product name "YX7200B35") with 170 parts by mass of a polyfunctional hydrogenated bisphenol A diglycidyl ether epoxy compound (manufactured by Mitsubishi Chemical Corporation, product name "YX8000"), 0.2 parts by mass of a silane coupling agent (manufactured by Shin-Etsu Chemical Co., Ltd., product name "KBM-4803"), 2 parts by mass of a thermal cationic polymerization initiator (manufactured by Sanshin Chemical Industry Co., Ltd., product name "San-Aid SI-B3"), and 2 parts by mass of a thermal cationic polymerization initiator (manufactured by Sanshin Chemical Industry Co., Ltd., product name "San-Aid SI-B7").

[0081] [Example 1] (Preparation of wiring film) The curable adhesive obtained in Preparation Example 1 was applied to a 38 μm-thick release film (manufactured by Lintec Corporation, product name "SP-382150") to a thickness of 15 μm, and cut into a rectangle of 250 mm × 320 mm to prepare an adhesive sheet. A gold-plated tungsten wire (diameter 10 μm, hereinafter also referred to as wire) was prepared as a conductive linear body. Next, the obtained adhesive sheet was wound around a drum member with a rubber outer circumferential surface, with the surface of the pressure-sensitive adhesive layer facing outward and without wrinkles, and both ends of the adhesive sheet in the circumferential direction were fixed with double-sided tape. The wire wound around the bobbin was attached to the surface of the pressure-sensitive adhesive layer of the adhesive sheet located near the end of the drum member, and the wire was wound around the drum member while being unwound, and the drum member was gradually moved in a direction parallel to the drum axis so that the wire was wound around the drum member while drawing a spiral at equal intervals of 3 mm. As a result, a wiring body was formed with 96 wires arranged on the surface of the adhesive. Thereafter, the wires were cut, and the wiring body was removed from the drum member. The wiring body was cut to a width of 40×82 mm so that 12 wires could be taken out, and a wiring body film was produced.

[0082] (Preparation of substrate with electrodes) Silver paste was screen-printed on a borosilicate glass substrate (Kawamura Kuzo Shoten Co., Ltd.) to a width of 2 mm and an interelectrode distance of 7.8 mm, and then dried at a temperature of 150°C for 30 minutes to form strip electrodes with a thickness of 17 μm. The strip electrodes were then electrolessly plated to produce a substrate with electrodes. The material, water absorption, and thickness of the substrate are shown in Table 1.

[0083] (Creating wiring sheets) The obtained wiring film was attached to the obtained electrode-attached substrate so that the electrodes were located at both ends of the wires. After that, it was heated at a temperature of 120°C and a pressure of 0.5 MPa for 30 minutes to harden the adhesive and form a resin layer, thereby producing a wiring sheet. The flatness and transmittance of the obtained wiring sheet are shown in Table 1. The storage modulus of the resin layer at 23°C is 2.2 × 10 9 The storage modulus of the resin layer at 105°C is 1.6 × 10 9 Pa. The water absorption rate of the resin layer was 1.7%.

[0084] [Example 2] A wiring sheet was produced in the same manner as in Example 1, except that the borosilicate glass substrate (manufactured by Kawamura Kyuzo Shoten Co., Ltd.) was changed to float glass (manufactured by Nippon Sheet Glass Co., Ltd.).

[0085] [Example 3] A wiring sheet was produced in the same manner as in Example 1, except that the borosilicate glass (manufactured by Kawamura Kyuzo Shoten Co., Ltd.) used as the substrate was changed to polystyrene (manufactured by Kyoei Resin Co., Ltd.).

[0086] [Example 4] A wiring sheet was produced in the same manner as in Example 1, except that the borosilicate glass substrate (manufactured by Kawamura Kyuzo Shoten Co., Ltd.) was changed to polycarbonate (manufactured by Takiron C.I. Co., Ltd.).

[0087] [Comparative Example 1] A wiring sheet was produced in the same manner as in Example 1, except that the borosilicate glass substrate (manufactured by Kawamura Kyuzo Shoten Co., Ltd.) was changed to an acrylic resin (manufactured by Toagosei Co., Ltd., product name "Aronix Sheet").

[0088] [Comparative Example 2] A wiring sheet was produced in the same manner as in Example 1, except that the borosilicate glass substrate (manufactured by Kawamura Kyuzo Shoten Co., Ltd.) was changed to polyvinyl chloride (manufactured by Takiron Co., Ltd.).

[0089] [Comparative Example 3] A wiring sheet was produced in the same manner as in Example 1, except that the substrate, borosilicate glass (manufactured by Kawamura Kyuzo Shoten Co., Ltd.), was changed to ABS (manufactured by Hitachi Chemical Co., Ltd.).

[0090] [Table 1]

[0091] The wiring sheets obtained in Examples 1 to 4 were evaluated for flatness with good results, which confirmed that the present invention can prevent deformation of the wiring sheet. [Explanation of symbols]

[0092] 1...low water absorption base layer, 2...wiring body, 21...conductive linear body, 3...resin layer, 4...electrode, 100...wiring sheet.

Claims

1. The conductive material includes a low water absorption base layer, a wiring body in which a plurality of conductive linear bodies are arranged at intervals, a resin layer that directly or indirectly supports the wiring body, and a pair of electrodes that directly contact the conductive linear bodies. Wiring sheet.

2. The wiring sheet according to claim 1 , The low water absorption rate base layer has a water absorption rate of 0.3% or less when left for 48 hours at a temperature of 85° C. and a humidity of 85% RH. Wiring sheet.

3. The wiring sheet according to claim 1 or 2, The resin layer has a water absorption rate of 0.8% or more when left for 48 hours at a temperature of 85° C. and a humidity of 85% RH. Wiring sheet.

4. The wiring sheet according to claim 1 or 2, The storage modulus of the resin layer at 23° C. is 5.0×10 6 Pa or more, 1.0×10 10 Pa or less, Wiring sheet.

5. The wiring sheet according to claim 1 or 2, The low water absorption base layer has a thickness of 0.5 mm or more. Wiring sheet.

6. The wiring sheet according to claim 1 or 2, The transmittance of near-infrared light having a wavelength of 1000 nm is 70% or more. Wiring sheet.

7. The wiring sheet according to claim 1 or 2, Used as a heater for sensors Wiring sheet.

Citation Information

Patent Citations

  • Flat heater component

    JP2002063984A

  • Near-infrared sensor cover

    JP2019168345A

  • Wiring sheet

    WO2021225142A1

  • Heat-generating film and method for manufacturing heat-generating film

    WO2021157532A1